CN105017944A - 一种环保油漆的生产方法 - Google Patents

一种环保油漆的生产方法 Download PDF

Info

Publication number
CN105017944A
CN105017944A CN201410167413.9A CN201410167413A CN105017944A CN 105017944 A CN105017944 A CN 105017944A CN 201410167413 A CN201410167413 A CN 201410167413A CN 105017944 A CN105017944 A CN 105017944A
Authority
CN
China
Prior art keywords
mixture
stirring
container
heated
aromatic solvent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410167413.9A
Other languages
English (en)
Inventor
王志龙
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201410167413.9A priority Critical patent/CN105017944A/zh
Publication of CN105017944A publication Critical patent/CN105017944A/zh
Pending legal-status Critical Current

Abstract

一种环保油漆的生产方法,其特征在于首先将10-12%顺丁烯二酸酐、10-15%邻苯二甲酸酐和10-16%1、2-丙二醇放在一个容器内搅拌,加热到40-80℃,直至完全溶解,然后将1-3%乙二醇、0.1-1%对苯二酚36-45%聚酯树脂和20-30%芳烃溶剂油放在另一个容器中进行搅拌,加热到50-100℃,再两种溶液在室温下搅拌均匀,然后加入研磨机中进行研磨。

Description

一种环保油漆的生产方法
技术领域
 本发明涉及一种化工材料的生产方法,尤其是一种环保油漆的生产方法。
背景技术
目前许多有机油漆品种多,用途广泛,现有的有机油漆在生产过程中大多 使用苯溶剂,油漆中苯含量在70%左右,这样会严重污染环境,影响人类健康。 
发明内容
本发明的目的就是为了克服上述现有技术的不足,提供一种组成简单、配 方合理、性能可靠,对环境和人类无污染的环保油漆的生产方法。 
为达到上述目的,本发明通过以下方法实现: 
一种环保油漆的生产方法,其特征在于首先将10-12%顺丁烯二酸酐、10 -15%邻苯二甲酸酐和10-16%1、2-丙二醇放在一个容器内搅拌,加热到40-80 ℃,直至完全溶解,然后将1-3%乙二醇、0.1-1%对苯二酚36-45%聚酯树 脂和20-30%芳烃溶剂油放在另一个容器中进行搅拌,加热到50-100℃,再两 种溶液在室温下搅拌均匀,然后加入研磨机中进行研磨。 
本发明以芳烃溶剂油代替苯溶剂,沸点接近苯溶剂,但其不含苯、甲苯、 二甲苯。制作和使用不会对人类和环境造成污染,具有环保功能。本发明芳烃 溶剂油可用于生产系列有机油漆。 
具体实施方式
实施例1: 
1、由8kg顺丁烯二酸酐、10kg邻苯二甲酸酐和10kg 1、2-丙二醇放在一 个容器内搅拌,加热到50℃。直至完全溶解。 
2、将1kg乙二醇、0.2kg对苯二酚40.8kg聚酯树脂和30kg芳烃溶剂油放 在另一个容器中进行搅拌,加热到80℃。 
3、将工艺流程1、2得到的两种溶液在室温下搅拌均匀,然后加入研磨机 中进行研磨。 
4、最后把工艺流程3得到的混合液体进行包装。 
本环保油漆制作的工艺过程和传统的油漆基本相同,其特点是由芳烃溶剂油 代替苯溶剂,芳烃溶剂油由石脑油蒸馏提炼,其中不含苯、甲苯、二甲苯。制 作的油漆漆膜丰满,附着力强。挥发速度适中,使用不会对人类和环境造成污 染,具有环保功能。 
实施例2: 
1、由10kg顺丁烯二酸酐、11kg邻苯二甲酸酐和15kg 1、2-丙二醇放在 一个容器内搅拌,加热到50℃。直至完全溶解。 
2、将2kg乙二醇、0.5kg对苯二酚36.5kg聚酯树脂和25kg芳烃溶剂油放 在另一个容器中进行搅拌,加热到80℃。 
3、将工艺流程1、2得到的两种溶液在室温下搅拌均匀,然后加入研磨机 中进行研磨。 
4、最后把工艺流程3得到的混合液体进行包装。

Claims (1)

1.一种环保油漆的生产方法,其特征在于首先将10-12%顺丁烯二酸酐、10- 15%邻苯二甲酸酐和10-16%1、2--丙二醇放在一个容器内搅拌,加热到 40-80℃,直至完全溶解,然后将1-3%乙二醇、0.1-1%对苯二酚36- 45%聚酯树脂和20-30%芳烃溶剂油放在另一个容器中进行搅拌,加热到 50-100℃,再两种溶液在室温下搅拌均匀,然后加入研磨机中进行研磨。
CN201410167413.9A 2014-04-24 2014-04-24 一种环保油漆的生产方法 Pending CN105017944A (zh)