CN104552533A - 一种复古木地板的生产方法 - Google Patents
一种复古木地板的生产方法 Download PDFInfo
- Publication number
- CN104552533A CN104552533A CN201310499008.2A CN201310499008A CN104552533A CN 104552533 A CN104552533 A CN 104552533A CN 201310499008 A CN201310499008 A CN 201310499008A CN 104552533 A CN104552533 A CN 104552533A
- Authority
- CN
- China
- Prior art keywords
- pseudo
- classic
- water
- production method
- solid wood
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种复古木地板的生产方法,它通过使用乳酸菌对实木基材进行生物着色,并放大了木纹效果,再使用水性复古漆,用高热灯使其速干,从而产生皴裂效果,最后用UV面漆覆盖。本发明的生产方法,可以使木地板具有明显的古旧风格,可以大大提升复古木地板的品质。而且由于本发明的方法中有放大木纹的效果,因此本发明还可以使速生木材也能加工成效果优良的复古木地板。
Description
技术领域
本发明涉及一种地板,特别是一种复古木地板的生产方法。
背景技术
复古木地板又称仿古地板,它是表面用艺术形式通过特殊加工成具有古典风格的地板。复古风格地板在大空间内使用更容易发挥整体效果,如国外的乡村别墅、农场小院等空间,在我国早期的大户型商品房或乡间别墅选择古典装饰风格时最适合使用复古风格地板。正是应对“大环境需求”,复古木地板的规格也越做越大。
高品质的复古木地板,通常需要在木地板表面加工出明细的木纹,使其具备较明显的古典风格。但是天然木纹受限于板材本身的品质,各种速生木材以现有工艺加工成复古木地板后,木纹十分不明显,因此严重影响到复古木地板的古典效果。
发明内容
本发明的目的在于,提供一种复古木地板的生产方法。它可以使木地板具有更好的古旧效果,且能适用于各种速生木材。
本发明的技术方案:一种复古木地板的生产方法,其特点是,包括以下步骤:
①对实木基材进行养生,为了保证产品质量,对新入库的基材一定要先测试含水率做好记录然后制定养生时间(一般10—25天);
②开片、开槽,根据基材的最大化利用要选择合适的产品规格,把成本降到最低;
③二次养生,;为了保证产品质量的稳定;
④对实木基材进行拉丝抛光处理使实木基材的木纹具有立体效果;
⑤在实木基材的上表面分散开设多个孔径大小随机的浅孔,浅孔用于产生结疤效果,
⑥在实木基板的上表面涂覆酵母菌发酵液,保持室温在25摄氏度,保温2天,这2天里,酵母菌在实木基材表面新陈代谢,代谢过程中对实木基材的表面进行了着色,而且由于实木基材本身存在疏密差异,这个差异使得乳酸菌的着色渗透能力也出现差异,从而乳酸菌的生物着色放大了木纹效果;而上一步开设的浅孔由于沉积较多的酵母菌发酵液,因此着色最为暗沉,效果极其类似木材结痂处;
⑦干燥后作抛光处理,去除酵母菌发酵液的结垢;
⑧涂覆水性复古漆,然后使用高热灯光曝晒,使水性复古漆速干皴裂;
⑨分多层涂覆UV面漆,固化,得成品。
上述的复古木地板的生产方法中,所述水性复古漆,按质量份计,包含水性树脂20份,水性分散剂3份,成膜助剂2份,水性消泡剂0.2份,纯净水30份和水性增调剂0.4份。
前述的复古木地板的生产方法中,所述实木基材为速生木材。
与现有技术相比,本发明通过使用乳酸菌对实木基材进行生物着色,并放大了木纹效果,再使用水性复古漆,用高热灯使其速干,从而产生皴裂效果,最后用UV面漆覆盖。本发明的生产方法,可以使木地板具有明显的古旧风格,可以大大提升复古木地板的品质。而且由于本发明的方法中有放大木纹的效果,因此本发明还可以使速生木材也能加工成效果优良的复古木地板。
具体实施方式
下面结合实施例对本发明作进一步的说明,但并不作为对本发明限制的依据。
实施例。一种复古木地板的生产方法,包括以下步骤:
①对实木基材进行养生,为了保证产品质量,对新入库的基材一定要先测试含水率做好记录然后制定养生时间(一般10—25天);
②开片、开槽,根据基材的最大化利用要选择合适的产品规格,把成本降到最低;
③二次养生,;为了保证产品质量的稳定;
④对实木基材进行拉丝抛光处理使实木基材的木纹具有立体效果;
⑤在实木基材的上表面分散开设多个孔径大小随机的浅孔,浅孔用于产生结疤效果,
⑥在实木基板的上表面涂覆酵母菌发酵液,保持室温在25摄氏度,保温2天,这2天里,酵母菌在实木基材表面新陈代谢,代谢过程中对实木基材的表面进行了着色,而且由于实木基材本身存在疏密差异,这个差异使得乳酸菌的着色渗透能力也出现差异,从而乳酸菌的生物着色放大了木纹效果;而上一步开设的浅孔由于沉积较多的酵母菌发酵液,因此着色最为暗沉,效果极其类似木材结痂处;
⑦干燥后作抛光处理,去除酵母菌发酵液的结垢;
⑧涂覆水性复古漆,然后使用高热灯光曝晒,使水性复古漆速干皴裂;
⑨分多层涂覆UV面漆,固化,得成品。
所述水性复古漆,按质量份计,包含水性树脂20份,水性分散剂3份,成膜助剂2份,水性消泡剂0.2份,纯净水30份和水性增调剂0.4份。所述实木基材为速生木材。
Claims (3)
1.一种复古木地板的生产方法,其特征在于,包括以下步骤:
①对实木基材进行养生;
②开片、开槽;
③二次养生;
④对实木基材进行拉丝抛光处理;
⑤在实木基材的上表面分散开设多个孔径大小随机的浅孔;
⑥在实木基板的上表面涂覆酵母菌发酵液,保持室温在25摄氏度,保温2天;
⑦干燥后作抛光处理;
⑧涂覆水性复古漆,然后使用高热灯光曝晒,使水性复古漆速干皴裂;
⑨分多层涂覆UV面漆,固化,得成品。
2.根据权利要求1所述的复古木地板的生产方法,其特征在于:所述水性复古漆,按质量份计,包含水性树脂20份,水性分散剂3份,成膜助剂2份,水性消泡剂0.2份,纯净水30份和水性增调剂0.4份。
3.根据权利要求1所述的复古木地板的生产方法,其特征在于:所述实木基材为速生木材。