CN105365012A - Toughening and strengthening pretreating agent for wicker for wickerwork and preparation method of toughening and strengthening pretreating agent - Google Patents

Toughening and strengthening pretreating agent for wicker for wickerwork and preparation method of toughening and strengthening pretreating agent Download PDF

Info

Publication number
CN105365012A
CN105365012A CN201510738876.0A CN201510738876A CN105365012A CN 105365012 A CN105365012 A CN 105365012A CN 201510738876 A CN201510738876 A CN 201510738876A CN 105365012 A CN105365012 A CN 105365012A
Authority
CN
China
Prior art keywords
wicker
pretreating agent
toughening
strengthening
preparation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510738876.0A
Other languages
Chinese (zh)
Inventor
王静
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Funan Mingyu Wicker-Wood Crafts Co Ltd
Original Assignee
Funan Mingyu Wicker-Wood Crafts Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Funan Mingyu Wicker-Wood Crafts Co Ltd filed Critical Funan Mingyu Wicker-Wood Crafts Co Ltd
Priority to CN201510738876.0A priority Critical patent/CN105365012A/en
Publication of CN105365012A publication Critical patent/CN105365012A/en
Pending legal-status Critical Current

Abstract

The invention relates to the technical field of modification treatment of wicker for wickerwork, in particular to a toughening and strengthening pretreating agent for wicker for wickerwork and a preparation method of the toughening and strengthening pretreating agent. The toughening and strengthening pretreating agent is prepared from, by weight, 10-12 parts of silica sol with the solid content of 20%-25%, 0.4-0.5 part of polyethylene glycol 4000, 5-8 parts of glycerinum, 0.1-0.2 part of secondary alkane sulphonate sodium, 0.2-0.3 part of sodium glycerophosphate, 1-2 parts of hydrophilic silicon oil and 40-50 parts of water. The pretreating agent has good permeability; after glycerinum, sodium glycerophosphate and silica sol in the pretreating agent permeate into fibers, the effects such as softening, toughening and strengthening can be achieved; compatibility of the pretreating agent and vegetable cells is good; modification is efficient and lasting; by means of added hydrophilic silicon oil, the weaving performance of the wicker is improved, and the yellowing resistance and washing resistance of products are improved; and the service life of the products woven through the pretreated wicker is longer, bearing capacity is increased, and the use range is further widened.

