CN102304593A - 一种铁水预处理渣打水冷却方法 - Google Patents

一种铁水预处理渣打水冷却方法 Download PDF

Info

Publication number
CN102304593A
CN102304593A CN201110270463A CN201110270463A CN102304593A CN 102304593 A CN102304593 A CN 102304593A CN 201110270463 A CN201110270463 A CN 201110270463A CN 201110270463 A CN201110270463 A CN 201110270463A CN 102304593 A CN102304593 A CN 102304593A
Authority
CN
China
Prior art keywords
slag
cooling
spray
spray water
ton
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201110270463A
Other languages
English (en)
Inventor
罗胜
雷玮
史永林
马达
高卯根
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanxi Taigang Stainless Steel Co Ltd
Original Assignee
Shanxi Taigang Stainless Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanxi Taigang Stainless Steel Co Ltd filed Critical Shanxi Taigang Stainless Steel Co Ltd
Priority to CN201110270463A priority Critical patent/CN102304593A/zh
Publication of CN102304593A publication Critical patent/CN102304593A/zh
Pending legal-status Critical Current

Abstract

一种铁水预处理渣打水冷却方法,属于冶金炼铁领域,在冷却场地铁路线上方设置喷淋水嘴,预处理渣使用渣罐经铁道线运输至冷却现场,打开喷淋水阀门,其喷淋水流量为4-6吨/小时,喷淋时间为10-20小时,吨渣耗水量为0.3-0.6吨。喷淋水淬后预处理渣经冷却过程,由渣砣基本变为粉状,不存在红渣,不产生扬尘,渣冷却时间短,加快了渣罐运输周转。

Description

一种铁水预处理渣打水冷却方法
技术领域:
本发明属于冶金炼铁领域,具体涉及一种铁水预处理渣打水冷却方法。
背景技术
铁水预处理渣是冶金企业在冶炼前为了使原料铁水符合要求对铁水进行预处理产生的。铁水预处理可分为以降低S含量为目的预处理和以降低P、S、Si含量为目的预处理两种。脱除S预处理产生的铁水渣称脱硫渣,渣中S含量较高;脱除P、S、Si的预处理产生的铁水渣称三脱渣,渣中P、S、Si的含量较高。
目前普遍应用的预处理渣自然空冷存在以下问题:渣容易结成大块,为后步渣处理带来难度;空冷需时间较长,难以满足冶金过程生产节奏;冷却后作业不当容易产生扬尘。
还有一些冶金企业把预处理渣汇入普通钢渣合并处理,缺点在于和普通渣钢发生混料,增大了整批钢渣中选出的金属料的P、S含量。
发明内容
为了缩短冷却时间,同时避免扬尘污染,本发明提供一种铁水预处理渣打水冷却方法。
冷却场地铁路线上方设置喷淋水嘴,预处理渣使用渣罐经铁道线运输至冷却现场,打开喷淋水阀门,其喷淋水流量为4-6吨/小时,喷淋时间为10-20小时,吨渣耗水量为0.3-0.6吨。
喷淋水淬后预处理渣经冷却过程,由渣砣基本变为粉状,不存在红渣,不产生扬尘。喷淋过程结束后倾翻到指定场地,再运输到处理线进行后步处理。
本发明可解决预处理渣的冷却问题,避免扬尘污染;水淬急冷后,避免了大渣砣的形成,为铁水预处理渣的后步处理创造条件;缩短了渣冷却时间,加快了渣罐运输周转;减少了大渣砣的再次运输、加工处理的环节,降低了加工成本。
具体实施方式
冷却场地铁路线上方设置喷淋水嘴,预处理渣使用渣罐经铁道线运输至冷却现场,打开喷淋水阀门,其喷淋水流量为4-6吨/小时,喷淋时间为12小时。
喷淋过程预处理渣即在渣罐内冷却,该过程中钢渣中的渣砣基本变为粉状,不存在红渣,不产生扬尘。喷淋过程结束后无需静置,即可将渣罐运输到钢渣处理线进行后步处理。

Claims (1)

1. 一种铁水预处理渣打水冷却方法,其特征是在冷却场地铁路线上方设置喷淋水嘴,预处理渣使用渣罐经铁道线运输至冷却现场,打开喷淋水阀门,其喷淋水流量为4-6吨/小时,喷淋时间为10-20小时,吨渣耗水量为0.3-0.6吨。
CN201110270463A 2011-09-14 2011-09-14 一种铁水预处理渣打水冷却方法 Pending CN102304593A (zh)