CN101618442B - 一种连铸中间包用还原性覆盖剂 - Google Patents
一种连铸中间包用还原性覆盖剂 Download PDFInfo
- Publication number
- CN101618442B CN101618442B CN2008100435987A CN200810043598A CN101618442B CN 101618442 B CN101618442 B CN 101618442B CN 2008100435987 A CN2008100435987 A CN 2008100435987A CN 200810043598 A CN200810043598 A CN 200810043598A CN 101618442 B CN101618442 B CN 101618442B
- Authority
- CN
- China
- Prior art keywords
- percent
- covering agent
- equal
- reductive
- less
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本发明涉及一种连铸中间包用还原性覆盖剂。主要解决高碱度中间包覆盖剂存在的粘度高、易结壳,无法消除进入钢水中的氧的技术问题。本发明的化学组分的重量百分比为:CaO:26%~38%;Al2O3:≤16%;Al:2.5%-6%;Ca:3%-5%;MgO:2%~10%;SiO2:20%-35%;C≤8%;Fe2O3:≤4%;Na2O+K2O≤1.5%;FeO≤1.5%;控制水分≤0.8%;碱度R≥1.2。本发明是一种用于钢铁冶炼的辅料。
Description
技术领域:
本发明涉及一种用于钢铁冶炼的辅料,特别涉及一种用于中间包的具有还原性功能的覆盖剂。
背景技术:
随着用户对钢材质量日益苛刻的要求,钢中夹杂物含量必须越来越少,在连铸浇钢过程中,如果浇铸的保护性差,进入空气到中间包钢液中,或钢水下渣到中间包中,钢水就会增氧,引起夹杂。这就要求钢水在浇铸过程中,严格控制空气及渣的进入,但浇铸过程,钢水很难达到全封闭,经常发生吸入空气或下渣情况。
目前国内外的连铸中间包用覆盖剂采用提高碱度(1.5-2.5)的办法,增加其吸收夹杂功能,已查到的专利有:申请号:CN200410016591.8,名称:高碱度中间包覆盖剂。申请号:CN200610119185.3,名称:高碱度中间包覆盖剂及其生产方法。这些专利不具备造成还原性气氛,其原理是提高覆盖剂中的CaO含量,吸收钢水中的夹杂,以减少连铸中间包钢水夹杂。但缺点是粘度过高,易结壳,另外,不能去除钢水中的氧,即对于已经进入钢水或覆盖剂中的的氧,无法去除。因此目前还没有还原性覆盖剂的报道。
发明内容:
本发明的目的是提供一种用于连铸中间包的具有还原性功能的覆盖剂,主要解决高碱度中间包覆盖剂存在的粘度高、易结壳,无法消除进入钢水中的氧的技术问题。本发明主要作用是在中间包钢液面上形成还原性气氛,阻碍空气中氧或下渣中的氧进入钢水,以及降低覆盖剂中的∑(FeO+MnO)%,提高钢水的纯净度,减少钢中夹杂。本发明的化学组分的重量百分比为:CaO:26%~38%;Al2O3:≤16%;Al:2.5%-6%;Ca:3%-5%;MgO:2%~10%;SiO2:20%-35%;C≤8%;Fe2O3:≤4%;Na2O+K2O≤1.5%;FeO≤1.5%;控制水分≤0.8%;碱度(R=(CaO+MgO)/SiO2)R≥1.2。
覆盖剂是以矿物为主的配方组份,其中的Al2O3,Na2O、K2O、FeO和Fe2O3是矿物带进的,含量应控制严格,在有些中间包覆盖剂中,因Na2O、K2O和FeO含量低,不体现出。
