CN103171354A - 一种高分子聚合物香薰饰品及其制备方法 - Google Patents

一种高分子聚合物香薰饰品及其制备方法 Download PDF

Info

Publication number
CN103171354A
CN103171354A CN2013100702705A CN201310070270A CN103171354A CN 103171354 A CN103171354 A CN 103171354A CN 2013100702705 A CN2013100702705 A CN 2013100702705A CN 201310070270 A CN201310070270 A CN 201310070270A CN 103171354 A CN103171354 A CN 103171354A
Authority
CN
China
Prior art keywords
molecular polymer
essence
high molecular
ornament
aroma
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2013100702705A
Other languages
English (en)
Inventor
陈索斌
王彦芳
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
QINGDAO JINWANG APPLIED CHEMISTRY CO Ltd
Original Assignee
QINGDAO JINWANG APPLIED CHEMISTRY CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by QINGDAO JINWANG APPLIED CHEMISTRY CO Ltd filed Critical QINGDAO JINWANG APPLIED CHEMISTRY CO Ltd
Priority to CN2013100702705A priority Critical patent/CN103171354A/zh
Publication of CN103171354A publication Critical patent/CN103171354A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种高分子聚合物香薰饰品及其制备方法,该香薰饰品包括高分子聚合物微粒和香精,香精重量比例为两者总量的1-30%,其方法包括下列步骤:1香精浸泡:在封闭的容器中将高分子聚合物EVA、PU、医用PVC等微粒,室温下用香精浸泡24-48h,香精添加比例为1-30%,制作成各类缓释型长效的香熏粒子;2注塑成型:螺杆挤出温度控制在熔点以上20-30℃,本发明螺杆挤出温度控制在110-145℃。本发明的香薰饰品具有持香时间长,可塑性强等突出优势,可以制作颗粒状,也可以通过设备注塑成各种形状,产品的品质均一,生产效率高。

