Prior art keywords
sulfur
fertilizer
sulphur
powder
diammonium phosphate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN2009101029881A
Other languages
English (en)
Other versions
CN101768026A (zh
Inventor
张红映
徐春
刘显波
肖升
代光元
邓永达
李伟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wengfu Zijin Chemical Industry Co Ltd
Original Assignee
Wengfu Group Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wengfu Group Co Ltd filed Critical Wengfu Group Co Ltd
Priority to CN2009101029881A priority Critical patent/CN101768026B/zh
Publication of CN101768026A publication Critical patent/CN101768026A/zh
Application granted granted Critical
Publication of CN101768026B publication Critical patent/CN101768026B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Images

Landscapes

  • Fertilizers (AREA)

Abstract

一种用磷酸二铵装置加硫磺粉生产硫肥的方法该方法包括以下步骤:第一步,将硫磺磨成硫磺粉;第二步,根据产品中含硫的需求量,按硫与硫酸的比例计量,硫磺粉与硫酸送入给料槽,并充分搅拌均匀;第三步,用泵将给料槽中的混合物料加入管式反应器中,与气氨一起在高温下混合反应,硫磺粉依靠反应热熔融后与料浆一起充分接触;第四步,喷出来的料浆和返料一起用喷浆泵打入造粒机内喷浆涂布造粒,混合均匀后得到粒料;第五步,将粒料送入干燥机内用热风干燥,再破碎筛分,制得硫肥。本发明用现有的磷酸二铵装置制得含有氮、磷、硫三种农作物营养元素的肥料,为生产硫肥开拓了一条方便畅通的工艺路线。适用于磷肥企业的品种更新。

Description

用磷酸二铵装置加硫磺粉生产硫肥的方法
技术领域
本发明涉及磷肥,也涉及硫肥,具体而言,涉及用磷酸二铵装置生产硫肥的方法。
背景技术
所谓硫肥,是含有作物需要的中量养分硫的肥料。传统的硫肥生产技术一是在磷酸二铵产品采取外包裹液态硫磺的方式来生产硫肥,另一种是在造粒机里面采取和喷浆同步的方式喷液态硫磺,使之和物料一起喷浆造粒。但这些方式存在混合不均匀的弊病,硫磺有可能与物料无法充分混合和接触,直接形成块状和颗粒,使产品达不到要求;而外包裹的方式在包装和运输的过程中有可能磨损、粉化,导致硫磺养分的损失。
现有技术申请中国专利的有96193527.8号“含硫肥料及其制备方法”、99120285.6号“复合含硫肥料及其制造方法”、01139524.9号“利用磷石膏和粉煤灰生产硅钙硫肥料及其方法”、01801260.4号“含硫肥料组合物及其制备方法”、200610172825.7号“含硫肥料组合物及其制备方法”。目前尚未见到用磷酸二铵装置生产硫肥的专利技术。
发明内容
本发明的目的在于提供一种用磷酸二铵装置加硫磺粉生产硫肥的方法,从而克服传统硫肥生产的缺点,利用磷酸二铵现有装置加硫磺粉直接生产硫肥。
发明人在无数次实验的基础上,发明的用磷酸二铵装置加硫磺粉生产硫肥的方法包括:
第一步,将硫磺磨细成硫磺粉;
第二步,根据产品中含硫的需求量,即单质硫或硫酸根的比例需求,按硫与硫酸的比例计量,硫磺粉与硫酸送入给料槽,并充分搅拌均匀;
第三步,用泵将给料槽中的混合物料加入管式反应器中,与气氨一起在高温下混合反应,硫磺粉依靠反应热熔融后与料浆一起充分接触;
第四步,喷出来的料浆和返料一起用喷浆泵打入造粒机内喷浆涂布造粒,使硫磺均匀的分布在产品当中去,混合均匀后得到粒料;
第五步,将粒料送入干燥机内用热风干燥,再破碎筛分,制得硫肥。
上述第一步中,所述硫磺粉是水磨或干磨磨细的,硫磺粉的细度为100目。
上述第二步中,所述的硫酸为98%的浓硫酸。
上述第三步中,管式反应器中的反应温度为120℃,物料在管式反应器中的停留时间为1~2秒。
上述第四步中,所述喷浆泵的喷浆管为夹套管,用压力为1.0~1.6MPa、温度在210℃左右的中压蒸汽加热保温,使混合物料中的液态硫磺不因温度降低而产生凝固;所述返料占料浆总质量的1/4。
上述第五步中,所述干燥机的热风温度≤250℃,出口的物料水分不高于2.0%;所述硫肥产品的质量指标为:有效P2O5≥40%;总氮≥17%;水分≤2.0%;筛分后的产品粒度为2~4mm的≥90%;硫含量(单质硫、结合硫)≤10%,其中单质硫≤5%、结合硫≤5%。
发明人指出:硫磺粉和硫酸的加入量是按硫肥产品的质量来计算的,通常取硫肥含硫10%为基准。
发明人还指出,在整个工艺流程中,要通过加洗液或水来控制料浆的密度和粘度,从而保证料浆的良好的流动性。
本发明提供的用磷酸二铵装置加硫磺粉生产硫肥的方法,可以用现有的磷酸二铵装置和预中和的方式制得含有氮、磷、硫三种农作物营养元素的肥料,为生产硫肥开拓了一条方便畅通的工艺路线。适用于磷肥企业的品种更新。
附图说明
附图为本发明方法的工艺流程示意框图。
具体实施方式
瓮福(集团)有限责任公司磷酸二铵装置两个系列均采用磷酸二铵装置生产含硫磷肥产品。具体做法是:
首先将硫磺磨细成细度为100目的硫磺粉;根据产品中含硫的需求量,即单质硫或硫酸根的比例需求,按硫含量(单质硫、结合硫)≤10%的比例计量,将硫磺粉与98%的硫酸送入给料槽,并充分搅拌均匀;用泵将给料槽中的混合物料加入管式反应器中,与气氨一起在120℃下混合反应2秒钟,硫磺粉依靠反应热熔融后与料浆一起充分接触;喷出来的料浆和返料一起用喷浆泵打入造粒机内喷浆涂布造粒,使硫磺均匀的分布在产品当中去,混合均匀后得到粒料;喷出来的料浆和返料一起用喷浆泵打入造粒机内喷浆涂布造粒,混合均匀后得到粒料,约1/4的料浆作为返料;喷浆泵的喷浆管为夹套管,用压力为1.0~1.6MPa、温度在210℃左右的中压蒸汽加热保温;最后将粒料送入干燥机内用240℃~250℃的热风干燥,再破碎筛分,制得硫肥。
采用本方法成功地生产出硫肥,产品的各项指标符合要求,外观质量也不错,得到了用户的好评;系统的稳定性、安全性都很好,可以为集团公司创造上亿元的经济价值。

