- CN103246089A CN103246089A CN2012102494577A CN201210249457A CN103246089A CN 103246089 A CN103246089 A CN 103246089A CN 2012102494577 A CN2012102494577 A CN 2012102494577A CN 201210249457 A CN201210249457 A CN 201210249457A CN 103246089 A CN103246089 A CN 103246089A
- Authority
- CN
- China
- Prior art keywords
- front frame
- frame
- moulding mixture
- sheet
- laser welding
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Images
Abstract
本发明涉及一种液晶显示面板用前框及镭焊工艺,包括以下步骤:1)冲压加工:将原材料经模具冲压成完全相同的L型料片;2)激光拼焊:将L型料片用激光拼焊机焊接成中空的矩型前框;步骤1)所述L型料片的两端为直端。采用本发明的液晶显示面板用五金前框,原材料经冲压加工后,可以用拼焊加工的方法焊接成中空的前框结构,改变原有的由一整片原材料片进行加工,再将中间部分剥离掉,浪费大片中间废料的情况,达到节省材料的目的,材料利用率可由70%提高到90%,节约了生产成本;改变了原有的由两大小形状不一致的L型料片对焊形成前框的方法,采用完全相同的L型料片焊接形成前框,且无需进行倒角设计,制造工艺简单。
Description
技术领域
本发明涉及一种液晶显示面板用前框及镭焊工艺。
背景技术
随着液晶显示器( Liquid Crystal Display,简称LCD)市场的扩大,LCD中背光模组类产品的生产加工量逐渐增大。五金件前框、背板是背光模组类产品中必不可少的零组件,五金冲压行业中生产五金件前框、背板的厂商大幅增加,对原材料的需求也水涨船高。目前的前框结构在生产前框类产品时,需使用一整片原材料片进行加工,再将中间部分剥离冲掉,约70%材料以中间废料的形式被浪费掉,导致原材料利用率较低,不利于节约材料成本,无形中增加了生产成本。本发明的申请人设计了一种液晶显示面板用五金前框(申请号201110083042.2),该前框由两大小形状不一致的L型料片对焊形成,料片的端部结构不同,某些部分还需进行倒角设计,制作加工较为繁琐。
发明内容
本发明的目的在于克服上述问题,提供一种新型的液晶显示面板用前框及镭焊工艺,提高原材料利用率,节约材料成本,制造工艺简单。
为实现上述目的,本发明所采用的技术方案为: 液晶显示面板用前框,其特征在于:包括两片完全相同的L型料片,两片L型料片对焊成中空的矩形前框。
前述的液晶显示面板用前框,所述的L型料片的两端为直端。
前述的液晶显示面板用前框,所述的矩形前框的大小为15英寸以上。
液晶显示面板用前框镭焊工艺,包括以下步骤:1)冲压加工:将原材料经模具冲压成完全相同的L型料片;2)激光拼焊:将L型料片用激光拼焊机焊接成中空的矩型前框。
前述的液晶显示面板用前框镭焊工艺,步骤1)所述L型料片的两端为直端。
本发明的有益效果为:采用本发明的液晶显示面板用五金前框,原材料经冲压加工后,可以用拼焊加工的方法焊接成中空的前框结构,改变原有的由一整片原材料片进行加工,再将中间部分剥离掉,浪费大片中间废料的情况,达到节省材料的目的,材料利用率可由70%提高到90%,节约了生产成本;改变了原有的由两大小形状不一致的L型料片对焊形成前框的方法,采用完全相同的L型料片焊接形成前框,且无需进行倒角设计,制造工艺简单。
附图说明
图1是本发明原材料的冲压示意图;
图2是本发明液晶显示面板用前框示意图;
图3为图2中L型料片的焊接位置示意图;
其中,1原材料,2 L型料片,3直端。
具体实施方式
图为本发明的优选实施例,下面结合附图对本发明作进一步描述:其中,1原材料,2 L型料片,3直端。
根据图1-图3,液晶显示面板用前框,其特征在于:包括两片完全相同的L型料片2,两片L型料片2对焊成中空的矩形前框。L型料片2的两端为直端3。
矩形前框的大小为15英寸以上。
液晶显示面板用前框镭焊工艺,包括以下步骤:1)冲压加工:将原材料1经模具冲压成完全相同的L型料片2;2)激光拼焊:将L型料片2用激光拼焊机焊接成中空的矩型前框。
前述的液晶显示面板用前框镭焊工艺,步骤1)所述L型料片2的两端为直端3。
采用本发明的液晶显示面板用五金前框,原材料1经冲压加工后,可以用拼焊加工的方法焊接成中空的前框结构,改变原有的由一整片原材料片进行加工,再将中间部分剥离掉,浪费大片中间废料的情况,达到节省材料的目的,材料利用率可由70%提高到90%,节约了生产成本;改变了原有的由两大小形状不一致的L型料片对焊形成前框的方法,采用完全相同的L型料片焊接形成前框,且无需进行倒角设计,制造工艺简单。
上述实施例不以任何形式限制本发明,凡采用等同替换或等效变换的方式所获得的技术方案,均落在本发明的保护范围内。
Claims (5)
1.液晶显示面板用前框,其特征在于:包括两片完全相同的L型料片,两片L型料片对焊成中空的矩形前框。
2. 根据权利要求1所述的液晶显示面板用前框,其特征在于:所述的L型料片的两端为直端。
3. 根据权利要求2所述的液晶显示面板用前框,其特征在于:所述的矩形前框的大小为10.1英寸以上。
4. 液晶显示面板用前框镭焊工艺,其特征在于,包括以下步骤:1)冲压加工:将原材料经模具冲压成完全相同的L型料片;2)激光拼焊:将L型料片用激光拼焊机焊接成中空的矩型前框。
5. 根据权利要求4所述的液晶显示面板用前框镭焊工艺,其特征在于:步骤1)所述L型料片的两端为直端。
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN2012102494577A CN103246089A (zh) | 2012-07-19 | 2012-07-19 | 液晶显示面板用前框及镭焊工艺 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN2012102494577A CN103246089A (zh) | 2012-07-19 | 2012-07-19 | 液晶显示面板用前框及镭焊工艺 |
Publications (1)
Publication Number | Publication Date |
---|---|
CN103246089A true CN103246089A (zh) | 2013-08-14 |
Family
ID=48925709