Description

一种高分子聚合物香薰饰品及其制备方法
技术领域
本发明涉及一种高分子聚合物香薰饰品。
背景技术
香薰饰品是选取一定的载体,将香料固定下来,再缓慢的释放到环境中,起到清新空气、除臭芳香、防霉防蛀、驱除异味、提神醒脑之功效。凡是具有微孔结构,具有大的比表面积、可以容纳香精油的材料均可用于香薰产品的制作。目前市面上应用比较广泛的为蜡烛、石膏、藤条、棉麻香包等等,上述材质载体无法制作纹路精细的产品,且纯粹手工操作,生产效率低。
发明内容
本发明所要解决的技术问题是提供一种高分子聚合物香薰饰品及其制备方法。
为解决上述技术问题,本发明采用的技术方案是:
一种高分子聚合物香薰饰品,包括高分子聚合物微粒和香精,香精重量比例为两者总量的1-30%,高分子聚合物是PE(聚乙烯)、EVA(乙烯和醋酸乙烯共聚物)、TPU(热塑性聚氨酯弹性体)、PU(聚氨酯)、PP(聚丙烯)、PET(聚对苯二甲酸乙二醇酯)、医用PVC(聚氯乙烯)、PA(聚氨酯)、PC(聚碳酸酯)中的一种。
优选的,高分子聚合物微粒为EVA、PU、医用PVC中的一种。该类高分子聚合物密度大,和香料结合紧密,可以使得有效成份缓慢释放,延长持香时间。
可以选取特定的香精,从而赋予香薰饰品除了具有清新空气外还具有安神、去除异味等功能性。
一种制备上述高分子聚合物香薰饰品的方法,包括下列步骤:
(1)香精浸泡
在封闭的容器中将高分子聚合物微粒室温下用香精浸泡24-48h,浸泡后香精占总重量的比例为1-30%,制作成各类缓释型长效的香熏粒子。因为高分子聚合物微粒吸附香精的能力各不相同,且有最大吸附范围,经过实际的实验测量称量,可以达到15%左右,所以用于香精浸泡的添加比例根据需要确定用量。
(2)注塑成型
注塑:填料,将香薰粒子装填如设备中,设置设备参数,螺杆挤出温度控制在熔点以上20-30℃,本申请中螺杆挤出温度控制在110-145℃。其中PVC熔化温度高:185-205℃,因此挤出温度需要控制在200-230℃,模具温度:20-50℃,注射压力:可大到1500bar;保压压力:可大到1000bar;注射速度:制备厚度5mm及以上件时选用中档注射速度,制备厚度为5mm以下及复杂件时选用高档注射速度。
本发明申请的香薰饰品具有持香时间长,可塑性强等突出优势,可以制作颗粒状,也可以通过设备注塑成各种形状,产品的品质均一,生产效率高。
具体实施方式
实施例1
取5kg粒径为2-3mm的EVA颗粒,加入3kg的香精,放入封闭的容器中进行浸泡,浸泡时间为48h,所得香薰粒子过滤,称重计算香精的吸收率。香薰粒子直接可以作为产品出售,也可以通过注塑方式进一步加工成各种形状产品。
注塑:填料,将香薰粒子装填如设备中,设置设备参数,螺杆挤出温度为110℃;模具温度:20-50℃;注射压力1500bar;保压压力1000bar。注射速度:制备厚度5mm及以上件时选用中档注射速度,制备厚度为5mm以下及复杂件时选用高档注射速度。
实施例2
取5kg粒径为2-3mm的PU颗粒,加入1kg的香精,放入封闭的容器中进行浸泡,浸泡时间为24h,所得香薰粒子过滤,称重计算香精的吸收率。香薰粒子直接可以作为产品出售,也可以通过注塑方式进一步加工成各种形状产品。
注塑:填料,将香薰粒子装填如设备中,设置设备参数,螺杆挤出温度为145℃;模具温度:20-50℃;注射压力1500bar;保压压力1000bar。注射速度:制备厚度5mm及以上件时选用中档注射速度,制备厚度为5mm以下及复杂件时选用高档注射速度。
实施例3
取5kg粒径为2-3mm的医用PVC颗粒,加入2kg的香精,放入封闭的容器中进行浸泡,浸泡时间为24h,所得香薰粒子过滤,称重计算香精的吸收率。香薰粒子直接可以作为产品出售,也可以通过注塑方式进一步加工成各种形状产品。
注塑:填料,将香薰粒子装填如设备中,设置设备参数,螺杆挤出温度为200℃;模具温度:20-50℃;注射压力1500bar;保压压力1000bar。注射速度:制备厚度5mm及以上件时选用中档注射速度,制备厚度为5mm以下及复杂件时选用高档注射速度。
实施例4
取5kg粒径为2-3mm的医用PVC颗粒,加入3kg的香精,放入封闭的容器中进行浸泡,浸泡时间为48h,所得香薰粒子过滤,称重计算香精的吸收率。香薰粒子直接可以作为产品出售,也可以通过注塑方式进一步加工成各种形状产品。
注塑:填料,将香薰粒子装填如设备中,设置设备参数,螺杆挤出温度为230℃;模具温度:20-50℃;注射压力1500bar;保压压力1000bar。注射速度:制备厚度5mm及以上件时选用中档注射速度,制备厚度为5mm以下及复杂件时选用高档注射速度。
实施例5
取5kg粒径为2-3mm的PE颗粒,加入3kg的香精,放入封闭的容器中进行浸泡,浸泡时间为48h,所得香薰粒子过滤,称重计算香精的吸收率。香薰粒子直接可以作为产品出售,也可以通过注塑方式进一步加工成各种形状产品。
注塑:填料,将香薰粒子装填如设备中,设置设备参数,螺杆挤出温度为120℃;模具温度:20-50℃;注射压力1500bar;保压压力1000bar。注射速度:制备厚度5mm及以上件时选用中档注射速度,制备厚度为5mm以下及复杂件时选用高档注射速度。

Claims (3)

1.一种高分子聚合物香薰饰品,其特征在于,包括高分子聚合物微粒和香精,香精重量比例为两者总量的1-30%,高分子聚合物是PE(聚乙烯)、EVA(乙烯和醋酸乙烯共聚物)、TPU(热塑性聚氨酯弹性体)、PU(聚氨酯)、PP(聚丙烯)、PET(聚对苯二甲酸乙二醇酯)、医用PVC(聚氯乙烯)、PA(聚氨酯)、PC(聚碳酸酯)中的一种。
2.根据权利要求1所述的高分子聚合物香薰饰品,其特征在于,其中高分子聚合物微粒为EVA、PU、医用PVC中的一种。
3.一种制备权利要求1中高分子聚合物香薰饰品的方法,其特征在于,包括下列步骤:
(1)香精浸泡
在室温下,在封闭的容器中将高分子聚合物微粒用香精浸泡24-48h,制作成各类缓释型长效的香熏粒子;
(2)注塑成型
注塑:填料,将香薰粒子装填如设备中,设置设备参数,螺杆挤出温度为110-145℃;模具温度:20-50℃;注射压力1500bar;保压压力1000bar;注射速度:制备厚度5mm及以上件时选用中档注射速度,制备厚度为5mm以下及复杂件时选用高档注射速度。
CN2013100702705A 2013-03-06 2013-03-06 一种高分子聚合物香薰饰品及其制备方法 Pending CN103171354A (zh)