CN101892330A - 降低甲醛含量的皮革加工方法 - Google Patents
降低甲醛含量的皮革加工方法 Download PDFInfo
- Publication number
- CN101892330A CN101892330A CN2010102176217A CN201010217621A CN101892330A CN 101892330 A CN101892330 A CN 101892330A CN 2010102176217 A CN2010102176217 A CN 2010102176217A CN 201010217621 A CN201010217621 A CN 201010217621A CN 101892330 A CN101892330 A CN 101892330A
- Authority
- CN
- China
- Prior art keywords
- leather
- formaldehyde
- formaldehyde content
- dyeing
- product
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开一种降低甲醛含量的皮革加工方法,在填充染色加脂工序中,采用RDN、203和OS作为填充树脂材料,先进行填充;在染色、固酸、水洗后,再在30℃下,加入与皮料质量相等的水,以及占皮料质量1%的甲醛捕促剂在转鼓中转动40分钟,即出皮交下一工序。本发明一方面通过填充材料方面降低了皮革产品的甲醛含量;另一方面通过增加清除工序进一步降低了皮革产品的甲醛含量。本发明制得产品在测试中甲醛含量低于20ppm,达到童孩用品的要求。
Description
技术领域
本发明涉及皮革的加工方法,特别与可以降低甲醛含量的皮革加工方法有关。
背景技术
甲醛是无色、具有强烈刺激性气味,是一种原浆毒物,能与蛋白质结合。吸入高浓度甲醛后,会出现呼吸道的严重刺激和水肿、眼刺痛、头痛,也可发生支气管哮喘。皮肤直接接触甲醛,可引起皮炎、色斑、坏死等。经常吸入少量甲醛,能引起慢性中毒,出现粘膜充血、皮肤刺激症、过敏性皮炎、指甲角化和脆弱、甲床指端疼痛等,可表现出头痛、乏力、胃纳差、心悸、失眠、体重减轻以及植物神经紊乱等各种症状。大量使用粘合剂的地方,比如人造板,常会含有甲醛。此外,甲醛还可来自纺织品、皮革制品、化妆品、清洁剂、杀虫剂、消毒剂、防腐剂、印刷油墨、纸张等多类产品。
现有技术中,皮革加工方法是:毛皮组批——称重——预浸水——水洗——主浸水——保毛脱毛浸灰——出鼓——去肉——修边——片皮——称重——无铵脱灰——无铵软化——水洗——浸酸——排水——鞣制——加废铬夜——提碱——废铬液升温——废铬液回收——蓝皮出鼓——搭马——入库——分级——搭马陈放——挤水——削匀——回湿——排水——复鞣——排水——中和——水洗——填充染色加脂——固定——降温——出鼓搭马——静置——挤水伸展——真空——挂晾干燥——回湿——打软——回油——摔软——出鼓——绷板——入库分选——涂饰。
通常,在填充染色加脂工序中,是采用R16、DFS2、R11和OS等作为填充树脂材料,这些材料含甲醛都在200ppm以上。加工时,先将根据皮革产品加工的具体配方,将相应比例的DFS2或R11、R16和OS放入转鼓中转45分钟。
如此加工生产,制得的产品中甲醛含量在50~150ppm范围内,而欧盟进口要求在成人用品的甲醛含量应低于50ppm,童孩用品的甲醛含量应低于20ppm,产品中的甲醛含量太高,达不到欧盟进口产品的要求,实有待于改进。
发明目的
本发明的目的是在于提供一种降低甲醛含量的皮革加工方法,使产品的甲醛含量达到要求。
为了达到上述目的,本实用新型的解决方案是:
降低甲醛含量的皮革加工方法,在填充染色加脂工序中,采用RDN、203和OS作为填充树脂材料,先进行填充;在染色、固酸、水洗后,再在30℃下,加入与皮料质量相等的水,以及占皮料质量1%的甲醛捕促剂在转鼓中转动40分钟,即出皮交下一工序。
采用上述方案后,本发明与现有技术相比:
一、在填充染色加脂工序中,选择低游离甲醛的材料RDN代替原有高甲醛含量的R16、DFS2、R11,RDN是一种密胺类的填充树脂单宁,成革柔软饱满,RDN产品含甲醛在20以下,已完全进行缩合反应,不会放出甲醛气体,而多种树脂鞣剂常有的缺点是使浴液或皮革中放出甲醛气体等,所以,本发明首先通过填充材料方面降低了皮革产品的甲醛含量;
二、在染色固酸水洗后,再加入甲醛捕促剂彻底清除游离甲醛,所以,本发明还通过增加清除工序进一步降低了皮革产品的甲醛含量。
这样,本发明可确保制得的皮革产品测试达标。制得产品在测试中甲醛含量低于20ppm,达到童孩用品的要求。
具体实施例
本发明揭示了一种降低甲醛含量的皮革加工方法,是对原有加工方法的改进。在原有的其他工序不变的基础上,仅将填充染色加脂工序中采用的填充树脂由原来的R16、DFS2、R11和OS改为RDN、203和OS,选择低游离甲醛的材料RDN代替原有高甲醛含量的R16、DFS2、R11,选择蛋白有机填料203代替部分填充树脂用量,使材料的甲醛含量降低;在染色、固酸、水洗后,在30℃下,加入与皮料质量相等的水,以及占皮料质量1%的甲醛捕促剂在转鼓中转动40分钟,出皮交下一工序。
所述的甲醛捕捉剂是可高效去除革中的游离甲醛,对其他性能无影响,使用方便。用于染色固酸后,也可在染色加油固酸后换新液使用,再进行正常的套染固色等。根据皮中可能含有的游离甲醛量添加本产品。甲醛捕捉剂为无色液体,Ph值(1∶9):3.0~4.5,有效物含量(%):39±1.0。
具体实施例
在生产皮革时,原填充染色加脂工序所用的填充配方中DFS2或R111.5%,R16 1.5%,OS1%改为RDN 1.5%,203 1.5%,OS 1%,在转鼓中转动45分钟,进行填充,染色、固酸、水洗后,在30℃下,加入与皮料质量相等的水,以及占皮料质量1%的甲醛捕促剂在转鼓中转动40分钟,即出皮交下一工序。
制得产品在测试中甲醛含量低于20ppm,达到童孩鞋的要求。
Claims (1)
1.降低甲醛含量的皮革加工方法,其特征在于:在填充染色加脂工序中,采用RDN、203和OS作为填充树脂材料,先进行填充;在染色、固酸、水洗后,再在30℃下,加入与皮料质量相等的水,以及占皮料质量1%的甲醛捕促剂在转鼓中转动40分钟,即出皮交下一工序。