CN103924395A - Double-faced woollen spun fingering yarn machine embroidering method and application thereof - Google Patents

Double-faced woollen spun fingering yarn machine embroidering method and application thereof Download PDF

Info

Publication number
CN103924395A
CN103924395A CN201410150688.1A CN201410150688A CN103924395A CN 103924395 A CN103924395 A CN 103924395A CN 201410150688 A CN201410150688 A CN 201410150688A CN 103924395 A CN103924395 A CN 103924395A
Authority
CN
China
Prior art keywords
machine
embroidery
fingering
yarn
spun
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410150688.1A
Other languages
Chinese (zh)
Other versions
CN103924395B (en
Inventor
龚雪鸥
苗晓光
刘有才
徐冀燕
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
BEIJING SNOWLOTUS CASHMERE CO LTD
Tsinghua University
Original Assignee
BEIJING SNOWLOTUS CASHMERE CO LTD
Tsinghua University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by BEIJING SNOWLOTUS CASHMERE CO LTD, Tsinghua University filed Critical BEIJING SNOWLOTUS CASHMERE CO LTD
Priority to CN201410150688.1A priority Critical patent/CN103924395B/en
Publication of CN103924395A publication Critical patent/CN103924395A/en
Application granted granted Critical
Publication of CN103924395B publication Critical patent/CN103924395B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention provides a double-faced woollen spun fingering yarn machine embroidering method. The method comprises the steps of providing a textile fabric and woollen spun fingering yarns; embroidering a preset patterned layout on the textile fabric with the woollen spun fingering yarns as embroidery threads by virtue of an embroidery machine to obtain a machine-embroidered crude product; washing the machine-embroidered crude product to dissolve the woollen spun fingering yarns of the patterned layout partially; and drying the washed machine-embroidered crude product to obtain a machine-embroidered finished product, wherein the woollen spun fingering yarn is blended wool formed by cashmere and water soluble fibers with the weight ratio of 45:55. The new application of the woollen spun fingering yarn in the textile industry is developed firstly by the method, and the prepared machine-embroidered finished product has fluffy, hazy and hairy appearance effects.

Description

The methods and applications of the two-sided machine embroidery of woollen spun fingering yarn
Technical field
The present invention relates to field of textiles.Particularly, the present invention relates to the methods and applications of the two-sided machine embroidery of woollen spun fingering yarn.
Background technology
The history that machine embroidery is come out existing over one hundred year.1828, Frenchman J. Hellman was invented the Sewing machines that is exclusively used in embroidery.In next year, he is sold to Switzerland, Britain by this patent, and machine embroidery is popular in Europe thus.1829, english embroidery artist H. Houldsworth was created use multi-color cord machine embroidery ramage.Since the sixties in 20th century, the machine embroidery development of the U.S., Germany, Japan, France is very fast, product is fabric mainly with chemical fibre, the sophisticated equipments such as multiple-head type electronic embroidery machine that adopt computer program to control, full-automatic continuous embroidered pattern on whole cloth, machine embroidery method of stitchings is changeable, novel design, rich color.The machine embroidery thirties of 20th century is spread to China, and has had larger development 50~sixties, and successfully transplanted the works such as figure painting, scenery with hills and waters the sixties, and manufacture experimently into machine embroidery double-faced embroidery embroidery.
Embroidery product adopts fibers material as embroidering the embroidered pattern of line conventionally, but the embroidered pattern needle tracking of fibers material is more clear, can not reach effect fluffy, dim, lint.If using knitting yarn as embroidering line by than being easier to reach effect fluffy, dim, lint, but the brute force of current knitting yarn is low, number is lower, line slightly makes it cannot carry out machine embroidery as embroidering line at all.Even spun yarn slubbing yarn relative to spining semi-worsted yarn yarn is thinner in hosiery yarns, number is higher, have any surface finish, high resilience, the powerful feature such as good, but it is still larger to use it for machine embroidery difficulty.Therefore urgently develop a kind of knitting yarn that is suitable for machine embroidery and can reaches the effect of fluffy, dim, lint.
Summary of the invention
The present invention is intended to solve at least to a certain extent one of technical problem in correlation technique.For this reason, one object of the present invention is to propose the method for the two-sided machine embroidery of a kind of woollen spun fingering yarn, utilizes the method can embroideredly obtain having the embroidery product of hairy unique look.
