- wood
- solid wood
- impregnated
- soak
- accelerator
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Chemical And Physical Treatments For Wood And The Like (AREA)
Abstract
本发明涉及一种浸塑木的固化方法,将组合单体浸渍于任意型低档实木,装入塑料复合袋真空包装密封后,输送至加速器下,按指定工作参数进行辐照,使其瞬间固化,获得美观,坚硬的优质浸塑木。此技术方案可利用加速器束下设备,直接投入流水线产业化生产,可取得满意的效果。
Description
本发明涉及一种改性浸塑(实)木的固化方法,即在密闭罐里放置任意形状低挡木材,真空,注入单体,充分浸渍单体后取出,再装入复合塑料袋中真空密封,输送至加速器高压电子束流下瞬间固化,即可获得古朴典雅,坚硬的高档浸塑(实)木。
背景技术:
目前共知的(实)木塑复合材料辐射固化法是将浸塑木凭人工搬运到Co-60源室后照射固化,获得的产品色泽稍暗,均匀度稍差的木塑复合材料(ZL 96 1 21219.5).
国内工业用钴源辐照站几乎都是综合用途,专用木塑复合材料的辐照站建设费昂贵,我国还没有。当浸塑木固化时存在凭人工搬运,堆放,控制剂量调解难等诸多不便;更重要的问题是钴源半衰期为5.2年,最大的利用率35-40%,导致损失浪费。日本福岛核电站发生事故以来,公众对核技术恐惧心加大,工作难度增加了。《进入21世纪以来,由于环境问题,废源的处理及钴源供应紧张,不论是美日,还是欧洲大型嘎吗辐照装置的发展速度明显放慢,高能量大功率加速器有替代钴源辐照装置的发展趋势,(中,日,韩放射性同位素与辐射利用会议 报告文集2004,11.29.250页 中国工业嘎吗辐照装置的现状与发展王传祯)》
发明内容:
为适应流水线上生产优质浸塑(实)木,在技术方案上:1,关注苯乙烯,丙烯酸甲酯,过氧化苯甲酰等单体组合。2,利用加速器高压带电离子束流。将真空浸渍单体的(实)木型材用复合塑料袋真空密封后,放置于束下载物循环车上,调整工作参数,让车进入工作室,用带电离子束流辐照,即刻完成固化后匀速驶外,顺利完成固化过程,在流水线上获得优质浸塑(实)木,这样完全可以实现产业化。
具体实施方式:
本发明的目的在于寻找适合于浸塑(实)木产业化生产的新技术方案。首先制备单体组分,即苯乙烯,甲基丙烯酸甲酯,过氧化苯甲酰等。更重要的是,调整好RDI高压型电子加速器参数:电子束能量:3MeV束流;40mA功率:120KW.应用带电粒子束流辐照浸塑(实)木,吸收剂量20-70M rad,瞬间平稳完成固化,获得高档浸塑(实)木。《应用加速器装置不仅结构紧凑,易操作,维修简单,可在任何需要的时候开机,停机,无废源处理,无放射性沾污,更重要的是:一,离子束流的能量和强度,即束功率可在大范围内平滑调节;二,离子束流大,平均流强可达数十数百耗安(mA);三,离子束流方向性强,性能好,利用率达70%以上。(中,日,韩放射性同位素与辐射利用会议 报告文集 275页 应用加速器产业发展的思考 黄正新 赵文彦 等)》
Claims (1)
1.本发明涉及一种改性浸塑木的固化方法,选择低档的任意型天然材,向木质自然间隙里注入液体单体(如:苯乙烯,甲基丙烯酸甲酯等),在电子加速器的高压电子束流照射下,经瞬间固化,使木塑聚合成一个整体,形成美观,优质高档的新材料-实木复合材料。其技术方案要点就是远离放射能,利用指定参数下的电子束流,使浸渍单体的实木瞬间固化,制成典雅并强化的优质浸塑实木,即可转型为规模生产阶段。
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN2011101923528A CN102407546A (zh) | 2010-09-09 | 2011-07-01 | 浸塑木的固化方法 |
Applications Claiming Priority (3)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201020533685.3 | 2010-09-09 | ||
CN201020533685 | 2010-09-09 | ||
CN2011101923528A CN102407546A (zh) | 2010-09-09 | 2011-07-01 | 浸塑木的固化方法 |
Publications (1)
Publication Number | Publication Date |
---|---|
CN102407546A true CN102407546A (zh) | 2012-04-11 |
Family
ID=45910049
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CN2011101923528A Pending CN102407546A (zh) | 2010-09-09 | 2011-07-01 | 浸塑木的固化方法 |
Country Status (1)
Country | Link |
---|---|
CN (1) | CN102407546A (zh) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN105563597A (zh) * | 2015-12-10 | 2016-05-11 | 中国科学院高能物理研究所 | 辐照制备地热地板基材及其加工方法 |
Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH09116203A (ja) * | 1995-10-18 | 1997-05-02 | Tokin Corp | 圧電トランス |
