CN101915643A - 焊缝气压试漏工艺 - Google Patents
焊缝气压试漏工艺 Download PDFInfo
- Publication number
- CN101915643A CN101915643A CN 201010220725 CN201010220725A CN101915643A CN 101915643 A CN101915643 A CN 101915643A CN 201010220725 CN201010220725 CN 201010220725 CN 201010220725 A CN201010220725 A CN 201010220725A CN 101915643 A CN101915643 A CN 101915643A
- Authority
- CN
- China
- Prior art keywords
- leak test
- weld seam
- metal mouth
- test metal
- leakage check
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种焊缝气压试漏工艺,包括清理焊缝、制作焊缝试漏金属嘴和试漏接管、焊接焊缝试漏金属嘴、试漏检查等步骤。本发明工艺简单,针对焊缝试漏,加气空间小、试漏时间短,因此大大减少了工时;试漏压力小,对焊缝无损伤,而且用洗涤剂水可以快而确切地找准缺陷;可检查焊缝健全性,因此可靠性大;本发明与现有无损检查不同,无需专家分析,普通操作人员也可进行检查操作,发现是否存在焊接缺陷;本发明无需购买专用检测设备,节约检测费用。
Description
技术领域:
本发明涉及一种焊缝气压试漏工艺。
背景技术:
对变压器中间有间隙的焊缝(接头焊缝)及法兰内径蹲放式结构,目前尚无较好的试漏方法。
发明内容:
本发明的目的在于提供一种方法简单、试漏效果好的焊缝气压试漏工艺。
本发明的技术解决方案是:
一种焊缝气压试漏工艺,其特征是:包括下列步骤:
(1)清理焊缝:将焊缝表面进行清洁处理;
(2)制作焊缝试漏金属嘴和试漏接管:焊缝试漏金属嘴为一中空金属件,中空金属件的端部表面呈锥状面;试漏接管为与一端与焊缝试漏金属嘴连接,另一端与送气管连接的管子;
(3)焊接焊缝试漏金属嘴:将焊缝试漏金属嘴点焊在焊缝的外侧、焊缝对应的两金属件接合处,焊缝试漏金属嘴端部的锥状面与焊缝对应的两金属件接合处接触;焊接时,从焊缝试漏金属嘴一侧至少50mm处向焊缝试漏金属嘴方向焊接,焊接焊缝试漏金属嘴的上半周,从焊缝试漏金属嘴另一侧至少50mm处向焊缝试漏金属嘴方向焊接,焊接焊缝试 漏金属嘴的下半周;
(4)试漏检查:将试漏接管一端与焊缝试漏金属嘴连接,另一端与送气管连接;然后充气、保压;在焊缝上涂上洗涤液,若发现冒气泡,用粉笔做标记,并对粉笔标记部分进行再焊接,并重新实施试漏检查;如无冒气泡现象,即可放气。
本发明工艺简单,针对焊缝试漏,加气空间小、试漏时间短,因此大大减少了工时;试漏压力小,对焊缝无损伤,而且用洗涤剂水可以快而确切地找准缺陷;可检查焊缝健全性,因此可靠性大;本发明与现有无损检查不同,无需专家分析,普通操作人员也可进行检查操作,发现是否存在焊接缺陷;本发明无需购买专用检测设备,节约检测费用。
附图说明:
下面结合附图和实施例对本发明作进一步说明。
图1是本发明焊缝试漏金属嘴的结构示图。
图2是试漏接管的结构示图。
图3是焊接焊缝试漏金属嘴的示意图。
图4、图5是本发明不同焊缝形式时的试验状态图。
具体实施方式:
一种焊缝气压试漏工艺,包括下列步骤:
(1)清理焊缝:将焊缝表面进行清洁处理;
(2)制作焊缝试漏金属嘴和试漏接管:焊缝试漏金属嘴1为一中空金属件,中空金属件的端部表面呈锥状面;试漏接管2为与一端与焊缝试漏金属嘴连接,另一端与送气管连接的管子;
(3)焊接焊缝试漏金属嘴:将焊缝试漏金属嘴点焊在焊缝的外侧、焊缝对应的两金属件接合处,焊缝试漏金属嘴端部的锥状面与焊缝对应的两金属件接合处接触;焊接时,从焊缝试漏金属嘴一侧至少50mm处向焊缝试漏金属嘴方向焊接,焊接焊缝试漏金属嘴的上半周,从焊缝试漏金属嘴另一侧至少50mm处向焊缝试漏金属嘴方向焊接,焊接焊缝试漏金属嘴的下半周;
(4)试漏检查:将试漏接管一端(设有外螺纹)插入焊缝试漏金属嘴中螺纹连接,另一端(台阶状一端)与送气管连接;然后充气、保压;在焊缝上涂上肥皂水或其他洗涤液,若发现冒气泡,用粉笔做标记,并对粉笔标记部分进行再焊接,并重新实施试漏检查;如无冒气泡现象,即可放气。
Claims (1)
1.一种焊缝气压试漏工艺,其特征是:包括下列步骤:
(1)清理焊缝:将焊缝表面进行清洁处理;
(2)制作焊缝试漏金属嘴和试漏接管:焊缝试漏金属嘴为一中空金属件,中空金属件的端部表面呈锥状面;试漏接管为与一端与焊缝试漏金属嘴连接,另一端与送气管连接的管子;
(3)焊接焊缝试漏金属嘴:将焊缝试漏金属嘴点焊在焊缝的外侧、焊缝对应的两金属件接合处,焊缝试漏金属嘴端部的锥状面与焊缝对应的两金属件接合处接触;焊接时,从焊缝试漏金属嘴一侧至少50mm处向焊缝试漏金属嘴方向焊接,焊接焊缝试漏金属嘴的上半周,从焊缝试漏金属嘴另一侧至少50mm处向焊缝试漏金属嘴方向焊接,焊接焊缝试漏金属嘴的下半周;
(4)试漏检查:将试漏接管一端与焊缝试漏金属嘴连接,另一端与送气管连接;然后充气、保压;在焊缝上涂上洗涤液,若发现冒气泡,用粉笔做标记,并对粉笔标记部分进行再焊接,并重新实施试漏检查;如无冒气泡现象,即可放气。