CN104250506A - 一种耐黄变涂料 - Google Patents
一种耐黄变涂料 Download PDFInfo
- Publication number
- CN104250506A CN104250506A CN201410453055.8A CN201410453055A CN104250506A CN 104250506 A CN104250506 A CN 104250506A CN 201410453055 A CN201410453055 A CN 201410453055A CN 104250506 A CN104250506 A CN 104250506A
- Authority
- CN
- China
- Prior art keywords
- parts
- minute
- stirred
- stirring
- deionized water
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
本发明公开了一种耐黄变涂料,它是由下述重量份的原料组成的:硅酸镁铝2-4、聚天冬氨酸0.5-1、对甲苯磺酰肼0.6-1、硬脂酸钙2-3、柠檬酸三丁酯3-4、三甲基羟乙基乙二胺0.5-1、硅藻土10-14、氟化钙2-4、氮化铝1-2、抗氧剂DLTP0.8-2、六甲基环三硅氧烷80-100、丙烯酸己酯130-200、去离子水500-600、甲基丙烯酸丁酯120-170、过硫酸钾2-4、op-103-4、十二烷基二甲基溴化铵1-2、甲基丙烯酸异辛酯20-30、粘结助剂3-6,本发明的涂料流动性、流平性、表面硬度、抗磨抗划伤性强,涂层表面抗污性好,防腐蚀、耐黄变性好,对环境是适应性好。
Description
技术领域
本发明主要涉及涂料领域,尤其涉及一种耐黄变涂料。
背景技术
涂于物体表面能形成具有保护、装饰或特殊性能(如绝缘、防腐、标志等)的固态涂膜的一类液体或固体材料的总称,包括油(性)漆、水性漆、粉末涂料。漆是可流动的液体涂料,包括油(性)漆及水性漆。油漆是以有机溶剂为介质或高固体、无溶剂的油性漆。水性漆是可用水溶解或用水分散的涂料。涂料作为家庭装修的主材之一,在装饰装修中占的比例较大,购买涂料的合格与否直接影响到整体装修效果和居室的环境,有时甚至会对人体的健康产生极大的危害。目前随着各种各样涂料的产生,对涂料的品质要求也不断提高,而不断提高涂料质量对于建筑、生活都可以起到很大的帮助作用。
发明内容
本发明目的就是提供一种耐黄变涂料。
本发明是通过以下技术方案实现的:
一种耐黄变涂料,其特征在于它是由下述重量份的原料组成的:
硅酸镁铝2-4、聚天冬氨酸0.5-1、对甲苯磺酰肼0.6-1、硬脂酸钙2-3、柠檬酸三丁酯3-4、三甲基羟乙基乙二胺0.5-1、硅藻土10-14、氟化钙2-4、氮化铝1-2、抗氧剂DLTP 0.8-2、六甲基环三硅氧烷80-100、丙烯酸己酯130-200、去离子水500-600、甲基丙烯酸丁酯120-170、过硫酸钾2-4、op-10 3-4、十二烷基二甲基溴化铵1-2、甲基丙烯酸异辛酯20-30、粘结助剂3-6;
所述的粘结助剂是由下述重量份的各原料组成的:
硅丙乳液30-36、生石膏微粉2-3、聚乙烯醇3-4、过硫酸钾1-2、氨基树脂0.7-1、纳米麦饭石粉3-4、聚乙二醇二甲基丙烯酸酯2-3、去离子水16-20;
将生石膏微粉、聚乙烯醇混合,在70-80℃下保温搅拌5-10分钟,加入过硫酸钾,搅拌至常温,加入硅丙乳液重量的50-60%,60-100转/分搅拌分散2-4分钟;
将氨基树脂加入到去离子水中,搅拌均匀后加入聚乙二醇二甲基丙烯酸酯,100-200转/分搅拌分散6-10分钟;
将上述处理后的各原料与剩余各原料混合,300-400转/分搅拌分散10-15分钟,即得所述粘结助剂。
一种耐黄变涂料的制备方法,其特征在于包括以下步骤:
(1)取上述甲基丙烯酸丁酯重量的50-60%、丙烯酸己酯重量的50-60%混合,搅拌均匀,得单体a;
(2)将剩余的甲基丙烯酸丁酯、丙烯酸己酯与六甲基环三硅氧烷混合,在60-70℃下保温搅拌6-10分钟,加入甲基丙烯酸异辛酯、硬脂酸钙、柠檬酸三丁酯,搅拌至常温,得单体b;
(3)取过硫酸钾,加入上述去离子水重量的10-20%,搅拌均匀,得引发剂溶液;
(4)取op-10与剩余去离子水重量的10-20%混合,搅拌均匀后加入对甲苯磺酰肼,在50-60℃下保温搅拌3-10分钟,加入引发剂溶液,升高至温度为65-70℃,保温搅拌20-30分钟,滴加上述单体a,在2-4 小时内滴完,滴加完毕后在上述温度下保温20-30分钟,得种子乳液;
(5)在上述种子乳液中滴加单体b,滴加时间为100-120分钟,滴加完毕后,在70-80℃下保温1-2小时,冷却,用200-250目筛网过滤出料;
(6)将上述步骤(5)得到的物料与剩余各原料混合,800-1200转/分搅拌分散20-30分钟,即得所述耐黄变涂料。
