CN104264441B - 一种超耐用阻燃蚕丝面料的制造方法 - Google Patents

一种超耐用阻燃蚕丝面料的制造方法 Download PDF

Info

Publication number
CN104264441B
CN104264441B CN201410443771.8A CN201410443771A CN104264441B CN 104264441 B CN104264441 B CN 104264441B CN 201410443771 A CN201410443771 A CN 201410443771A CN 104264441 B CN104264441 B CN 104264441B
Authority
CN
China
Prior art keywords
silk fabric
retardant
flame
fabric
fire
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201410443771.8A
Other languages
English (en)
Other versions
CN104264441A (zh
Inventor
周继东
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU SANLIAN HOUSEHOLD TEXTILE CO., LTD.
Original Assignee
Haimen Jinqilin Rosewood Investment And Development Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Haimen Jinqilin Rosewood Investment And Development Co Ltd filed Critical Haimen Jinqilin Rosewood Investment And Development Co Ltd
Priority to CN201410443771.8A priority Critical patent/CN104264441B/zh
Publication of CN104264441A publication Critical patent/CN104264441A/zh
Application granted granted Critical
Publication of CN104264441B publication Critical patent/CN104264441B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种超耐用阻燃蚕丝面料的制造方法,包括以下步骤:(1)将蚕丝面料放置于等离子体表面处理仪中进行接枝处理;(2)将蚕丝面料取出后立即放置于阻燃剂蒸汽中,静置;(3)将蚕丝面料取出洗涤,去除表面残液,用平拉福机烘干得到阻燃蚕丝面料。本发明工艺简便,通过调节等离子体处理的时间与强度和蒸汽的浓度,制备的蚕丝面料不但保留了织物本身轻盈透气,手感舒适的特性,而且阻燃性能高,经久耐用。

