CN102443930A - 一种无弹力丝涤棉混纺面料 - Google Patents
一种无弹力丝涤棉混纺面料 Download PDFInfo
- Publication number
- CN102443930A CN102443930A CN2011103352193A CN201110335219A CN102443930A CN 102443930 A CN102443930 A CN 102443930A CN 2011103352193 A CN2011103352193 A CN 2011103352193A CN 201110335219 A CN201110335219 A CN 201110335219A CN 102443930 A CN102443930 A CN 102443930A
- Authority
- CN
- China
- Prior art keywords
- cotton
- blending
- polyester
- lining
- fibers
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种无弹力丝涤棉混纺面料,由经纱和纬纱交织而成,经纱由涤纶纤维和棉纤维混纺而成,混纺质量百分比为涤纶纤维占40%、棉纤维占60%;纬纱由涤纶短纤维和长绒棉混纺而成,混纺质量百分比为涤纶短纤维占35%、长绒棉占65%。这种不含弹力丝即氨纶丝的涤棉混纺面料,弹性和尺寸稳定,有较好的吸湿排汗性,可用于运动服、休闲服等舒适性服饰,符合当前服装面料向舒适、健康、安全和功能性方面发展的要求。
Description
技术领域
本发明涉及纺织面料领域,特别是涉及一种无弹力丝涤棉混纺面料。
背景技术
吸湿排汗涤纶纤维表面有微细沟槽形成的毛细管,人体表面的湿气和汗水通过毛细管芯吸作用被迅速转移传递到织物外层纤维表面,使内层保持干爽,从而避免了常规涤纶穿着不舒适和闷热感。吸湿排汗涤纶纤维及其混纺产品可用于运动服、休闲服等舒适性服饰,符合当前服装面料向舒适、健康、安全和功能性方面发展的要求。
目前,市场弹力面料需求量大,但大部分含氨纶丝的弹力织物不耐高温,不耐热浓碱,加工时难以去除折痕,难以达到规定的弹性和尺寸稳定性。由于弹力坯布下机后,其幅宽方向的回收缩可高达40%~60%,在加工时,极易导致布面起皱和卷边,生产难度大。含氨纶弹力织物会受到碱和有效氯的攻击,使弹力纤维断健水解,造成弹性和强力下降,并且高温也会损失强力及弹性,因此大大限制了其加工条件,很多功能性整理不适合于氨纶弹力织物,如抗皱整理,防水、防油、防污整理。而一般涤棉混纺织物耐高温,适合于工装面料加工,对加工工艺条件要求不苛刻,适合所有的后整理加工,市场需求量大,价格便宜,颜色丰富、手感柔软,但缺点是弹力较差,穿着不舒服、不美观、档次低。因此,研究一种不含弹力丝即氨纶丝的涤棉混纺面料,获得具有弹力的涤棉混纺面料,可以克服上述织物的缺点,利用其优点。
发明内容
本发明主要解决的技术问题是提供一种无弹力丝涤棉混纺面料,能够获得具有弹力的涤棉混纺面料并且能吸湿排汗。
为解决上述技术问题,本发明采用的一个技术方案是:提供一种无弹力丝涤棉混纺面料,由经纱和纬纱交织而成,经纱由涤纶纤维和棉纤维混纺而成,混纺质量百分比为涤纶纤维占40%、棉纤维占60%;纬纱由涤纶短纤维和长绒棉混纺而成,混纺质量百分比为涤纶短纤维占35%、长绒棉占65%。
在本发明一个较佳实施例中,所述面料经密为90根/英尺。
