CN103864056B - 一种碳微球的制备方法 - Google Patents

一种碳微球的制备方法 Download PDF

Info

Publication number
CN103864056B
CN103864056B CN201410139702.8A CN201410139702A CN103864056B CN 103864056 B CN103864056 B CN 103864056B CN 201410139702 A CN201410139702 A CN 201410139702A CN 103864056 B CN103864056 B CN 103864056B
Authority
CN
China
Prior art keywords
carbosphere
preparation
deionized water
carry out
hydro
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201410139702.8A
Other languages
English (en)
Other versions
CN103864056A (zh
Inventor
马望京
琚伟
宫清涛
张天宝
张建刚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangsu Zhongneng Environmental Protection Technology Co.,Ltd.
Original Assignee
Nanjing Rui Ying Environmental Protection Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nanjing Rui Ying Environmental Protection Technology Co Ltd filed Critical Nanjing Rui Ying Environmental Protection Technology Co Ltd
Priority to CN201410139702.8A priority Critical patent/CN103864056B/zh
Publication of CN103864056A publication Critical patent/CN103864056A/zh
Application granted granted Critical
Publication of CN103864056B publication Critical patent/CN103864056B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种碳微球的制备方法,将柚子皮与去离子水以一定比例混和均匀,然后倒于反应釜内衬中后,置于烘箱中于一定温度下进行水热反应,反应完成后取出反应釜并冷却至室温,得到棕黄色的水溶液分散体系;静置,取出上清液进行离心分离,用去离子水洗涤晾干后所得固体,获得碳微球。本发明操作简单、绿色环保,所获得的碳微球可广泛用于纳米技术、光电转换和催化等领域。

Description

一种碳微球的制备方法
技术领域
本发明属于化学及纳米材料领域,涉及一种碳微球的制备方法。
背景技术
碳纳米材料如富勒烯、碳纳米管和石墨烯等因其具有各种独特性质而成为近几年纳米科学研究的热点。碳微球因其具有形貌规整、导热系数高、耐热性能良好、物理与化学性能稳定等优点,引起广泛关注,在电磁学、生物、物理、化学化工、材料学等多领域中具有极大应用价值。碳微球的制备与研究工作具有重要意义。其制备方法多种多样,各有千秋,水热法因原料价廉易得、成本低、能耗少、工艺绿色环保、设备简单易操作等优点,成为近年来制备碳微球的研究热点。
发明内容
本发明的目的是提供一种碳微球的制备方法,该制备方法利用柚子皮与去离子水,通过水热法获得尺寸形貌规整的碳微球,操作简单,绿色环保。
本发明的目的是通过以下技术方案来实现的:
一种碳微球的制备方法,其特征在于该方法包括以下步骤:
1)将柚子皮与去离子水以任意比例倒入反应釜内衬中,置于烘箱中进行水热反应;
2)反应完成后取出反应釜并冷却至室温,得到棕黄色的水溶液分散体系;
3)静置,取出上清液进行离心分离,用去离子水洗涤并晾干后所得固体,获得分散均匀的碳微球。
本发明中,柚子皮与去离子水可以以任意比例混合,优选的,柚子皮与去离子水的质量比为:1:80-80:1,柚子皮为柚子皮内侧。
所述的水热反应的温度为150-210℃;水热反应的时间为1-10小时。
本发明的优点是:操作简单、绿色环保,所获得的碳微球尺寸形貌规整,可广泛用于纳米技术、光电转换和催化等领域。利用扫描电镜对本发明制备得到的碳微球进行测定,结果显示碳微球形貌规整。
附图说明
图1是本发明实施例1制备得到的碳微球的电镜照片图。
图2是本发明实施例2制备得到的碳微球的电镜照片图。
具体实施方式
实施例1
一种碳微球的制备方法,将柚子皮与去离子以质量比为1:80的比例倒于反应釜聚四氟乙烯内衬中,置于烘箱中进行水热反应,水热反应的温度为150℃,反应10小时后取出反应釜并冷却至室温,得到棕黄色的水溶液分散体系;静置,取出上清液进行离心分离,用去离子水洗涤所得固体,经3-4次离心分离和洗涤晾干后,获得分散均匀的碳微球。测试结果显示:制备的碳微球尺寸均匀,见图1。
实施例2
又一种碳微球的制备方法,将柚子皮与去离子水以质量比为1:1的比例混和均匀,然后倒于反应釜中后置于烘箱中进行水热反应,水热反应的温度为180℃,反应5小时后取出反应釜并冷却至室温,得到棕黄色的水溶液分散体系;静置,取出上清液进行离心分离,用去离子水洗涤所得固体,经离心分离和洗涤晾干后,获得分散均匀的碳微球。测试结果显示:制备的碳微球尺寸均匀,见图2。
实施例3
将柚子皮与去离子水以质量比为80:1的比例混和均匀,然后倒于反应釜中后置于烘箱中进行水热反应,水热反应的温度为210℃,反应1小时后取出反应釜并冷却至室温,得到棕黄色的水溶液分散体系;静置,取出上清液进行离心分离,用去离子水洗涤所得固体,经多次离心分离和洗涤晾干后,获得分散均匀的碳微球。

Claims (3)

1.一种碳微球的制备方法,其特征在于该方法包括以下步骤:
1)将柚子皮与去离子水以1:1-80:1的比例倒入反应釜内衬中,置于烘箱中进行水热反应;水热反应的温度为150-210℃,水热反应的时间为5-10小时;
2)反应完成后取出反应釜并冷却至室温,得到棕黄色的水溶液分散体系;
3)静置,取出上清液进行离心分离,用去离子水洗涤所得固体,晾干后获得分散均匀的碳微球。
2.根据权利要求1所述的碳微球的制备方法,其特征在于:所述的柚子皮为柚子皮内侧。
3.根据权利要求1所述的碳微球的制备方法,其特征在于:经3-4次离心分离和洗涤晾干后所得固体,获得分散均匀的碳微球。
CN201410139702.8A 2014-04-04 2014-04-04 一种碳微球的制备方法 Active CN103864056B (zh)