Claims (5)

1.一种用磷酸二铵装置加硫磺粉生产硫肥的方法,其特征在于该方法包括以下步骤:
第一步,将硫磺磨细成硫磺粉;
第二步,根据产品中含硫的需求量,即单质硫或硫酸根之一的比例需求,按硫与硫酸的比例计量,硫磺粉与98%硫酸送入给料槽,并充分搅拌均匀;
第三步,用泵将给料槽中的混合物料加入管式反应器中,与气氨一起在120℃下混合反应,硫磺粉依靠反应热熔融后与料浆一起充分接触;
第四步,喷出来的料浆和返料一起用喷浆泵打入造粒机内喷浆涂布造粒,使硫磺均匀的分布在产品当中去,混合均匀后得到粒料;
第五步,将粒料送入干燥机内用热风干燥,再破碎筛分,制得硫肥。
2.如权利要求1所述的方法,其特征在于第一步中,所述硫磺粉是水磨或干磨磨细的,硫磺粉的细度为100目。
3.如权利要求1所述的方法,其特征在于第三步中,物料在管式反应器中的停留时间为1~2秒。
4.如权利要求1所述的方法,其特征在于第四步中,所述喷浆泵的喷浆管为夹套管,用压力为1.0~1.6MPa、温度在210℃左右的中压蒸汽加热保温;所述返料占料浆总质量的1/4。
5.如权利要求1所述的方法,其特征在于第五步中,所述干燥机的热风温度≤250℃,出口物料水分不高于2.0%;所述硫肥产品的质量指标为:有效P2O5≥40%;总氮≥17%;水分≤2.0%;筛分后产品粒度在2~4mm的≥90%;硫含量≤10%,其中单质硫≤5%、结合硫≤5%。
CN2009101029881A 2009-12-28 2009-12-28 用磷酸二铵装置加硫磺粉生产硫肥的方法 Active CN101768026B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2009101029881A CN101768026B (zh) 2009-12-28 2009-12-28 用磷酸二铵装置加硫磺粉生产硫肥的方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2009101029881A CN101768026B (zh) 2009-12-28 2009-12-28 用磷酸二铵装置加硫磺粉生产硫肥的方法

Publications (2)

Publication Number Publication Date
CN101768026A CN101768026A (zh) 2010-07-07
CN101768026B true CN101768026B (zh) 2012-08-15

Family

ID=42501152

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2009101029881A Active CN101768026B (zh) 2009-12-28 2009-12-28 用磷酸二铵装置加硫磺粉生产硫肥的方法

Country Status (1)

