CN102531489A - Middle elastic relief rough coating - Google Patents
Middle elastic relief rough coating Download PDFInfo
- Publication number
- CN102531489A CN102531489A CN2011104257711A CN201110425771A CN102531489A CN 102531489 A CN102531489 A CN 102531489A CN 2011104257711 A CN2011104257711 A CN 2011104257711A CN 201110425771 A CN201110425771 A CN 201110425771A CN 102531489 A CN102531489 A CN 102531489A
- Authority
- CN
- China
- Prior art keywords
- percent
- coating
- powder
- elasticity
- plucking
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention relates to a chemical material, in particular to middle elastic relief rough coating, which comprises the following materials in percentage by weight: stuffing: 25 percent of white cement, 5 percent of sierozem, 35 percent of triple superphosphate, 10 percent of barium sulfate, 20 percent of wollastonite; rubber powder: 0.8 percent of hydroxypropyl methyl cellulose, 3.0 percent of re-dispersible latex powder, 0.5 percent of wood fiber, and 0.7 percent of polyvinyl alcohol powder 24-88 P. The middle elastic relief rough coating disclosed by the invention is more advantageous in wear-resistance and crack-resistance than common flat coating or elastic coating, cracks on a wall can be effectively bridged by virtue of the elasticity of the coating, and the coating is particularly suitable for areas with strong sunlight by virtue of the excellent anti-ultraviolet radiation function.
Description
Technical field
The present invention relates to a kind of chemical materials, relate in particular to a kind of middle level elasticity embossment galling paint.
Background technology
The exterior coating long-term exposure receives the shadow of daylight, rainwater, dust storm, cold and hot variation etc. in the open air, after after a while, the outward appearance of facing ftractures, peels off, efflorescence, variable color, fade, phenomenon such as mistake.Particularly in the Northwest, dry, ultraviolet ray is strong; Day and night temperature is big, causes wall crazing, and building cracks is a modal problem in the current building operation quality; Perplexing current construction industry for a long time always; Fissured appearance not only influences the attractive in appearance of architectural coating, and can have a negative impact to buildings itself, even harm.Buildings is many to be basic unit with the cement sand plaster.Motar reduces the sclerosis crack that produces owing to volume when sclerosis; During temperature variation, expand with heat and contract with cold and the temperature that produces becomes the crack; Do wet the variation, the desciccation crack that the drying shrinkage that rises owing to wetting produces; The ponding freeze thawing, the freeze thawing crack that produces owing to the water freezing volumetric expansion; Basic unit's sedimentation produces structural cracks etc., and the crack of basic unit causes protecting the decorative coveringn cracking.
Summary of the invention
For addressing the above problem, the invention provides a kind of middle level elasticity embossment galling paint that can overcome above-mentioned shortcoming.
Technical scheme of the present invention is:
A kind of middle level elasticity embossment plucking lacquer, according to weight percent meter, composed of the following components:
Stopping composition:White cement 25%, grey calcium 5%, coarse whiting 35%, permanent white 10%, wollastonite 20%
The rubber powder class:Vltra tears 0.8%, redispersible latex powder 3.0%, wood fibre 0.5%, pva powder 24-88P 0.7%.
Further, described white cement is 325 white cements.
Further, the viscosity of described Vltra tears is 100000mPas.
Above-mentioned materials is added in the powder stirrer successively, stirred 20-30 minutes, be finished product, adding an amount of water during use can become plucking or anaglyph.
Plucking rolls with plucking, and embossment is used spray gun.
Slightly polishing with emery cloth in construction completion back, can get final product for one to two time by outer brush rubber-emulsion paint.
Beneficial effect of the present invention:
Elasticity embossment plucking lacquer in middle level of the present invention is than common flat be coated with or elastic coating has more wear-resistant and cracking resistance advantage, and pliable and tough speciality is the be full of cracks of bridging body of wall effectively, and it is regional strongly that its excellent ultra-violet radiation resisting function is particularly useful for sunshine.See through the texture of stereo natural, show the aestheticism artistic style of building especially.Pliable and tough thick and heavy material is selected different instruments and construction gimmick for use, can create the grain effect of different style, makes architectural appearance have uniqueness, activity and individual character.
Embodiment
Below in conjunction with concrete embodiment the present invention is done further explanation.
A kind of middle level elasticity embossment plucking lacquer
,According to weight percent meter, composed of the following components, stopping composition: white cement (32.5) 25%, grey calcium 5%, coarse whiting 35%, permanent white 10%, wollastonite 20%; Rubber powder class: Vltra tears (100,000 viscosity) 0.8%, redispersible latex powder 3.0%, wood fibre 0.5%, pva powder 24-88P 0.7%.Above-mentioned materials is added in the powder stirrer successively, stirred 20-30 minutes, be finished product, adding an amount of water during use can become plucking or anaglyph.
Plucking rolls with plucking, and embossment is used spray gun.
Slightly polishing with emery cloth in construction completion back, can get final product for one to two time by outer brush rubber-emulsion paint.
Claims (3)
1. a middle level elasticity embossment plucking lacquer is characterized in that, and is composed of the following components according to weight percent meter, stopping composition: white cement 25%, grey calcium 5%, coarse whiting 35%, permanent white 10%, wollastonite 20%
Rubber powder class: Vltra tears 0.8%, redispersible latex powder 3.0%, wood fibre 0.5%, pva powder 24-88P 0.7%.
2. middle level according to claim 1 elasticity embossment plucking lacquer, it is characterized in that: described white cement is 325 white cements.
3. middle level according to claim 1 elasticity embossment plucking lacquer, it is characterized in that: the viscosity of described Vltra tears is 100000mPas.