CN104974584A - Preparation method of paint diluent - Google Patents

Preparation method of paint diluent Download PDF

Info

Publication number
CN104974584A
CN104974584A CN201510380230.XA CN201510380230A CN104974584A CN 104974584 A CN104974584 A CN 104974584A CN 201510380230 A CN201510380230 A CN 201510380230A CN 104974584 A CN104974584 A CN 104974584A
Authority
CN
China
Prior art keywords
oil
parts
soya
paint
naphthenate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510380230.XA
Other languages
Chinese (zh)
Inventor
唐毓典
韦韬
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Liuzhou Billion Supplies LLC
Original Assignee
Liuzhou Billion Supplies LLC
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Liuzhou Billion Supplies LLC filed Critical Liuzhou Billion Supplies LLC
Priority to CN201510380230.XA priority Critical patent/CN104974584A/en
Publication of CN104974584A publication Critical patent/CN104974584A/en
Pending legal-status Critical Current

Abstract

The invention discloses a preparation method of a paint diluent. The paint diluents is composed of, by weight, 55 to 60 parts of soya-bean oil, 30 to 35 parts of flax seed oil, 3 to 8 parts of China wood oil, 1 to 4 parts of manganese naphthenate, and 0.5 to 2 parts of cobalt naphthenate. The preparation method comprises following steps: soya-bean oil, flax seed oil, and China wood oil are mixed according to a corresponding weight ratio, and are delivered into an oxidizing kettle; an obtained mixture is stirred to be uniform, and is heated to 85 DEG C; air is injected into the mixture via an air pipe; oil oxidation is carried out, and the temperature of an obtained product is increased to 105 to 110 DEG C automatically; at that temperature, air is injected continuously for oxidation until relative density is detected to be 0.929 to 0.930; manganese naphthenate and cobalt naphthenate are added according to a corresponding weight ratio, an obtained mixed material is stirred and is subjected to continuous blowing for 35min so as to obtain the paint diluent finished product. The paint diluent is capable of satisfying dilution requirements, and reducing loss of enterprises and consumers.