在本发明一个较佳实施例中,所述面料纬密为50根/英尺。
在本发明一个较佳实施例中,所述涤纶短纤维规格为(1.11dtex~2.22dtex)×(38mm~51mm)的吸湿排汗涤纶异形纤维。
在本发明一个较佳实施例中,所述长绒棉为库尔勒长绒棉。
本发明的有益效果是:本发明生产及产品质量稳定,其织物有较好的吸湿性,其吸湿排汗性可通过控制纱线的细度或织物的组织结构进行调节,是一种不含弹力丝即氨纶丝的涤棉混纺面料,获得具有弹力的涤棉混纺面料。
具体实施方式
下面对本发明的较佳实施例进行详细阐述,以使本发明的优点和特征能更易于被本领域技术人员理解,从而对本发明的保护范围做出更为清楚明确的界定。
一种无弹力丝涤棉混纺面料,由经纱和纬纱交织而成,经纱由涤纶纤维和棉纤维混纺而成,混纺质量百分比为涤纶纤维占40%、棉纤维占60%;纬纱由涤纶短纤维和长绒棉混纺而成,混纺质量百分比为涤纶短纤维占35%、长绒棉占65%。本发明中所称的无弹力丝的涤棉混纺织物的坯布,制造时,不加弹力丝,幅宽为67英寸,纱支经纬为20S,密度为90×50,坯布制造时,制成的是20S以上纱支的涤棉混纺面料,纱支密度越小弹性越好。
所述面料经密为90根/英尺,纬密为50根/英尺;所述涤纶短纤维规格为(1.11dtex~2.22dtex)×(38mm~51mm)的吸湿排汗涤纶异形纤维;所述长绒棉为库尔勒长绒棉。根据吸湿排汗混纺纱的特点,细纱工序采用“低速度、小钳口隔距、重加压”的工艺原则,合理配用钢领和钢丝圈,以减少毛羽和断头。加压量适当偏大,以提高成纱条干水平,减少成纱千米细节、粗节、棉结数量。细纱车间相对湿度适宜,一般控制在57%~60%,使生产正常进行。细纱工序工艺配置为:两品种纺纱锭速均为14000~15000r/min,后区牵伸1~3倍,纱前区牵伸18~30倍;粗纱工序是加工吸湿排汗混纺纱的关键工序,该工序要进一步提高纤维的伸直平行度,改善条干均匀度,粗纱中纤维的抗扭和抗弯刚度的改善对减少成纱毛羽有重要影响,。鉴于上述原因,采用轻定量、小捻度的工艺配置,粗纱定量定为5~6g/10 m,粗纱捻度3~9捻/10cm,前区牵伸8~12倍,后区牵伸1~3倍。这样就能要保持良好的结构,并提高粗纱内在质量,有利于细纱牵伸和摩擦力界的稳定。因此混纺纱的吸湿排汗特性更加稳定,效果更加明显。
本发明生产及产品质量稳定,其织物有较好的吸湿性,其吸湿排汗性可通过控制纱线的细度或织物的组织结构进行调节,是一种不含弹力丝即氨纶丝的涤棉混纺面料,获得具有弹力的涤棉混纺面料。
以上所述仅为本发明的实施例,并非因此限制本发明的专利范围,凡是利用本发明说明书内容所作的等效结构或等效流程变换,或直接或间接运用在其他相关的技术领域,均同理包括在本发明的专利保护范围内。
Claims (5)
1.一种无弹力丝涤棉混纺面料,其特征在于:由经纱和纬纱交织而成,经纱由涤纶纤维和棉纤维混纺而成,混纺质量百分比为涤纶纤维占40%、棉纤维占60%;纬纱由涤纶短纤维和长绒棉混纺而成,混纺质量百分比为涤纶短纤维占35%、长绒棉占65%。
2.根据权利要求1所述无弹力丝涤棉混纺面料,其特征在于:所述面料经密为90根/英尺。
3.根据权利要求1所述无弹力丝涤棉混纺面料,其特征在于:所述面料纬密为50根/英尺。
4.根据权利要求1所述无弹力丝涤棉混纺面料,其特征在于:所述涤纶短纤维规格为(1.11dtex~2.22dtex)×(38mm~51mm)的吸湿排汗涤纶异形纤维。
5.根据权利要求1所述无弹力丝涤棉混纺面料,其特征在于:所述长绒棉为库尔勒长绒棉。