CN1257776A (zh) * | 1998-12-24 | 2000-06-28 | 中国科学院生物物理研究所 | 一种生产防腐、阻燃、力学性能优良的木材高聚物复合材料的方法及产品 |
WO2005042175A1 (en) * | 2003-10-28 | 2005-05-12 | The Research Foundation At State University Of Newyork | Treating wood with reactive monomers |
-
2011
- 2011-07-01 CN CN2011101923528A patent/CN102407546A/zh active Pending
Patent Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH09116203A (ja) * | 1995-10-18 | 1997-05-02 | Tokin Corp | 圧電トランス |
CN1257776A (zh) * | 1998-12-24 | 2000-06-28 | 中国科学院生物物理研究所 | 一种生产防腐、阻燃、力学性能优良的木材高聚物复合材料的方法及产品 |
WO2005042175A1 (en) * | 2003-10-28 | 2005-05-12 | The Research Foundation At State University Of Newyork | Treating wood with reactive monomers |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN105563597A (zh) * | 2015-12-10 | 2016-05-11 | 中国科学院高能物理研究所 | 辐照制备地热地板基材及其加工方法 |
CN105563597B (zh) * | 2015-12-10 | 2018-07-20 | 中国科学院高能物理研究所 | 辐照制备地热地板基材及其加工方法 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN102516570B (zh) | 一种芳纶纤维增强树脂基复合材料及其制备方法 | |
CN105529429B (zh) | 圆柱形锂离子电池的注液方法 | |
NZ705993A (en) | Processing biomass | |
WO2009120868A3 (en) | Filled resins and method for making filled resins | |
CN102407546A (zh) | 浸塑木的固化方法 | |
CN104441136B (zh) | 脲醛树脂浸渍和电子束辐射固化制作木塑复合材料的工艺 | |
CN104277231A (zh) | 一种降解壳聚糖的方法 | |
CN204568793U (zh) | 全自动锂电池x射线检测设备的下料治具移动装置 | |
WO2008068466A3 (en) | Method and apparatus for reducing the radioactivity of a particle | |
CN204747470U (zh) | 一种球墨铸铁用风力清砂装置 | |
CN204145872U (zh) | 一种卧式自屏蔽加速器 | |
CN203831372U (zh) | 一种翻转工装 | |
CN104249802A (zh) | 一种新能源滑板车 | |
CN107278010A (zh) | 一种在等离子体强磁场位置注入中性束的磁镜装置 | |
CN204054682U (zh) | 一种改良的树脂传递成型装置 | |
CN204711516U (zh) | 一种立柱导向套拆解组装装置 | |
CN201711477U (zh) | 搓牙机加料装置 | |
CN202765822U (zh) | 自动加料系统 | |
CN203134387U (zh) | 一种核能控制装置的箱体结构 | |
CN204920344U (zh) | 一种简易升降式立体停车设备导向轮调整装置 | |
CN103694694A (zh) | 一种耐腐蚀性磁性塑胶 | |
CN108163116A (zh) | 一种具有太阳能和摩擦发电双重功能的滑板车 | |
CN202778911U (zh) | 一种用于印铁容器uv机电磁烘干装置 | |
CN206335266U (zh) | 一种激光热切机的收料机构 | |
CN205205660U (zh) | 磁铁增速式缆索机器人安全回程机构 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
C06 | Publication | ||
PB01 | Publication | ||
C10 | Entry into substantive examination | ||
SE01 | Entry into force of request for substantive examination | ||
DD01 | Delivery of document by public notice |
Addressee: Kang Xiruo Document name: the First Notification of an Office Action |
|
C12 | Rejection of a patent application after its publication | ||
RJ01 | Rejection of invention patent application after publication |
Application publication date: 20120411 |