CN101565209A - 用煤矸石生产净水剂硫酸铝铁钙 - Google Patents

用煤矸石生产净水剂硫酸铝铁钙 Download PDF

Info

Publication number
CN101565209A
CN101565209A CNA2009101478452A CN200910147845A CN101565209A CN 101565209 A CN101565209 A CN 101565209A CN A2009101478452 A CNA2009101478452 A CN A2009101478452A CN 200910147845 A CN200910147845 A CN 200910147845A CN 101565209 A CN101565209 A CN 101565209A
Authority
CN
China
Prior art keywords
water purification
purification agent
coal slack
coal gangue
coal
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA2009101478452A
Other languages
English (en)
Inventor
葛文会
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNA2009101478452A priority Critical patent/CN101565209A/zh
Publication of CN101565209A publication Critical patent/CN101565209A/zh
Pending legal-status Critical Current

Abstract

本发明是一种用煤矸石生产净水剂硫酸铝铁钙,先把煤矸石粉碎,在控制温度下燃烧,把烧得到的矸石灰粉碎至粉末状,也可以用自燃矸石灰,与稀硫酸反应,生成硫酸铝和硫酸亚铁的混合溶液,然后用石灰水调整pH值,就得到新型净水剂:硫酸铝铁钙。

Description

用煤矸石生产净水剂硫酸铝铁钙
技术领域
本发明涉及煤化工业,对煤矸石的综合利用。
背景技术
煤矿的煤矸石是废弃物,少数用来修路。
发明内容
为了避免煤矸石在煤矿自燃和利用煤石中的氧化铝及氧化铁,本发明是:先把煤矸石经过控制温度的燃烧后,粉碎成粉末状,与稀硫酸按比例混合,在容器中加热加速反应,生成硫酸铝和硫酸亚铁的混合溶液,用石灰水调整溶液的pH值,使其在5.8-6.5之间,这样的溶液是新型复合式净水剂,也可以把溶液浓缩成为固体。
具体实施方式
先把煤矸石焙烧,温度控制在750℃-850℃之间,得到的灰由于成分中的氧化铝在这个温度下可以结构转型,可以与稀硫酸、盐酸进行反应,生成硫酸铝或者氯化铝,因此叫作活性矸石灰,煤矸石自燃后的红白块料也可以,把这种灰块粉碎至粉末状,投放到反应容器中,再按比例加入稀硫酸加热,使其反应加速,间断性地搅拌,取样分析,当反应结束后,把液体和固体都放出来,放到一个沉淀池子中使其沉淀,然后把上面的液体导出,把下面的碴子用清水洗两遍,洗液留另用,碴子弃去,接下来往反应液中缓慢地加入石灰水,并同时搅拌,间断地取样分析,当pH值到5.8-6.5时,停止往里加石灰水,然后静止,沉淀,然后,导出上面的液体,就是净水剂,下面碴子用清水洗两遍,洗液留用,碴子弃掉,液体产品可以经过加热浓缩得到固体产品。

Claims (1)

1.一种用煤矸石生产净水剂硫酸铝铁钙,其特征在于,先把煤矸石燃烧,使其中的氧化铝具有活性,也可以用自燃矸石的红白块料,粉碎成粉末状,然后按比例在反应容器中与硫酸或者盐酸受热反应,先经过燃烧除碳,对于反应后的溶液用石灰水调整pH值。
CNA2009101478452A 2009-06-16 2009-06-16 用煤矸石生产净水剂硫酸铝铁钙 Pending CN101565209A (zh)