CN104044280A - 一种塑料板件合模缝隙处理方法 - Google Patents

一种塑料板件合模缝隙处理方法 Download PDF

Info

Publication number
CN104044280A
CN104044280A CN201410281704.0A CN201410281704A CN104044280A CN 104044280 A CN104044280 A CN 104044280A CN 201410281704 A CN201410281704 A CN 201410281704A CN 104044280 A CN104044280 A CN 104044280A
Authority
CN
China
Prior art keywords
gap
plastics plate
processing method
matched moulds
agent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410281704.0A
Other languages
English (en)
Inventor
过俊宏
肖运根
章隆泉
顾肖红
陈伟新
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wuxi Chongan District Technology Innovation Service Center
Original Assignee
Wuxi Chongan District Technology Innovation Service Center
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wuxi Chongan District Technology Innovation Service Center filed Critical Wuxi Chongan District Technology Innovation Service Center
Priority to CN201410281704.0A priority Critical patent/CN104044280A/zh
Publication of CN104044280A publication Critical patent/CN104044280A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种塑料板件合模缝隙处理方法,属于加工方法领域。塑料板件合模缝隙处理方法步骤包括打磨,加贴遮盖带,填补料,打磨补土等。本发明提供的塑料板件合模缝隙处理方法,可沿缝隙宽度进行填补,补料不会覆盖塑料板件的板件面,人工操作简单,填补缝隙效果好。

Description

一种塑料板件合模缝隙处理方法
技术领域
本发明涉及一种塑料板件合模缝隙处理方法,属于加工方法领域。
背景技术
塑料板件之间组合会产生大量缝隙,缝隙的修补一般通过人工进行修补,这是由于塑料板件之间的缝隙较小,且塑料板件的平面试不规则的几何面,不可能采用机械进行修补。人工修补常见问题是修补范围无法控制,经常会覆盖板件,造车个清理不便。
发明内容
本发明针对上述不足提供了一种塑料板件合模缝隙处理方法。
本发明采用如下技术方案:
本发明提供的一种塑料板件合模缝隙处理方法,步骤如下:
1)、将塑料板件进行假组,确定缝隙大小,有无锯齿刺;
2)、对塑料板件的结合处进行打磨,去除边缘锯齿刺;
3)、组合固定打磨完成后的塑料板件;
4)、在组合后的塑料板件之间的缝隙边缘两侧分别加贴遮盖带;
5)、对缝隙内填充补土剂;
6)、等补土剂硬化后,去除遮盖带;
7)、打磨缝隙内的补土剂。
本发明所述的塑料板件合模缝隙处理方法,所述的步骤2)中针对塑料板件缝隙内壁锯齿刺进行打磨处理。
本发明所述的塑料板件合模缝隙处理方法,所述的步骤4)中的遮盖带为透明胶带。
本发明所述的塑料板件合模缝隙处理方法,所述的步骤5)中的补土剂为缓干型补土剂。
本发明所述的塑料板件合模缝隙处理方法,所述的步骤6)中采用吹风机对补土剂进行硬化处理。
有益效果
本发明提供的塑料板件合模缝隙处理方法,可沿缝隙宽度进行填补,补料不会覆盖塑料板件的板件面,人工操作简单,填补缝隙效果好。
 
具体实施方式
下面对本发明进一步详细说明:
一种塑料板件合模缝隙处理方法,步骤如下:
1)、将塑料板件进行假组,确定缝隙大小,有无锯齿刺;
2)、对塑料板件的结合处进行打磨,去除边缘锯齿刺;
3)、组合固定打磨完成后的塑料板件;
4)、在组合后的塑料板件之间的缝隙边缘两侧分别加贴遮盖带;
5)、对缝隙内填充补土剂;
6)、等补土剂硬化后,去除遮盖带;
7)、打磨缝隙内的补土剂。
步骤2)中针对塑料板件缝隙内壁锯齿刺进行打磨处理;遮盖带为透明胶带。补土剂为缓干型补土剂。采用吹风机对补土剂进行硬化处理。

Claims (5)

1.一种塑料板件合模缝隙处理方法,其特征在于:步骤如下:
1)、将塑料板件进行假组,确定缝隙大小,有无锯齿刺;
2)、对塑料板件的结合处进行打磨,去除边缘锯齿刺;
3)、组合固定打磨完成后的塑料板件;
4)、在组合后的塑料板件之间的缝隙边缘两侧分别加贴遮盖带;
5)、对缝隙内填充补土剂;
6)、等补土剂硬化后,去除遮盖带;
7)、打磨缝隙内的补土剂。
2.根据权利要求1所述的塑料板件合模缝隙处理方法,其特征在于:所述的步骤2)中针对塑料板件缝隙内壁锯齿刺进行打磨处理。
3.根据权利要求1所述的塑料板件合模缝隙处理方法,其特征在于:所述的步骤4)中的遮盖带为透明胶带。
4.根据权利要求1所述的塑料板件合模缝隙处理方法,其特征在于:所述的步骤5)中的补土剂为缓干型补土剂。
5.根据权利要求1所述的塑料板件合模缝隙处理方法,其特征在于:所述的步骤6)中采用吹风机对补土剂进行硬化处理。
CN201410281704.0A 2014-06-23 2014-06-23 一种塑料板件合模缝隙处理方法 Pending CN104044280A (zh)