CN111154314A - Energy-saving low-cost paint diluent - Google Patents

Energy-saving low-cost paint diluent Download PDF

Info

Publication number
CN111154314A
CN111154314A CN201811326772.9A CN201811326772A CN111154314A CN 111154314 A CN111154314 A CN 111154314A CN 201811326772 A CN201811326772 A CN 201811326772A CN 111154314 A CN111154314 A CN 111154314A
Authority
CN
China
Prior art keywords
parts
oil
preservative
titanium dioxide
energy
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN201811326772.9A
Other languages
Chinese (zh)
Inventor
周爱克
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Yangzhou Jinmei Textile Co ltd
Original Assignee
Yangzhou Jinmei Textile Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yangzhou Jinmei Textile Co ltd filed Critical Yangzhou Jinmei Textile Co ltd
Priority to CN201811326772.9A priority Critical patent/CN111154314A/en
Publication of CN111154314A publication Critical patent/CN111154314A/en
Withdrawn legal-status Critical Current

Abstract

The invention discloses an energy-saving and low-cost paint thinner which comprises the following components in parts by weight: titanium dioxide: 55-60 parts; linseed oil: 28-35 parts; preservative: 3-8 parts; manganese naphthenate: 1-4 parts; ethylene dichloride: 0.5-3 parts; titanium dioxide, linseed oil and a preservative are added into an oxidation kettle according to corresponding weight part ratios, the mixture is stirred uniformly, the mixture is heated to 85 ℃, air is blown into oil through an air pipe, the oil is oxidized and is heated to 105-.

Description

Energy-saving low-cost paint diluent
Technical Field
The invention relates to the technical field of chemical production, in particular to an energy-saving and low-cost paint thinner.
Background
When people buy paint coatings, the paint coatings are generally matched with a diluent, the diluent is a liquid substance which is added with good miscibility with resin and is used for reducing the viscosity of the resin and improving the processing performance, and the diluent comprises a reactive diluent and a non-reactive diluent. The thermosetting resin in paint coating needs to be added with thinner to reduce its viscosity for further processing, and these thinner are all organic solvents which are cheaper than resin in practice, so as to reduce the processing cost, however, in the prior art, because the configuration of the thinner is not reasonable, the thinner in the production cannot achieve the required dilution effect, especially for thick paint, and brings loss to manufacturers and consumers.
Disclosure of Invention
In order to solve the technical problems, the invention provides the paint thinner with energy saving and low cost, the preparation method has reasonable configuration, and the prepared paint thinner can meet the dilution requirement and reduce the loss of enterprises and consumers.
The purpose of the invention is realized by the following technical scheme: an energy efficient, low cost paint thinner comprising:
(1) the components are as follows: titanium dioxide: 55-60 parts; linseed oil: 28-35 parts; preservative: 3-8 parts; manganese naphthenate: 1-4 parts; ethylene dichloride: 0.5-3 parts;
(2) adding titanium dioxide, linseed oil and a preservative into an oxidation kettle according to corresponding weight part ratios, uniformly stirring, heating to 85 ℃, blowing air into oil through an air pipe to oxidize the oil and automatically heating to 105-plus 110 ℃, continuously blowing air for oxidation at the temperature until the relative density is measured to reach 0.929-0.930, then installing corresponding weight part ratios, adding dichloroethane and manganese naphthenate, uniformly stirring, and continuously blowing for 35min to obtain the finished product of the oil paint thinner.
The invention relates to an energy-saving and low-cost paint thinner, which comprises the following components in parts by weight: titanium dioxide: 55-60 parts; linseed oil: 28-35 parts; preservative: 3-8 parts; manganese naphthenate: 1-4 parts; ethylene dichloride: 0.5-3 parts; titanium dioxide, linseed oil and a preservative are added into an oxidation kettle according to corresponding weight part ratios, the mixture is stirred uniformly, the mixture is heated to 85 ℃, air is blown into oil through an air pipe, the oil is oxidized and is heated to 105-.
Detailed Description
Example 1
The paint thinner with energy saving and low cost provided by the embodiment of the invention comprises the following components: the composition comprises the following components in parts by weight: titanium dioxide: 58 parts of a mixture; linseed oil: 34 parts of (a); preservative: 5 parts of a mixture; manganese naphthenate: 2 parts of (1); ethylene dichloride: 1 part; and (2) adding titanium dioxide, linseed oil and a preservative into an oxidation kettle according to the corresponding weight part ratio, uniformly stirring, heating to 85 ℃, blowing air into oil through an air pipe to oxidize the oil and automatically heating to 105 plus 110 ℃, continuously blowing air for oxidization at the temperature until the relative density is measured to reach 0.929-0.930, then adding dichloroethane and manganese naphthenate according to the corresponding weight part ratio, uniformly stirring, and continuously blowing for 35min to obtain the finished paint product.
Example 2
This example is substantially the same as the embodiment of example 1, except that: the weight portion ratio of each component is as follows: titanium dioxide: 55 parts of (1); linseed oil: 30 parts of (1); preservative: 3 parts of a mixture; manganese naphthenate: 1 part; ethylene dichloride: 0.5 part.
Example 3
This example is substantially the same as the embodiment of example 1, except that: the weight portion ratio of each component is as follows: titanium dioxide: 60 parts; linseed oil: 35 parts of (B); preservative: 8 parts of a mixture; manganese naphthenate: 4 parts of a mixture; ethylene dichloride: and 2 parts.
The paint thinner with energy saving and low cost is reasonable in preparation method, and can meet the dilution requirement and reduce the loss of enterprises and consumers.
Finally, it should be noted that: the above description is only a preferred embodiment of the present invention, and not intended to limit the present invention, and it will be obvious to those skilled in the art that the technical solutions described in the foregoing embodiments may be adjusted, or some technical features may be equivalently replaced, and any modifications, equivalents, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims (1)

1. An energy-saving low-cost paint thinner is characterized by comprising:
(1) the components are as follows: titanium dioxide: 55-60 parts; linseed oil: 28-35 parts; preservative: 3-8 parts; manganese naphthenate: 1-4 parts; ethylene dichloride: 0.5-3 parts;
(2) adding titanium dioxide, linseed oil and a preservative into an oxidation kettle according to corresponding weight part ratios, uniformly stirring, heating to 85 ℃, blowing air into oil through an air pipe to oxidize the oil and automatically heating to 105-plus 110 ℃, continuously blowing air for oxidation at the temperature until the relative density is measured to reach 0.929-0.930, then installing corresponding weight part ratios, adding dichloroethane and manganese naphthenate, uniformly stirring, and continuously blowing for 35min to obtain the finished product of the oil paint thinner.
CN201811326772.9A 2018-11-08 2018-11-08 Energy-saving low-cost paint diluent Withdrawn CN111154314A (en)