According to an aspect of the present invention, the present invention proposes the method for the two-sided machine embroidery of a kind of woollen spun fingering yarn, comprising:
Textiles and woollen spun fingering yarn are provided;
Utilize embroidery machine using woollen spun fingering yarn as embroider line on described textiles embroidered preset play an edition layout, to obtain machine embroidery crude product;
Described machine embroidery crude product is washed to processing, the woollen spun fingering yarn of playing version layout described in forming is partly dissolved;
The described machine embroidery crude product through washing is dried to processing, to obtain machine embroidery finished product;
Wherein, described woollen spun fingering yarn is the blended knitting wool of cashmere and water-soluble fibre, and the mass ratio of described cashmere and water-soluble fibre is 45:55.
Utilize thus said method first woollen spun fingering yarn to be applied to machine embroidery, and the machine embroidery finished product preparing have fluffy, the dim and brushy effect of outward appearance.
In addition, the method for the two-sided machine embroidery of woollen spun fingering yarn according to the above embodiment of the present invention can also have following additional technical characterictic:
According to some embodiments of the present invention, the reaching the standard grade and roll off the production line of described machine embroidery is described woollen spun fingering yarn.Can realize two-sided machine embroidery thus, to further improve the aesthetic feeling of product.
According to some embodiments of the present invention, the brute force of described woollen spun fingering yarn is 300~360cN, and number is 60.Can further improve the embroidery property of woollen spun fingering yarn thus.
According to some embodiments of the present invention, multi-functional two, described embroidery machine Wei Tian island embroidery machine TMLH II-902.Can further improve aesthetic feeling and the texture of machine embroidery finished product thus.
According to some embodiments of the present invention, described embroidered be to adopt to embroider pins No. 11, stitch length be 3~5mm and 200 pins/minute speed carry out.Can effectively prevent thus broken string, plug line, improve the aesthetic feeling of machine embroidery finished product.
According to some embodiments of the present invention, described washing is processed by described machine embroidery crude product is soaked and completed for 15-30 minute in 40 degrees Celsius of water.Thus can be so that the water-soluble fibre in woollen spun fingering yarn all dissolves, so that machine embroidery finished product presents brushy outward appearance.
According to a further aspect in the invention, the present invention proposes a kind of embroidered fine and soft face machine embroidery fabric of woollen spun fingering yarn that utilizes, described woollen spun fingering yarn is the blended knitting wool of cashmere and water-soluble fibre, and the mass ratio of described cashmere and water-soluble fibre is 45:55.
According to some embodiments of the present invention, in order to utilize, foregoing method is embroidered to be formed described fine and soft face machine embroidery fabric.
In accordance with a further aspect of the present invention, the present invention proposes the purposes of a kind of woollen spun fingering yarn in machine embroidery, described woollen spun fingering yarn is the blended knitting wool of cashmere and water-soluble fibre, and the mass ratio of described cashmere and water-soluble fibre is 45:55.Open up thus the new application of woollen spun fingering yarn in textile industry, and realized the effect unique that woollen spun fingering yarn is brought into play in machine embroidery.
Accompanying drawing explanation
Fig. 1 is the flow chart of the method for the two-sided machine embroidery of woollen spun fingering yarn according to an embodiment of the invention.
Fig. 2 is the obverse and reverse design sketch that utilizes according to an embodiment of the invention the fine and soft face machine embroidery fabric before the embroidered washing of woollen spun fingering yarn is processed.
Fig. 3 is the obverse and reverse design sketch that utilizes according to an embodiment of the invention the fine and soft face machine embroidery fabric after the embroidered washing of woollen spun fingering yarn is processed.
Fig. 4 is the reverse side design sketch that utilizes according to an embodiment of the invention the embroidered embroidery fabric of woollen spun fingering yarn.
The specific embodiment
Describe embodiments of the invention below in detail, the example of described embodiment is shown in the drawings, and wherein same or similar label represents same or similar element or has the element of identical or similar functions from start to finish.Below by the embodiment being described with reference to the drawings, be exemplary, be intended to for explaining the present invention, and can not be interpreted as limitation of the present invention.
