CN103756026B CN201310646719.8A CN201310646719A CN103756026B CN 103756026 B CN103756026 B CN 103756026B CN 201310646719 A CN201310646719 A CN 201310646719A CN 103756026 B CN103756026 B CN 103756026B
Authority
CN
China
Prior art keywords
mixing
zinc oxide
ferrocene
vulcanization accelerator
ring
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201310646719.8A
Other languages
English (en)
Other versions
CN103756026A (zh
Inventor
连秉卫
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangdong Gaohang Intellectual Property Operation Co ltd
NANTONG JIUWANG ELECTRONIC Co.,Ltd.
Original Assignee
TONGLING RIXING ELECTRONICS Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TONGLING RIXING ELECTRONICS Co Ltd filed Critical TONGLING RIXING ELECTRONICS Co Ltd
Priority to CN201310646719.8A priority Critical patent/CN103756026B/zh
Publication of CN103756026A publication Critical patent/CN103756026A/zh
Application granted granted Critical
Publication of CN103756026B publication Critical patent/CN103756026B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Landscapes

  • Compositions Of Macromolecular Compounds (AREA)
  • Sealing Material Composition (AREA)

Abstract

本发明公开了一种电容器专用本发明橡胶料密封圈,其特征在于,由下列重量份的原料制成:天然橡胶64-68、丁苯橡胶32-34、氧化锌3-4、2,5-二甲基-2,5-双(过氧化叔丁基)己烷2-3、三烯丙基异氰尿酸酯2-3、硫化钡5-8、硫化锌3-5、炭黑34-38、纳米二氧化硅6-9、菜籽油2-5、促进剂TMTD?1.3-1.7、氧化锌1-2、氧化镁2-3、防老剂RD0.8-1.2、二茂铁1-2、改性凹凸棒土12-15;本发明添加改性凹凸棒土,改善了胶料的工艺性能,使用环保型配合剂,减少其毒副作用和对环境的污染;本发明具有良好的耐油耐压性,使用寿命长。

