CN103934280A - 一种冷轧带钢头部加厚轧制的控制方法 - Google Patents

一种冷轧带钢头部加厚轧制的控制方法 Download PDF

Info

Publication number
CN103934280A
CN103934280A CN201410148617.8A CN201410148617A CN103934280A CN 103934280 A CN103934280 A CN 103934280A CN 201410148617 A CN201410148617 A CN 201410148617A CN 103934280 A CN103934280 A CN 103934280A
Authority
CN
China
Prior art keywords
rolling
cold
steel head
strip steel
thickness
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410148617.8A
Other languages
English (en)
Inventor
陈欣
郭迪
王清
程永刚
傅海
刘禹
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ANGANG CONSTRUCTION CONSORTIUM Co Ltd
Original Assignee
ANGANG CONSTRUCTION CONSORTIUM Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ANGANG CONSTRUCTION CONSORTIUM Co Ltd filed Critical ANGANG CONSTRUCTION CONSORTIUM Co Ltd
Priority to CN201410148617.8A priority Critical patent/CN103934280A/zh
Publication of CN103934280A publication Critical patent/CN103934280A/zh
Pending legal-status Critical Current

Abstract

本发明涉及钢铁轧制生产领域,特别涉及一种冷轧带钢头部加厚轧制的控制方法,其特征在于,能自动启动带钢头部加厚轧制,其具体操作步骤如下:1)实时通过工业计算机进行判断,如果当前钢卷设定轧制厚度小于0.3mm,当冷轧带钢头部运行至距离第一架冷轧机4m以内时,自动在带钢轧制厚度设定值的基础上,增加0.25mm的厚度值;2)把通过工业计算机,产生各台轧机的速度输出值,自动进行带钢头部加厚轧制;3)当带钢头部离开最后架次冷轧机距离大于15m时,自动停止带钢头部加厚轧制,轧制厚度恢复为工业计算机数据库下发的设定值厚度。与现有技术相比,本发明有益效果是:避免了操作工人因为人为的失误,保证了生产效率。

Description

一种冷轧带钢头部加厚轧制的控制方法
技术领域
本发明涉及钢铁轧制生产领域,特别涉及一种冷轧带钢头部加厚轧制的控制方法。
背景技术
目前冷连轧生产过程中,在轧制小于0.3mm厚度冷轧板时,需要操作工人手动选择冷轧带钢头部加厚轧制,容易产生人为的判断失误,甚至出现忘记了选择带钢头部加厚,使带钢头部厚度过小、硬度不足,缠绕在卷取机上,无法卸下钢卷,只能切割破坏钢卷,既浪费成品钢卷,又耗费大量生产时间。
发明内容
本发明的目的是提供一种冷轧带钢头部加厚轧制的控制方法,在操作工人没有及时手动选择冷轧带钢头部加厚轧制时,能自动启动冷轧带钢头部加厚轧制程序,避免因为带钢头部厚度小于0.3mm,硬度不足,缠绕在卷取机上,无法卸下钢卷的情况发生。
为实现上述目的,本发明通过以下技术方案实现:
一种冷轧带钢头部加厚轧制的控制方法,能自动启动带钢头部加厚轧制,避免人为操作失误,其具体操作步骤如下:
1)实时通过工业计算机进行判断,如果当前钢卷设定轧制厚度小于0.3mm,当冷轧带钢头部运行至距离第一架冷轧机4m以内时,自动在带钢轧制厚度设定值的基础上,增加0.25mm的厚度值;
2)把这个厚度值通过工业计算机转化成冷轧机的附加速度因子,将附加速度因子输入速度斜坡发生器程序模块,产生各台轧机的速度输出值,控制各台轧机的速度,自动进行带钢头部加厚轧制;
3)当带钢头部离开最后架次冷轧机距离大于15m时,自动停止带钢头部加厚轧制,轧制厚度恢复为工业计算机数据库下发的设定值厚度。
与现有技术相比,本发明有益效果是:
能自动启动冷轧带钢头部的加厚轧制,避免了操作工人因为人为的失误,没有手动选择冷轧带钢头部加厚轧制,导致无法从卷取机上卸下钢卷的情况发生,保证了生产效率,避免了产品和设备的损坏。
附图说明
图1是本发明与现有技术中冷轧机速度变化对比示意图;
图2是五架冷轧机轧制流程示意图。
图中:1-第一架冷轧机2-第二架冷轧机3-第三架冷轧机4-第四架冷轧机5-第五架冷轧机6-测厚仪7-飞剪8-卷取机
×表示冷轧机正常的轧制速度
+表示自动启动冷轧带钢头部加厚轧制时冷轧机的速度
具体实施方式
下面结合附图对本发明具体实施方式作进一步说明:
以五架冷轧机轧制流程为例,见图2,说明本发明一种冷轧带钢头部加厚轧制的控制方法,能实现自动启动带钢头部加厚轧制,避免人为操作失误,其具体操作步骤如下:
1)通过编制的工业计算机程序,在冷连轧计算机数据库中,提取当前生产线上的钢卷数据,判断当前钢卷设定轧制厚度是否小于0.3mm,如果当前钢卷设定轧制厚度小于0.3mm,则继续判断冷轧带钢头部位置;通过轧机入口的寻孔仪器反馈信号给工业计算机,计算带钢头部位置,判断是否距离第一架冷轧机4m,如果距离小于4m,自动启动冷轧带钢头部加厚轧制程序,在当前钢卷设定轧制厚度的基础上,增加0.25mm的厚度;
2)把这个厚度值通过工业计算机转化成冷轧机的附加速度因子,将附加速度因子输入速度斜坡发生器程序模块,产生各台轧机的速度输出值,控制各台轧机的速度,速度变化对比如图1所示;各台冷轧机速度相应增加,只有第五架冷轧机(最后面的冷轧机)速
度不变,由于冷轧机入口速度增加,出口速度不变,说明进料增加,冷轧板宽度不变,轧机出口冷轧板厚度必然增加,保证了冷轧板有足够硬度,可以顺利从卷取机上卸下钢卷;
3)当自动启动冷轧带钢头部加厚轧制程序后,工业计算机实时判断带钢头部离开第五架冷轧机距离大于15m时,自动停止冷轧带钢头部加厚轧制程序,冷轧机自动恢复初始运行速度,轧制厚度自动恢复为工业计算机数据库下发的设定值厚度,开始正常生产轧制。

Claims (1)

1.一种冷轧带钢头部加厚轧制的控制方法,其特征在于,能自动启动带钢头部加厚轧制,避免人为操作失误,其具体操作步骤如下:
1)实时通过工业计算机进行判断,如果当前钢卷设定轧制厚度小于0.3mm,当冷轧带钢头部运行至距离第一架冷轧机4m以内时,自动在带钢轧制厚度设定值的基础上,增加0.25mm的厚度值;
2)把这个厚度值通过工业计算机转化成冷轧机的附加速度因子,将附加速度因子输入速度斜坡发生器程序模块,产生各台轧机的速度输出值,控制各台轧机的速度,自动进行带钢头部加厚轧制;
3)当带钢头部离开最后架次冷轧机距离大于15m时,自动停止带钢头部加厚轧制,轧制厚度恢复为工业计算机数据库下发的设定值厚度。
CN201410148617.8A 2014-04-14 2014-04-14 一种冷轧带钢头部加厚轧制的控制方法 Pending CN103934280A (zh)