Embroidery product is used the embroidery line of fibers material embroidered conventionally, due to fibers material smoother, powerful large, easily embroidered, is not prone to broken string, but the embroidered pattern needle tracking of fibers material is more clear, can not reach effect fluffy, dim, lint.Knitting wool is that cashmere yarn or cashmere line are to take goat cashmere as raw material, warp and hair, carded, spun yarn, winder, doubling, the yarn that the link such as twist thread (spinning also need first slivering) is made.Adopt knitting wool can reach effect fluffy, dim, lint as embroidering line, but because cashmere fiber is shorter, slubbing is difficult to high-count yarn spun line, the sense that product shortage is frivolous, fluffy, and spun yarn product does not have the softness of woolen fabrics and plentiful.Woollen spun fingering yarn brute force is low, and number is lower, and generally, from 14 to 32, filoplume is many, and the twist is low, uses it for computerized embroidery and has certain difficulty, does not use in the market woollen spun fingering yarn to do the embroidery product of embroidering line.
The present invention has puted forth effort to research and propose a kind of method that can utilize woollen spun fingering yarn to carry out machine embroidery, the application that the method is woollen spun fingering yarn provides new thinking, utilize the embroidered machine embroidery finished product positive and negative obtaining of the method all to there is brushy outward appearance simultaneously, not only feel is comfortable, and visual effect is also very unique.
The method of describing the two-sided machine embroidery of woollen spun fingering yarn of the embodiment of the present invention below with reference to Fig. 1, the method comprises:
Textiles and woollen spun fingering yarn are provided;
Utilize embroidery machine using woollen spun fingering yarn as embroider line on textiles embroidered preset play an edition layout, to obtain machine embroidery crude product;
Machine embroidery crude product is washed to processing, and the woollen spun fingering yarn that makes formation play version layout is partly dissolved;
Machine embroidery crude product through washing is dried to processing, to obtain machine embroidery finished product;
Wherein, woollen spun fingering yarn is the blended knitting wool of cashmere and water-soluble fibre, and the mass ratio of cashmere and water-soluble fibre is 45:55.
The technology is processed from slubbing cashmere yarn, the configuration of production device hardware, machine embroidery is beaten three aspects of version design and is started with, research and solve yarn strength, the twist, tension force, needle plate, embroider the series technique difficult problems such as pin configuration, enriched the colored type gradation of product, wash out after suede, fleece fabrics combines together with embroidering line, has realized brushy unique products outward appearance, and the method provides strong technical support for cashmere product exploitation.
Describe the concrete steps of method of the two-sided machine embroidery of woollen spun fingering yarn of the above embodiment of the present invention below in detail:
S100: textiles and woollen spun fingering yarn are provided
According to a particular embodiment of the invention, first provide textiles, so that at its surperficial embroidered pattern.According to a particular embodiment of the invention, textiles can be cashmere blanket, fleece fabrics, silk fabrics, wall cloth etc.According to a particular embodiment of the invention, woollen spun fingering yarn is the blended knitting wool of cashmere and water-soluble fibre, and wherein, the mass ratio of cashmere and water-soluble fibre is 45:55.By being mixed with a certain proportion of water-soluble fibre in cashmere, increasing the bulking intensity of slubbing cashmere product and slide waxy thus, also improved the brute force of woollen spun fingering yarn, improved the number of woollen spun fingering yarn, increase the spinnability of cashmere line, according to a particular embodiment of the invention, the brute force with the woollen spun fingering yarn of above-mentioned mass ratio is 300~360cN, and number is 60.The product of integrated use machine embroidery explained hereafter, not only can strengthen the expressive force of color and flower type, and after water-soluble fibre is washed off, cashmere product is more soft, fluffy, shows a kind of brushy unique look and textural effect.Therefore, the present invention carries out technological improvement to slubbing cashmere yarn in advance, is that 45:55 carries out blending and prepares woollen spun fingering yarn by cashmere and water-soluble fibre according to mass ratio, this woollen spun fingering yarn can reach the requirement of machine embroidery to yarn tension and the twist, can make thus it can on flannelette blanket or fleece fabrics, carry out computer embroidery, realize two-sided machine embroidery, make product there is brushy unique skin texture outward appearance.Cashmere content in woollen spun fingering yarn is according to the abovementioned embodiments of the present invention 45%, can be so that utilize the embroidered embroidery obtaining of this woollen spun fingering yarn to reduce cashmere cost on the basis of appearance requirement meeting, if cashmere content is lower than 45%, make water-soluble fibre content too much, after processing, washing dissolves completely, remaining a small amount of cashmere ratio is easier to occur obscission, makes dim design or excalation, and then affects the quality of embroidery and attractive in appearance.What therefore, adopt cashmere and water-soluble fibre is that woollen spun fingering yarn that 45:55 blending obtains carries out machine embroidery and not only can save cost, the quality assurance that can also improve machine embroidery finished product simultaneously according to mass ratio.