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CN2012102494577A Pending CN103246089A (zh) | 2012-07-19 | 2012-07-19 | 液晶显示面板用前框及镭焊工艺 |
Country Status (1)
Country | Link |
---|---|
CN (1) | CN103246089A (zh) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN103439811A (zh) * | 2013-08-20 | 2013-12-11 | 乐视致新电子科技(天津)有限公司 | 一种显示设备边框的制作方法及显示设备 |
Citations (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US6231202B1 (en) * | 1998-08-20 | 2001-05-15 | Matsushita Electric Industrial Co., Ltd. | Lighting unit and liquid crystal display device using the same |
JP2002290079A (ja) * | 2001-03-26 | 2002-10-04 | Matsushita Electric Works Ltd | 電子機器収納ボックス |
CN2671078Y (zh) * | 2003-11-11 | 2005-01-12 | 州巧科技股份有限公司 | Lcd面板框架 |
CN102126085A (zh) * | 2011-04-02 | 2011-07-20 | 昆山宝锦激光拼焊有限公司 | 液晶显示面板用五金前框激光焊接工艺 |
-
2012
- 2012-07-19 CN CN2012102494577A patent/CN103246089A/zh active Pending
Patent Citations (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US6231202B1 (en) * | 1998-08-20 | 2001-05-15 | Matsushita Electric Industrial Co., Ltd. | Lighting unit and liquid crystal display device using the same |
JP2002290079A (ja) * | 2001-03-26 | 2002-10-04 | Matsushita Electric Works Ltd | 電子機器収納ボックス |
CN2671078Y (zh) * | 2003-11-11 | 2005-01-12 | 州巧科技股份有限公司 | Lcd面板框架 |
CN102126085A (zh) * | 2011-04-02 | 2011-07-20 | 昆山宝锦激光拼焊有限公司 | 液晶显示面板用五金前框激光焊接工艺 |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN103439811A (zh) * | 2013-08-20 | 2013-12-11 | 乐视致新电子科技(天津)有限公司 | 一种显示设备边框的制作方法及显示设备 |
CN103439811B (zh) * | 2013-08-20 | 2016-06-22 | 乐视致新电子科技(天津)有限公司 | 一种显示设备边框的制作方法及显示设备 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN105785611A (zh) | 背板及用于制造背板支架的模具 | |
CN201637970U (zh) | 液晶显示器用外框架和液晶显示器 | |
CN101357436B (zh) | 组合式框架的制造方法及其冲压设备 | |
CN202018551U (zh) | 液晶显示面板用五金前框 | |
CN102126085A (zh) | 液晶显示面板用五金前框激光焊接工艺 | |
CN101823106A (zh) | 平板显示器用金属框架的制造方法 | |
CN102122088A (zh) | 一种lcd面板框架及制造方法 | |
CN103246089A (zh) | 液晶显示面板用前框及镭焊工艺 | |
CN203465491U (zh) | 组装框、液晶显示模组和液晶显示装置 | |
CN202735625U (zh) | 液晶显示面板用前框 | |
CN208542867U (zh) | 一种用于液晶电视生产使用的金属边框折弯装置 | |
CN201995243U (zh) | 一种显示屏面板框架 | |
CN101979205A (zh) | 过紧密联板设计的电路板波峰焊接夹具 | |
CN201702708U (zh) | 一种工装夹具 | |
CN106180389A (zh) | 曲面电视液晶显示器背板冲压模具生产工艺方法 | |
CN101856699A (zh) | 一种屏蔽罩的生产工艺 | |
CN202771121U (zh) | Tft lcd框架 | |
CN104384340A (zh) | 组合式发动机仓边梁前部外板拉延模具 | |
CN203415806U (zh) | 组装rj11的自动装配机 | |
CN205436783U (zh) | 一种冲压模具的翻边拉深复合模 | |
CN204257624U (zh) | 一种新型bga器件 | |
CN201240997Y (zh) | 加工玻璃容器用的模具 | |
CN101670507A (zh) | 一种冷凝器钎焊工装定位装置 | |
CN101422944A (zh) | 屏幕外框的射出成型方法 | |
CN104162768B (zh) | 链条零件成型加工方法 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
C06 | Publication | ||
PB01 | Publication | ||
C10 | Entry into substantive examination | ||
SE01 | Entry into force of request for substantive examination | ||
C12 | Rejection of a patent application after its publication | ||
RJ01 | Rejection of invention patent application after publication |
Application publication date: 20130814 |