CN101869861A - 重钙湿法研磨分散剂的滴加方法 - Google Patents

重钙湿法研磨分散剂的滴加方法 Download PDF

Info

Publication number
CN101869861A
CN101869861A CN 201010211615 CN201010211615A CN101869861A CN 101869861 A CN101869861 A CN 101869861A CN 201010211615 CN201010211615 CN 201010211615 CN 201010211615 A CN201010211615 A CN 201010211615A CN 101869861 A CN101869861 A CN 101869861A
Authority
CN
China
Prior art keywords
dispersant
slurry
pulp
vertical
ground
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 201010211615
Other languages
English (en)
Other versions
CN101869861B (zh
Inventor
李刚
罗兴华
周俊
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
CHANGDE LEIXIN MINERALS TECHNOLOGY Co Ltd
Original Assignee
CHANGDE LEIXIN MINERALS TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by CHANGDE LEIXIN MINERALS TECHNOLOGY Co Ltd filed Critical CHANGDE LEIXIN MINERALS TECHNOLOGY Co Ltd
Priority to CN2010102116150A priority Critical patent/CN101869861B/zh
Publication of CN101869861A publication Critical patent/CN101869861A/zh
Application granted granted Critical
Publication of CN101869861B publication Critical patent/CN101869861B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

重钙湿法研磨分散剂的滴加方法,用2台立式搅拌磨串联生产,1号磨进行粗磨,2号磨进行细磨,选用的分散剂为聚丙烯酸钠盐和聚丙烯酸,依据重钙浆料的pH值选用,当浆料呈中性时,选用中性的聚丙烯酸钠盐,当浆料呈碱性时,选用酸性的聚丙烯酸,浆料的固含量为75~78%,浆料中,固体矿物为方解石或石灰石,分散剂滴加后,分散剂的分子将矿物颗粒进行包裹,降低了矿物颗粒之间的粘聚性,增加了浆料的流便性和分散助磨性,搅拌磨上部的滴加,使浆料溢流更加流畅,使浆料顺利通过筛网,搅拌磨中部的滴加,提高了浆料的可磨性,提高了磨机的效率,同时也调节了浆料的pH值,使浆料呈现出弱碱性的稳定状态。