Description

一种电容器专用混炼胶密封圈及其制备方法
技术领域
本发明涉及橡胶复合材料加工领域,特别是一种电容器专用混炼胶密封圈及其制备方法。
背景技术
电容器通常简称为电容,是电子设备中大量使用的电子元件之一,广泛应用于电路的隔直通交、耦合、旁路、滤波、调谐回路、能量转换、控制等方面。电容器由壳体、电容芯子、端盖及接线端子组成,电容器壳体内装有浸渍介质,浸渍介质一般为植物油或矿物油,电容器的密封部位均设有密封垫或密封圈,由于电容器的工作环境千差万别,有的电容器需要在恶劣的环境下工作,电容器密封垫需要耐高温、耐寒、耐酸碱、耐盐雾等有不同要求。
发明内容
本发明的目的是提供一种电容器专用本发明橡胶料密封圈及其制备方法。
为了实现本发明的目的,本发明通过以下方案实施:
一种电容器专用本发明橡胶料密封圈,由下列重量份的原料制成:天然橡胶64-68、丁苯橡胶32-34、氧化锌3-4、2,5-二甲基-2,5-双(过氧化叔丁基)己烷2-3、三烯丙基异氰尿酸酯2-3、硫化钡5-8、硫化锌3-5、炭黑34-38、纳米二氧化硅6-9、菜籽油2-5、促进剂TMTD1.3-1.7、氧化锌1-2、氧化镁2-3、防老剂RD0.8-1.2、二茂铁1-2、改性凹凸棒土12-15;
所述改性凹凸棒土由下列重量份的原料制成:凹凸棒土20-24、甲苯二异氰酸酯3-4、二缩三丙二醇二丙烯酸酯2-3、粘土12-15、纳米二氧化钛3-4、氟化锆1-2、甲基三乙氧基硅烷1-2、二茂铁1-2、促进剂TMTD1-2、氢氧化铝8-10、2-氨基-2-甲基-1-丙醇2-3、花椒籽油1-2;制备方法是将凹凸棒土、粘土混合放入煅烧炉中在700-720℃下煅烧3-4小时,冷却,放入10-12%盐酸溶液中浸泡1-2小时,过滤取出,用清水洗净烘干,粉碎成200-300目粉末,与其它剩余成分混合,研磨分散1-2小时,即得。
本发明所述电容器专用本发明橡胶料密封圈,由以下具体步骤制成:将天然橡胶、丁苯橡胶、氧化锌、2,5-二甲基-2,5-双(过氧化叔丁基)己烷、三烯丙基异氰尿酸酯加入密炼机中,加热至80-90℃,混炼3-5min;然后升温至110-130℃,再加入硫化钡、硫化锌、炭黑、纳米二氧化硅、菜籽油、促进剂TMTD,混炼6-8min,再加入氧化锌、氧化镁、防老剂RD继续混炼4-6min,加入其余剩余成分混炼5-6min,即得本发明橡胶料。
本发明的优异效果是:本发明添加改性凹凸棒土,改善了胶料的工艺性能,使用环保型配合剂,减少其毒副作用和对环境的污染;本发明具有良好的耐油耐压性,使用寿命长。
具体实施方式
下面通过具体实例对本发明进行详细说明。
一种电容器专用本发明橡胶料密封圈,由下列重量份(公斤)的原料制成:天然橡胶64、丁苯橡胶32、氧化锌3、2,5-二甲基-2,5-双(过氧化叔丁基)己烷2、三烯丙基异氰尿酸酯2、硫化钡5、硫化锌3、炭黑34、纳米二氧化硅6、菜籽油2、促进剂TMTD1.3、氧化锌1、氧化镁2、防老剂RD0.8、二茂铁1、改性凹凸棒土12;
所述改性凹凸棒土由下列重量份(公斤)的原料制成:凹凸棒土20、甲苯二异氰酸酯3、二缩三丙二醇二丙烯酸酯2、粘土12、纳米二氧化钛3、氟化锆1、甲基三乙氧基硅烷1、二茂铁1、促进剂TMTD1、氢氧化铝8、2-氨基-2-甲基-1-丙醇2、花椒籽油1;制备方法是将凹凸棒土、粘土混合放入煅烧炉中在700-720℃下煅烧3-4小时,冷却,放入10-12%盐酸溶液中浸泡1-2小时,过滤取出,用清水洗净烘干,粉碎成200-300目粉末,与其它剩余成分混合,研磨分散1-2小时,即得。
本发明所述电容器专用本发明橡胶料密封圈,由以下具体步骤制成:将天然橡胶、丁苯橡胶、氧化锌、2,5-二甲基-2,5-双(过氧化叔丁基)己烷、三烯丙基异氰尿酸酯加入密炼机中,加热至80-90℃,混炼3-5min;然后升温至110-130℃,再加入硫化钡、硫化锌、炭黑、纳米二氧化硅、菜籽油、促进剂TMTD,混炼6-8min,再加入氧化锌、氧化镁、防老剂RD继续混炼4-6min,加入其余剩余成分混炼5-6min,即得本发明橡胶料。
用本发明的耐腐蚀橡胶密封圈与普通胶料物理性能对比如下表。
——————————————————————————————————————
从表中可以看出用本发明的橡胶密封圈产品,综合性能比较好。

Claims (2)

