CN102350128A - 一种活性碳纤维滤芯及其制备方法 - Google Patents
一种活性碳纤维滤芯及其制备方法 Download PDFInfo
- Publication number
- CN102350128A CN102350128A CN2011102638085A CN201110263808A CN102350128A CN 102350128 A CN102350128 A CN 102350128A CN 2011102638085 A CN2011102638085 A CN 2011102638085A CN 201110263808 A CN201110263808 A CN 201110263808A CN 102350128 A CN102350128 A CN 102350128A
- Authority
- CN
- China
- Prior art keywords
- activated carbon
- carbon fiber
- fiber filter
- filter core
- preparation
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种活性碳纤维滤芯及其制备方法,其主要是将组成原料有硅藻土、高岭土、三聚氰酰胺聚酯、木质粉、粘合剂、水、碳粉、秸秆灰烬、蛭石、天然沸石、碎毛发按一定重量份比例混合搅拌后经注浆成型或压坯成型,干燥后在900-1300℃煅烧,即得该活性碳纤维滤芯。本发明制备方法简单,配方合理,成本低,制得的活性碳纤维滤芯耐热、耐磨性好。
Description
技术领域
本发明涉及一种活性碳纤维滤芯及其制备方法,属于汽车制造领域。
背景技术
众所周知,传统的活性碳纤维滤芯的滤孔均极细微,并呈高密度分布,因此对于水浊度较高的地区,极容易遭污泥或铁锈等较粗颗粒杂质阻塞,而影响其过滤水量,故通常均于该高密度滤芯的前面再设置一道或一道以上具有较大滤孔的低密度滤芯,利用前置滤芯预先去除水中较粗颗粗杂质、污泥、悬浮物质等,借以保护后置活性碳滤芯、离子交换树脂滤芯或半透膜(R0)滤芯等高密度滤芯,使其不致被较粗颗粗杂质被覆而影响其滤净或吸附等功能。其主要缺陷在于:常用的前置滤芯,其不外乎是由PP塑胶、纤维、毛线等材质构成,故一经阻塞后即必须抛弃,无法再次冲洗以供重复使用,其不仅消耗性大,造成人力物力负担,且由于不符合环保条件,无法在短时间内完成分解,以致在日后均成为环境高污染物质,不符合经济环保要求。
发明内容
为了解决现有技术的不足和缺陷,本发明的目的在于提供一种活性碳纤维滤芯及其制备方法。本发明制备方法简单,配方合理,成本低,制得的活性碳纤维滤芯耐热、耐磨性好。
为了实现上述目的本发明采用如下技术方案:
活性碳纤维滤芯,其特征在于其组成原料的重量份为:有硅藻土37-39份、高岭土10-15份、三聚氰酰胺聚酯20-30份、木质粉6-9份、粘合剂6-8份、水40-50份、碳粉10-15份、秸秆灰烬3-5份、蛭石10-15份、天然沸石10-15份、碎毛发10-15份。
所述的活性碳纤维滤芯的制备方法,其特征在于:按组成原料的重量份称取各组成原料,混合搅拌后经注浆成型或压坯成型,干燥后在900-1300℃煅烧,即得该活性碳纤维滤芯。
所述的活性碳纤维滤芯,其特征在于:所述的粘合剂选自粘合剂CMC。
本发明的有益效果:
本发明制备方法简单,配方合理,成本低,制得的活性碳纤维滤芯耐热、耐磨性好。
具体实施方式
实施例1:活性碳纤维滤芯,其组成原料的重量份为:有硅藻土38份、高岭土10份、三聚氰酰胺聚酯20份、木质粉7份、粘合剂CMC 7份、水45份、碳粉12份、秸秆灰烬4份、蛭石12份、天然沸石12份、碎毛发12份。
活性碳纤维滤芯的制备方法:按组成原料的重量份称取各组成原料,混合搅拌后经注浆成型或压坯成型,干燥后在900-1300℃煅烧,即得该活性碳纤维滤芯。
所制得活性碳纤维滤芯的静态水吸附量17.5%;抗压强度4765N;相容性0.0085%。
实施例2:活性碳纤维滤芯,其组成原料的重量份为:有硅藻土39份、高岭土15份、三聚氰酰胺聚酯30份、木质粉6份、粘合剂CMC 6份、水50份、碳粉10份、秸秆灰烬3份、蛭石10份、天然沸石10份、碎毛发10份。
活性碳纤维滤芯的制备方法:按组成原料的重量份称取各组成原料,混合搅拌后经注浆成型或压坯成型,干燥后在900-1300℃煅烧,即得该活性碳纤维滤芯。
所制得活性碳纤维滤芯的静态水吸附量17.8%;抗压强度4978N;相容性0.0092%。
实施例3:活性碳纤维滤芯,其组成原料的重量份为:有硅藻土38份、高岭土12份、三聚氰酰胺聚酯25份、木质粉9份、粘合剂CMC 8份、水40份、碳粉15份、秸秆灰烬5份、蛭石15份、天然沸石15份、碎毛发15份。
活性碳纤维滤芯的制备方法:按组成原料的重量份称取各组成原料,混合搅拌后经注浆成型或压坯成型,干燥后在900-1300℃煅烧,即得该活性碳纤维滤芯。
所制得活性碳纤维滤芯的静态水吸附量18.3%;抗压强度4980N;相容性0.0094%。
Claims (3)
1.一种活性碳纤维滤芯,其特征在于其组成原料的重量份为:有硅藻土37-39份、高岭土10-15份、三聚氰酰胺聚酯20-30份、木质粉6-9份、粘合剂6-8份、水40-50份、碳粉10-15份、秸秆灰烬3-5份、蛭石10-15份、天然沸石10-15份、碎毛发10-15份。
2.一种如权利要求1所述的活性碳纤维滤芯的制备方法,其特征在于:按组成原料的重量份称取各组成原料,混合搅拌后经注浆成型或压坯成型,干燥后在900-1300℃煅烧,即得该活性碳纤维滤芯。
3.根据权利要求1所述的活性碳纤维滤芯,其特征在于:所述的粘合剂选自粘合剂CMC。