Description

重钙湿法研磨分散剂的滴加方法
技术领域
本发明涉及重钙湿法研磨的生产,即重钙湿法研磨分散剂的滴加方法。
背景技术
高目度的矿物粉体的湿法研磨技术国外70年代已开始研究,在研磨的浆料中,分散剂的滴加是湿法粉剂研磨的一项重要技术,国内的湿法研磨,2000年才起步,用国产的研磨设备生产高目度浆料,分散剂的滴加尚没有成熟的方法,特别是D98级超微细浆钙,国内由于对分散剂的滴加方法没有掌握,产品生产不出来,技术质量指标达不到标准。
发明内容
针对国产的3600升立式搅拌研磨设备和方解石为主的矿石特性,为了生产D98级的浆钙,本发明提出了一种重钙湿法研磨分散剂的滴加方法。
这种重钙湿法研磨分散剂的滴加方法,用2台立式搅拌磨串联生产,1号磨进行粗磨,2号磨进行细磨,选用的分散剂为聚丙烯酸钠盐和聚丙烯酸,其特征在于,依据重钙浆料的PH值选用,当浆料呈中性时,选用中性的聚丙烯酸钠盐,当浆料呈碱性时,选用酸性的聚丙烯酸,浆料的固含量为75~78%,浆料中,固体矿物为方解石或石灰石,其化学成份主要为CaCO3,每吨滴加时浆料温度为25℃~60℃。
分散剂在1号立式搅拌磨机中滴加量为每吨浆料滴加4~5kg;在2号立式搅拌磨机中,滴加量为每吨浆料滴加3~4kg。
注入前先将分散剂溶于水中,在1号立式搅拌磨中,水与分散剂的比为1∶1~2,在2号立式搅拌磨中,水与分散剂的比为1∶2~3,然后用滴加泵注入,连续生产,连续注入。
在1号立式搅拌磨中,从顶部和中部同时注入,顶部的注入量为1号立式搅拌磨总量的1/4,在中部的注入量为1号立式搅拌磨总量的3/4;在2号立式搅拌磨中,也是从顶部和中部同时注入,顶部的注入量为2号立式搅拌磨总量的1/3,在中部的注入量为2号立式搅拌磨总量的2/3。
在1号立式搅拌磨中,主要滴加中性的分散剂,在2号立式搅拌磨中,主要滴加中性偏酸性的分散剂。
分散剂滴加后,分散剂的分子将矿物颗粒进行包裹,降低了矿物颗粒之间的粘聚性,增加了浆料的流便性和分散助磨性,搅拌磨上部的滴加,使浆料溢流更加流畅,使浆料顺利通过筛网,搅拌磨中部的滴加,提高了浆料的可磨性,提高了磨机的效率,同时也调节了浆料的PH值,使浆料呈现出弱碱性的稳定状态。
具体实施方式
下面举1个实施例对本发明详细说明如下:这种重钙湿法研磨分散剂的滴加方法,用2台立式搅拌磨串联生产,1号磨进行粗磨,2号磨进行细磨,选用的分散剂为聚丙烯酸钠盐和聚丙烯酸,依据重钙浆料的PH值选用,当浆料呈中性时,选用中性的聚丙烯酸钠盐,当浆料呈碱性时,选用酸性的聚丙烯酸,浆料的固含量为76%,浆料中,固体矿物为方解石,其化学成份主要为CaCO3,每吨滴加时浆料温度为28℃,分散剂在1号立式搅拌磨机中滴加量为每吨浆料滴加4.5kg;在2号立式搅拌磨机中,滴加量为每吨浆料滴加3.5kg。
注入前先将分散剂溶于水中,在1号立式搅拌磨中,水与分散剂的比为1∶1.5,在2号立式搅拌磨中,水与分散剂的比为1∶2.5,然后用滴加泵注入,连续生产,连续注入。
在1号立式搅拌磨中,从顶部和中部同时注入,顶部的注入量为1号立式搅拌磨总量的1/4,在中部的注入量为1号立式搅拌磨总量的3/4;在2号立式搅拌磨中,也是从顶部和中部同时注入,顶部的注入量为2号立式搅拌磨总量的1/3,在中部的注入量为2号立式搅拌磨总量的2/3。
在1号立式搅拌磨中,主要滴加中性的分散剂聚丙烯酸钠盐,在2号立式搅拌磨中,主要滴加中性偏酸性的分散剂聚丙烯酸。

Claims (5)

1.重钙湿法研磨分散剂的滴加方法,用2台立式搅拌磨串联生产,1号磨进行粗磨,2号磨进行细磨,选用的分散剂为聚丙烯酸钠盐和聚丙烯酸,其特征在于,依据重钙浆料的PH值选用,当浆料呈中性时,选用中性的聚丙烯酸钠盐,当浆料呈碱性时,选用酸性的聚丙烯酸,浆料的固含量为75~78%,浆料中,固体矿物为方解石或石灰石,其化学成份主要为CaCO3,每吨滴加时浆料温度为25℃~60℃。
2.根据权利要求1所述的重钙湿法研磨分散剂的滴加方法,其特征在于,分散剂在1号立式搅拌磨机中滴加量为每吨浆料滴加4~5kg;在2号立式搅拌磨机中,滴加量为每吨浆料滴加3~4kg。
3.根据权利要求1所述的重钙湿法研磨分散剂的滴加方法,其特征在于,注入前先将分散剂溶于水中,在1号立式搅拌磨中,水与分散剂的比为1∶1~2,在2号立式搅拌磨中,水与分散剂的比为1∶2~3,然后用滴加泵注入,连续生产,连续注入。
4.根据权利要求1所述的重钙湿法研磨分散剂的滴加方法,其特征在于,在1号立式搅拌磨中,从顶部和中部同时注入,顶部的注入量为1号立式搅拌磨总量的1/4,在中部的注入量为1号立式搅拌磨总量的3/4;在2号立式搅拌磨中,也是从顶部和中部同时注入,顶部的注入量为2号立式搅拌磨总量的1/3,在中部的注入量为2号立式搅拌磨总量的2/3。
5.根据权利要求1所述的重钙湿法研磨分散剂的滴加方法,其特征在于,在1号立式搅拌磨中,主要滴加中性的分散剂,在2号立式搅拌磨中,主要滴加中性偏酸性的分散剂。
CN2010102116150A 2010-06-24 2010-06-24 重钙湿法研磨分散剂的滴加方法 Active CN101869861B (zh)