Prior art keywords
parts
antibacterial
slag
coal ash
mucine
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410025568.9A
Other languages
English (en)
Inventor
任劲松
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ANHUI SHENGREN NEW BUILDING MATERIAL Co Ltd
Original Assignee
ANHUI SHENGREN NEW BUILDING MATERIAL Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ANHUI SHENGREN NEW BUILDING MATERIAL Co Ltd filed Critical ANHUI SHENGREN NEW BUILDING MATERIAL Co Ltd
Priority to CN201410025568.9A priority Critical patent/CN103833313A/zh
Publication of CN103833313A publication Critical patent/CN103833313A/zh
Pending legal-status Critical Current

Links

Abstract

本发明公开了一种抗菌加气砖,其是由下述重量份的原料制得:硅酸盐水泥15-25、脱硫石膏18-22、煤灰渣4-6,淀粉1-2,铝粉0.1-0.2、羧甲基纤维素钠1-2、苯丙乳液3-5,四氧化三铁0.1-0.2、硬脂酸1-2、淤泥4-8、锰渣12-15、三乙醇胺1-2、乙二醇1-3,木质素磺酸钙1-2,助剂3-6;本发明抗菌性能优异,同时抗裂性能相对较高,,满足常规加气砖性能要求。

Description

一种抗菌加气砖
技术领域
本发明涉及加气砖领域,确切地说是一种抗菌加气砖。
背景技术
 加气砖,指的是通过高温蒸压设备工艺生产的加气混凝土砌块,现有加气砖品种单一,性能差,无法满足日益增加的市场需求。
发明内容
本发明的目的在于提供一种抗菌加气砖。
上述目的通过以下方案实现:
一种抗菌加气砖,其特征在于:其是由下述重量份的原料制得:
硅酸盐水泥15-25、脱硫石膏18-22、煤灰渣4-6,淀粉1-2,铝粉0.1-0.2、羧甲基纤维素钠1-2、苯丙乳液3-5,四氧化三铁0.1-0.2、硬脂酸1-2、淤泥4-8、锰渣12-15、三乙醇胺1-2、乙二醇1-3,木质素磺酸钙1-2,助剂3-6;
所述的助剂由下述重量份的原料制得:膨润土10-15,煤灰渣6-8、钢渣5-8、凹凸棒土15-18、醋酸钠1-2、氧化铜1-2、明胶 0.2-0.4,氯化石蜡 2.8-3.3、异构醇聚氧乙烯醚  0.2-0.4、硅烷偶联剂KH550  2-4;
所述的助剂的制备方法为:
取煤灰渣、钢渣混匀后,破碎,所得粉料于720-800℃下于煅烧2-4小时,再取出冷却,与凹凸棒土、明胶以及适量水混匀后,研磨30-50分钟,取出加12-18%的氢氧化钠溶液调PH为8-8.5,再加入膨润土,研磨浆料至400-500目后,再加盐酸溶液调为中性,喷雾干燥,所得粉末与其它剩余原料混合,混合均匀即得。
所述的一种抗菌加气砖,其特征在于:
制备方法为:
(1)将除水泥、铝粉、羧甲基纤维素钠以外的其它原料混匀,加入适量水,在30-35℃下搅拌均匀后,再加入水泥、铝粉、羧甲基纤维素钠,搅拌均匀,得混合水泥浆料;
(2)将混合水泥浆料浇筑入模成型,后在35-42℃下预养3-4小时,脱模,切割,蒸压养护后,即得。
本发明的有益效果为:本发明抗菌性能优异,同时抗裂性能相对较高,,满足常规加气砖性能要求。
具体实施方式
一种抗菌加气砖,其是由下述重量kg的原料制得:
硅酸盐水泥25、脱硫石膏22、煤灰渣4,淀粉1,铝粉0.2、羧甲基纤维素钠2、苯丙乳液3,四氧化三铁0.2、硬脂酸1、淤泥8、锰渣15、三乙醇胺1、乙二醇3,木质素磺酸钙2,助剂6;
所述的助剂由下述重量kg的原料制得:膨润土15,煤灰渣8、钢渣5、凹凸棒土18、醋酸钠2、氧化铜1、明胶 0.4,氯化石蜡 3.3、异构醇聚氧乙烯醚  0.4、硅烷偶联剂KH550  3;
所述的助剂的制备方法为:
取煤灰渣、钢渣混匀后,破碎,所得粉料于800℃下于煅烧4小时,再取出冷却,与凹凸棒土、明胶以及适量水混匀后,研磨40分钟,取出加12%的氢氧化钠溶液调PH为8,再加入膨润土,研磨浆料至500目后,再加盐酸溶液调为中性,喷雾干燥,所得粉末与其它剩余原料混合,混合均匀即得。
所述的一种抗菌加气砖,
制备方法为:
(1)将除水泥、铝粉、羧甲基纤维素钠以外的其它原料混匀,加入适量水,在35℃下搅拌均匀后,再加入水泥、铝粉、羧甲基纤维素钠,搅拌均匀,得混合水泥浆料;
(2)将混合水泥浆料浇筑入模成型,后在38℃下预养4小时,脱模,切割,蒸压养护后,即得。
本实施例所得加气砖的平均容重为660kg/m3,保温性能好,平均值抗压强度为8.2MPa。

