Prior art keywords
brightener
parts
oxide
removal
copolymer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201110442573.6A
Other languages
English (en)
Other versions
CN102532793A (zh
Inventor
彭朕财
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shenzhen Xin Hengli Science And Technology Ltd
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201110442573.6A priority Critical patent/CN102532793B/zh
Publication of CN102532793A publication Critical patent/CN102532793A/zh
Application granted granted Critical
Publication of CN102532793B publication Critical patent/CN102532793B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Abstract

本发明公开了一种塑料去纹增亮剂,其包括:增亮剂15~30份,去纹剂10~30份,氧化物30~60份,耦合剂0.5~3份,聚合物载体20~40份,润滑剂2~10份,稳定剂0.5~4份。该塑料去纹增亮剂在塑料制备过程中可以吸水并增加韧性和强度,提高塑料质量及合格率。

Description

一种塑料去纹增亮剂及其制备方法
技术领域
本发明涉及一种塑料管材或制品的配料及其制备方法。 
背景技术
塑料是当今社会中常用的封装、包装材料,在很多领域中具有广泛应用。为了资源重复利用,需要将塑料回收利用,重新成型,但是由于在前一次制造或使用时各种因素的影响,导致重新制造成型的塑料有很多水纹或混杂物,导致其韧性和强度下降,并且不平整,有花面。例如,在塑料管材或制品加工中因本身分子结构原因,多次回收造粒受热分解原因,或加有填充料原因等造成韧性下降,脆性增加,导致制成的塑料产品质量下降。另外,有些物料因用水拉条造粒,料中混杂了一些水分,另一些物料因本身分子结构为强极性分子极易吸收空气中的水分,再生回收料和PS、PA、ABS等强极性的塑料原料,导致成型产品中产生银纹、水气或流纹等,造成产品合格率不高。 
发明内容
本发明公开了一种塑料去纹增亮剂,其能吸水又能增加韧性和强度,提高塑料质量及合格率。 
本发明的塑料去纹增亮剂包括:增亮剂15~30份,去纹剂10~30份,氧化物30~60份,耦合剂0.5~3份,聚合物载体20~40份,润 滑剂2~10份,稳定剂0.5~4份;其中 
所述的增亮剂为丙烯晴-苯乙烯的共聚物、苯乙烯-丁二烯嵌段共聚物、丁二烯-苯乙烯共聚物、马来酸酐接枝聚烯烃中的至少一种; 
所述的去纹剂为蒙脱土、滑石粉、镁晶须、超微碳酸钙中的至少一种; 
所述的氧化物为氧化镁、氧化锌、氧化钙、氧化钡中的至少一种; 
所述的耦合剂为硅烷耦合剂; 
所述的聚合物载体为聚苯乙烯、丙烯腈-丁二烯-苯乙烯共聚物、尼龙、乙烯-醋酸乙烯共聚物、乙烯-丙烯酸乙酯共聚物、乙烯-丙烯酸共聚物、高密度聚乙烯、线性低密度聚乙烯、低密度聚乙烯、聚丙烯中的至少一种; 
所述的润滑剂为石蜡、聚乙烯蜡、聚丙烯蜡、高沸点溶剂油、白油、环烷油、邻苯二甲酸二辛酯、邻苯二甲酸二丁酯中的至少一种; 
所述的稳定剂为硬脂酸、硬脂酸钙、硬脂酸钠、硬脂酸钡、硬脂酸锌中的至少一种。 
本发明的塑料去纹增亮剂的制备方法为:将增亮剂、去纹剂、氧化物、耦合剂、聚合物载体、润滑剂和稳定剂按上述的配比范围在高速搅拌机中搅拌捏合、混合反应均匀。 
具体实施方式