本渣系中Ca和Al是该类型覆盖剂中不可缺少的成分,其作用是形成还原性气氛,起到去除氧的作用。这两中元素量不可过多,否则反而引起烧损,起不到减少钢和渣中氧的作用,又增加成本。因此把覆盖剂中的Ca和Al控制在适量范围,才能形成稳定的还原性气氛,并且成本也不高。还原性覆盖剂的作用原理如下:
如果中间包钢水吸入空气或大包下渣造成覆盖剂渣中氧量过高,则有如下反应:
〔Ca〕+〔O〕=(CaO)
2〔Al〕+3〔O〕=(Al2O3)
产生的(CaO)和(Al2O3)与覆盖剂中的(SiO2)结合在一起,形成(CaOAl2O3SiO2)低熔点(1450℃)大型夹杂上浮于钢液面的覆盖剂渣中,从而起到去除钢水中的氧的作用。
本发明有益效果:本发明连铸中间包还原性覆盖剂用渣,既能吸收钢水中的夹杂,又能去除进入钢水或覆盖剂中的氧,对减少浇钢过程的夹杂具有良好的效果。
具体实施方式:
配方组成见表1:
表1为本发明化学组分的重量百分比(%)
成分(%) | SiO2 | CaO | Al2O3 | MgO | C全 | Fe2O3 | Ca | Al | Na2O+K2O | FeO | H2O | R |
配比 | 20~35 | 26~38 | ≤16.0 | 2~10 | ≤8.0 | ≤4.0 | 35 | 2.5-6 | ≤1.5 | ≤1.5 | ≤0.8 | ≥1.2 |
实施方式:本发明按传统制作中间包覆盖剂配制,加入钙铁合金,其含量按覆盖剂中钙的含量而定,其粒度为粉状,或为80-100目。另外再配入铝灰,其加入量按覆盖剂中铝的含量而定。与覆盖剂中其它组分一起混合而成。其实例配方组成见表2:
表2为本发明实施例15化学组分的重量百分比(%)
成分(%) | SiO2 | CaO | Al2O3 | MgO | C全 | Fe2O3 | Ca | Al | Na2O+K2O | FeO |
配比1 | 35 | 37 | 8 | 7 | 0 | 3 | 3 | 4 | 1.5 | 1.5 |
配比2 | 27.5 | 34 | 15 | 5 | 4 | 3 | 4 | 5 | 1.5 | 1.0 |
配比3 | 25 | 32 | 15 | 8 | 4 | 4 | 4 | 6 | 1.0 | 1.0 |
配比4 | 30 | 27 | 16 | 10 | 3.5 | 3.0 | 3.0 | 5 | 1.0 | 1.0 |
配比5 | 29 | 26 | 15 | 10 | 5 | 3 | 5 | 5 | 1.0 | 1.0 |
该成品采用双层塑料包装,具体包装规格要求按现场加料要求的标准执行。使用效果:使用本发明还原性覆盖剂,其效果显著。表3是传统无还原性覆盖剂和本发明的还原性覆盖剂对降低中间包钢液面覆盖剂渣中的氧化性(FeO+MnO)%和降低钢水中全氧的效果:
表3本发明还原性覆盖剂降氧效果
覆盖剂 | 覆盖剂氧化性(FeO+MnO)% | 中间包钢水全氧(ppm) |
传统覆盖剂 | 4.5%-6.7% | 35-45 |
本发明还原性覆盖剂 | 2.3%3.5% | 2530 |
可见,使用本发明的具有还原性覆盖剂后,能较传统无还原性的覆盖剂降低氧化性,从而有效提高其还原性,减少钢水中的氧。
Claims (2)
1.一种连铸中间包用还原性覆盖剂,其特征是化学组分的重量百分比为:CaO:26%~38%;Al2O3:≤16%;Al:2.5%-6%;Ca:3%-5%;MgO:2%~10%;SiO2:20%-35%;C≤8%;Fe2O3:≤4%;Na2O+K2O≤1.5%;FeO≤1.5%。
2.根据权利要求1所述的一种连铸中间包用还原性覆盖剂,其特征是(CaO+MgO)/SiO2≥1.2。