本发明的优点是:
本发明的涂料流动性、流平性、表面硬度、抗磨抗划伤性强,涂层表面抗污性好,防腐蚀、耐黄变性好,对环境是适应性好。本发明的粘结助剂中加入的生石膏微粉和聚乙烯醇,可以有效的改善涂层表面的质感,与过硫酸钾、硅丙乳液混合,具有很好的粘结性,增强涂膜的抗剥离强度和稳定性。
具体实施方式
实施例1
一种耐黄变涂料,其特征在于它是由下述重量份的原料组成的:
硅酸镁铝2、聚天冬氨酸0.5、对甲苯磺酰肼0.6、硬脂酸钙3、柠檬酸三丁酯3、三甲基羟乙基乙二胺0.5、硅藻土14、氟化钙4、氮化铝2、抗氧剂DLTP 0.8、六甲基环三硅氧烷100、丙烯酸己酯200、去离子水600、甲基丙烯酸丁酯170、过硫酸钾2、op-10 4、十二烷基二甲基溴化铵2、甲基丙烯酸异辛酯30、粘结助剂6;
所述的粘结助剂是由下述重量份的各原料组成的:
硅丙乳液36、生石膏微粉3、聚乙烯醇4、过硫酸钾1、氨基树脂0.7、纳米麦饭石粉3、聚乙二醇二甲基丙烯酸酯3、去离子水20;
将生石膏微粉、聚乙烯醇混合,在80℃下保温搅拌10分钟,加入过硫酸钾,搅拌至常温,加入硅丙乳液重量的60%,100转/分搅拌分散4分钟;
将氨基树脂加入到去离子水中,搅拌均匀后加入聚乙二醇二甲基丙烯酸酯,200转/分搅拌分散6-10分钟;
将上述处理后的各原料与剩余各原料混合,300转/分搅拌分散15分钟,即得所述粘结助剂。
一种耐黄变涂料的制备方法,其特征在于包括以下步骤:
(1)取上述甲基丙烯酸丁酯重量的60%、丙烯酸己酯重量的60%混合,搅拌均匀,得单体a;
(2)将剩余的甲基丙烯酸丁酯、丙烯酸己酯与六甲基环三硅氧烷混合,在60℃下保温搅拌10分钟,加入甲基丙烯酸异辛酯、硬脂酸钙、柠檬酸三丁酯,搅拌至常温,得单体b;
(3)取过硫酸钾,加入上述去离子水重量的20%,搅拌均匀,得引发剂溶液;
(4)取op-10与剩余去离子水重量的20%混合,搅拌均匀后加入对甲苯磺酰肼,在60℃下保温搅拌10分钟,加入引发剂溶液,升高至温度为70℃,保温搅拌30分钟,滴加上述单体a,在4 小时内滴完,滴加完毕后在上述温度下保温30分钟,得种子乳液;
(5)在上述种子乳液中滴加单体b,滴加时间为120分钟,滴加完毕后,在80℃下保温2小时,冷却,用250目筛网过滤出料;
(6)将上述步骤(5)得到的物料与剩余各原料混合,1200转/分搅拌分散30分钟,即得所述耐黄变涂料。
性能测试:
延伸率:≥300% ;
不透水性:0.3MPa( 一个小时不透水)。
Claims (2)
1.一种耐黄变涂料,其特征在于它是由下述重量份的原料组成的:
硅酸镁铝2-4、聚天冬氨酸0.5-1、对甲苯磺酰肼0.6-1、硬脂酸钙2-3、柠檬酸三丁酯3-4、三甲基羟乙基乙二胺0.5-1、硅藻土10-14、氟化钙2-4、氮化铝1-2、抗氧剂DLTP 0.8-2、六甲基环三硅氧烷80-100、丙烯酸己酯130-200、去离子水500-600、甲基丙烯酸丁酯120-170、过硫酸钾2-4、op-10 3-4、十二烷基二甲基溴化铵1-2、甲基丙烯酸异辛酯20-30、粘结助剂3-6;
所述的粘结助剂是由下述重量份的各原料组成的:
硅丙乳液30-36、生石膏微粉2-3、聚乙烯醇3-4、过硫酸钾1-2、氨基树脂0.7-1、纳米麦饭石粉3-4、聚乙二醇二甲基丙烯酸酯2-3、去离子水16-20;
将生石膏微粉、聚乙烯醇混合,在70-80℃下保温搅拌5-10分钟,加入过硫酸钾,搅拌至常温,加入硅丙乳液重量的50-60%,60-100转/分搅拌分散2-4分钟;
将氨基树脂加入到去离子水中,搅拌均匀后加入聚乙二醇二甲基丙烯酸酯,100-200转/分搅拌分散6-10分钟;
将上述处理后的各原料与剩余各原料混合,300-400转/分搅拌分散10-15分钟,即得所述粘结助剂。
2.一种如权利要求1所述的耐黄变涂料的制备方法,其特征在于包括以下步骤:
(1)取上述甲基丙烯酸丁酯重量的50-60%、丙烯酸己酯重量的50-60%混合,搅拌均匀,得单体a;
(2)将剩余的甲基丙烯酸丁酯、丙烯酸己酯与六甲基环三硅氧烷混合,在60-70℃下保温搅拌6-10分钟,加入甲基丙烯酸异辛酯、硬脂酸钙、柠檬酸三丁酯,搅拌至常温,得单体b;
(3)取过硫酸钾,加入上述去离子水重量的10-20%,搅拌均匀,得引发剂溶液;
(4)取op-10与剩余去离子水重量的10-20%混合,搅拌均匀后加入对甲苯磺酰肼,在50-60℃下保温搅拌3-10分钟,加入引发剂溶液,升高至温度为65-70℃,保温搅拌20-30分钟,滴加上述单体a,在2-4 小时内滴完,滴加完毕后在上述温度下保温20-30分钟,得种子乳液;
(5)在上述种子乳液中滴加单体b,滴加时间为100-120分钟,滴加完毕后,在70-80℃下保温1-2小时,冷却,用200-250目筛网过滤出料;
(6)将上述步骤(5)得到的物料与剩余各原料混合,800-1200转/分搅拌分散20-30分钟,即得所述耐黄变涂料。