Country Link
CN (1) CN101768026B (zh)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CA2809598C (en) * 2010-08-27 2018-07-17 Ccr Technologies, Ltd. Method for producing fertilizers containing dispersed micronized sulphur
CN104788161A (zh) * 2015-04-17 2015-07-22 湖北富邦科技股份有限公司 一种采用硫磺生产高硫磷铵肥料的方法
CN105800574B (zh) * 2016-04-14 2017-11-21 云南云天化股份有限公司 一种含硫磷铵的制备方法

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN87107537A (zh) * 1986-12-18 1988-08-24 氮及肥田料化学公司 制造含硫酸铵的磷酸铵的改进管式反应器
CN1306955A (zh) * 2000-02-01 2001-08-08 江西贵溪化肥厂 一种生产氮磷钾复合肥的工艺
CN1306952A (zh) * 2000-02-01 2001-08-08 江西贵溪化肥厂 一种生产磷酸二铵复合肥的工艺

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN87107537A (zh) * 1986-12-18 1988-08-24 氮及肥田料化学公司 制造含硫酸铵的磷酸铵的改进管式反应器
CN1306955A (zh) * 2000-02-01 2001-08-08 江西贵溪化肥厂 一种生产氮磷钾复合肥的工艺
CN1306952A (zh) * 2000-02-01 2001-08-08 江西贵溪化肥厂 一种生产磷酸二铵复合肥的工艺

Also Published As

Publication number Publication date
CN101768026A (zh) 2010-07-07

Similar Documents

Publication Publication Date Title
CN101921149B (zh) 尿浆氨酸法生产无填充剂的增效复合肥料及其生产方法
CN101768025B (zh) 用磷酸二铵装置生产硫肥的方法
CN103936524B (zh) 一种脲醛缓释复合肥的生产方法
CN102249777B (zh) 化学合成氨化硫基复合肥的生产方法
CN102633553B (zh) 一种高塔磷铵复合肥的生产方法
CN101648838B (zh) 用晶状硫酸铵或粉状硫酸铵生产粒状硫酸铵的方法
CN102153392B (zh) 一种缓释脲甲醛复合肥的生产方法
CN101367682B (zh) 一种共溶料浆管式反应器制造复合肥的方法
CN105800574B (zh) 一种含硫磷铵的制备方法
CN100354235C (zh) 一种复合肥的喷浆造粒方法
CN101570455A (zh) 用有机-无机粘结剂生产颗粒硫酸铵产品的方法
CN101768026B (zh) 用磷酸二铵装置加硫磺粉生产硫肥的方法
CN101508607A (zh) 一种脲硫酸长效缓释复合肥的制备方法
CN100575316C (zh) 尿硫基复合肥制备工艺方法
CN102093128B (zh) 一种掺混肥营养填充料及其制备方法
CN104892061A (zh) 一种含硫磷肥的制备方法
CN103396186A (zh) 一种用污水处理渣生产硫磷铵产品的工艺及装置
CN103360145A (zh) 一种用尾矿渣生产硫磷铵产品的工艺
CN105431396A (zh) 用于生产颗粒氮钾肥的方法
CN101337847B (zh) 一种高氮硫基氮磷钾复合肥的生产方法
CN104072260B (zh) 一种生产复合肥料的生产系统
CN106831055A (zh) 一种喷浆造粒生产高氮硫基冲施复合肥的方法
CN202072638U (zh) 一种硝基复合肥制备装置
CN106146109A (zh) 一种复合肥的喷浆造粒方法
CN106831002A (zh) 一种粒状重过磷酸钙节能生产方法

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
ASS Succession or assignment of patent right

Owner name: WENGFU ZIJIN CHEMICAL INDUSTRY CO., LTD.

Effective date: 20130924

C41 Transfer of patent application or patent right or utility model
TR01 Transfer of patent right

Effective date of registration: 20130924

Address after: 550002 Guizhou city of Guiyang province Nanming City Road No. 57 Wengfu International Building 23 buildings

Patentee after: Wengfu (Group) Co., Ltd.

Patentee after: Wengfu Zijin Chemical Industry Co., Ltd.

Address before: 550002 Guizhou city of Guiyang province Nanming City Road No. 57 Wengfu International Building 23 buildings

Patentee before: Wengfu (Group) Co., Ltd.

CP02 Change in the address of a patent holder
CP02 Change in the address of a patent holder

Address after: 550500 Guizhou Province, Qiannan Buyei and Miao Autonomous Prefecture Fuquan Racecourse town Yingbin Road No. 1 Wengfu group

Co-patentee after: WENGFU ZIJIN CHEMICAL INDUSTRY Co.,Ltd.

Patentee after: WENGFU GROUP Co.,Ltd.

Address before: 23, 550002 floor, International Building, No. 57, South City Road, Nanming District, Guiyang, Guizhou

Co-patentee before: WENGFU ZIJIN CHEMICAL INDUSTRY Co.,Ltd.

Patentee before: WENGFU GROUP Co.,Ltd.