CN102658581B - 轻质矩形夹芯板砖的生产方法及生产设备 - Google Patents
轻质矩形夹芯板砖的生产方法及生产设备 Download PDFInfo
- Publication number
- CN102658581B CN102658581B CN201210142225.1A CN201210142225A CN102658581B CN 102658581 B CN102658581 B CN 102658581B CN 201210142225 A CN201210142225 A CN 201210142225A CN 102658581 B CN102658581 B CN 102658581B
- Authority
- CN
- China
- Prior art keywords
- light
- insulation material
- heat insulation
- brick
- heated board
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本发明涉及一种轻质矩形夹芯板砖的生产方法及生产设备,其特征在于:至少包括以下步骤,a)采用具有上开口的凹状模具;b)在凹状模具底部注入底层水泥砂浆料;c)在底层水泥砂浆料上放入网格材料;d)在网格材料上放入轻质保温材料;e)在轻质保温材料上注入上层水泥砂浆料;f)通过压板压置在凹状模具上层,使浆料完整包覆在轻质保温材料外层以形成夹芯防火保温板砖坯料;g)振动压实坯料。通过上述的生产方法和生产设备制得的本发明轻质矩形夹芯板砖体内设有轻质夹芯板材,从而让砖体的重量较轻,方便搬运,也大大节省了生产成本,也有利于制得较密实的砖体。
Description
技术领域:
本发明涉及一种轻质矩形夹芯防火保温板砖的生产方法及生产设备。
背景技术:
砖,建筑用的人造小型块材,俗称砖头,分烧结砖(主要指粘土砖)和非烧结砖(灰砂砖、 粉煤灰砖等),烧结砖以粘土(包括页岩、煤矸石等粉料)为主要原料,经泥料处理、成型、干燥和焙烧而成;非烧结砖也叫免烧砖,一般由粘合剂粘贴或高压蒸馏而成。不论上述哪种砖,其重量均较大,不仅浪费原材料,而且搬运不方便;而目前砖的生产方法和成型设备无法让成型后的砖能具备多种功用。
发明内容:
本发明的目的在于提供一种轻质矩形夹芯防火保温板砖的的生产方法及生产设备,该轻质矩形夹芯防火保温板砖的的生产方法及生产设备及有利于制得较轻且密实多功能的砖体、方便其搬运及安装使用。
本发明轻质矩形夹芯防火保温板砖的生产方法,其特征在于:至少包括以下步骤,
a)采用具有上开口的凹状模具;
b)在凹状模具底部注入底层水泥砂浆料;
c)在底层水泥砂浆料上放入网格材料;
d)在网格材料上放入轻质保温材料;
e)在轻质保温材料上注入上层水泥砂浆料;
f) 通过压板压置在凹状模具上层,使浆料完整包覆在轻质保温材料外层以形成夹芯防火保温板砖坯料;
g)振动压实坯料。
上述步骤中,在放入轻质保温材料与注入上层水泥砂浆料步骤之间,还增加有注入一层浆料和铺设一层玻璃纤维网格布或钢丝网格的步骤。
上述振动压实坯料采用的是高频数控振动压实坯料,其振动频率为510HZ以上,振动时间11分钟以上。
上述轻质保温材料为挤塑板、聚氨酯板或岩棉板中的一种。
本发明轻质矩形夹芯板砖的生产设备依次包括有喷涂浆机、第一物料输送机、高频数控振动机、第二物料输送机、自动推高机、物料干燥机和下料输送机。
上述高频数控振动机包括有底座和振动架,所述振动架包括有承放凹状模具的平台架和固定在平台架上的压板以及让压板下压的液压缸组件,所述平台架两端活动支撑在底座的两侧,所述底座上设有驱动平台架高频振动的电机或气动振动机。
上述喷涂浆机在凹状模具中注入上层水泥砂浆料后通过第一物料输送机输送往高频数控振动机,经过高频数控振动压实坯料后经第二物料输送机输送往自动推高机、物料干燥机高温干燥,干燥时间是1个小时,经过干燥后由下料输送机输出。
