CN103770175A - 木材的表面处理方法 - Google Patents

木材的表面处理方法 Download PDF

Info

Publication number
CN103770175A
CN103770175A CN201310668166.6A CN201310668166A CN103770175A CN 103770175 A CN103770175 A CN 103770175A CN 201310668166 A CN201310668166 A CN 201310668166A CN 103770175 A CN103770175 A CN 103770175A
Authority
CN
China
Prior art keywords
woods
timber
treatment method
shellac
surface treatment
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310668166.6A
Other languages
English (en)
Inventor
黄建荣
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
CHANGSHU XINLEI WOOD FACTORY
Original Assignee
CHANGSHU XINLEI WOOD FACTORY
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by CHANGSHU XINLEI WOOD FACTORY filed Critical CHANGSHU XINLEI WOOD FACTORY
Priority to CN201310668166.6A priority Critical patent/CN103770175A/zh
Publication of CN103770175A publication Critical patent/CN103770175A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种木材的表面处理方法,包括如下步骤:1)在43℃烘干木材,使木材的含水率控制在2%-2.5%.;2)先用精刨子刨切木材表面,再用砂纸打磨;3)在打磨好的木材表面涂覆虫胶清漆;4)在涂覆好虫胶清漆的木材表面涂覆虫胶腻子;5)将涂覆好虫胶腻子的木材通过砂纸打磨;6)在砂磨后的木材表面涂覆清漆。本发明能够有效地解决木材的表面缺陷,提高生产效率,降低成本。

Description

木材的表面处理方法
技术领域
本发明涉及木材的表面处理方法。
背景技术
木材表面一般都具有一系列的天然缺陷,包括钝碴、木毛、节子、裂纹、虫眼、伤痕等。另外,有些木材内含有单宁、松脂、树脂、挥发性油类与矿物质等,这些都会影响木材表面的清洁度。因此,在木材制成家具之前,需要对木材表面进行处理,以除去这些缺陷。现有的处理方法需采用有机溶剂对木材进行清洗、漂白等工艺,耗时长、效率低、成本大。 
发明内容
本发明的目的在于提供一种木材的表面处理方法,其能够有效地解决木材的表面缺陷,提高生产效率,降低成本。
为实现上述目的,本发明的技术方案是设计一种木材的表面处理方法,包括如下步骤:
1)在43℃烘干木材,使木材的含水率控制在2%-2.5%.;
2)先用精刨子刨切木材表面,再用砂纸打磨;
3)在打磨好的木材表面涂覆虫胶清漆;
4)在涂覆好虫胶清漆的木材表面涂覆虫胶腻子;
5)将涂覆好虫胶腻子的木材通过砂纸打磨;
6)在砂磨后的木材表面涂覆清漆。 
本发明的优点和有益效果在于:供一种木材的表面处理方法,其能够有效地解决木材的表面缺陷,提高生产效率,降低成本。
具体实施方式
下面结合实施例,对本发明的具体实施方式作进一步描述。以下实施例仅用于更加清楚地说明本发明的技术方案,而不能以此来限制本发明的保护范围。
本发明具体实施的技术方案是:
实施例1
一种木材的表面处理方法,包括如下步骤:
1)在43℃烘干木材,使木材的含水率控制在2%%.;
2)先用精刨子刨切木材表面,再用砂纸打磨;
3)在打磨好的木材表面涂覆虫胶清漆;
4)在涂覆好虫胶清漆的木材表面涂覆虫胶腻子;
5)将涂覆好虫胶腻子的木材通过砂纸打磨;
6)在砂磨后的木材表面涂覆清漆。
实施例2
一种木材的表面处理方法,包括如下步骤:
1)在43℃烘干木材,使木材的含水率控制在2.5%.;
2)先用精刨子刨切木材表面,再用砂纸打磨;
3)在打磨好的木材表面涂覆虫胶清漆;
4)在涂覆好虫胶清漆的木材表面涂覆虫胶腻子;
5)将涂覆好虫胶腻子的木材通过砂纸打磨;
6)在砂磨后的木材表面涂覆清漆。
实施例3
一种木材的表面处理方法,包括如下步骤:
1)在43℃烘干木材,使木材的含水率控制在2.3%.;
2)先用精刨子刨切木材表面,再用砂纸打磨;
3)在打磨好的木材表面涂覆虫胶清漆;
4)在涂覆好虫胶清漆的木材表面涂覆虫胶腻子;
5)将涂覆好虫胶腻子的木材通过砂纸打磨;
6)在砂磨后的木材表面涂覆清漆。
以上所述仅是本发明的优选实施方式,应当指出,对于本技术领域的普通技术人员来说,在不脱离本发明技术原理的前提下,还可以做出若干改进和润饰,这些改进和润饰也应视为本发明的保护范围。

Claims (1)

1.木材的表面处理方法,其特征在于,包括如下步骤:
1)在43℃烘干木材,使木材的含水率控制在2%-2.5%.;
2)先用精刨子刨切木材表面,再用砂纸打磨;
3)在打磨好的木材表面涂覆虫胶清漆;
4)在涂覆好虫胶清漆的木材表面涂覆虫胶腻子;
5)将涂覆好虫胶腻子的木材通过砂纸打磨;
6)在砂磨后的木材表面涂覆清漆。
CN201310668166.6A 2013-12-11 2013-12-11 木材的表面处理方法 Pending CN103770175A (zh)