According to a particular embodiment of the invention, the pattern effect for preparing the machine embroidery finished product that the woollen spun fingering yarn preparing by doubling twisting method with identical proportioning of woollen spun fingering yarn finally obtains for machine embroidery by blending method is better, the yarn strength that doubling twisting method obtains significantly improves, but, because water-soluble fibre long filament is different from cashmere yarn material, during machine embroidery, strand easily separates, and cashmere yarn is easily broken, and water soluble fiber is powerful large, not easily broken, the cashmere yarn alluvial of fracture, cannot continue embroidery, affects product quality and production efficiency.
S200: using woollen spun fingering yarn as embroidering line embroidered pattern on textiles
According to a particular embodiment of the invention, utilize embroidery machine using above-mentioned woollen spun fingering yarn as embroider line on the above-mentioned textiles providing embroidered preset play an edition layout, to obtain machine embroidery crude product.
According to a particular embodiment of the invention, above-mentioned machine embroidery reaches the standard grade and rolls off the production line and be woollen spun fingering yarn.Can keep thus reaching the standard grade and lower wire material, color, uniform tension in order.
According to a particular embodiment of the invention, embroidery machine can adopt embroidery machine TMLH II-902, multi-functional two, island, field.TMLH series is extraordinary type, can adapt to yarn tension at a high speed, while running up, can detect rapidly the broken string of reaching the standard grade or roll off the production line, and because having adopted spring center lane and having locked line structure, makes to embroider line tension and stitching more stable, smooth and easy.And adopt embroidery machine TMLH II-902, multi-functional two, island, field to carry out two-sided machine embroidery, can enrich the level of colored type and color, wash out after suede, embroider line and fleece fabrics and combine together, realized brushy unique products outward appearance.According to concrete example of the present invention, the version layout of beating presetting needs and process matching, and pattern mates aesthetic feeling and the texture that can improve embroidered pattern with the skill of handling needles.Conventionally can adopt flat pin, the compound basic skill of handling needles such as pin of filling out, establish less trimming, otherwise fabric backing easily be filled in line.In addition, the scope of the tension adjustment that rolls off the production line and reach the standard grade is very limited, and the adjusting of tension force is crucial, is also difficult point.
According to concrete example of the present invention, embroidered can employing embroidered pin for No. 11-14, stitch length be 3~5mm and 200 pins/minute speed carry out.Therefore, by combination, play version layout, adjust the skill of handling needles, needle tracking and density, then be aided with tension adjustment, could realize gratifying effect.Simultaneously according to concrete example of the present invention, if for example the elasticity of cashmere blanket or fleece fabrics is large for the textiles providing, can uses water-soluble embroidery to be lining with frame and fix, can further reduce embroidered difficulty thus.
According to concrete example of the present invention, can also suitably adjust the pressing line tension that embroidery machine is crossed line spring, because the brute force of woollen spun fingering yarn is little, suitably reduce pressing line tension, the generation of the phenomenons such as the easy broken string that the tension that can effectively prevent from reaching the standard grade causes, the easy plug line of rolling off the production line.While pressing line tension is also difficult for too small, otherwise the pine of reaching the standard grade, stitching is irregular, finally affects fabric attractive in appearance.Specifically can suitably adjust lower line tension it is mated with upper line tension, change No. 11 simultaneously and embroider pin, reduce machine speed embroidery, adopt the speed of 200 pins/min.Can further improve aesthetic feeling and the texture of embroidered pattern thus.
S300: washing is processed
According to a particular embodiment of the invention, machine embroidery crude product is washed to processing, the woollen spun fingering yarn that makes formation play version layout is partly dissolved.Particularly, in washing processing procedure, the water-soluble fibre in the woollen spun fingering yarn that is mainly used for embroidering all dissolves, and then makes product more soft, fluffy, shows a kind of brushy unique look and textural effect.
