CN104388731B - 一种铝合金精炼剂及其制备方法 - Google Patents

一种铝合金精炼剂及其制备方法 Download PDF

Info

Publication number
CN104388731B
CN104388731B CN201410666533.3A CN201410666533A CN104388731B CN 104388731 B CN104388731 B CN 104388731B CN 201410666533 A CN201410666533 A CN 201410666533A CN 104388731 B CN104388731 B CN 104388731B
Authority
CN
China
Prior art keywords
refining agent
parts
present
preparation
aluminum
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201410666533.3A
Other languages
English (en)
Other versions
CN104388731A (zh
Inventor
王洪初
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Suzhou Zhuhu Bohui Technology Co ltd
Original Assignee
Wuxi Hongsheng Aluminium Industry Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wuxi Hongsheng Aluminium Industry Co Ltd filed Critical Wuxi Hongsheng Aluminium Industry Co Ltd
Priority to CN201410666533.3A priority Critical patent/CN104388731B/zh
Publication of CN104388731A publication Critical patent/CN104388731A/zh
Application granted granted Critical
Publication of CN104388731B publication Critical patent/CN104388731B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明提供一种铝合金精炼剂,所述精炼剂由以下质量份数的各组分组成:NaCl 30‑35份、KCl 28‑32份、Na2SiF6 15‑28份、Na2CO3 3‑8份、NaF 3‑8份、CaS 1‑3份。本发明还提供其制备方法。本发明的精炼剂具有优良的精炼和清渣性能,能有效去除铝液中的夹杂物与气体,起到净化铝液的作用,处理后的铝液中氢含量低于0.12ml/gAl。本发明的精炼剂的制备方法简单,可操作性强。

Description

一种铝合金精炼剂及其制备方法
技术领域
本发明涉及一种铝合金精炼剂。
背景技术
在生产中,铝合金溶液在凝固过程中,铝合金溶液中的氢原子自发的形成氢气分子,氢气分子和以非金属夹杂物在凝固时候形成气泡,而夹杂是铝合金铸件中产生缺陷的主要原因,铝合金溶液中绝大部分的杂质和气体来自于回炉料,故在铝合金熔炼时,铝合金的精炼处理必不可少。通过精炼提高铝合金的冶金质量显得非常重要,目前所用精炼剂普遍存在着精炼效果不佳的问题。
发明内容
为了解决现有技术中存在的问题,本发明提供了一种铝合金精炼剂;为此,本发明还提供其制备方法。
本发明提供一种铝合金精炼剂,所述精炼剂由以下质量份数的各组分组成:NaCl 30-35份、KCl 28-32份、Na2SiF6 15-28份、Na2CO3 3-8份、NaF 3-8份、CaS 1-3份。
优选地,所述精炼剂由以下质量份数的各组分组成:NaCl 32份、KCl 30份、Na2SiF6 22份、Na2CO3 6份、NaF 5份、CaS 2份。
本发明还提供上述铝合金精炼剂的制备方法,是将配方量的各组分混合均匀,充分搅拌,放入坩埚中过热熔化除去结晶水,再保温30~60分钟;最后,冷却后加工,即可得到精炼剂。
本发明的精炼剂具有优良的精炼和清渣性能,能有效去除铝液中的夹杂物与气体,起到净化铝液的作用,处理后的铝液中氢含量低于0.12ml/gAl。本发明的精炼剂的制备方法简单,可操作性强。
具体实施方式
以下的实施例便于更好地理解本发明,但并不限定本发明。下述实施例中的实验方法,如无特殊说明,均为常规方法。
实施例1
本发明的铝合金精炼剂的配方如下:
NaCl 32kg、KCl 30kg、Na2SiF6 22kg、Na2CO3 6kg、NaF 5kg、CaS 2kg。
本发明的铝合金精炼剂的制备方法如下:
将配方量的各组分混合均匀,充分搅拌,放入坩埚中过热熔化除去结晶水,再保温45分钟;最后,冷却后加工,即可得到精炼剂。
实施例2
本发明的铝合金精炼剂的配方如下:
NaCl 35kg、KCl 32kg、Na2SiF6 28kg、Na2CO3 3kg、NaF 3kg、CaS 1kg。
本发明的铝合金精炼剂的制备方法如下:
将配方量的各组分混合均匀,充分搅拌,放入坩埚中过热熔化除去结晶水,再保温30分钟;最后,冷却后加工,即可得到精炼剂。
实施例3
本发明的铝合金精炼剂的配方如下:
NaCl 30kg、KCl 28kg、Na2SiF6 15kg、Na2CO3 8kg、NaF 8kg、CaS 3kg。
本发明的铝合金精炼剂的制备方法如下:
将配方量的各组分混合均匀,充分搅拌,放入坩埚中过热熔化除去结晶水,再保温60分钟;最后,冷却后加工,即可得到精炼剂。
实施例4
本发明的铝合金精炼剂的配方如下:
NaCl 33kg、KCl 29kg、Na2SiF6 18kg、Na2CO3 5kg、NaF 4kg、CaS 1kg。
本发明的铝合金精炼剂的制备方法如下:
将配方量的各组分混合均匀,充分搅拌,放入坩埚中过热熔化除去结晶水,再保温50分钟;最后,冷却后加工,即可得到精炼剂。
使用时,将本发明的精炼剂放入精炼罐中,当铝合金液体温度达到700-740℃时,向所述精炼罐内通入氮气,将本发明的精炼剂送入铝合金液体中。
最后应说明的是:以上所述仅为本发明的优选实施例而已,并不用于限制本发明,尽管参照前述实施例对本发明进行了详细的说明,对于本领域的技术人员来说,其依然可以对前述各实施例所记载的技术方案进行修改,或者对其中部分技术特征进行等同替换。凡在本发明的精神和原则之内,所作的任何修改、等同替换、改进等,均应包含在本发明的保护范围之内。

Claims (3)

1.一种铝合金精炼剂,其特征在于:所述精炼剂由以下质量份数的各组分组成:NaCl 30-35份、KCl 28-32份、Na2SiF6 15-28份、Na2CO3 3-8份、NaF 3-8份、CaS 1-3份;所述铝合金精炼剂的制备方法为:将配方量的各组分混合均匀,充分搅拌,放入坩埚中过热熔化除去结晶水,再保温30~60分钟;最后,冷却后加工,即可得到精炼剂。
2.根据权利要求1所述的铝合金精炼剂,其特征在于:所述精炼剂由以下质量份数的各组分组成:NaCl 32份、KCl 30份、Na2SiF6 22份、Na2CO3 6份、NaF 5份、CaS 2份。
3.权利要求1或2所述的铝合金精炼剂的制备方法,其特征在于:是将配方量的各组分混合均匀,充分搅拌,放入坩埚中过热熔化除去结晶水,再保温30~60分钟;最后,冷却后加工,即可得到精炼剂。
CN201410666533.3A 2014-11-20 2014-11-20 一种铝合金精炼剂及其制备方法 Active CN104388731B (zh)