CN104059383B - 黑色染料的制备方法 - Google Patents

黑色染料的制备方法 Download PDF

Info

Publication number
CN104059383B
CN104059383B CN201410297618.9A CN201410297618A CN104059383B CN 104059383 B CN104059383 B CN 104059383B CN 201410297618 A CN201410297618 A CN 201410297618A CN 104059383 B CN104059383 B CN 104059383B
Authority
CN
China
Prior art keywords
lower floor
sediment
black dyes
hide
minutes
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201410297618.9A
Other languages
English (en)
Other versions
CN104059383A (zh
Inventor
何叶
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangzhou Yihong Chemical Co., Ltd.
Original Assignee
Rongshui Guangxi Snow Weasel Science And Technology Development Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Rongshui Guangxi Snow Weasel Science And Technology Development Co Ltd filed Critical Rongshui Guangxi Snow Weasel Science And Technology Development Co Ltd
Priority to CN201410297618.9A priority Critical patent/CN104059383B/zh
Publication of CN104059383A publication Critical patent/CN104059383A/zh
Application granted granted Critical
Publication of CN104059383B publication Critical patent/CN104059383B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种黑色染料的制备方法,属于印染领域。本发明先将牛皮放入锅内,加水熬成牛皮膏;然后将炭打碎,放入豆浆机内,加入水,粉碎,倒出、静置,倒去上层溶液,保留下层沉降物,继续重复几次,直至得到的下层沉降物的粒度达到50纳米~100纳米;将得到的下层沉降物与之前的牛皮膏混合均匀,制成所需形态的黑色染料。本发明制得的黑色染料所染织物、服饰色泽柔和自然,色牢度较高,不易退色、变色,对人体无害,是一种环保、天然的染料。

