CN103831171A - 一种磷矿浮选捕收剂及其制备方法 - Google Patents

一种磷矿浮选捕收剂及其制备方法 Download PDF

Info

Publication number
CN103831171A
CN103831171A CN201410117916.5A CN201410117916A CN103831171A CN 103831171 A CN103831171 A CN 103831171A CN 201410117916 A CN201410117916 A CN 201410117916A CN 103831171 A CN103831171 A CN 103831171A
Authority
CN
China
Prior art keywords
phosphate rock
collecting agent
flotation
rock floating
base substance
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410117916.5A
Other languages
English (en)
Inventor
李松清
尚衍波
魏明安
朱阳戈
郑桂兵
孙昊
张行荣
肖婉琴
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Beijing General Research Institute of Mining and Metallurgy
Original Assignee
Beijing General Research Institute of Mining and Metallurgy
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Beijing General Research Institute of Mining and Metallurgy filed Critical Beijing General Research Institute of Mining and Metallurgy
Priority to CN201410117916.5A priority Critical patent/CN103831171A/zh
Publication of CN103831171A publication Critical patent/CN103831171A/zh
Pending legal-status Critical Current

Abstract

一种磷矿浮选捕收剂,涉及一种特别适用于高镁中低品位磷块岩反浮选脱镁和极低磷品位磷铁矿正浮选浮选磷灰石的捕收剂及其制备方法。其特征在于该捕收剂由基本物质与水混合而成:其基本物质包括硬脂酸钠和磺酸盐。本发明的捕收剂不仅适用于磷块岩的反浮选脱镁,也适用于磷铁矿的正浮选回收磷灰石。针对高镁磷块岩在低温条件下反浮选脱镁可以获得低MgO含量的磷精矿并具有较高的P2O5回收率;针对极低P2O5品位磷铁矿在低温条件下正浮选回收磷灰石可以获得高质量的磷精矿并具有较高的P2O5回收率。本捕收剂具有选择性好,耐低温﹑用量适中且价格适中等特点。

Description

一种磷矿浮选捕收剂及其制备方法
技术领域
一种磷矿浮选捕收剂及其制备方法,涉及一种特别适用于高镁中低品位磷块岩反浮选脱镁和极低磷品位磷铁矿正浮选浮选磷灰石的捕收剂及其制备方法。
背景技术
我国磷矿资源储量较大,70%属于沉积岩型磷块岩,主要分布在中南和西南地区。高镁中低品位磷块岩中含镁矿物主要是白云石,湿法加工磷肥用一类品级磷矿石要求镁磷比(MgO/P2O5)不大于2%,白云石含量越低,越有利于降低磷肥生产成本。中国北方地区的磷矿主要来源于磷铁矿,磷铁矿中的磷主要以磷灰石形式存在,原矿P2O5品位普遍在10%以下,最低在2-3%,各个矿区的磷灰石浮选难易度与矿石性质、药剂配方有很大关系。而且北方地区严寒气候时间较长,冬天磷矿浮选普遍采用加温浮选,药剂用量大,能耗高,生产成本偏高。
发明内容
本发明的目的就是针对上述已有技术存在的不足,提供一种复配表面活性剂,选择性好,耐低温﹑用量适中且价格适中的磷矿浮选捕收剂。
本发明的目的是通过以下技术方案实现的。
一种磷矿浮选捕收剂,其特征在于该捕收剂由基本物质与水混合而成:其基本物质包括硬脂酸钠和磺酸盐。
本发明的一种磷矿浮选捕收剂,其特征在于其基本物质包括还包括羧酸酯。
本发明的一种磷矿浮选捕收剂,其特征在于其基本物质与水的质量比为1:3-50。
本发明的一种磷矿浮选捕收剂,其特征在于其基本物质的重量组份为硬脂酸钠0.4-0.6份,磺酸盐0.1-0.4份,羧酸酯0-0.5份。
本发明的一种磷矿浮选捕收剂,其特征在于其硬脂酸钠为工业皂片或工业皂粒。
本发明的一种磷矿浮选捕收剂,其特征在于其磺酸盐为具有12-18个碳原子的磺酸盐。
本发明的一种磷矿浮选捕收剂,其特征在于其羧酸酯为至少一种羧酸与甘油的酯。
本发明的一种磷矿浮选捕收剂,其特征在于其羧酸选自基于天然植物或动物油的具有6-30个碳原子的天然存在的脂肪酸。
本发明的一种磷矿浮选捕收剂,其特征在于其磺酸盐为十二烷基磺酸钠或十二烷基苯磺酸钠。
本发明的一种磷矿浮选捕收剂的制备方法,其特征在于其制备过程按重量份计,将0.4份~0.6份硬脂酸钠和0.1~0.4份磺酸盐和0~0.5份羧酸酯混合为基本物质,再将基本物质按比例加入水搅拌,制得反浮选脱镁捕收剂。
本发明的一种磷矿浮选捕收剂的制备方法,其特征在于其制备过程中基本物质加入水搅拌,是在40-50℃温度、 800r/m的搅拌速度条件下,搅拌20min后制得反浮选脱镁捕收剂。
本发明的一种磷矿浮选捕收剂,针对高镁中低品位磷块岩反浮选脱镁和极低磷品位磷铁矿正浮选磷灰石过程,适用的原料磷块岩的P2O5含量在20%左右,MgO含量在3-10%左右,脱除含镁矿物后的磷精矿P2O5含量在30%左右,可以生产出MgO含量低于1.3%的磷精矿,且磷精矿P2O5回收率高。它可以适用的原料磷铁矿P2O5含量在2-10%左右,正浮选浮选磷灰石得到的磷精矿P2O5含量在35%以上,且磷精矿P2O5回收率高。
   本发明的捕收剂不仅适用于磷块岩的反浮选脱镁,也适用于磷铁矿的正浮选回收磷灰石。针对高镁磷块岩在低温条件下反浮选脱镁可以获得低MgO含量的磷精矿并具有较高的P2O5回收率;针对极低P2O5品位磷铁矿在低温条件下正浮选回收磷灰石可以获得高质量的磷精矿并具有较高的P2O5回收率。本捕收剂具有选择性好,耐低温﹑用量适中且价格适中等特点。
本发明的捕收剂不仅适用于高镁磷块岩的反浮选脱镁,也适用于磷铁矿的正浮选回收磷灰石。这对于我国大量的中低品位高镁磷块岩资源的开发和降低磷铁矿正浮选回收磷灰石的浮选成本,具有非常重要的意义。
具体实施方式
本发明的一种磷矿浮选捕收剂,由基本物质与水混合而成:基本物质与水的质量比为1:3~50:其中基本物质的组份为硬脂酸钠0.4-0.6份,磺酸盐0.1-0.4份,羧酸酯0-0.5份。其制备过程按重量份计,将0.4份~0.6份硬脂酸钠和0.1~0.4份磺酸盐和0~0.5份羧酸酯混合为基本物质,再按比例加入水搅拌,搅拌温度40-50℃,搅拌速度800r/m,搅拌20min后制得反浮选脱镁捕收剂。
本发明的实施例所用原料均从市场购置。
试验例1
按重量份计,将0.6份硬脂酸钠和0.4份十二烷基磺酸钠混合并搅拌均匀,再加入20份水,加温搅拌,搅拌温度40-50℃,搅拌速度为800r/m,,搅拌时间20min后得到成品。
贵州某中低品位高镁磷块岩反浮选脱镁试验:入选原矿P2O5品位为21.22%,MgO品位为5.43%,经过一次粗选浮选流程,浮选pH值3-5,浮选温度8-10℃,捕收剂用量为600g/t,可获得P2O5品位为29.19%,MgO品位为1.23%,P2O5作业回收率92.44%的磷精矿。
试验例2
按重量份计,将0.6份硬脂酸钠和0.3份十二烷基苯磺酸钠和0.1份羧酸酯混合并搅拌均匀,再加入20份水,加温搅拌,搅拌温度40-50℃,搅拌速度为800r/m,,搅拌时间20min后得到成品。
河北某磷铁矿正浮选磷灰石试验:入选原矿P2O5品位为2.21%,经过一次粗选两次精选一次扫选闭路浮选流程,浮选pH值9-10,浮选温度8-10℃,捕收剂用量为800g/t,可获得P2O5品位为35.57%, P2O5回收率88.54%的磷精矿。
试验例3
按重量份计,将0.6份硬脂酸钠和0.2份十二烷基磺酸钠和0.2份羧酸酯混合并搅拌均匀,再加入20份水,加温搅拌,搅拌温度40-50℃,搅拌速度为800r/m,,搅拌时间20min后得到成品。
河北某磷铁矿正浮选磷灰石试验:入选原矿P2O5品位为2.15%,经过一次粗选两次精选一次扫选闭路浮选流程,浮选pH值9-10,浮选温度8-10℃,捕收剂用量为800g/t,可获得P2O5品位为33.27%, P2O5回收率91.05%的磷精矿。