为了使本领域技术人员更详细的了解本发明的塑料去纹增亮剂的组分尤其制作方法,下面通过具体实施方式描述本发明的技术方案。 
本发明的塑料去纹增亮剂包括:增亮剂15~30份,去纹剂10~30份,氧化物30~60份,耦合剂0.5~3份,聚合物载体20~40份,润 滑剂2~10份,稳定剂0.5~4份;其中, 
所述的增亮剂为丙烯晴-苯乙烯的共聚物、苯乙烯-丁二烯嵌段共聚物、丁二烯-苯乙烯共聚物、马来酸酐接枝聚烯烃中的至少一种; 
所述的去纹剂为蒙脱土、滑石粉、镁晶须、超微碳酸钙中的至少一种; 
所述的氧化物为氧化镁、氧化锌、氧化钙、氧化钡中的至少一种; 
所述的耦合剂为硅烷耦合剂、铝酸脂耦合剂、钛酸脂耦合剂中的至少一种; 
所述的聚合物载体为聚苯乙烯、丙烯腈-丁二烯-苯乙烯共聚物、尼龙、乙烯-醋酸乙烯共聚物、乙烯-丙烯酸乙酯共聚物、乙烯-丙烯酸共聚物、高密度聚乙烯、线性低密度聚乙烯、低密度聚乙烯、聚丙烯中的至少一种; 
所述的润滑剂为石蜡、聚乙烯蜡、聚丙烯蜡、高沸点溶剂油、白油、环烷油、二辛酯 、二丁酯 中的至少一种; 
所述邻苯二甲酸二辛酯 俗称二辛酯 ,所述邻苯二甲酸二丁酯 俗称二丁酯 。 
所述的稳定剂为硬脂酸、硬脂酸钙、硬脂酸钠、硬脂酸钡、硬脂酸锌中的至少一种。 
本发明的塑料去纹增亮剂的制备方法为:将增亮剂、去纹剂、氧化物、耦合剂、聚合物载体、润滑剂、稳定剂等各组份物料按上述的配比范围在高速搅拌机中搅拌捏合、混合反应均匀。 
实施例1: 
取60kg氧化镁、15kg滑石粉、5kg镁晶须投入500L高速搅拌机组中,高速搅拌到机温升至105℃,加入用1kg钛酸脂耦合剂,高搅升温 至125℃,加入0.8kg硬脂酸稳定剂和2kg白油,再高搅混合反应升温至145℃,将物料放入冷混机中,搅拌冷却至60℃,加入2kg聚乙烯腊,8kg丙烯晴-苯乙烯的共聚物,10kg丁二烯-苯乙烯共聚物,25kg丙烯腈-丁二烯-苯乙烯共聚物搅拌均匀后出锅。 
实施例2: 
取60kg氧化钙、20kg超微碳酸钙、5kg蒙脱土投入500L高速搅拌机组中,高速搅拌到机温升至95℃,加入用1.2kg硅烷耦合剂,高搅升温至120℃,加入1kg硬脂酸钙稳定剂和3kg环烷油,再高搅混合反应升温至140℃,将物料放入冷混机中,搅拌冷却至60℃,加入3kg聚乙烯腊,10kg马来酸酐接枝聚乙烯的弹性体,25kg高密度聚乙烯搅拌均匀后出锅。 
实施例3: 
取60kg氧化锌、25kg蒙脱土投入500L高速搅拌机组中,高速搅拌到机温升至100℃,加入用2kg铝酸脂耦合剂,高搅升温至120℃,加入1.5kg硬脂酸锌稳定剂和2.5kg白油,再高搅混合反应升温至140℃,将物料放入冷混机中,搅拌冷却至60℃,加入4kg聚乙烯腊,10kg苯乙烯-丁二烯嵌段共聚物,10kg丁二烯-苯乙烯共聚物,15kg聚苯乙烯搅拌均匀后出锅。然后加入乙醇配成溶液,溶质与溶剂的重量比为1:10~30。 
实施例4: 
取60kg氧化镁、10kg镁晶须投入500L高速搅拌机组中,高速搅拌到机温升至90℃,加入用1.4kg钛酸脂耦合剂,高搅升温至125℃,加入1kg硬脂酸钠稳定剂和2.5kg环烷油,再高搅混合反应升温至145℃,将物料放入冷混机中,搅拌冷却至60℃,加入2kg聚丙烯腊,10kg 丙烯晴-苯乙烯的共聚物,10kg马来酸酐接枝聚丙烯的弹性体,20kg尼龙搅拌均匀后出锅,然后加入乙醇配成溶液,溶质与溶剂的重量比为1:20。 
本发明塑料去纹增亮剂及其制备方法的优点在于:提供了一种既能吸水又能增加韧性和强度,提高产品质量的用于塑料成型加工中的吸水增韧母料及其制备方法,解决了现有塑料成型加工中因原料原因变脆、受潮而影响产品质量的问题,在塑料管材、注塑成型、中空吹塑成型等多种塑料成型工艺中掺用0.5‰~2‰本发明的产品能达到增韧、消除银纹、水纹等的效果。 
本发明的塑料去纹增亮剂的用法简单,只需在混料时加入,与塑料混合加热烘烤后即可挤出、注塑或吹塑成型。其可以令塑料更容易着色,本产品能粘附色粉,令着色均匀,减少使用分散剂或扩散油。由于该去纹增亮剂为透明物料,不含杂质和沉淀物,对塑料透明度和颜色不会造成任何影响。 