Description

A kind of manufacture method of paint thinner
Technical field
The present invention relates to chemical production technical field, be specifically related to a kind of manufacture method of paint thinner.
Background technology
People are when buying paint, generally all thinner can be had as paint is supporting, thinner is a kind of in order to reduce resin viscosity, improves its processing performance and the liquid substance good with resin miscible that add, has reactive thinner and non-activated thinner.In paint, thermosetting resin need add thinner and is convenient to further processing to reduce its viscosity, these thinners are in fact all the organic solvents more cheap than resin, therefore also rise cut down finished cost cause Lian Zuoyong, but in prior art, due to the unreasonable allocation of its thinner, cause the place's thinner produced not reach the dilution effect of requirement, especially for paste paint, bring loss to producer and human consumer.
Summary of the invention
In order to solve the problems of the technologies described above, the invention provides a kind of manufacture method of paint thinner, rationally, obtained paint thinner can reach dilution requirement to the configuration of this manufacture method, reduces the loss of enterprise and human consumer.
Object of the present invention carrys out specific implementation by the following technical programs:
A manufacture method for paint thinner, comprising:
(1) by each component of following parts by weight proportioning:
Soya-bean oil: 55-60 part;
Oleum lini: 30-35 part;
Tung oil: 3-8 part;
Manganese naphthenate: 1-4 part;
Cobalt naphthenate: 0.5-2 part;
(2) by soya-bean oil, oleum lini, tung oil according to adding in stills for air blowing after corresponding parts by weight proportioning, stir, be heated to 85 DEG C, be blown in oil by airduct by air, make oil oxidation and be warming up to 105-110 DEG C voluntarily, keeping at this temperature is blown into atmospheric oxidation, reach till 0.929 ~ 0.930 until mensuration relative density, then corresponding weight is installed and adds cobalt naphthenate, manganese naphthenate, stir evenly, continue blowing 35min i.e. obtained paint thinner finished product.
The manufacture method of a kind of paint thinner of the present invention, comprises by each component of following parts by weight proportioning: soya-bean oil: 55-60 part; Oleum lini: 30-35 part; Tung oil: 3-8 part; Manganese naphthenate: 1-4 part; Cobalt naphthenate: 0.5-2 part; By soya-bean oil, oleum lini, tung oil according to adding in stills for air blowing after corresponding parts by weight proportioning, stir, be heated to 85 DEG C, by airduct, air is blown in oil, make oil oxidation and be warming up to 105-110 DEG C voluntarily, keep at this temperature and be blown into atmospheric oxidation, reach till 0.929 ~ 0.930 until mensuration relative density, then corresponding weight is installed and adds cobalt naphthenate, manganese naphthenate, stir evenly, continue blowing 35min i.e. obtained paint thinner finished product, obtained paint thinner can reach dilution requirement, reduces the loss of enterprise and human consumer.
Embodiment
embodiment 1
The manufacture method of a kind of paint thinner described in the embodiment of the present invention, comprising:
(1) by each component of following parts by weight proportioning:
Soya-bean oil: 58 parts;
Oleum lini: 34 parts;
Tung oil: 5 parts;
Manganese naphthenate: 2 parts;
Cobalt naphthenate: 1 part;
(2) by soya-bean oil, oleum lini, tung oil according to adding in stills for air blowing after corresponding parts by weight proportioning, stir, be heated to 85 DEG C, be blown in oil by airduct by air, make oil oxidation and be warming up to 105-110 DEG C voluntarily, keeping at this temperature is blown into atmospheric oxidation, reach till 0.929 ~ 0.930 until mensuration relative density, then corresponding weight is installed and adds cobalt naphthenate, manganese naphthenate, stir evenly, continue blowing 35min i.e. obtained paint thinner finished product.
embodiment 2
The present embodiment is substantially identical with the embodiment of embodiment 1, and difference is: the parts by weight proportioning of each component is: soya-bean oil: 55 parts; Oleum lini: 30 parts; Tung oil: 3 parts; Manganese naphthenate: 1 part; Cobalt naphthenate: 0.5 part.
embodiment 3
The present embodiment is substantially identical with the embodiment of embodiment 1, and difference is: the parts by weight proportioning of each component is: soya-bean oil: 60 parts; Oleum lini: 35 parts; Tung oil: 8 parts; Manganese naphthenate: 4 parts; Cobalt naphthenate: 2 parts.
The manufacture method of a kind of paint thinner of the present invention, rationally, obtained paint thinner can reach dilution requirement to the configuration of this manufacture method, reduces the loss of enterprise and human consumer.
Last it is noted that the foregoing is only the preferred embodiments of the present invention; be not limited to the present invention; for a person skilled in the art; it still can regulate the technical scheme described in foregoing embodiments; or equivalent replacement is carried out to wherein portion of techniques feature; within the spirit and principles in the present invention all, any amendment done, equivalent replacement, improvement etc., all should be included within protection scope of the present invention.

Claims (1)

1. a manufacture method for paint thinner, is characterized in that, comprising:
(1) by each component of following parts by weight proportioning:
Soya-bean oil: 55-60 part;
Oleum lini: 30-35 part;
Tung oil: 3-8 part;
Manganese naphthenate: 1-4 part;
Cobalt naphthenate: 0.5-2 part;
(2) by soya-bean oil, oleum lini, tung oil according to adding in stills for air blowing after corresponding parts by weight proportioning, stir, be heated to 85 DEG C, be blown in oil by airduct by air, make oil oxidation and be warming up to 105-110 DEG C voluntarily, keeping at this temperature is blown into atmospheric oxidation, reach till 0.929 ~ 0.930 until mensuration relative density, then corresponding weight is installed and adds cobalt naphthenate, manganese naphthenate, stir evenly, continue blowing 35min i.e. obtained paint thinner finished product.
CN201510380230.XA 2015-07-02 2015-07-02 Preparation method of paint diluent Pending CN104974584A (en)