CN101463460A - 真空镀膜镀层基片局部蚀刻工艺 - Google Patents
真空镀膜镀层基片局部蚀刻工艺 Download PDFInfo
- Publication number
- CN101463460A CN101463460A CNA2008101535643A CN200810153564A CN101463460A CN 101463460 A CN101463460 A CN 101463460A CN A2008101535643 A CNA2008101535643 A CN A2008101535643A CN 200810153564 A CN200810153564 A CN 200810153564A CN 101463460 A CN101463460 A CN 101463460A
- Authority
- CN
- China
- Prior art keywords
- substrate
- film
- protective membrane
- vacuum coating
- etching
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种真空镀膜镀层基片局部蚀刻工艺,它包括按如下工艺步骤:将整张基片表面进行真空镀膜、排版印刷、贴分切型保护膜、揭部分保护膜、蚀刻;在压膜机上安装分切刀具,使基片压贴保护膜和分切保护膜同步进行;压膜和分切是在同一台机器上同时进行的,先切后压连续完成,本发明的优点是,充分体现节能需求,在降低生产过程原材料的消耗的同时,满足了产品局部区域无镀层的要求,整个工艺过程仅进行一次镀膜就可进行后续工序,然后即可生产出高品质的产品,该工艺降低了成本,提高了效率;因此,本发明提供的镀层基片局部蚀刻工艺思路新颖、具有创造性和较高的实用性,有推广价值。
Description
技术领域
本发明涉及蚀刻工艺,特别涉及一种真空镀膜镀层基片局部蚀刻工艺。
技术背景
随着真空镀膜技术及镀膜之后对基材表面加工技术的发展,用户对真空镀膜产品颜色的要求越来越高,真空镀膜是在真空中把金属、合金或化学物进行蒸发(或溅射),使其沉积在被涂覆的物体(称基片)上。然而,单靠油墨本身的颜色效果是无法达到要求的,于是依靠真空镀膜,再通过油墨遮盖达到颜色要求,受到越来越多客户的追捧。随着真空镀膜的普及,用户的要求也越来越高,逐渐出现了产品局部区域无镀层(如:单件产品有两处透光区域,要求一处有镀层,一处无镀层)的要求。要达到这种效果常采用的方式就是多次镀膜--印刷--蚀刻,这无疑是一种成本上的浪费。这就对我们怎样降低成本,并且不影响生产效率提出了新的挑战。
发明内容
本发明的目的是克服现有技术的不足,提出一种无需多次镀膜-印刷-蚀刻,而仅经一次真空镀膜的镀层基片实现局部蚀刻的工艺方法。
本发明是通过这样的技术方案实现的:一种真空镀膜镀层基片局部蚀刻工艺,其特征是包括按如下工艺步骤:
(1)将整张基片(金属板/塑料板/透明、半透明、有色胶片)表面进行真空镀膜;
(2)在已镀膜基片表面采用丝网印刷的方法,印刷出产品图案;
(3)对已镀膜、且膜层表面已印刷出产品图案的基片压贴保护膜;
(4)在已压贴保护膜的基片表面,沿产品图案即需要蚀刻镀层区域边界分切保护膜;
(5)手工揭去需要蚀刻镀层区域的保护膜;
(6)进行蚀刻;
(7)揭去所有保护膜,水洗烘干。
上述过工艺程中,基片压贴保护膜和分切保护膜步骤可以分步进行,也可在压膜机上安装分切刀具,使基片压贴保护膜和分切保护膜同步进行;所述的工艺步骤中,基片压贴保护膜和分切保护膜步骤是在压膜机上安装分切刀具,由同一台压膜机进行压膜和分切,先分切后压膜连续完成。
本发明的优点是,充分体现节能需求,在降低生产过程原材料的消耗的同时,满足了产品局部区域无镀层的要求,使通常采用的多次镀膜--印刷--蚀刻的工艺过程得到简化,整个工艺过程仅进行一次镀膜就可进行后续工序,然后即可生产出高品质的产品,该工艺降低了成本,提高了效率。因此,本发明提供的镀层基片局部蚀刻工艺思路新颖、具有创造性和较高的实用性,有推广价值。
附图说明
图1已分切并贴保护膜的基片示意图;
图2已揭去保护膜并蚀刻的成品示意图。
具体实施方式
为了使本发明的目的、技术方案及优点更加清楚明白,以下结合附图及实施例,对本发明进行进一步详细说明,应当理解,此处所描述的具体实施例仅仅用以解释本发明,并不用于限定本发明。
本发明的实施例的工艺流程是:
真空镀膜→排版印刷→贴分切型保护膜→揭部分保护膜→蚀刻其具体工艺步骤如下:
(1)基片选用0.64mm的PC或者PMMA片材,在片材表面进行真空镀膜;
(2)排版印刷:将预先设计的产品有规律排列,采用丝网印刷的方法在基片表面用油墨印刷所要求产品图形;
(3)分切、压贴保护膜:沿基片需要蚀刻镀层区域边界分切保护膜;在本实施例中:在贴膜机上按照蚀刻要求安装分切刀具,使用分切刀具使贴到产品上的保护膜为条状,分别覆盖基片镀层需保留和需蚀刻的区域;
(4)依次将基片需要蚀刻的局部区域保护膜揭去;
(5)蚀刻:通过蚀刻药液洗去多余镀层,再将剩余保护膜全部揭去水洗烘干。
本发明的实施例中,在贴膜机上安装数把分切刀具,使用贴膜机机器对整张基材贴保护膜,在贴膜过程中保护膜被分切成条状膜。压膜和分切是在同一台机器上同时进行的,先切后压连续完成。
图1为已分切并贴保护膜的基片示意图;图中斜线区域部分是将要揭去的保护膜;图2为已揭去保护膜并蚀刻的成品示意图,点状区域部分为最终保留镀层;
保护膜胶粘度要适中,既要有粘性还要保证不能有胶转移,以上蚀刻,水洗,烘干过程为同一生产线连续完成。
Claims (2)
1、一种真空镀膜镀层基片局部蚀刻工艺,其特征是包括按如下工艺步骤:
(1)将整张基片(金属板/塑料板/透明、半透明、有色胶片)表面进行真空镀膜;
(2)在已镀膜基片表面采用丝网印刷的方法,印刷出产品图案;
(3)对已镀膜、且膜层表面已印刷出产品图案的基片压贴保护膜;
(4)在已压贴保护膜的基片表面,沿产品图案即需要蚀刻镀层区域边界分切保护膜;
(5)手工揭去需要蚀刻镀层区域的保护膜;
(6)进行蚀刻;
(7)揭去所有保护膜,水洗烘干。
2、如权利要求1所述的真空镀膜镀层基片局部蚀刻工艺,其特征是所述的工艺步骤中,基片压贴保护膜和分切保护膜步骤是在压膜机上安装分切刀具,由同一台压膜机进行压膜和分切,先分切后压膜连续完成。