CN103694518B - 一种耐氧化复合橡胶电容器密封圈及其制备方法 - Google Patents

一种耐氧化复合橡胶电容器密封圈及其制备方法 Download PDF

Info

Publication number
CN103694518B
CN103694518B CN201310646683.3A CN201310646683A CN103694518B CN 103694518 B CN103694518 B CN 103694518B CN 201310646683 A CN201310646683 A CN 201310646683A CN 103694518 B CN103694518 B CN 103694518B
Authority
CN
China
Prior art keywords
resistance
carbon black
stearic acid
mixing
oxidation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201310646683.3A
Other languages
English (en)
Other versions
CN103694518A (zh
Inventor
连秉卫
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangdong Gaohang Intellectual Property Operation Co ltd
NANTONG JIUWANG ELECTRONIC Co.,Ltd.
Original Assignee
TONGLING RIXING ELECTRONICS Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TONGLING RIXING ELECTRONICS Co Ltd filed Critical TONGLING RIXING ELECTRONICS Co Ltd
Priority to CN201310646683.3A priority Critical patent/CN103694518B/zh
Publication of CN103694518A publication Critical patent/CN103694518A/zh
Application granted granted Critical
Publication of CN103694518B publication Critical patent/CN103694518B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种耐氧化复合橡胶电容器密封圈,其特征在于,由下列重量份的原料制成:丁腈橡胶45-50、三元乙丙橡胶45-50、防老剂MB?2-3、硬脂酸3-4、石蜡8-10、增塑剂DOP?4-5、白炭黑23-27、氢氧化铝12-14、三氧化二锑4-6、硬脂酸锌8-12、氧化锌2-3、偶联剂1.5-2.5、硬脂酸2.2-2.4、N330炭黑35-38、改性凹凸棒土12-15;本发明添加改性凹凸棒土,改善了胶料的工艺性能,使用环保型配合剂,减少其毒副作用和对环境的污染;本发明具有良好的耐氧化性、耐老化性、耐油性以及阻燃性,成本低。

Description

一种耐氧化复合橡胶电容器密封圈及其制备方法
技术领域
本发明涉及橡胶复合材料加工领域,特别是一种耐氧化复合橡胶电容器密封圈及其制备方法。
背景技术
电容器通常简称为电容,是电子设备中大量使用的电子元件之一,广泛应用于电路的隔直通交、耦合、旁路、滤波、调谐回路、能量转换、控制等方面。电容器由壳体、电容芯子、端盖及接线端子组成,电容器壳体内装有浸渍介质,浸渍介质一般为植物油或矿物油,电容器的密封部位均设有密封垫或密封圈,由于电容器的工作环境千差万别,有的电容器需要在恶劣的环境下工作,电容器密封垫需要耐高温、耐寒、耐酸碱、耐盐雾等有不同要求。
发明内容
本发明的目的是提供一种耐氧化复合橡胶电容器密封圈及其制备方法。
为了实现本发明的目的,本发明通过以下方案实施:
一种耐氧化复合橡胶电容器密封圈,由下列重量份的原料制成:丁腈橡胶45-50、三元乙丙橡胶45-50、防老剂MB2-3、硬脂酸3-4、石蜡8-10、增塑剂DOP4-5、白碳黑23-27、氢氧化铝12-14、三氧化二锑4-6、硬脂酸锌8-12、氧化锌2-3、偶联剂1.5-2.5、硬脂酸2.2-2.4、N330炭黑35-38、改性凹凸棒土12-15;
所述改性凹凸棒土由下列重量份的原料制成:凹凸棒土20-24、甲苯二异氰酸酯3-4、二缩三丙二醇二丙烯酸酯2-3、粘土12-15、纳米二氧化钛3-4、氟化锆1-2、甲基三乙氧基硅烷1-2、二茂铁1-2、促进剂TMTD1-2、氢氧化铝8-10、2-氨基-2-甲基-1-丙醇2-3、花椒籽油1-2;制备方法是将凹凸棒土、粘土混合放入煅烧炉中在700-720℃下煅烧3-4小时,冷却,放入10-12%盐酸溶液中浸泡1-2小时,过滤取出,用清水洗净烘干,粉碎成200-300目粉末,与其它剩余成分混合,研磨分散1-2小时,即得。
本发明所述耐氧化复合橡胶电容器密封圈,由以下具体步骤制成:将丁腈橡胶、三元乙丙橡胶、防老剂MB、硬脂酸、石蜡加入密炼机中,加热至80-90℃,混炼3-5min;然后升温至110-130℃,再加入增塑剂DOP、白碳黑、氢氧化铝、三氧化二锑、硬脂酸锌、氧化锌,混炼6-8min,再加入偶联剂、硬脂酸、N330炭黑继续混炼4-6min,加入其余剩余成分混炼6-8min,即得本发明橡胶料。
本发明的优异效果是:本发明添加改性凹凸棒土,改善了胶料的工艺性能,使用环保型配合剂,减少其毒副作用和对环境的污染;本发明具有良好的耐氧化性、耐老化性、耐油性以及阻燃性,成本低。
具体实施方式
下面通过具体实例对本发明进行详细说明。
一种耐氧化复合橡胶电容器密封圈,由下列重量份(公斤)的原料制成:丁腈橡胶45、三元乙丙橡胶45、防老剂MB2、硬脂酸3、石蜡8、增塑剂DOP4、白碳黑23、氢氧化铝12、三氧化二锑4、硬脂酸锌8、氧化锌2、偶联剂1.5、硬脂酸2.2、N330炭黑35、改性凹凸棒土12;
所述改性凹凸棒土由下列重量份(公斤)的原料制成:凹凸棒土20、甲苯二异氰酸酯3、二缩三丙二醇二丙烯酸酯2、粘土12、纳米二氧化钛3、氟化锆1、甲基三乙氧基硅烷1、二茂铁1、促进剂TMTD1、氢氧化铝8、2-氨基-2-甲基-1-丙醇2、花椒籽油1;制备方法是将凹凸棒土、粘土混合放入煅烧炉中在700-720℃下煅烧3-4小时,冷却,放入10-12%盐酸溶液中浸泡1-2小时,过滤取出,用清水洗净烘干,粉碎成200-300目粉末,与其它剩余成分混合,研磨分散1-2小时,即得。
本发明所述耐氧化复合橡胶电容器密封圈,由以下具体步骤制成:将丁腈橡胶、三元乙丙橡胶、防老剂MB、硬脂酸、石蜡加入密炼机中,加热至80-90℃,混炼3-5min;然后升温至110-130℃,再加入增塑剂DOP、白碳黑、氢氧化铝、三氧化二锑、硬脂酸锌、氧化锌,混炼6-8min,再加入偶联剂、硬脂酸、N330炭黑继续混炼4-6min,加入其余剩余成分混炼6-8min,即得本发明橡胶料。
用本发明的耐腐蚀橡胶密封圈与普通胶料物理性能对比如下表。
从表中可以看出用本发明的橡胶密封圈产品,综合性能比较好。

