CN103601933B - 一种电容器用耐油防腐橡胶密封圈及其制备方法 - Google Patents

一种电容器用耐油防腐橡胶密封圈及其制备方法 Download PDF

Info

Publication number
CN103601933B
CN103601933B CN201310520341.7A CN201310520341A CN103601933B CN 103601933 B CN103601933 B CN 103601933B CN 201310520341 A CN201310520341 A CN 201310520341A CN 103601933 B CN103601933 B CN 103601933B
Authority
CN
China
Prior art keywords
powder
mixing
oil resistance
rubber seal
rubber
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310520341.7A
Other languages
English (en)
Other versions
CN103601933A (zh
Inventor
王进
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ANHUI KING-AUTO ELECTRONIC TECHNOLOGY CO., LTD.
Original Assignee
ANHUI QIAITE ELECTRONIC TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ANHUI QIAITE ELECTRONIC TECHNOLOGY Co Ltd filed Critical ANHUI QIAITE ELECTRONIC TECHNOLOGY Co Ltd
Priority to CN201310520341.7A priority Critical patent/CN103601933B/zh
Publication of CN103601933A publication Critical patent/CN103601933A/zh
Application granted granted Critical
Publication of CN103601933B publication Critical patent/CN103601933B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种电容器用耐油防腐橡胶密封圈,其特征在于,由下列重量份的原料制成:氯丁橡胶(CR121)65-75、丁基橡胶(CBK139)30-35、海泡石粉14-18、蛭石粉5-8、天然橡胶10-12、氯化钙3-5、氯化亚铜2-3、硅藻粉5-8、膨润土粉4-5、氧化锌2-3、N330炭黑34-38、沉淀法白炭黑16-20、交联剂?TAIC?1-2、3-氨丙基三甲氧基硅烷1-2、促进剂DM??3-4、改性凹凸棒土10-12;本发明添加改性凹凸棒土,改善了胶料的工艺性能,使用环保型配合剂,减少其毒副作用和对环境的污染;本发明成本低,使用寿命长,而且具有良好的耐油、耐腐蚀性。

Description

一种电容器用耐油防腐橡胶密封圈及其制备方法
技术领域
本发明涉及橡胶复合材料加工领域,特别是一种电容器用耐油防腐橡胶密封圈及其制备方法。
背景技术
电容器通常简称为电容,是电子设备中大量使用的电子元件之一,广泛应用于电路的隔直通交、耦合、旁路、滤波、调谐回路、能量转换、控制等方面。电容器由壳体、电容芯子、端盖及接线端子组成,电容器壳体内装有浸渍介质,浸渍介质一般为植物油或矿物油,电容器的密封部位均设有密封垫或密封圈,由于电容器的工作环境千差万别,有的电容器需要在恶劣的环境下工作,电容器密封垫需要耐高温、耐寒、耐酸碱、耐盐雾等有不同要求。
发明内容
本发明的目的是提供一种电容器用耐油防腐橡胶密封圈及其制备方法。
为了实现本发明的目的,本发明通过以下方案实施:
一种电容器用耐油防腐橡胶密封圈,由下列重量份的原料制成:氯丁橡胶(CR121)65-75、丁基橡胶(CBK139)30-35、海泡石粉14-18、蛭石粉5-8、天然橡胶10-12、氯化钙3-5、氯化亚铜2-3、硅藻粉5-8、膨润土粉4-5、氧化锌2-3、N330炭黑34-38、沉淀法白炭黑16-20、交联剂TAIC1-2、3-氨丙基三甲氧基硅烷1-2、促进剂DM3-4、改性凹凸棒土10-12;
所述改性凹凸棒土由下列重量份的原料制成:凹凸棒土20-24、甲苯二异氰酸酯3-4、双季戊四醇六丙烯酸酯2-3、硅藻土3-4、甲基三乙氧基硅烷2-3、海泡石10-12、氟化锆1-2、丁香油2-3、抗坏血酸1-2、高岭土3-4、丙烯酸-2-羟基丙酯2-3、刚玉粉2-3、花椒籽油1-2;制备方法是将凹凸棒土、硅藻土、海泡石、高岭土混合放入煅烧炉中在700-720℃下煅烧3-4小时,冷却,放入10-12%盐酸溶液中浸泡1-2小时,过滤取出,用清水洗净烘干,粉碎成200-300目粉末,与其它剩余成分混合,研磨分散1-2小时,即得。
本发明所述电容器用耐油防腐橡胶密封圈,由以下具体步骤制成:将丁基橡胶(CBK139)、海泡石粉、蛭石粉加入密炼机中,加热至130-150℃,混炼3-5min;然后降温至80-90℃,再加入氯丁橡胶(CR121)、天然橡胶、氯化钙、氯化亚铜、硅藻粉、膨润土粉、氧化锌,混炼6-8min,再加入N330炭黑、沉淀法白炭黑、交联剂TAIC、3-氨丙基三甲氧基硅烷继续混炼4-6min,加入其余剩余成分混炼4-6min,即得本发明橡胶料。
本发明的优异效果是:本发明添加改性凹凸棒土,改善了胶料的工艺性能,使用环保型配合剂,减少其毒副作用和对环境的污染;本发明成本低,使用寿命长,而且具有良好的耐油、耐腐蚀性。
具体实施方式
下面通过具体实例对本发明进行详细说明。
一种电容器用耐油防腐橡胶密封圈,由下列重量份(公斤)的原料制成:氯丁橡胶(CR121)65、丁基橡胶(CBK139)30、海泡石粉14、蛭石粉5、天然橡胶10、氯化钙3、氯化亚铜2、硅藻粉5、膨润土粉4、氧化锌2、N330炭黑34、沉淀法白炭黑16、交联剂TAIC1、3-氨丙基三甲氧基硅烷1、促进剂DM3、改性凹凸棒土10;
所述改性凹凸棒土由下列重量份(公斤)的原料制成:凹凸棒土20、甲苯二异氰酸酯3、双季戊四醇六丙烯酸酯2、硅藻土3、甲基三乙氧基硅烷2、海泡石10、氟化锆1、丁香油2、抗坏血酸1、高岭土3、丙烯酸-2-羟基丙酯2、刚玉粉2、花椒籽油1;制备方法是将凹凸棒土、硅藻土、海泡石、高岭土混合放入煅烧炉中在700-720℃下煅烧3-4小时,冷却,放入10-12%盐酸溶液中浸泡1-2小时,过滤取出,用清水洗净烘干,粉碎成200-300目粉末,与其它剩余成分混合,研磨分散1-2小时,即得。
本发明所述电容器用耐油防腐橡胶密封圈,由以下具体步骤制成:将丁基橡胶(CBK139)、海泡石粉、蛭石粉加入密炼机中,加热至130-150℃,混炼3-5min;然后降温至80-90℃,再加入氯丁橡胶(CR121)、天然橡胶、氯化钙、氯化亚铜、硅藻粉、膨润土粉、氧化锌,混炼6-8min,再加入N330炭黑、沉淀法白炭黑、交联剂TAIC、3-氨丙基三甲氧基硅烷继续混炼4-6min,加入其余剩余成分混炼4-6min,即得本发明橡胶料。
用本发明的耐腐蚀橡胶密封圈与普通胶料物理性能对比如下表。
从表中可以看出用本发明的橡胶密封圈产品,综合性能比较好。