Description

黑色染料的制备方法
技术领域
本发明属于印染领域,尤其涉及一种黑色染料的制备方法。
背景技术
目前,常用的染料是合成染料,其所染织物、服饰等不仅容易造成褪色,而且由于其原料、中间体大多属致癌性物质,不仅污染环境,还直接使穿着者、接触者或生产者受害。
随着生活水平的不断提高,人们越来越关注自身的健康,追求绿色产品和绿色消费已成为趋势。因此,一种环保、天然、无害的染料将替代过去常用的合成染料。
发明内容
本发明解决的技术问题是提供一种黑色染料,该方法制得的黑色染料所染织物、服饰色泽柔和自然,色牢度较高,不易退色、变色,对人体无害,是一种环保、天然的染料。
为了解决上述技术问题,本发明所采用的技术方案是:
一种黑色染料的制备方法,该方法包括以下步骤:
A、将牛皮放入锅内,加水熬成膏状物,得到牛皮膏,备用;
B、先将炭打碎,然后放入豆浆机内,加入1~3倍水,粉碎30分钟~40分钟,倒出、静置1小时~3小时,倒去上层溶液,保留下层沉降物;
C、将B步骤下层沉降物再放入豆浆机内,加入1~3倍水,粉碎30分钟~40分钟,倒出、静置1小时~3小时,倒去上层溶液,保留下层沉降物;
D、继续重复C步骤,直至得到的下层沉降物的粒度达到50纳米~100纳米;
E、按质量比D步骤得到的下层沉降物:A步骤得到的牛皮膏=1:0.01~0.1的比例将所述下层沉降物与所述牛皮膏混合均匀,制成所需形态的黑色染料。
由于采用上述技术方案,本发明得到的有益效果是:
1、本发明整个制备过程中无有害物质添加,也没有有害废物产生,其制得的黑色染料对人体无害,所染织物、服饰呈黑色,颜色均匀,色泽柔和自然,色牢度较高,不易退色、变色。
2、本发明采用的原料炭天然,其制成的黑色染料具有吸附作用,用于染制织物、服饰等,可使所染织物、服饰等具有消毒除臭的作用。
具体实施方式
以下结合具体实施例对本发明作进一步详述,而本发明的保护范围并非仅仅局限于以下实施例。
实施例1
本黑色染料的制备方法包括以下步骤:
A、将牛皮放入锅内,加水熬成膏状物,得到牛皮膏,备用;
B、先将炭打碎,然后放入豆浆机内,加入1倍水,粉碎30分钟,倒出、静置3小时,倒去上层溶液,保留下层沉降物;
C、将B步骤下层沉降物再放入豆浆机内,加入1倍水,粉碎30分钟,倒出、静置3小时,倒去上层溶液,保留下层沉降物;
D、继续重复C步骤,直至得到的下层沉降物的粒度达到100纳米;
E、将1kgD步骤得到的所述下层沉降物与0.01kgA所述牛皮膏混合均匀,然后压制成块状的黑色染料。
将本实施例制得的黑色染料用于染制衣服,然后将所染衣服进行清洗、浸泡,发现其清洗、浸泡后的废水依然澄清、无色,清洗、浸泡后的衣服颜色无变化。由此可得,本实施例制得的黑色染料所染织物、服饰色牢度好。
实施例2
本黑色染料的制备方法包括以下步骤:
A、将牛皮放入锅内,加水熬成膏状物,得到牛皮膏,备用;
B、先将炭打碎,然后放入豆浆机内,加入3倍水,粉碎40分钟,倒出、静置1小时,倒去上层溶液,保留下层沉降物;
C、将B步骤下层沉降物再放入豆浆机内,加入3倍水,粉碎40分钟,倒出、静置1小时,倒去上层溶液,保留下层沉降物;
D、继续重复C步骤,直至得到的下层沉降物的粒度达到50纳米;
E、将1kgD步骤得到的下层沉降物与0.1kgA步骤得到的牛皮膏混合均匀,然后压制成块状的黑色染料。
将本实施例制得的黑色染料用于染制衣服,然后将所染衣服进行清洗、浸泡,发现其清洗、浸泡后的废水依然澄清、无色,清洗、浸泡后的衣服颜色无变化。由此可得,本实施例制得的黑色染料所染织物、服饰色牢度好。
实施例3
本黑色染料的制备方法包括以下步骤:
A、将牛皮放入锅内,加水熬成膏状物,得到牛皮膏,备用;
B、先将炭打碎,然后放入豆浆机内,加入2倍水,粉碎36分钟,倒出、静置1.5小时,倒去上层溶液,保留下层沉降物;
C、将B步骤下层沉降物再放入豆浆机内,加入2倍水,粉碎36分钟,倒出、静置1.5小时,倒去上层溶液,保留下层沉降物;
D、继续重复C步骤,直至得到的下层沉降物的粒度达到70纳米;
E、将1kgD步骤得到的下层沉降物与0.05kgA步骤得到的牛皮膏混合均匀,加水搅拌,制得液状的黑色染料。
将本实施例制得的黑色染料用于染制衣服,然后将所染衣服进行清洗、浸泡,发现其清洗、浸泡后的废水依然澄清、无色,清洗、浸泡后的衣服颜色无变化。由此可得,本实施例制得的黑色染料所染织物、服饰色牢度好。

Claims (1)

1.一种黑色染料的制备方法,其特征在于包括以下步骤:
A、将牛皮放入锅内,加水熬成膏状物,得到牛皮膏,备用;
B、先将炭打碎,然后放入豆浆机内,加入1~3倍水,粉碎30分钟~40分钟,倒出、静置1小时~3小时,倒去上层溶液,保留下层沉降物;
C、将B步骤下层沉降物再放入豆浆机内,加入1~3倍水,粉碎30分钟~40分钟,倒出、静置1小时~3小时,倒去上层溶液,保留下层沉降物;
D、继续重复C步骤,直至得到的下层沉降物的粒度达到50纳米~100纳米;
E、按质量比D步骤得到的下层沉降物:A步骤得到的牛皮膏=1:0.01~0.1的比例将所述下层沉降物与所述牛皮膏混合均匀,制成所需形态的黑色染料。
CN201410297618.9A 2014-06-29 2014-06-29 黑色染料的制备方法 Expired - Fee Related CN104059383B (zh)