1.一种电容器专用混炼胶密封圈,其特征在于,由下列重量份的原料制成:天然橡胶64-68、丁苯橡胶32-34、氧化锌3-4、2,5-二甲基-2,5-双(过氧化叔丁基)己烷2-3、三烯丙基异氰尿酸酯2-3、硫化钡5-8、硫化锌3-5、炭黑34-38、纳米二氧化硅6-9、菜籽油2-5、促进剂TMTD1.3-1.7、氧化锌1-2、氧化镁2-3、防老剂RD0.8-1.2、二茂铁1-2、改性凹凸棒土12-15;
所述改性凹凸棒土由下列重量份的原料制成:凹凸棒土20-24、甲苯二异氰酸酯3-4、二缩三丙二醇二丙烯酸酯2-3、粘土12-15、纳米二氧化钛3-4、氟化锆1-2、甲基三乙氧基硅烷1-2、二茂铁1-2、促进剂TMTD1-2、氢氧化铝8-10、2-氨基-2-甲基-1-丙醇2-3、花椒籽油1-2;所述改性凹凸棒土的制备方法是将凹凸棒土、粘土混合放入煅烧炉中在700-720℃下煅烧3-4小时,冷却,放入10-12%盐酸溶液中浸泡1-2小时,过滤取出,用清水洗净烘干,粉碎成200-300目粉末,与甲苯二异氰酸酯、二缩三丙二醇二丙烯酸酯、纳米二氧化钛、氟化锆、甲基三乙氧基硅烷、二茂铁、促进剂TMTD、氢氧化铝、2-氨基-2-甲基-1-丙醇、花椒籽油混合,研磨分散1-2小时,即得。
2.根据权利要求1所述电容器专用混炼胶密封圈,其特征在于,由以下具体步骤制成:将天然橡胶、丁苯橡胶、氧化锌、2,5-二甲基-2,5-双(过氧化叔丁基)己烷、三烯丙基异氰尿酸酯加入密炼机中,加热至80-90℃,混炼3-5min;然后升温至110-130℃,再加入硫化钡、硫化锌、炭黑、纳米二氧化硅、菜籽油、促进剂TMTD,混炼6-8min,再加入氧化锌、氧化镁、防老剂RD继续混炼4-6min,加入二茂铁、改性凹凸棒土混炼5-6min,即得。
CN201310646719.8A 2013-12-04 2013-12-04 一种电容器专用混炼胶密封圈及其制备方法 Expired - Fee Related CN103756026B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201310646719.8A CN103756026B (zh) 2013-12-04 2013-12-04 一种电容器专用混炼胶密封圈及其制备方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201310646719.8A CN103756026B (zh) 2013-12-04 2013-12-04 一种电容器专用混炼胶密封圈及其制备方法

Publications (2)

Publication Number Publication Date
CN103756026A CN103756026A (zh) 2014-04-30
CN103756026B true CN103756026B (zh) 2016-02-17

Family

ID=50523364

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201310646719.8A Expired - Fee Related CN103756026B (zh) 2013-12-04 2013-12-04 一种电容器专用混炼胶密封圈及其制备方法

Country Status (1)

Country Link
CN (1) CN103756026B (zh)

Families Citing this family (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104086874B (zh) * 2014-07-01 2016-04-20 安徽江威精密制造有限公司 一种阻燃电容器薄膜专用填料及其制备方法
CN104086861B (zh) * 2014-07-01 2016-03-23 安徽江威精密制造有限公司 一种抗菌阻燃电容器薄膜专用填料及其制备方法
CN104086859B (zh) * 2014-07-01 2016-04-20 安徽江威精密制造有限公司 一种阻燃电容器薄膜专用填料及其制备方法
CN108912505A (zh) * 2018-06-04 2018-11-30 广州市美村橡胶科技有限公司 一种具有耐磨耐油耐酸碱腐蚀的食品级橡胶混炼胶混合材料及其制备方法

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101497026A (zh) * 2009-01-16 2009-08-05 江苏澳特邦非金属矿业有限公司 一种降低注射用大豆油茴香胺值的脱色剂及其制备方法
CN102617900A (zh) * 2012-04-10 2012-08-01 浙江天鸿汽车用品有限公司 无橡胶气味且具杀菌功能的橡胶制品组合物
CN102731848A (zh) * 2012-05-30 2012-10-17 芜湖荣基密封系统有限公司 一种耐磨多种橡胶混炼胶密封圈

Family Cites Families (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US8124206B2 (en) * 2008-10-30 2012-02-28 Momentive Performance Materials, Inc. Sulfur-containing cycloaliphatic compound, filled sulfur-vulcanizable elastomer composition containing sulfur-containing cycloaliphatic compound and articles fabricated therefrom