Claims (2)

1.一种抗菌加气砖,其特征在于:其是由下述重量份的原料制得:
硅酸盐水泥15-25、脱硫石膏18-22、煤灰渣4-6,淀粉1-2,铝粉0.1-0.2、羧甲基纤维素钠1-2、苯丙乳液3-5,四氧化三铁0.1-0.2、硬脂酸1-2、淤泥4-8、锰渣12-15、三乙醇胺1-2、乙二醇1-3,木质素磺酸钙1-2,助剂3-6;
所述的助剂由下述重量份的原料制得:膨润土10-15,煤灰渣6-8、钢渣5-8、凹凸棒土15-18、醋酸钠1-2、氧化铜1-2、明胶 0.2-0.4,氯化石蜡 2.8-3.3、异构醇聚氧乙烯醚  0.2-0.4、硅烷偶联剂KH550  2-4;
所述的助剂的制备方法为:
取煤灰渣、钢渣混匀后,破碎,所得粉料于720-800℃下于煅烧2-4小时,再取出冷却,与凹凸棒土、明胶以及适量水混匀后,研磨30-50分钟,取出加12-18%的氢氧化钠溶液调PH为8-8.5,再加入膨润土,研磨浆料至400-500目后,再加盐酸溶液调为中性,喷雾干燥,所得粉末与其它剩余原料混合,混合均匀即得。
2.根据权利要求1所述的一种抗菌加气砖,其特征在于:
制备方法为:
(1)将除水泥、铝粉、羧甲基纤维素钠以外的其它原料混匀,加入适量水,在30-35℃下搅拌均匀后,再加入水泥、铝粉、羧甲基纤维素钠,搅拌均匀,得混合水泥浆料;
(2)将混合水泥浆料浇筑入模成型,后在35-42℃下预养3-4小时,脱模,切割,蒸压养护后,即得。
CN201410025568.9A 2014-01-21 2014-01-21 一种抗菌加气砖 Pending CN103833313A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201410025568.9A CN103833313A (zh) 2014-01-21 2014-01-21 一种抗菌加气砖

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201410025568.9A CN103833313A (zh) 2014-01-21 2014-01-21 一种抗菌加气砖

Publications (1)

Publication Number Publication Date
CN103833313A true CN103833313A (zh) 2014-06-04

Family

ID=50797258

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201410025568.9A Pending CN103833313A (zh) 2014-01-21 2014-01-21 一种抗菌加气砖

Country Status (1)

Country Link
CN (1) CN103833313A (zh)

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104058682A (zh) * 2014-05-29 2014-09-24 蚌埠华东石膏有限公司 一种抗菌加气砖
CN104193278A (zh) * 2014-07-31 2014-12-10 寿县维东建材商贸有限公司 一种新型环保彩瓦及其制备方法
CN104557108A (zh) * 2014-12-19 2015-04-29 安徽中龙建材科技有限公司 一种抗菌防霉加气砌块及其制备方法
CN105418001A (zh) * 2015-11-09 2016-03-23 当涂县科辉商贸有限公司 一种耐老化寿命长的蒸压加气混凝土砌块及其制作方法
CN105439503A (zh) * 2015-11-10 2016-03-30 当涂县科辉商贸有限公司 一种可吸附异味的抑菌蒸压加气混凝土砌块及其制作方法
CN107324683A (zh) * 2017-06-29 2017-11-07 马鞍山市志诚科技有限公司 一种加气砖中发泡改性粉及其制作工艺
CN112851343A (zh) * 2021-01-20 2021-05-28 陈彩霞 一种抑菌耐磨陶瓷及其制备方法

Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102875073A (zh) * 2012-08-25 2013-01-16 马鞍山豹龙新型建材有限公司 一种加气砖
CN102887671A (zh) * 2012-09-03 2013-01-23 蚌埠爱民汽车服务有限公司五河新型环保建材厂 一种利用硅藻土生产的加气砖及其加工方法
CN103449769A (zh) * 2013-07-31 2013-12-18 潘逸东 一种抗菌加气砖
CN103467049A (zh) * 2013-08-05 2013-12-25 安徽中龙建材科技有限公司 一种添加丙纶纤维的加气砖的制备方法
CN103467007A (zh) * 2013-08-05 2013-12-25 安徽中龙建材科技有限公司 一种添加复配凹凸棒土颗粒的加气砖

Patent Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102875073A (zh) * 2012-08-25 2013-01-16 马鞍山豹龙新型建材有限公司 一种加气砖
CN102887671A (zh) * 2012-09-03 2013-01-23 蚌埠爱民汽车服务有限公司五河新型环保建材厂 一种利用硅藻土生产的加气砖及其加工方法
CN103449769A (zh) * 2013-07-31 2013-12-18 潘逸东 一种抗菌加气砖
CN103467049A (zh) * 2013-08-05 2013-12-25 安徽中龙建材科技有限公司 一种添加丙纶纤维的加气砖的制备方法
CN103467007A (zh) * 2013-08-05 2013-12-25 安徽中龙建材科技有限公司 一种添加复配凹凸棒土颗粒的加气砖

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104058682A (zh) * 2014-05-29 2014-09-24 蚌埠华东石膏有限公司 一种抗菌加气砖
CN104193278A (zh) * 2014-07-31 2014-12-10 寿县维东建材商贸有限公司 一种新型环保彩瓦及其制备方法
CN104557108A (zh) * 2014-12-19 2015-04-29 安徽中龙建材科技有限公司 一种抗菌防霉加气砌块及其制备方法
CN105418001A (zh) * 2015-11-09 2016-03-23 当涂县科辉商贸有限公司 一种耐老化寿命长的蒸压加气混凝土砌块及其制作方法
CN105439503A (zh) * 2015-11-10 2016-03-30 当涂县科辉商贸有限公司 一种可吸附异味的抑菌蒸压加气混凝土砌块及其制作方法
CN107324683A (zh) * 2017-06-29 2017-11-07 马鞍山市志诚科技有限公司 一种加气砖中发泡改性粉及其制作工艺
CN112851343A (zh) * 2021-01-20 2021-05-28 陈彩霞 一种抑菌耐磨陶瓷及其制备方法

Similar Documents

Publication Publication Date Title
CN103833313A (zh) 一种抗菌加气砖
CN103664104A (zh) 一种利用固体废弃物制备的保温砂浆
CN103833312A (zh) 一种隔热加气砖
CN103833315A (zh) 一种防冻加气砖
CN103496903A (zh) 一种保温砂浆
CN103693914B (zh) 一种保温砂浆
CN103771788A (zh) 一种耐用加气砖
CN103449765A (zh) 一种防腐蚀加气砖的制备方法
CN104557116A (zh) 一种加气混凝土砌块及其制备方法
CN105859316A (zh) 一种抗压强度高加气砖
CN104291743A (zh) 一种陶瓷砖粘结砂浆及其制备方法
CN103755299A (zh) 一种具有多种矿物的保温砂浆
CN104058682A (zh) 一种抗菌加气砖
CN111268988B (zh) 一种高耐水免煅烧磷石膏基边坡砌块材料及其制备
CN102875191B (zh) 一种加气混凝土砌块的制备工艺
CN103708794B (zh) 一种建筑外墙上使用的防水保温砂浆
CN103539420A (zh) 一种金刚砂保温砂浆
CN103626448A (zh) 一种利用固体废弃物制备的保温砂浆
CN104058644A (zh) 一种耐腐蚀加气砖
CN108821637A (zh) 一种半干法石膏助剂及其制备方法
CN103992070A (zh) 电解锰渣蒸压砖的制作工艺
CN104058703B (zh) 一种抗裂加气砖
CN103664099A (zh) 一种环保无机保温砂浆
CN103833314A (zh) 一种抗裂加气砖
CN103771895A (zh) 一种耐腐蚀加气砖

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
RJ01 Rejection of invention patent application after publication
RJ01 Rejection of invention patent application after publication

Application publication date: 20140604