CN105542742A - 一种稠油降粘剂及其制备方法 - Google Patents

一种稠油降粘剂及其制备方法 Download PDF

Info

Publication number
CN105542742A
CN105542742A CN201610112018.XA CN201610112018A CN105542742A CN 105542742 A CN105542742 A CN 105542742A CN 201610112018 A CN201610112018 A CN 201610112018A CN 105542742 A CN105542742 A CN 105542742A
Authority
CN
China
Prior art keywords
heavy oil
viscosity reducer
preparation
fatty acid
propylene oxide
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610112018.XA
Other languages
English (en)
Inventor
王凯健
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
YANGZHOU RUNDA OILFIELD CHEMICALS CO Ltd
Original Assignee
YANGZHOU RUNDA OILFIELD CHEMICALS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by YANGZHOU RUNDA OILFIELD CHEMICALS CO Ltd filed Critical YANGZHOU RUNDA OILFIELD CHEMICALS CO Ltd
Priority to CN201610112018.XA priority Critical patent/CN105542742A/zh
Publication of CN105542742A publication Critical patent/CN105542742A/zh
Pending legal-status Critical Current

Abstract

本发明及一种稠油降粘剂及其制备方法。先按投料比称取一定量的各个单体,先将脂肪酸甲酯置于可密封的反应容器中,升温至50±5℃,抽真空后再用N2置换残余空气,搅拌升温至130-140℃,在压力0.2-0.4mpa下,加入催化剂后,滴加环氧乙烷,再滴加环氧丙烷,反应6-8小时后,冷却至室温,加入十二烷基二甲基甜菜碱、甲醇、水混合均匀,及得降粘剂成品。本产品具有用量小、降粘效果好、对稠油使用性能广的特点。

Description

一种稠油降粘剂及其制备方法
技术领域
本发明涉及一种稠油降粘剂及其制备方法。
背景技术
随着石油的不断开采,地球上石油储量尤其是常规原油储量不断减少。在已探明的石油资源中,稠油所占比例越来越大,稠油的开采变得越来越重要。但由于稠油具有特殊的高粘度和高凝点的特性,在开发和应用的各个方面都遇到一些技术难题。而且稠油含有较多的胶质、沥青质,它们造成原油在储层和井筒中的流动性变差,给开采带来许多不便。稠油的特殊性质决定了稠油的开采、输送、必然是围绕稠油的降粘,降凝改性或改质处理进行的。随着高新技术的发展,采油、储运、炼制的技术也不断进步,提出化学降粘技术是目前最具潜力、最有前途的降粘方法之一。
发明内容
为了克服稠油粘度高,采出工艺复杂和开采成本高等问题,本发明提供一种稠油用降粘剂及其制备方法,其制备出的降粘剂按Q/SHCG65-2013标准实验,能有效降低稠油粘度。并将降粘剂加入稠油油井,能明显降低抽油机负荷,提高日产液量。
本发明稠油降粘剂,其产品组成为:
脂肪酸甲酯5-10份、催化剂0.5-1份、环氧乙烷20-30份、环氧丙烷3-6份、十二烷基二甲基甜菜碱10-20份、甲醇10-20份、水50-60份。
所述催化剂为氢氧化钾或氢氧化钠的一种。
其具体的制备方法为:
先按投料比称取一定量的各个单体,将脂肪酸甲酯置于可密封的反应容器中,升温至45-55℃,抽真空后再用N2置换残余空气,搅拌升温至130-140℃,在压力0.2-0.4mpa下,加入催化剂后,滴加环氧乙烷,再滴加环氧丙烷,反应6-8小时后,冷却至50-60℃,加入十二烷基二甲基甜菜碱、甲醇、水,混合均匀,即得降粘剂成品。
本发明所具有的有益效果是:
1、本发明所使用的各原料成本低廉,并且不会给后续中的炼油设备造成腐蚀,节约成本,提高设备的利用率。
2、生产工艺流程简单,操作方法简便,可以实现自动化连续生产,机械化程度高,适宜普及推广和工业化生产。
3、一些小分子有机酸、醇、胺、酰胺可以破坏沥青质聚集体的网状结构,使稠油粘度降低,然而直接将这些化合物加入稠油时,降粘效果并不理想。本发明采用脂肪酸甲酯与环氧乙烷、环氧丙烷的聚合物和十二烷基二甲基甜菜碱这些化合物配合使用,降粘效果十分明显。
4、本发明在江苏油田、华东油田得到广泛使用,均取得良好效果,其中江苏油田瓦庄区块原为电加热开采,使用此降粘剂后,电加热杆全部停用,年节省电费上百万元。
具体实施方式
实施例1
将160g脂肪酸甲酯投入装有搅拌器、冷凝回流、温度计及加热套的2L反应釜中,升温至50℃,密封反应釜,真空泵抽真空后,通入N2吹扫20min后,搅拌升温至135℃,压力0.2mpa下,加入20g氢氧化钠,滴加400g环氧乙烷,再滴加100g环氧丙烷,反应8小时后,冷却至50℃,加入300g十二烷基二甲基甜菜碱、300g甲醇、600g水,混合均匀,即得降粘剂成品。
实施例2
将150Kg脂肪酸甲酯投入装有搅拌器、冷凝回流、温度计及加热套的2m3不锈钢反应釜中,升温至50℃,密封反应釜,真空泵抽真空后,通入N2吹扫20min后,搅拌升温至135℃,压力0.3mpa下,加入20Kg氢氧化钾,滴加500Kg环氧乙烷,再滴加120Kg环氧丙烷,反应7小时后,冷却至60℃,加入400kg十二烷基二甲基甜菜碱、220Kg甲醇、500Kg水,混合均匀,即得降粘剂成品。
经检测,性质如下:
本实验参考中石化Q/SHCG65-2013《稠油降粘剂技术要求》标准进行评价,实验结果如下表所示:

Claims (3)

1.一种稠油降粘剂,其特征在于,包括以下组分(质量份):脂肪酸甲酯5-10份、催化剂0.5-1份、环氧乙烷20-30份、环氧丙烷3-6份、十二烷基二甲基甜菜碱10-20份、甲醇10-20份、水50-60份。
2.根据权利要求1所述的稠油降粘剂,其特征在于,催化剂为氢氧化钾或氢氧化钠的一种。
3.一种稠油降粘剂的制备方法,其特征在于,按以下步骤进行:先按投料比称取一定量的各个单体,将脂肪酸甲酯置于可密封的反应容器中,升温至45-55℃,抽真空后再用N2置换残余空气,搅拌升温至130-140℃,在压力0.2-0.4mpa下,加入催化剂后,滴加环氧乙烷,再滴加环氧丙烷,反应6-8小时后,冷却至50-60℃,加入十二烷基二甲基甜菜碱、甲醇、水,混合均匀,得降粘剂成品。
CN201610112018.XA 2016-02-29 2016-02-29 一种稠油降粘剂及其制备方法 Pending CN105542742A (zh)