According to a particular embodiment of the invention, washing is processed by above-mentioned machine embroidery crude product is soaked and completed for 15-30 minute in 40 degrees Celsius of water.Thus can be so that water-soluble fibre fully dissolve in woollen spun fingering yarn, and then make product reach soft, fluffy effect.
S400: dry processing
According to a particular embodiment of the invention, the above-mentioned machine embroidery crude product through washing is dried to processing, to obtain machine embroidery finished product.Dry processing can adopt nature to dry, and can further improve and suede effect thus.
The method effective integration of the two-sided machine embroidery of woollen spun fingering yarn according to the above embodiment of the present invention knitting technology, woollen spun fingering yarn production technology and machine embroidery technique, the method has been widened colored type and color and the effective scope of embroidery product, has promoted the development of high-grade knitted embroidery product.Utilize the machine embroidery finished product that said method prepares to put and also there is fine ornamental value as handicraft simultaneously.
According to a further aspect in the invention, the present invention proposes a kind of embroidered fine and soft face machine embroidery fabric of woollen spun fingering yarn that utilizes.According to a particular embodiment of the invention, woollen spun fingering yarn is the blended knitting wool of cashmere and water-soluble fibre, and the mass ratio of cashmere and water-soluble fibre is 45:55.Utilize thus the embroidered embroidery product obtaining of this woollen spun fingering yarn more soft, fluffy, show brushy unique look and textural effect.
According to a particular embodiment of the invention, fine and soft face machine embroidery fabric is to utilize foregoing woollen spun fingering yarn to carry out embroidered the forming of method of machine embroidery.Utilize thus the method that woollen spun fingering yarn is combined with machine embroidery, the embroidered product obtaining has brushy unique look and textural effect.
In accordance with a further aspect of the present invention, the invention allows for the purposes of a kind of woollen spun fingering yarn in machine embroidery, according to a particular embodiment of the invention, this woollen spun fingering yarn is the blended knitting wool of cashmere and water-soluble fibre, and the mass ratio of cashmere and water-soluble fibre is 45:55.There is thus the range of application that the woollen spun fingering yarn of above-mentioned feature has been opened up woollen spun fingering yarn, woollen spun fingering yarn brute force is in the past low, number is low is not easy for machine embroidery, but the embroidery effect that woollen spun fingering yarn can reach for machine embroidery is other embroider lines for example fibers material do not reach, what the present invention proposed carries out according to 45:55 mass ratio brute force and the number that novel woollen spun fingering yarn that blending obtains has improved woollen spun fingering yarn by cashmere and water-soluble fibre, can meet the requirement of machine embroidery to powerful and yarn count, the product that simultaneously utilizes the embroidered pattern of this woollen spun fingering yarn to obtain after washing is processed can show brushy unique look.Therefore, the purposes of the woollen spun fingering yarn of the above embodiment of the present invention in machine embroidery opened up the new application of woollen spun fingering yarn in textile industry, and realized the effect unique that woollen spun fingering yarn is brought into play in machine embroidery.
Embodiment
Take cashmere blanket as textiles, and elasticity and the thickness of this cashmere blanket are moderate, without using to embroider to serve as a contrast, fix.
The blended knitting wool that the mass ratio of cashmere and water-soluble fibre of take is 45:55 is to embroider line, and this blended knitting wool prepares by blending, and blended weave is the blending method of existing textile industry application.
First computer is played an edition layout, adopt embroidery machine TMLH II-902, multi-functional two, island, field, select to embroider pin No. 11, stitch length be set be 3~5mm, machine speed and be 200 pins/minute, usining reaches the standard grade and roll off the production line is above-mentioned blended knitting wool as embroidering line, carry out embroideredly playing version layout, and regulate pressing line tension, prevent broken string, plug line.The embroidered machine embroidery crude product that obtains, is shown in Fig. 2 (the left figure in Fig. 2 is positive, and right figure is reverse side).The embroidered cashmere blanket completing is immersed in to 15-30 minute in 40 degrees Celsius of water.Carried out nature and dried, obtained machine embroidery finished product, seen Fig. 3 (the left figure in Fig. 3 is positive, and right figure is reverse side).
As shown in Figure 3, the positive and negative dough effect of the machine embroidery finished product obtaining is all good, uncork line situation.And the machine embroidery finished product in Fig. 3 shows fluffy, obfuscation and brushy external appearance characteristic compared with the machine embroidery crude product in Fig. 2.