Description

一种超耐用阻燃蚕丝面料的制造方法
技术领域:
本发明属于纺织领域,具体涉及一种超耐用阻燃蚕丝面料的制造方法。
背景技术:
随着许多发达国家制定或修订了相应的纺织品阻燃法规及测试方法,对纺织品的阻燃性能提出了更高的要求,研制安全环保的蚕丝类阻燃纺织品,对提高蚕丝产品的附加值及市场竞争力有很大的意义。
蚕丝的极限氧指数为23-24左右,相对棉、粘胶等纤维素纤维属不易燃纤维,但其应用已经逐渐从传统的服用材料扩展到室内及飞机上的装饰材料,因此其阻燃性能需要进一步的提高。
蚕丝为天然纤维,不能通过与阻燃剂共混纺丝的方法进行耐久性阻燃,只能通过对纤维或者织物的后处理来达到阻燃的目的。常用的方法是利用三聚氰胺树脂、有机磷系等阻燃剂,通过浸渍的方法在蚕丝织物表面接枝阻燃成分,在最大限度保留基材原有风格的基础上,获得优良的阻燃效果,但是通常水洗30次左右,面料的阻燃性能将显著下降。
发明内容:
本发明的目的是提供一种超耐用阻燃蚕丝面料的制造方法,本发明方法工艺简便,制备的面料不但保留了蚕丝织物轻盈透气,手感舒适的特性,而且阻燃性能高,经久耐用。
本发明的目的通过如下技术方案实现:
一种超耐用阻燃蚕丝面料的制造方法,包括以下步骤:
(1)将蚕丝面料放置于等离子体表面处理仪中进行接枝处理;
(2)将蚕丝面料取出后立即放置于阻燃剂蒸汽中,静置;
(3)将蚕丝面料取出洗涤,去除表面残液,用平拉福机烘干得到阻燃蚕丝面料。
作为上述技术方案的优选,步骤1所述的等离子处理时间为3-10min,强度为50-300W,气体流量为100-300mL/min。
作为上述技术方案的优选,所述步骤(2)中的阻燃剂为有机磷系阻燃剂,可以是磷酸酯阻燃剂、膦酸酯阻燃剂、有机磷酸盐阻燃剂中的任意一种,溶剂是去离子水或者醇类溶剂。
作为上述技术方案的优选,所述步骤(2)中的阻燃剂蒸汽中阻燃剂含量为30%-70%。
作为上述技术方案的优选,所述步骤(2)中的静置时间为2-3h。
作为上述技术方案的优选,所述步骤(3)中的洗涤为皂洗。
本发明的有益效果在于:利用等离子处理可以快速高效的活化蚕丝织物的表面,用蒸汽喷雾代替传统的溶液浸渍,能使溶液更好地渗透到蚕丝织物的表面,使表面均匀且牢固地接枝阻燃成分。通过调节等离子处理和蒸汽静置的条件,和采用有机磷系阻燃剂,在最大化保护蚕丝织物的原有特性的基础上,使织物的阻燃性能显著提高,并且由于阻燃剂与织物表面接枝牢固,可耐50次以上的水洗,阻燃性能不显著下降。
具体实施方式:
为了加深对本发明的理解,下面结合实施例对本发明作进一步详述,该实施例仅用于解释本发明,并不构成对本发明保护范围的限定。实施例1:
将蚕丝面料放置于等离子体表面处理仪中进行接枝处理,处理时间为3min,强度为300W,气体流量为100mL/min;
将蚕丝面料取出后立即放置于有机磷系阻燃剂蒸汽中,其中阻燃剂为磷酸酯阻燃剂,含量为30%,溶剂为去离子水,静置3h;
将蚕丝面料取出皂洗,去除表面残液,用平拉福机烘干得到阻燃蚕丝面料,其接枝率为10.3,极限氧指数LOI为27.3,断裂强度为361.2N。经过50次水洗后,其接枝率为9.6,极限氧指数LOI为26.5,断裂强度为360.1N。
实施例2:
将蚕丝面料放置于等离子体表面处理仪中进行接枝处理,处理时间为10min,强度为50W,气体流量为300mL/min;
将蚕丝面料取出后立即放置于有机磷系阻燃剂蒸汽中,其中阻燃剂为膦酸酯阻燃剂,含量为70%,溶剂为甲醇,静置2h;
将蚕丝面料取出皂洗,去除表面残液,用平拉福机烘干得到阻燃蚕丝面料,其接枝率为28.7,极限氧指数LOI为31.4,断裂强度为350.5N。经过50次水洗后,其接枝率为26.4,极限氧指数LOI为29.8,断裂强度为349.6N。
实施例3:
将蚕丝面料放置于等离子体表面处理仪中进行接枝处理,处理时间为5min,强度为100W,气体流量为200mL/min;
将蚕丝面料取出后立即放置于有机磷系阻燃剂蒸汽中,其中溶剂为有机磷酸盐阻燃剂,含量为50%,溶剂为去离子水,静置2.5h;
将蚕丝面料取出皂洗,去除表面残液,用平拉福机烘干得到阻燃蚕丝面料,其接枝率为24.7,极限氧指数LOI为28.6,断裂强度为355.7N。经过50次水洗后,其接枝率为23.1,极限氧指数LOI为27.4,断裂强度为354.9N。
实施例4:
将蚕丝面料放置于等离子体表面处理仪中进行接枝处理,处理时间为7min,强度为250W,气体流量为250mL/min;
将蚕丝面料取出后立即放置于有机磷系阻燃剂蒸汽中,其中溶剂为磷酸酯阻燃剂,含量为45%,溶剂为去离子水,静置2h;
将蚕丝面料取出皂洗,去除表面残液,用平拉福机烘干得到阻燃蚕丝面料,其接枝率为25.6,极限氧指数LOI为30.5,断裂强度为359.4。经过50次水洗后,其接枝率为24.6,极限氧指数LOI为29.8,断裂强度为358.7N。

Claims (1)

1.一种超耐用阻燃蚕丝面料的制造方法,其特征在于,该方法包括以下步骤:
(1)将蚕丝面料放置于等离子体表面处理仪中,在50-300W强度和100-300mL/min气体流量下进行接枝处理3-10min;
(2)将蚕丝面料取出后立即放置于含量为30%-70%的有机磷系阻燃剂蒸汽中,静置2-3h;
(3)将蚕丝面料取出皂洗,去除表面残液,用平拉幅机烘干得到阻燃蚕丝面料,
其中有机磷系阻燃剂是磷酸酯阻燃剂、膦酸酯阻燃剂、有机磷酸盐阻燃剂中的任意一种,溶剂是去离子水或者醇类溶剂。
CN201410443771.8A 2014-09-03 2014-09-03 一种超耐用阻燃蚕丝面料的制造方法 Active CN104264441B (zh)