CN101362590A CNA2007100778906A CN200710077890A CN101362590A CN 101362590 A CN101362590 A CN 101362590A CN A2007100778906 A CNA2007100778906 A CN A2007100778906A CN 200710077890 A CN200710077890 A CN 200710077890A CN 101362590 A CN101362590 A CN 101362590A
Authority
CN
China
Prior art keywords
furnace
fluidized bed
pyrite
bed furnace
baker
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA2007100778906A
Other languages
English (en)
Inventor
项拥军
李青春
刘水发
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangxi Copper Corp
Original Assignee
Jiangxi Copper Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangxi Copper Corp filed Critical Jiangxi Copper Corp
Priority to CNA2007100778906A priority Critical patent/CN101362590A/zh
Publication of CN101362590A publication Critical patent/CN101362590A/zh
Pending legal-status Critical Current

Links

Classifications

    • YGENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02PCLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
    • Y02P20/00Technologies relating to chemical industry
    • Y02P20/141Feedstock
    • Y02P20/145Feedstock the feedstock being materials of biological origin

Landscapes

  • Solid Fuels And Fuel-Associated Substances (AREA)

Abstract

本发明提供一种硫铁矿制酸沸腾炉升温方法,在烘炉煮锅之前,将沸腾炉清理干净并铺好冷渣;按传统的方案进行烘炉;烘炉结束后,往沸腾炉内投进木材,铺满炉膛,进行燃烧,待木材烧成木炭后,直接接气投料,本发明由于蓄积了烘炉煮锅的大量热量,保证了一次性点火升温、开车投料的成功,不仅节约了原料成本、还缩短了升温时间,而且避免了环境污染。

Description

一种硫铁矿制酸沸腾炉升温方法
技术领域:
本发明涉及硫铁矿制酸沸腾炉升温方法。
背景技术:
我国自然硫和其它形态硫储量不多,硫酸生产原料以硫铁矿为主。新建及刚经过大修重砌的沸腾炉第一次开车一般都要经过烘炉,之后在炉底铺上含硫在12—18%的矿料,再架设木材或用柴油进行升温,烘炉后清理工作量大,从烘炉煮锅完毕到开车所需时间长(6天左右),点火时又容易造成环境污染。
发明内容:
本发明的目的就是提供一种硫铁矿制酸沸腾炉升温方法。
本发明的方法如下:
(1)在烘炉煮锅之前,将沸腾炉清理干净并铺好冷渣;
(2)按传统的方案进行烘炉;
(3)烘炉结束后,往沸腾炉内投进木材,铺满炉膛,进行燃烧,待木材烧成木炭后,直接接气投料。
本发明由于蓄积了烘炉煮锅的大量热量,保证了一次性点火升温、开车投料的成功,不仅节约了原料成本、还缩短了升温时间,而且避免了环境污染。

Claims (1)

1.一种硫铁矿制酸沸腾炉升温方法,其方法如下:
(1)在烘炉煮锅之前,将沸腾炉清理干净并铺好冷渣;
(2)按传统的方案进行烘炉;
(3)烘炉结束后,往沸腾炉内投进木材,铺满炉膛,进行燃烧,待木材烧成木炭后,直接接气投料。
CNA2007100778906A 2007-08-07 2007-08-07 一种硫铁矿制酸沸腾炉升温方法 Pending CN101362590A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CNA2007100778906A CN101362590A (zh) 2007-08-07 2007-08-07 一种硫铁矿制酸沸腾炉升温方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CNA2007100778906A CN101362590A (zh) 2007-08-07 2007-08-07 一种硫铁矿制酸沸腾炉升温方法

Publications (1)

Publication Number Publication Date
CN101362590A true CN101362590A (zh) 2009-02-11

Family

ID=40389229

Family Applications (1)

Application Number Title Priority Date Filing Date
CNA2007100778906A Pending CN101362590A (zh) 2007-08-07 2007-08-07 一种硫铁矿制酸沸腾炉升温方法

Country Status (1)

Country Link
CN (1) CN101362590A (zh)

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102225749A (zh) * 2011-04-27 2011-10-26 瓮福(集团)有限责任公司 一种沸腾焙烧炉的开车方法
CN102745651A (zh) * 2012-07-17 2012-10-24 威海恒邦化工有限公司 一种节能、环保的沸腾炉升温方法
CN104456542A (zh) * 2014-10-30 2015-03-25 瓮福(集团)有限责任公司 一种沸腾炉节能升温方法
CN113003543A (zh) * 2021-04-26 2021-06-22 湖北鄂中生态工程股份有限公司 一种制硫酸用沸腾炉的快速点火方法

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102225749A (zh) * 2011-04-27 2011-10-26 瓮福(集团)有限责任公司 一种沸腾焙烧炉的开车方法
CN102225749B (zh) * 2011-04-27 2012-10-31 瓮福(集团)有限责任公司 一种沸腾焙烧炉的开车方法
CN102745651A (zh) * 2012-07-17 2012-10-24 威海恒邦化工有限公司 一种节能、环保的沸腾炉升温方法
CN104456542A (zh) * 2014-10-30 2015-03-25 瓮福(集团)有限责任公司 一种沸腾炉节能升温方法
CN113003543A (zh) * 2021-04-26 2021-06-22 湖北鄂中生态工程股份有限公司 一种制硫酸用沸腾炉的快速点火方法
CN113003543B (zh) * 2021-04-26 2023-09-26 湖北鄂中生态工程股份有限公司 一种制硫酸用沸腾炉的快速点火方法

Similar Documents

Publication Publication Date Title
CN101362590A (zh) 一种硫铁矿制酸沸腾炉升温方法
CN102745651A (zh) 一种节能、环保的沸腾炉升温方法
CN203033894U (zh) 一种并流蓄热双膛窑支撑拱结构
CN104130790A (zh) 一种间接换热的煤干馏工艺
CN101691493A (zh) 一种外燃内热式煤干馏炉
CN105776208B (zh) 一种活性焦的生产方法
CN104593015A (zh) 一种型焦炼制方法及其设备
CN104031666A (zh) 一种带有烟气余热利用功能的竹材炭化窑炉
CN106379866B (zh) 一种节能、环保的硫铁矿制酸沸腾炉点火方法
CN101691492A (zh) 一种煤干馏工艺
CN2814286Y (zh) 循环式沸腾炉
CN104100967A (zh) 一种煤矸石脱炭方法及循环流化床选矿锅炉
CN101638230A (zh) 一种生产活性炭的窑
CN201421186Y (zh) 高效节能减排循环流化床有机热载体锅炉
CN103756689A (zh) 横向往复加热、竖向排焦式炼焦炉
CN104676584A (zh) 一种生物质锅炉及其利用热能的方法
CN201158593Y (zh) 一种高效、节能活性炭活化炉
CN2679515Y (zh) 有害可燃气体高温燃烧处理及净化装置
CN208765473U (zh) 一种用于自燃式砖坯快速制砖的窑炉
CN203244796U (zh) 一种可用烟气和热空气生产固体产品的喷雾干燥装置
CN100422634C (zh) 供热制焦炭窑式锅炉
CN208898793U (zh) 两段式焦炉
CN1142243C (zh) 洁净节能焦炉
CN109704293A (zh) 一种焙烧法制酸沸腾炉点火方法
CN203123958U (zh) 使用固体燃料的化工反应炉

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Open date: 20090211