Comparative example
Utilize water-soluble fibre slurries to soak slubbing cashmere line (26) and improve yarn strength, concrete grammar comprises:
(1) first water-soluble fibre (water-soluble lining) water is dissolved, make the solution that paste is the same;
(2) then, cashmere line is wound around by how many amounts, washes and contract.Object is to allow cashmere line go out suede;
(3) by the cashmere line washing (just wash, do not need to dry), be immersed in the solution that (1) step makes, make cashmere line outside just superscribe one deck water-soluble fibre slurries;
(4) cashmere line of handling is dried, as floss silk, use.
To treated yarn, divide five groups to test, yarn strength data respectively: 361.3cn, 365.cn, 329.cn, 322.4.cn, 286.3.cn, brute force has improved 3 times.
Utilize yarn prepared by said method to carry out machine embroidery, experiment shows that this kind of yarn can only be for one side machine embroidery, and the serious (see figure 4) of plug line of fabric backing easily damage and embroider pin, and machine embroidery pattern effect is poor.
In the description of this description, the description of reference term " embodiment ", " some embodiment ", " example ", " concrete example " or " some examples " etc. means to be contained at least one embodiment of the present invention or example in conjunction with specific features, structure, material or the feature of this embodiment or example description.In this manual, to the schematic statement of above-mentioned term not must for be identical embodiment or example.And, the specific features of description, structure, material or feature can one or more embodiment in office or example in suitable mode combination.In addition,, not conflicting in the situation that, those skilled in the art can carry out combination and combination by the feature of the different embodiment that describe in this description or example and different embodiment or example.
Although illustrated and described embodiments of the invention above, be understandable that, above-described embodiment is exemplary, can not be interpreted as limitation of the present invention, and those of ordinary skill in the art can change above-described embodiment within the scope of the invention, modification, replacement and modification.

Claims (9)

1. a method for the two-sided machine embroidery of woollen spun fingering yarn, is characterized in that, comprising:
Textiles and woollen spun fingering yarn are provided;
Utilize embroidery machine using described woollen spun fingering yarn as embroider line on described textiles embroidered preset play an edition layout, to obtain machine embroidery crude product;
Described machine embroidery crude product is washed to processing, the woollen spun fingering yarn of playing version layout described in forming is partly dissolved;
The described machine embroidery crude product through washing is dried to processing, to obtain machine embroidery finished product;
Wherein, described woollen spun fingering yarn is the blended knitting wool of cashmere and water-soluble fibre, and the mass ratio of described cashmere and water-soluble fibre is 45:55.
2. method according to claim 1, is characterized in that, the reaching the standard grade and roll off the production line of described embroidered employing is described woollen spun fingering yarn.
3. method according to claim 1, is characterized in that, the brute force of described woollen spun fingering yarn is 300~360cN, and number is 60.
4. method according to claim 1, is characterized in that, embroidery machine TMLH II-902, multi-functional two, described embroidery machine Wei Tian island.
5. method according to claim 1, is characterized in that, described embroidered be to adopt to embroider pin No. 11-14, stitch length be 3~5mm and 200 pins/minute speed carry out.
6. method according to claim 1, is characterized in that, it is within 15-30 minute, to complete by described machine embroidery crude product is soaked in the water of 40 degrees Celsius that described washing is processed.
7. utilize the embroidered fine and soft face machine embroidery fabric of woollen spun fingering yarn, it is characterized in that, described woollen spun fingering yarn is the blended knitting wool of cashmere and water-soluble fibre, and the mass ratio of described cashmere and water-soluble fibre is 45:55.
8. fine and soft face machine embroidery fabric according to claim 7, is characterized in that, described fine and soft face machine embroidery fabric is embroidered the forming of method of utilizing described in claim 1-6 any one.
9. the purposes of woollen spun fingering yarn in machine embroidery, is characterized in that, described woollen spun fingering yarn is the blended knitting wool of cashmere and water-soluble fibre, and the mass ratio of described cashmere and water-soluble fibre is 45:55.
CN201410150688.1A 2014-04-15 2014-04-15 The methods and applications of the two-sided machine embroidery of woollen spun fingering yarn Expired - Fee Related CN103924395B (en)