CN101455996A - 单斜磁黄铁矿与方铅矿浮选分离新工艺 - Google Patents

单斜磁黄铁矿与方铅矿浮选分离新工艺 Download PDF

Info

Publication number
CN101455996A
CN101455996A CNA2007101790661A CN200710179066A CN101455996A CN 101455996 A CN101455996 A CN 101455996A CN A2007101790661 A CNA2007101790661 A CN A2007101790661A CN 200710179066 A CN200710179066 A CN 200710179066A CN 101455996 A CN101455996 A CN 101455996A
Authority
CN
China
Prior art keywords
monocline
galena
flotation separation
new technology
pyrrhotine
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CNA2007101790661A
Other languages
English (en)
Other versions
CN101455996B (zh
Inventor
宋永胜
李文娟
屈伟
姚国成
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
GRINM Resources and Environment Technology Co Ltd
Original Assignee
Beijing General Research Institute for Non Ferrous Metals
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Beijing General Research Institute for Non Ferrous Metals filed Critical Beijing General Research Institute for Non Ferrous Metals
Priority to CN2007101790661A priority Critical patent/CN101455996B/zh
Publication of CN101455996A publication Critical patent/CN101455996A/zh
Application granted granted Critical
Publication of CN101455996B publication Critical patent/CN101455996B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种单斜磁黄铁矿与方铅矿浮选分离的新工艺。该工艺采用(1)将矿物磨至一定粒度后;(2)利用醋酸与醋酸钠调节矿浆pH;(3)加入捕收剂和起泡剂,使方铅矿上浮,实现两种矿物的分离。其中:醋酸与醋酸钠配合调节矿浆至pH为3.6-5.6的范围内进行浮选,所用的捕收剂为黄原酸盐,矿浆中捕收剂浓度为5×10-5mol/L-2.5×10-4mol/L,所用起泡剂为醚醇或2号油,醚醇用量为10-15mg/L,2号油用量为12-25mg/L。采用该工艺可以使方铅矿的浮选回收率达到90%以上,而单斜磁黄铁矿的浮选回收率在10%以下,从而很好地实现两种矿物的分离。