Description

A kind of toughen and intensify pretreating agent for wicker plaiting article wicker and preparation method thereof
Technical field
The present invention relates to wicker plaiting article wicker modification treatment technology field, be specifically related to a kind of toughen and intensify pretreating agent for wicker plaiting article wicker and preparation method thereof.
Background technology
Wicker plaiting article is one of folks of china traditional handicraft product, people are just as common daily utility in ancient times, until after 20th century decades just rise gradually, the also project becoming selected areas of China foreign exchange earning gradually, Anhui Province has become one of three large wicker plaiting article production bases, the whole nation.
Wicker is as the material of wicker plaiting article, and it is by novel design, can be woven into that various honesty is natural, handsome in appearance, the practical art product of Portable durable.Along with industry development, product is constantly brought forth new ideas, and the willow having more Nover practical attractive in appearance is presented in face of client.But, because wicker is pure natural plant fiber, not humidity and drying, causes mechanical property to reduce, fracture of easily going mouldy, and bearing capacity is poor, govern further developing of product, if carry out pretreatment to wicker before establishment, improve the adaptability of its environment to external world, improve mechanical property, obtaining wicker plaiting article product quality like this will significantly be improved.
Summary of the invention
The object of the invention is to provide a kind of toughen and intensify pretreating agent for wicker plaiting article wicker and preparation method thereof, and in order to improve the serviceability of wicker, reach the object improving knitting quality, to achieve these goals, the technical solution used in the present invention is as follows:
A kind of toughen and intensify pretreating agent for wicker plaiting article wicker, it is characterized in that, this inorganic agent is made up of the raw material of following weight portion: solid content is Ludox 10-12, the Macrogol 4000 0.4-0.5 of 20-25%, glycerine 5-8, SAS 0.1-0.2, sodium glycero-phosphate 0.2-0.3, hydrophilic silicon oil 1-2, water 40-50.
For a preparation method for the toughen and intensify pretreating agent of wicker plaiting article wicker, it is characterized in that, the preparation method of this inorganic agent is:
(1) first SAS, sodium glycero-phosphate are dropped in water, stir after material is dissolved completely, mixed solution is heated to 40-50 DEG C, then adds Macrogol 4000, be uniformly mixed 30-40min, gained solution for standby;
(2) glycerine is dropwise added in Ludox slowly, and constantly stir, after dropwising, the solution of mixed solution with step (1) gained is mixed completely, then add other residual components, after being uniformly mixed, namely obtain wicker pretreating agent.
Pretreating agent advantage prepared by the present invention is: preparation method is simple for this pretreating agent, composition environment-protecting asepsis evil, it has good permeability, high pressure is utilized to be penetrated in wicker fiber during use, glycerine wherein, sodium glycero-phosphate, Ludox infiltrates through and can reach softening after in fiber, toughness reinforcing, the effects such as enhancing, and it is good with the compatibility of plant cell, modified high-efficient is lasting, the hydrophilic silicon oil added improves the establishment performance of wicker, improve the color inhibition of product, scrub resistance, the life of product be woven into through pretreated like this wicker is longer, bearing capacity increases, widen the scope of application further.
Detailed description of the invention
Embodiment
The pretreating agent of the present embodiment is obtained by the raw material of following weight portion (kilogram): solid content is Ludox 12, Macrogol 4000 0.4, glycerine 6, SAS 0.1, sodium glycero-phosphate 0.3, hydrophilic silicon oil 1.5, the water 45 of 20%.
The preparation method of the present embodiment inorganic agent is:
(1) first SAS, sodium glycero-phosphate are dropped in water, stir after material is dissolved completely, mixed solution is heated to 40-50 DEG C, then adds Macrogol 4000, be uniformly mixed 40min, gained solution for standby;
(2) glycerine is dropwise added in Ludox slowly, and constantly stir, after dropwising, the solution of mixed solution with step (1) gained is mixed completely, then add other residual components, after being uniformly mixed, namely obtain wicker pretreating agent.
The compression strength of passing through the untreated wicker of comparatively same batch of the wicker that this pre-treatment treatment is crossed on average improves 28%, and bending strength on average improves 30%, and the product bearing capacity be woven on average improves 38%.

Claims (2)

1. the toughen and intensify pretreating agent for wicker plaiting article wicker, it is characterized in that, this inorganic agent is made up of the raw material of following weight portion: solid content is Ludox 10-12, the Macrogol 4000 0.4-0.5 of 20-25%, glycerine 5-8, SAS 0.1-0.2, sodium glycero-phosphate 0.2-0.3, hydrophilic silicon oil 1-2, water 40-50.
2. the preparation method of a kind of toughen and intensify pretreating agent for wicker plaiting article wicker as claimed in claim 1, it is characterized in that, described preparation method is:
(1) first SAS, sodium glycero-phosphate are dropped in water, stir after material is dissolved completely, mixed solution is heated to 40-50 DEG C, then adds Macrogol 4000, be uniformly mixed 30-40min, gained solution for standby;
(2) glycerine is dropwise added in Ludox slowly, and constantly stir, after dropwising, the solution of mixed solution with step (1) gained is mixed completely, then add other residual components, after being uniformly mixed, namely obtain wicker pretreating agent.
CN201510738876.0A 2015-11-04 2015-11-04 Toughening and strengthening pretreating agent for wicker for wickerwork and preparation method of toughening and strengthening pretreating agent Pending CN105365012A (en)