CN102039767A - 一种蚀刻铜板画的制作方法 - Google Patents
一种蚀刻铜板画的制作方法 Download PDFInfo
- Publication number
- CN102039767A CN102039767A CN2009102043551A CN200910204355A CN102039767A CN 102039767 A CN102039767 A CN 102039767A CN 2009102043551 A CN2009102043551 A CN 2009102043551A CN 200910204355 A CN200910204355 A CN 200910204355A CN 102039767 A CN102039767 A CN 102039767A
- Authority
- CN
- China
- Prior art keywords
- etching
- pattern
- copperplate
- preparation
- polishing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种蚀刻铜板画的制作方法,利用本方法可制作出精美、大方、耐用、高雅的铜板画。本发明通过以下技术方案实现:用干净纱布蘸二甲苯或酒精揩去铜板表面油污,将已设计好的样画用复写纸印到铜板上,然后用不干胶把整块铜板全部密封起来。用刻刀按画面线条将图案镂空。刻画后将镂空画的铜板反面,放在热源上微微加热,排除空气。用蚀刻液浇到画面上,随即停止腐蚀,迅速用清水洗掉蚀刻液。用较细的金相砂纸按固定方向进行打磨抛光,抛光的要求是光亮平整,无痕迹划伤。用油漆或颜料进行着色后,用丙烯酸清漆罩光保护,或用丙烯酸烤漆罩光。
Description
技术领域:
本发明是关于工艺品的加工制作方法,更具体地说是一种关于蚀刻铜板画的制作方法。
背景技术:
铜板画的制造方法一般采用制画面胶片,铜板涂感光涂层膜,胶片和铜板贴紧进行感光处理,再将铜板进行显影、腐蚀、退感光涂层膜、上色、防腐、剪切、装框等几个工序组成的。该方成本比较高,而且没有进行罩光处理,产品容易退色。
发明内容:
本发明的目的是克服现有技术的缺点,提供一种新的铜板画制作方法。利用本技术方法制作的铜板画更加精美、大方、耐用、高雅。
本发明通过以下技术方案实现的:
1、清洗:用干净纱布蘸二甲苯或酒精揩两遍,除去铜板表面油污。为防止引燃,操作时严禁明火,不准吸烟。如没有二甲苯或酒精,亦可用热水掺高效洗衣粉替。但揩擦后,应再用干纱布揩干水分。
2、印画:将已设计好的样画用复写纸印到铜板上,然后用不干胶把整块铜板全部覆盖起来,要求密封。
3、刻版:用刻刀按画面线条将图案镂空。版面图案全部刻完后,为防止在刻画过程中周边的不干胶发生微小松动,导致蚀刻出来的画面产生毛边,刻画后应将镂空画的铜板反面,放在热源上微微加热,让不干胶软化,再用手在正面按压一遍,排除空气。
4、蚀刻:镂空的画面处已没有不干胶盖住,此时用蚀刻液(或盐酸8毫升,硝酸25.5毫升配制而成)浇到画面上。操作时要戴橡塑手套,以免烧伤。1次不行可进行2次或3次,直至认为达到要求后,即停止腐蚀,迅速用清水洗掉蚀刻液。然后,揭去不干胶,揩干水渍。
5、抛光:手工抛光可用较细的金相砂纸打磨抛光,打磨时须按固定方向进行,否则抛光面痕迹较难除去。也可在抛光机上抛光,还可用手电钻改制成小型抛光机使用。在抛光时应先将抛光膏涂在抛光轮上。抛光的要求是光亮平整,无痕迹划伤。
6、罩光:作品在着色前必须用酒精将表面清洗干净。经过清洗的作品,不能再用手接触,以免污染画面。操作时最好戴上白色手套。着色可用油漆或颜料,着色完毕待油漆或颜料干后,即可用丙烯酸清漆罩光保护,或用丙烯酸烤漆罩光更好。
具体实施方式:
1、裁料:按客户要求剪裁铜板。剪裁要方正,四角均为90度,四周折边或焊边,边向背面折,与铜板面成90度,边宽2-3厘米。
2、清洗:用干净纱布蘸二甲苯或酒精揩两遍,除去铜板表面油污。为防止引燃,操作时严禁明火,不准吸烟。如没有二甲苯或酒精,亦可用热水掺高效洗衣粉代替。但揩擦后,应再用干纱布揩干水分。
3、印画:将已设计好的样画用复写纸印到铜板上,然后用不干胶把整块铜板全部覆盖起来,要求密封。
4、刻版:用刻刀按画面线条将图案镂空。版面图案全部刻完后,为防止在刻画过程中周边的不干胶发生微小松动,导致蚀刻出来的画面产生毛边,刻画后应将镂空画的铜板反面,放在热源上微微加热,让不干胶软化,再用手在正面按压一遍,排除空气。
5、蚀刻:镂空的画面处已没有不干胶盖住,此时用蚀刻液(或盐酸8毫升,硝酸25.5毫升配制而成)浇到画面上。操作时要戴橡塑手套,以免烧伤。1次不行可进行2次或3次,直至认为达到要求后,即停止腐蚀,迅速用清水洗掉蚀刻液。然后,揭去不干胶,揩干水渍。
6、抛光:手工抛光可用较细的金相砂纸打磨抛光,打磨时须按固定方向进行,否则抛光面痕迹较难除去。也可在抛光机上抛光,还可用手电钻改制成小型抛光机使用。在抛光时应先将抛光膏涂在抛光轮上。抛光的要求是光亮平整,无痕迹划伤。
7、罩光:作品在着色前必须用酒精将表面清洗干净。经过清洗的作品,不能再用手接触,以免污染画面。操作时最好戴上白色手套。着色可用油漆或颜料,着色完毕待油漆或颜料干后,即可用丙烯酸清漆罩光保护,或用丙烯酸烤漆罩光更好。
注意事项
1、蚀刻铜板应选择表面光滑无伤痕的板材。
2、在配制蚀刻液时,要按要求配制并戴好防护镜、手套、口罩等,要做好通风。操作中严禁将水掺入酸中,以防溅出烧伤人;酸需要加水稀释时,只能将酸液缓慢加入适量冷水中,并不断搅拌。
3、蚀刻时每道工序完成后,要用水冲洗才能进行下道工序。
Claims (7)
1.一种蚀刻铜板画的制作方法,其特征在于铜板的制作工序有:清洗、印画、刻版、蚀刻、抛光、罩光。
2.根据权利要求1所述一种蚀刻铜板画的制作方法,其特征在于:所述清洗是用干净纱布蘸二甲苯或酒精揩除铜板表面油污。
3.根据权利要求1所述一种蚀刻铜板画的制作方法,其特征在于:所述印画是将已设计好的样画用复写纸印到铜板上,然后用不干胶把整块铜板全部密封起来。
4.根据权利要求1所述一种蚀刻铜板画的制作方法,其特征在于:所述刻版是用刻刀按画面线条将图案镂空。
5.根据权利要求1所述一种蚀刻铜板画的制作方法,其特征在于:所述蚀刻是用蚀刻液(盐酸8毫升,硝酸25.5毫升配制而成)浇到画面上。
6.根据权利要求1所述一种蚀刻铜板画的制作方法,其特征在于:所述抛光是用较细的金相砂纸按固定方向进行打磨抛光,抛光的要求是光亮平整,无痕迹划伤。
7.根据权利要求1所述一种蚀刻铜板画的制作方法,其特征在于:所述罩光是作品着色完毕待油漆或颜料干后,用丙烯酸清漆或者丙烯酸烤漆罩光保护。