Claims (2)

1.一种塑料去纹增亮剂,其特征在于,所述塑料去纹增亮剂包括:增亮剂15~30份,去纹剂10~30份,氧化物30~60份,耦合剂0.5~3份,聚合物载体20~40份,润滑剂2~10份,稳定剂0.5~4份;其中, 
所述增亮剂为丙烯晴-苯乙烯的共聚物、苯乙烯-丁二烯嵌段共聚物、丁二烯-苯乙烯共聚物、马来酸酐接枝聚烯烃中的至少一种; 
所述去纹剂为蒙脱土、滑石粉、镁晶须、超微碳酸钙中的至少一种; 
所述氧化物为氧化镁、氧化锌、氧化钙、氧化钡中的至少一种; 
所述耦合剂为硅烷耦合剂; 
所述聚合物载体为聚苯乙烯、丙烯腈-丁二烯-苯乙烯共聚物、尼龙、乙烯-醋酸乙烯共聚物、乙烯-丙烯酸乙酯共聚物、乙烯-丙烯酸共聚物、高密度聚乙烯、线性低密度聚乙烯、低密度聚乙烯、聚丙烯中的至少一种; 
所述润滑剂为石蜡、聚乙烯蜡、聚丙烯蜡、高沸点溶剂油、白油、环烷油、邻苯二甲酸二辛酯、邻苯二甲酸二丁酯中的至少一种; 
所述稳定剂为硬脂酸、硬脂酸钙、硬脂酸钠、硬脂酸钡、硬脂酸锌中的至少一种。 
2.一种制备如权利要求1所述的塑料去纹增亮剂的方法,其特征在于,包括如下步骤:将增亮剂、去纹剂、氧化物、耦合剂、聚合物载体、润滑剂和稳定剂按上述的配比范围在高速搅拌机中搅拌捏合、混合反应均匀。 
CN201110442573.6A 2011-12-27 2011-12-27 一种塑料去纹增亮剂及其制备方法 Expired - Fee Related CN102532793B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201110442573.6A CN102532793B (zh) 2011-12-27 2011-12-27 一种塑料去纹增亮剂及其制备方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201110442573.6A CN102532793B (zh) 2011-12-27 2011-12-27 一种塑料去纹增亮剂及其制备方法

Publications (2)

Publication Number Publication Date
CN102532793A CN102532793A (zh) 2012-07-04
CN102532793B true CN102532793B (zh) 2014-04-02

Family

ID=46340905

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201110442573.6A Expired - Fee Related CN102532793B (zh) 2011-12-27 2011-12-27 一种塑料去纹增亮剂及其制备方法

Country Status (1)

Country Link
CN (1) CN102532793B (zh)