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101497026A (zh) * 2009-01-16 2009-08-05 江苏澳特邦非金属矿业有限公司 一种降低注射用大豆油茴香胺值的脱色剂及其制备方法
CN102617900A (zh) * 2012-04-10 2012-08-01 浙江天鸿汽车用品有限公司 无橡胶气味且具杀菌功能的橡胶制品组合物
CN102731848A (zh) * 2012-05-30 2012-10-17 芜湖荣基密封系统有限公司 一种耐磨多种橡胶混炼胶密封圈

Also Published As

Publication number Publication date
CN103756026A (zh) 2014-04-30

Similar Documents

Publication Publication Date Title
CN103694518B (zh) 一种耐氧化复合橡胶电容器密封圈及其制备方法
CN103601933B (zh) 一种电容器用耐油防腐橡胶密封圈及其制备方法
CN103613798B (zh) 一种电容器专用丁腈橡胶密封圈及其制备方法
CN103601991A (zh) 一种新型环保电容器用密封圈及其制备方法
CN103709561B (zh) 混合橡胶电容器密封圈及其制备方法
CN103601918B (zh) 一种高性能电容器橡胶密封圈及其制备方法
CN103756026B (zh) 一种电容器专用混炼胶密封圈及其制备方法
CN103601980B (zh) 一种绝缘耐油电容器用橡胶密封圈及其制备方法
CN103613796A (zh) 一种耐油防腐电容器密封圈及其制备方法
CN103694580B (zh) 一种混合橡胶电容器密封圈及其制备方法
CN103694577B (zh) 一种耐氧化电容器橡胶密封圈及其制备方法
CN103694608B (zh) 一种橡胶电容器密封圈及其制备方法
CN103613897A (zh) 一种丁腈橡胶电容器密封垫及其制备方法
CN103756073B (zh) 一种电容器专用混炼橡胶密封垫及其制备方法
CN103756027A (zh) 一种新型混合橡胶电容器密封圈及其制备方法
CN103601926A (zh) 一种高强度电容器用橡胶密封垫及其制备方法
CN103694519B (zh) 一种丁腈橡胶电容器密封圈及其制备方法
CN103724842A (zh) 一种耐磨橡胶电容器密封圈及其制备方法
CN103601931B (zh) 一种电容器混炼胶密封垫及其制备方法
CN103613857B (zh) 一种绝缘耐油橡胶电容器密封圈及其制备方法
CN103627049A (zh) 一种电容器专用丁腈橡胶密封垫及其制备方法
CN103725016A (zh) 一种多种橡胶混炼胶电容器专用密封圈及其制备方法
CN103613864B (zh) 一种电容器用混炼橡胶密封圈及其制备方法
CN103613891A (zh) 一种电容器专用橡胶密封圈及其制备方法
CN103627118A (zh) 一种电容器橡胶密封垫及其制备方法

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
TR01 Transfer of patent right

Effective date of registration: 20170608

Address after: 226500, Nantong City, Jiangsu province Rugao City North Street Community Deng village 15 group, Rugao science and Technology Pioneer Park, building four, building A, block 1

Patentee after: NANTONG JIUWANG ELECTRONIC Co.,Ltd.

Address before: 510000 unit 2414-2416, building, No. five, No. 371, Tianhe District, Guangdong, China

Patentee before: GUANGDONG GAOHANG INTELLECTUAL PROPERTY OPERATION Co.,Ltd.

Effective date of registration: 20170608

Address after: 510000 unit 2414-2416, building, No. five, No. 371, Tianhe District, Guangdong, China

Patentee after: GUANGDONG GAOHANG INTELLECTUAL PROPERTY OPERATION Co.,Ltd.

Address before: 244000 Private Industrial Park, Anhui, Tongling

Patentee before: TONGLING RIXING ELECTRONICS Co.,Ltd.

TR01 Transfer of patent right
CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20160217

Termination date: 20201204

CF01 Termination of patent right due to non-payment of annual fee