CN103462266A - 一种在服饰上热转印硅胶的工序 - Google Patents
一种在服饰上热转印硅胶的工序 Download PDFInfo
- Publication number
- CN103462266A CN103462266A CN2013104308958A CN201310430895A CN103462266A CN 103462266 A CN103462266 A CN 103462266A CN 2013104308958 A CN2013104308958 A CN 2013104308958A CN 201310430895 A CN201310430895 A CN 201310430895A CN 103462266 A CN103462266 A CN 103462266A
- Authority
- CN
- China
- Prior art keywords
- silica gel
- transfer printing
- hot transfer
- hot
- dress ornament
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种在服饰上热转印硅胶的工序。目前在服饰上印刷有硅胶制成的商标和图案工艺步骤复杂,生产效率较低,难以满足大批量、低成本的生产需要。本发明其特征在于包括如下步骤:(1)先用电脑把图形制作好然后导入激光机软件,调试好激光火力后激光雕刻图形,并在热转印载体上按设定大小的图案或字体形状将硅胶固化,制成硅胶制品;(2)将硅胶制品底部垫纸撕下,用定位纸格定位好后贴在裁片上;(3)将需要转烫的裁片平铺在烫板上,转烫机自动转烫,待转烫到预定时间后,主控制器自动升起,拿出裁片,再将裁片反面进行转烫。本发明的热转印硅胶制品的方法,操作工序步骤简单,容易操作实施,能够有效地控制硅胶制品的质量。
Description
技术领域
本发明涉及服饰制作领域,更具体地涉及一种在服饰上热转印硅胶的工序。
背景技术
目前在服饰上印刷有硅胶制成的商标和图案等往往是通过传统的印刷方法完成。即直接在纺织品上印刷硅胶制品,由于直接在服饰品上印刷硅胶制品,如果在印刷的过程中,硅胶制品成型不佳或服饰品位置或其他因素出现意外状况的时候,均会导致硅胶制品和服饰品的结合出现问题,降低产品质量,外观受到影响,增加了生产成本,并且这样的传统印刷方法,由于在印刷的过程中需要直接在服饰上印刷成型硅胶制品,工艺步骤复杂,生产效率较低,并且印刷的质量不够稳定,难以满足大批量、低成本的生产需要。
发明内容
本发明的目的是克服现有技术的不足,提供一种在服饰上热转印硅胶的工序,工序简单,操作方便,制出的服饰产品质量较高,外形佳。
为此,本发明采取如下技术方案:一种在服饰上热转印硅胶的工序,其特征在于包括如下步骤:
(1)先用电脑把图形制作好然后导入激光机软件,输出进入激光机系统,调试好激光火力后激光雕刻图形,并在热转印载体上按设定大小的图案或字体形状将硅胶固化,制成硅胶制品;
(2)将硅胶制品底部垫纸撕下,用定位纸格定位好后贴在裁片上;
(3)将需要转烫的裁片平铺在烫板上,将烫板推到主控制器下,转烫机自动转烫,待转烫到预定时间后,主控制器自动升起,拿出裁片,再将裁片反面进行转烫。
所述的转烫机的转烫温度为155~160度;正面转烫和反面转烫的时间为15~16秒。
所述转烫机的压力设置为0.5pa。
所述的转印载体为PET膜。
所述的硅胶为道康宁3631液体硅橡胶。
所述步骤(1) 中,能一次性在一热转印载体上制成若干个硅胶制品。
所述的裁片包括尼龙,布类,纺织品类、皮类等各类服饰品。
本发明的热转印硅胶制品的方法,操作工序步骤简单,容易操作实施,能够有效地控制硅胶制品的质量。采用本发明的工艺步骤和参数制出的服饰品与硅胶之间结合更为紧密贴合,全方位提升了产品品质,外观较佳。本发明采用的道康宁3631液体硅橡胶延伸率好,气味小,同时具有较好的防滑作用,不含溶剂,污染小。
具体实施例
下面结合具体实施例,进一步阐述本发明。
一种在服饰上热转印硅胶的工序,包括如下步骤:(1)先用电脑把图形制作好然后导入激光机软件,输出进入激光机系统,调试好激光火力后激光雕刻图形,将硅胶与固化剂按比例调配好,并在热转印载体上按设定大小的图案或字体形状将该硅胶固化,制成硅胶制品;(2)将硅胶制品底部垫纸撕下,用定位纸格定位好后贴在裁片上;(3)将需要转烫的裁片平铺在烫板上,将烫板推到主控制器下,用手再按一下硅胶制品以确保贴在裁片上的牢固度和转烫的位置正确。转烫机自动转烫,待转烫到预定时间后,主控制器自动升起,拿出裁片,再将裁片反面进行转烫。检查转烫好后的裁片,确认橡胶logo是否有烫牢固,如发现不牢固可再进行加烫一次。待裁片冷确后,再轻轻撕下LOGO表面的保护膜,可以待后工序完成后再撕下保护膜,以保护LOGO在后序的加工过程中不会被损坏和弄脏。
其中在转烫前先对机器的参数进行设置,转烫机的转烫温度为155~160度;正面转烫和反面转烫的时间为15~16秒,烫机的压力设置为0.5pa。
转印载体为PET膜,硅胶采用道康宁3631液体硅橡胶,裁片包括尼龙,布类,纺织品类、皮类等各类服饰品。
本发明可以先一次性同时在转印载体上大批量制成多个硅胶制品,然后再将硅胶制品转移印刷到纺织品上,该方法工序步骤简单,容易操作实施,能够有效地控制硅胶制品的质量。本发明采用的道康宁3631液体硅橡胶延伸率好,气味小,同时具有较好的防滑作用,不含溶剂。
需要特别指出的是,上述实施例的方式仅限于描述实施例,但本发明不止局限于上述方式,且本领域的技术人员据此可在不脱离本发明的范围内方便的进行修饰,因此本发明的范围应当包括本发明所揭示的原理和新特征的最大范围。
Claims (7)
1.一种在服饰上热转印硅胶的工序,其特征在于包括如下步骤:
(1)先用电脑把图形制作好然后导入激光机软件,输出进入激光机系统,调试好激光火力后激光雕刻图形,并在热转印载体上按设定大小的图案或字体形状将硅胶固化,制成硅胶制品;
(2)将硅胶制品底部垫纸撕下,用定位纸格定位好后贴在裁片上;
(3)将需要转烫的裁片平铺在转烫机的烫板上,将烫板推到主控制器下,转烫机自动转烫,待转烫到预定时间后,主控制器自动升起,拿出裁片,再将裁片反面进行转烫。
2.如权利要求1所述的一种在服饰上热转印硅胶的工序,其特征在于所述的转烫机的转烫温度为155~160度;正面转烫和反面转烫的时间为15~16秒。
3.如权利要求2所述的一种在服饰上热转印硅胶的工序,其特征在于所述转烫机的压力设置为0.5pa。
4.如权利要求3所述的一种在服饰上热转印硅胶的工序,其特征在于所述的热转印载体为PET膜。
5.如权利要求4所述的一种在服饰上热转印硅胶的工序,其特征在于所述的硅胶为道康宁3631液体硅橡胶。
6.如权利要求1所述的一种在服饰上热转印硅胶的工序,其特征在于所述步骤(1) 中,能一次性在一热转印载体上制成若干个硅胶制品。
7.如权利要求1所述的一种在服饰上热转印硅胶的工序,其特征在于所述的裁片包括尼龙,布类,纺织品类、皮类。