Families Citing this family (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105175765A (zh) * 2015-09-18 2015-12-23 颍上县龙裕扬工贸有限公司 一种塑料制品修饰加工用增亮膏
CN105694183A (zh) * 2016-04-14 2016-06-22 滁州市博康模具塑料有限公司 光泽度高的塑料垃圾桶及其制备方法
CN106084625A (zh) * 2016-07-29 2016-11-09 广东壹豪新材料科技股份有限公司 一种耐候免喷涂高光abs
CN106750706B (zh) * 2017-01-17 2018-05-22 江苏卡欧化工股份有限公司 一种环保型橡胶增亮剂

Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101148518A (zh) * 2007-11-02 2008-03-26 石明东 磷灰石在以塑料为基体的阻燃复合材料中的应用

Patent Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101148518A (zh) * 2007-11-02 2008-03-26 石明东 磷灰石在以塑料为基体的阻燃复合材料中的应用

Also Published As

Publication number Publication date
CN102532793A (zh) 2012-07-04

Similar Documents

Publication Publication Date Title
CN103571039B (zh) 高熔指聚丙烯组合物及其制备方法
CN104610654B (zh) 一种超细滑石粉聚丙烯填充色母粒及其制备方法
CN101128535B (zh) 生物降解聚酯树脂组合物、其制造方法及该组合物成型所得的成型体
CN101024709A (zh) 注塑级木塑复合材料及加工工艺
CN104371188A (zh) 一种强度大、光泽度高的再生塑料及其制备方法
CN103910920A (zh) 一种高耐热、耐寒的透明聚丙烯材料及其制备方法
CN102532793B (zh) 一种塑料去纹增亮剂及其制备方法
CN109181186A (zh) 一种可生物降解疏水性pva树脂复合材料
CN103992561A (zh) 一种聚烯烃母料制备管件的方法
CN103030886A (zh) 一种透明聚丙烯及其制备方法
CN109111710B (zh) 一种耐热型pla基可降解塑料瓶及其制备方法
CN102911454B (zh) 一种高抗冲pvc/abs/cpe管材及其制备方法
CN1919918A (zh) 一种塑料成型加工用的吸水增韧母料及其制备方法
CN101243136A (zh) 聚酯树脂组合物以及使用它的成型体
CN104231417A (zh) 一种聚烯烃硫酸钡透明母粒及其制备方法
CN105838047A (zh) 一种可生物降解改性木质素颗粒及其制造方法
CN110437538A (zh) 一种3d打印用聚丙烯耗材及其制备方法
CN102241855A (zh) 一种纳米级碳酸钙填充聚丙烯/聚乙烯共混制成的发泡材料及制备工艺
CN102532694A (zh) 一种高熔指的复合材料及其制备方法
CN102532744A (zh) Pvc/6000目重质碳酸钙抗静电电缆挂钩专用料及其制备技术
CN103059392B (zh) 一种塑料消泡剂
CN105462064A (zh) 一种聚丙烯/聚乙烯/木纤维复合材料及其制备方法
CN107090151A (zh) 一种具有较宽熔融加工窗口的聚乙烯醇组合物
CN110317401A (zh) 一种高耐候性复合高分子材料及其制备方法
CN105647008A (zh) 一种耐磨耐折聚丙烯复合鞋底材料的制备方法

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
ASS Succession or assignment of patent right

Owner name: SHENZHEN XINHENGLI TECHNOLOGY CO., LTD.

Free format text: FORMER OWNER: PENG ZHENCAI

Effective date: 20140624

C41 Transfer of patent application or patent right or utility model
COR Change of bibliographic data

Free format text: CORRECT: ADDRESS; FROM: 518173 SHENZHEN, GUANGDONG PROVINCE TO: 518000 SHENZHEN, GUANGDONG PROVINCE

TR01 Transfer of patent right

Effective date of registration: 20140624

Address after: 518000 10 Longgang community road, Henggang District, Shenzhen City, Guangdong Province, No. 505, six

Patentee after: SHENZHEN XIN HENGLI SCIENCE AND TECHNOLOGY Ltd.

Address before: Henggang Longgang District of Shenzhen City, Guangdong province 518173 about six dragon shenhuiroad Village No. 433

Patentee before: Peng Zhencai

CF01 Termination of patent right due to non-payment of annual fee
CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20140402

Termination date: 20211227