CN111154321A - Novel environment-friendly paint thinner - Google Patents
Novel environment-friendly paint thinner Download PDFInfo
- Publication number
- CN111154321A CN111154321A CN201811327538.8A CN201811327538A CN111154321A CN 111154321 A CN111154321 A CN 111154321A CN 201811327538 A CN201811327538 A CN 201811327538A CN 111154321 A CN111154321 A CN 111154321A
- Authority
- CN
- China
- Prior art keywords
- parts
- oil
- mixture
- air
- calcium carbonate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
The invention discloses a novel environment-friendly paint thinner which comprises the following components in parts by weight: calcium carbonate: 55-65 parts; ammonia water: 30-35 parts; tung oil: 3-10 parts; dichloropropane: 1-4 parts; cobalt naphthenate: 0.5-2 parts; calcium carbonate, ammonia water and tung oil are added into an oxidation kettle according to the corresponding weight part ratio, the mixture is stirred uniformly, the mixture is heated to 85 ℃, air is blown into the oil through an air pipe, the oil is oxidized and is heated to 105-.
Description
Technical Field
The invention relates to the technical field of chemical production, in particular to a novel environment-friendly paint thinner.
Background
When people buy paint coatings, the paint coatings are generally matched with a diluent, the diluent is a liquid substance which is added with good miscibility with resin and is used for reducing the viscosity of the resin and improving the processing performance, and the diluent comprises a reactive diluent and a non-reactive diluent. The thermosetting resin in paint coating needs to be added with thinner to reduce its viscosity for further processing, and these thinner are all organic solvents which are cheaper than resin in practice, so as to reduce the processing cost, however, in the prior art, because the configuration of the thinner is not reasonable, the thinner in the production cannot achieve the required dilution effect, especially for thick paint, and brings loss to manufacturers and consumers.
Disclosure of Invention
In order to solve the technical problems, the invention provides a novel environment-friendly paint diluent, the preparation method is reasonable in configuration, and the prepared paint diluent can meet the dilution requirement and reduce the loss of enterprises and consumers.
The purpose of the invention is realized by the following technical scheme: a novel environmentally friendly paint thinner comprising:
(1) the components are as follows: calcium carbonate: 55-65 parts; ammonia water: 30-35 parts; tung oil: 3-10 parts; dichloropropane: 1-4 parts; cobalt naphthenate: 0.5-2 parts;
(2) calcium carbonate, ammonia water and tung oil are added into an oxidation kettle according to the corresponding weight part ratio, the mixture is stirred uniformly, the mixture is heated to 85 ℃, air is blown into the oil through an air pipe, the oil is oxidized and is heated to 105-plus 110 ℃ automatically, air is continuously blown into the oxidation at the temperature until the relative density is measured to reach 0.929-0.930, then cobalt naphthenate and dichloropropane are added according to the corresponding weight part ratio, the mixture is stirred uniformly, and air is blown continuously for 35min to obtain the finished product of the paint thinner.
The invention relates to a novel environment-friendly paint thinner which comprises the following components in parts by weight: calcium carbonate: 55-65 parts; ammonia water: 30-35 parts; tung oil: 3-10 parts; dichloropropane: 1-4 parts; cobalt naphthenate: 0.5-2 parts; calcium carbonate, ammonia water and tung oil are added into an oxidation kettle according to the corresponding weight part ratio, the mixture is stirred uniformly, the mixture is heated to 85 ℃, air is blown into the oil through an air pipe, the oil is oxidized and is heated to 105-.
Detailed Description
Example 1
The novel environment-friendly paint thinner provided by the embodiment of the invention comprises: the composition comprises the following components in parts by weight: calcium carbonate: 58 parts of a mixture; ammonia water: 34 parts of (a); tung oil: 5 parts of a mixture; dichloropropane: 2 parts of (1); cobalt naphthenate: 1 part; and (2) adding calcium carbonate, ammonia water and tung oil into an oxidation kettle according to the corresponding weight part ratio, uniformly stirring, heating to 85 ℃, blowing air into the oil through an air pipe to oxidize the oil and automatically heating to 105 plus 110 ℃, continuously blowing air into the oil for oxidation at the temperature until the relative density is measured to reach 0.929-0.930, then adding cobalt naphthenate and dichloropropane according to the corresponding weight part ratio, uniformly stirring, and continuously blowing for 35min to obtain the finished paint product.
Example 2
This example is substantially the same as the embodiment of example 1, except that: the weight portion ratio of each component is as follows: calcium carbonate: 55 parts of (1); ammonia water: 30 parts of (1); tung oil: 3 parts of a mixture; dichloropropane: 1 part; cobalt naphthenate: 0.5 part.
Example 3
This example is substantially the same as the embodiment of example 1, except that: the weight portion ratio of each component is as follows: calcium carbonate: 60 parts; ammonia water: 35 parts of (B); tung oil: 8 parts of a mixture; dichloropropane: 4 parts of a mixture; cobalt naphthenate: and 2 parts.
The novel environment-friendly paint thinner disclosed by the invention is reasonable in preparation method, and the prepared paint thinner can meet the dilution requirement and reduce the loss of enterprises and consumers.
Finally, it should be noted that: the above description is only a preferred embodiment of the present invention, and not intended to limit the present invention, and it will be obvious to those skilled in the art that the technical solutions described in the foregoing embodiments may be adjusted, or some technical features may be equivalently replaced, and any modifications, equivalents, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
Claims (1)
1. A novel environment-friendly paint thinner is characterized by comprising:
(1) the components are as follows: calcium carbonate: 55-65 parts; ammonia water: 30-35 parts; tung oil: 3-10 parts; dichloropropane: 1-4 parts; cobalt naphthenate: 0.5-2 parts;
(2) calcium carbonate, ammonia water and tung oil are added into an oxidation kettle according to the corresponding weight part ratio, the mixture is stirred uniformly, the mixture is heated to 85 ℃, air is blown into the oil through an air pipe, the oil is oxidized and is heated to 105-plus 110 ℃ automatically, air is continuously blown into the oxidation at the temperature until the relative density is measured to reach 0.929-0.930, then cobalt naphthenate and dichloropropane are added according to the corresponding weight part ratio, the mixture is stirred uniformly, and air is blown continuously for 35min to obtain the finished product of the paint thinner.