Description

单斜磁黄铁矿与方铅矿浮选分离新工艺
技术领域
本发明涉及单斜磁黄铁矿与方铅矿浮选分离新工艺。
背景技术
磁黄铁矿是一种分布很广,可与多种矿物共生的铁的硫化矿物。由于铁原子的亏损数量不尽相同,使其不但在成分上发生变化,而且在结构上也有所偏离,其结构可由六方晶系演变为单斜晶系,这就造成了不同的磁黄铁矿在溶液中表现的浮选行为也各有差异,随着其结构由六方演变为单斜晶系,其可浮性逐渐由差变好,因此单斜磁黄铁矿的可浮性很好,与其它矿物的分离困难。磁黄铁矿的抑制及其与其它矿物的分离被视为选矿界的热点与难点。
发明内容
本发明的目的是提供一种单斜磁黄铁矿与方铅矿的浮选分离新工艺,利用本工艺可以使方铅矿的浮选回收率达到90%以上,而单斜磁黄铁矿的浮选回收率在10%以下,从而实现两种矿物的分离。
本发明的目的可以通过以下措施来实现:
(1)、将矿物磨至一定粒度后;
(2)、利用醋酸与醋酸钠调节矿浆pH;
(3)、加入捕收剂和起泡剂,使方铅矿上浮,实现两种矿物的分离。
其中:可采用:
将矿物磨至-0.074mm;
采用醋酸与醋酸钠调浆至pH为3.6-5.6的范围内搅拌3-8分钟;
所用的捕收剂为黄原酸盐,矿浆中捕收剂浓度为5×10-5mol/L-2.5×10-4mol/L,加入捕收剂搅拌作用1-5分钟;
所用的起泡剂为醚醇或2号油,醚醇用量为10-15mg/L,2号油用量为12-25mg/L,加入起泡剂搅拌作用1-5分钟;
浮选7-15分钟。
本发明的优点是:利用本工艺可以使方铅矿的浮选回收率达到90%以上,而单斜磁黄铁矿的浮选回收率在10%以下,从而实现两种矿物的分离。
(1)
附图说明
图1为本发明提供的单斜磁黄铁矿与方铅矿分离的工艺流程示意图。
实施例1
将矿物磨至-0.074mm,采用醋酸与醋酸钠调节矿浆至pH=4.0,搅拌5分钟,加入捕收剂丁基黄原酸钠,捕收剂浓度为2×10-4mol/L,搅拌2分钟,加入起泡剂丁基醚醇,用量为10mg/L,搅拌2分钟,浮选9分钟。浮选分离结果见表1。
表1 混合矿在矿浆pH为4.0时的浮选分离结果
Figure A200710179066D00041
实施例2
将矿物磨至-0.074mm,采用醋酸与醋酸钠调节矿浆至pH=4.67,搅拌5分钟,加入捕收剂丁基黄原酸钠,捕收剂浓度为2×10-4mol/L,搅拌2分钟,加入起泡剂丁基醚醇,用量为10mg/L,搅拌2分钟,浮选9分钟。浮选分离结果见表2。
表2 混合矿在矿浆pH为4.67时的浮选分离结果
Figure A200710179066D00042
实施例3
将矿物磨至-0.074mm,采用醋酸与醋酸钠调节矿浆至pH=5.0,搅拌5分钟,加入捕收剂丁基黄原酸钠,捕收剂浓度为2×10-4mol/L,搅拌2分钟,加入起泡剂丁基醚醇,用量为10mg/L,搅拌2分钟,浮选9分钟。浮选分离结果见表3。
表3 混合矿在矿浆pH为5.0时的浮选分离结果
Figure A200710179066D00051
实施例4
将矿物磨至-0.074mm,采用醋酸与醋酸钠调节矿浆至pH=3.6,搅拌5分钟,加入捕收剂丁基黄原酸钠,捕收剂浓度为2×10-4mol/L,搅拌2分钟,加入起泡剂乙基醚醇,用量为12mg/L,搅拌2分钟,浮选9分钟。浮选分离结果见表4。
表4 混合矿在矿浆pH为3.6时的浮选分离结果
Figure A200710179066D00052

Claims (7)

1、一种单斜磁黄铁矿与方铅矿浮选分离新工艺,其特征在于,它包括以下步骤:
(1)、将矿物磨至一定粒度后;
(2)、利用醋酸与醋酸钠调节矿浆pH;
(3)、加入捕收剂和起泡剂,使方铅矿上浮,实现两种矿物的分离。
2、根据权利要求1所述的单斜磁黄铁矿与方铅矿浮选分离新工艺,其特征在于,单斜磁黄铁矿是指以单斜磁黄铁矿为主,占全部磁黄铁矿的90%以上。
3、根据权利要求1或2所述的单斜磁黄铁矿与方铅矿浮选分离新工艺,其特征在于,矿物的磨矿细度为-0.074mm。
4、根据权利要求1或3所述的单斜磁黄铁矿与方铅矿浮选分离新工艺,其特征在于,醋酸与醋酸钠配合调浆后,矿浆的pH值在3.6-5.6的范围内,调浆搅拌3-8分钟。
5、根据权利要求1或3或4所述的单斜磁黄铁矿与方铅矿浮选分离新工艺,其特征在于,所用捕收剂为黄原酸盐,矿浆中捕收剂的浓度范围为5×10-5mol/L-2.5×10-4mol/L,加入捕收剂后搅拌时间为1-5分钟。
6、根据权利要求1或4或5所述的单斜磁黄铁矿与方铅矿浮选分离新工艺,其特征在于,所用起泡剂为醚醇或2号油,醚醇用量为10-15mg/L,2号油用量为12-25mg/L,加入起泡剂后搅拌时间为1-5分钟。
7、根据权利要求1的所述的单斜磁黄铁矿与方铅矿浮选分离新工艺,其特征在于,所需的浮选时间为7-15分钟。
CN2007101790661A 2007-12-10 2007-12-10 单斜磁黄铁矿与方铅矿浮选分离工艺 Expired - Fee Related CN101455996B (zh)