Claims (2)

1.一种耐氧化复合橡胶电容器密封圈,其特征在于,由下列重量份的原料制成:丁腈橡胶45-50、三元乙丙橡胶45-50、防老剂MB2-3、硬脂酸3-4、石蜡8-10、增塑剂DOP4-5、白炭黑23-27、氢氧化铝12-14、三氧化二锑4-6、硬脂酸锌8-12、氧化锌2-3、偶联剂1.5-2.5、硬脂酸2.2-2.4、N330炭黑35-38、改性凹凸棒土12-15;
所述改性凹凸棒土由下列重量份的原料制成:凹凸棒土20-24、甲苯二异氰酸酯3-4、二缩三丙二醇二丙烯酸酯2-3、粘土12-15、纳米二氧化钛3-4、氟化锆1-2、甲基三乙氧基硅烷1-2、二茂铁1-2、促进剂TMTD1-2、氢氧化铝8-10、2-氨基-2-甲基-1-丙醇2-3、花椒籽油1-2;制备方法是将凹凸棒土、粘土混合放入煅烧炉中在700-720℃下煅烧3-4小时,冷却,放入10-12%盐酸溶液中浸泡1-2小时,过滤取出,用清水洗净烘干,粉碎成200-300目粉末,与剩余成分混合,研磨分散1-2小时,即得。
2.根据权利要求1所述耐氧化复合橡胶电容器密封圈,其特征在于,由以下具体步骤制成:将丁腈橡胶、三元乙丙橡胶、防老剂MB、硬脂酸、石蜡加入密炼机中,加热至80-90℃,混炼3-5min;然后升温至110-130℃,再加入增塑剂DOP、白炭黑、氢氧化铝、三氧化二锑、硬脂酸锌、氧化锌,混炼6-8min,再加入偶联剂、硬脂酸、N330炭黑继续混炼4-6min,加入剩余成分混炼6-8min,即得。
CN201310646683.3A 2013-12-04 2013-12-04 一种耐氧化复合橡胶电容器密封圈及其制备方法 Expired - Fee Related CN103694518B (zh)