CN102773129A - 耐磨分体辊套 - Google Patents

耐磨分体辊套 Download PDF

Info

Publication number
CN102773129A
CN102773129A CN2011101187204A CN201110118720A CN102773129A CN 102773129 A CN102773129 A CN 102773129A CN 2011101187204 A CN2011101187204 A CN 2011101187204A CN 201110118720 A CN201110118720 A CN 201110118720A CN 102773129 A CN102773129 A CN 102773129A
Authority
CN
China
Prior art keywords
wear
wear resistant
medium
roller shell
basic unit
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2011101187204A
Other languages
English (en)
Inventor
夏阳
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
BEIJING NONVIA TECHNOLOGY DEVELOPMENT CO LTD
Original Assignee
BEIJING NONVIA TECHNOLOGY DEVELOPMENT CO LTD
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by BEIJING NONVIA TECHNOLOGY DEVELOPMENT CO LTD filed Critical BEIJING NONVIA TECHNOLOGY DEVELOPMENT CO LTD
Priority to CN2011101187204A priority Critical patent/CN102773129A/zh
Publication of CN102773129A publication Critical patent/CN102773129A/zh
Pending legal-status Critical Current

Abstract

本耐磨分体辊套由耐磨层和基层组成,耐磨层分成36块耐磨块,每块耐磨块由金属耐磨材料铸造成开口箱体,箱体内均匀镶嵌金属陶瓷,然后,采用液体金属耐磨材料浇铸,将金属陶瓷固定在箱体内。最后,将耐磨块用螺栓固定于基层上。耐磨分体辊套可应用于中速磨煤机磨辊,如RP、HP、MSP、ZGM等中速磨煤机。

Description

耐磨分体辊套
1、技术领域
本发明专利涉及一种电站锅炉中速磨煤机磨辊辊套。它能够根据中速磨煤机磨辊辊套磨损状况,整体或部分维修更换磨辊辊套。由于耐磨分体辊套采用金属陶瓷材料,使用寿命可达20000小时以上,而且更换或者维修方便,只需整体或者部分更换耐磨分体辊套的碾磨层,基层可以重复利用,节省材料成本。因此,中速磨煤机使用耐磨分体辊套,维修方便灵活,省时、省力且节约材料成本,使用寿命长。 
2、背景技术
由于中国经济的高速发展,对能源的需求越来越大,因此,发电企业对电煤的需求大大超过供给,引起电煤供应紧张,导致发电企业燃用煤质变差,入炉原煤可磨度降低,从而使得磨煤机出力降低,磨辊磨损严重,磨辊辊套使用寿命缩短。 
目前普遍使用的高铬耐磨辊套使用约6000小时,就需要将磨辊整体拆下拉到专门维修点进行堆焊修复,维修时间长,成本高。 
采用金属陶瓷整体铸造的磨辊辊套使用寿命可达20000小时以上,在一定程度上缓解了煤质变差和锅炉燃煤需求量增加的矛盾。但是,由于金属陶瓷磨辊辊套无法修复,使用寿命到期后就要报废,不能重复使用,而整体铸造的新磨辊辊套成本很高,限制了金属陶瓷整体铸造磨辊的推广应用。 
本耐磨分体辊套将金属陶瓷镶嵌于碾磨块内,耐磨层由36块相同的耐磨块组成,并固定在基层上。因此,本耐磨分体辊套因使用金属陶瓷,其使用寿命达到20000小时以上,同时,由于金属陶瓷镶嵌于耐磨块内,便于磨煤机磨辊维修和更换。 
3、发明内容
本发明专利提供了一种新型的中速磨煤机磨辊辊套。该磨辊辊套由碾磨层和基层组成,耐磨层由36块耐磨块组成,每块耐磨块由耐磨钢铸造成一个开口箱体,将金属陶瓷均匀镶嵌于箱体内,并将螺栓预制在箱体内,然后使用液体耐磨金属浇铸,使金属陶瓷与耐磨箱体成为一个整体,最后,将耐磨块固定于基层上,形成耐磨分体辊套。 
耐磨分体辊套分为两层:耐磨层和基层。 
1)基层——采用普通钢材铸造,然后进行机加工。 
2)耐磨层——由36块相同的耐磨块组成,分别采用螺栓固定在基层上。 
3)耐磨块——由耐磨钢材铸造成开口箱体,在箱体内镶嵌金属陶瓷,然后用液体耐 磨钢材浇铸,将耐磨材料固定在耐磨块箱体内。 
4、附图说明
附图说明:附图为耐磨分体辊套示意图。 
5、具体实施方式
1)针对不同型号的中速磨煤机磨辊尺寸,设计耐磨分体辊套基层和耐磨块模型。 
2)铸造耐磨分体辊套基层和耐磨块基体。 
3)对铸造好的耐磨分体辊套基层和耐磨块基体进行机加工。 
4)将金属陶瓷镶嵌于耐磨块内,并用液体耐磨金属材料进行浇铸。 
5)将耐磨块用螺栓固定在基层上。 

Claims (2)

1.本耐磨分体辊套由耐磨层和基层组成,耐磨层由36块相同的耐磨块组成,分别用螺栓固定在基层上。当磨辊因磨损或者损坏需要检修更换时,不需要将辊套整体拆下更换维修,只需直接将耐磨层整体更换或者将耐磨块部分更换,基层可重复利用,节约材料,节省维修时间,降低劳动强度。
2.在权利要求书1的基础上,本专利可用于RP中速磨煤机、HP中速磨煤机、MPS中速磨煤机和ZGM中速磨煤机磨辊辊套。
CN2011101187204A 2011-05-10 2011-05-10 耐磨分体辊套 Pending CN102773129A (zh)