Claims (11)

1.一种磷矿浮选捕收剂,其特征在于该捕收剂由基本物质与水混合而成:其基本物质包括硬脂酸钠和磺酸盐。
2.根据权利要求1所述的一种磷矿浮选捕收剂,其特征在于其基本物质包括还包括羧酸酯。
3.根据权利要求1所述的一种磷矿浮选捕收剂,其特征在于其基本物质与水的质量比为1:3-50。
4.根据权利要求1和2所述的一种磷矿浮选捕收剂,其特征在于其基本物质的重量组份为硬脂酸钠0.4-0.6份,磺酸盐0.1-0.4份,羧酸酯0-0.5份。
5.根据权利要求1所述的一种磷矿浮选捕收剂,其特征在于其硬脂酸钠为工业皂片或工业皂粒。
6.根据权利要求1所述的一种磷矿浮选捕收剂,其特征在于其磺酸盐为具有12-18个碳原子的磺酸盐。
7.根据权利要求1所述的一种磷矿浮选捕收剂,其特征在于其磺酸盐为十二烷基磺酸钠或十二烷基苯磺酸钠。
8.根据权利要求2所述的一种磷矿浮选捕收剂,其特征在于其羧酸酯为至少一种羧酸与甘油的酯。
9.根据权利要求2所述的一种磷矿浮选捕收剂,其特征在于其羧酸选自基于天然植物或动物油的具有6-30个碳原子的天然存在的脂肪酸。
10.根据权利要求1所述的一种磷矿浮选捕收剂的制备方法,其特征在于其制备过程按重量份计,将0.4份~0.6份硬脂酸钠和0.1~0.4份磺酸盐和0~0.5份羧酸酯混合为基本物质,再以基本物质按比例加入水搅拌,制得反浮选脱镁捕收剂。
11.根据权利要求10所述的一种磷矿浮选捕收剂的制备方法,其特征在于其制备过程中基本物质加入水搅拌,是在40-50℃温度、 800r/m的搅拌速度条件下,搅拌20min后制得反浮选脱镁捕收剂。
CN201410117916.5A 2014-03-27 2014-03-27 一种磷矿浮选捕收剂及其制备方法 Pending CN103831171A (zh)