CN103435004A - 基于模板复制技术的表面增强拉曼活性基底制备方法 - Google Patents
基于模板复制技术的表面增强拉曼活性基底制备方法 Download PDFInfo
- Publication number
- CN103435004A CN103435004A CN2013103169801A CN201310316980A CN103435004A CN 103435004 A CN103435004 A CN 103435004A CN 2013103169801 A CN2013103169801 A CN 2013103169801A CN 201310316980 A CN201310316980 A CN 201310316980A CN 103435004 A CN103435004 A CN 103435004A
- Authority
- CN
- China
- Prior art keywords
- polymetylmethacrylate
- caster
- active substrate
- nano
- layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (9)