通过上述的生产方法和生产设备制得的本发明轻质矩形夹芯防火保温板砖体内设有轻质夹芯防火保温板材,从而让砖体的重量较轻,具备多种使用功能方便搬运,也极大节省了生产成本和人工成本,也有利于制得较密实多功能的砖体。
附图说明:
图1是本发明轻质矩形夹芯防火保温板砖的构造示意图;
图2是本发明轻质矩形夹芯防火保温板砖另一种实施例构造示意图;
图3是本发明轻质矩形夹芯防火保温板砖成型模具的构造示意图;
图4是本发明轻质矩形夹芯防火保温板砖成型装置的构造示意图;
图5是本发明轻质矩形夹芯防火保温板砖成型设备的构造示意图。
具体实施方式:
本发明轻质矩形夹芯防火保温板砖,包括由水泥砂浆构成的矩形砖体1,砖体体内设有轻质保温夹芯板材2。
上述轻质夹芯防火保温板材为挤塑板、聚氨酯板或岩棉板中的一种。上述轻质夹芯防火保温板材呈矩形状。上述轻质保温材料设置在砖体的中心部。
在所述轻质保温材料厚度方向的一侧或两侧面上设有网格布3,网格布为玻璃纤维网格布或钢丝网格材料。
本发明轻质矩形夹芯防火保温板砖的生产方法,其特征在于:至少包括以下步骤,
a)采用具有上开口的凹状模具;
b)在凹状模具底部注入底层水泥砂浆料;
c)在底层水泥砂浆料上放入网格材料;
d)在网格材料上放入轻质保温材料;
e)在轻质保温材料上注入上层水泥砂浆料;
f) 通过压板压置在凹状模具上层,使浆料完整包覆在轻质保温材料外层以形成夹芯防火保温板砖坯料;
g)振动压实坯料。
为了更好的粘接,上述步骤中,在放入轻质保温材料与注入上层水泥砂浆料步骤之间,还增加有注入一层浆料和铺设一层玻璃纤维网格布或钢丝网格的步骤。
为了使砖体不容易产生孔隙,上述振动压实坯料采用的是高频数控振动压实坯料,其振动频率为510HZ以上,振动时间11分钟以上。
上述轻质保温材料为挤塑板、聚氨酯板或岩棉板中的一种。
本发明轻质矩形夹芯板砖的生产设备依次包括有喷涂浆机、第一物料输送机A1、高频数控振动机A2、第二物料输送机A3、自动推高机、物料干燥机A4和下料输送机A5。
上述高频数控振动机A3包括有底座A7和振动架A8,所述振动架A8包括有承放凹状模具5的平台架A9和固定在平台架上的压板A10以及让压板下压的液压缸组件,所述平台架两端活动支撑在底座的两侧,所述底座上设有驱动平台架高频振动的电机A11或气动振动机。
上述喷涂浆机在凹状模具中注入上层水泥砂浆料后通过第一物料输送机输送往高频数控振动机,经过高频数控振动压实坯料后经第二物料输送机输送往自动推高机、物料干燥机高温干燥,干燥时间是1个小时,经过干燥后由下料输送机输出。
通过上述的生产方法和生产设备制得的本发明轻质矩形夹芯防火保温板砖体内设有轻质夹芯防火保温板材,从而让砖体的重量较轻,方便搬运,也大大节省了生产成本,也有利于制得较密实的砖体。
Claims (4)
1.一种轻质矩形夹芯防火保温板砖的生产方法,其特征在于:至少包括以下步骤,
A、采用具有上开口的凹状模具;
B、在凹状模具底部注入底层水泥砂浆料;
C、在底层水泥砂浆料上放入网格材料;
D、在网格材料上放入轻质保温材料;
E、在轻质保温材料上注入上层水泥砂浆料;
F、通过压板压置在凹状模具上层,使浆料完整包覆在轻质保温材料外层以形成夹芯防火保温板砖坯料;
G、振动压实坯料。
2.根据权利要求1所述轻质矩形夹芯防火保温板砖的生产方法,其特征在于:上述步骤中,在放入轻质保温材料与注入上层水泥砂浆料步骤之间,还增加有注入一层浆料和铺设一层玻璃纤维网格布或钢丝网格的步骤。
3.根据权利要求2所述轻质矩形夹芯防火保温板砖的生产方法,其特征在于:所述振动压实坯料采用的是高频数控振动压实坯料,其振动频率为510HZ以上,振动时间11分钟以上。
4.根据权利要求3所述的轻质矩形夹芯防火保温板砖的生产方法,其特征在于:所述轻质保温材料为挤塑板、聚氨酯板或岩棉板中的一种。