Claims (2)

1.一种电容器用耐油防腐橡胶密封圈,其特征在于,由下列重量份的原料制成:氯丁橡胶CR12165-75、丁基橡胶CBK13930-35、海泡石粉14-18、蛭石粉5-8、天然橡胶10-12、氯化钙3-5、氯化亚铜2-3、硅藻粉5-8、膨润土粉4-5、氧化锌2-3、N330炭黑34-38、沉淀法白炭黑16-20、交联剂TAIC1-2、3-氨丙基三甲氧基硅烷1-2、促进剂DM3-4、改性凹凸棒土10-12;
所述改性凹凸棒土由下列重量份的原料制成:凹凸棒土20-24、甲苯二异氰酸酯3-4、双季戊四醇六丙烯酸酯2-3、硅藻土3-4、甲基三乙氧基硅烷2-3、海泡石10-12、氟化锆1-2、丁香油2-3、抗坏血酸1-2、高岭土3-4、丙烯酸-2-羟基丙酯2-3、刚玉粉2-3、花椒籽油1-2;制备方法是将凹凸棒土、硅藻土、海泡石、高岭土混合放入煅烧炉中在700-720℃下煅烧3-4小时,冷却,放入10-12%盐酸溶液中浸泡1-2小时,过滤取出,用清水洗净烘干,粉碎成200-300目粉末,与其它剩余成分混合,研磨分散1-2小时,即得。
2.根据权利要求1所述电容器用耐油防腐橡胶密封圈,其特征在于,由以下具体步骤制成:将丁基橡胶CBK139、海泡石粉、蛭石粉加入密炼机中,加热至130-150℃,混炼3-5min;然后降温至80-90℃,再加入氯丁橡胶CR121、天然橡胶、氯化钙、氯化亚铜、硅藻粉、膨润土粉、氧化锌,混炼6-8min,再加入N330炭黑、沉淀法白炭黑、交联剂TAIC、3-氨丙基三甲氧基硅烷继续混炼4-6min,加入其余剩余成分混炼4-6min,即得电容器用耐油防腐橡胶密封圈。
CN201310520341.7A 2013-10-28 2013-10-28 一种电容器用耐油防腐橡胶密封圈及其制备方法 Active CN103601933B (zh)