CN101270257A - 一种汽车烘干中涂漆 - Google Patents

一种汽车烘干中涂漆 Download PDF

Info

Publication number
CN101270257A
CN101270257A CNA2008100475128A CN200810047512A CN101270257A CN 101270257 A CN101270257 A CN 101270257A CN A2008100475128 A CNA2008100475128 A CN A2008100475128A CN 200810047512 A CN200810047512 A CN 200810047512A CN 101270257 A CN101270257 A CN 101270257A
Authority
CN
China
Prior art keywords
portions
resin
agent
good
parts
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA2008100475128A
Other languages
English (en)
Inventor
徐海潮
付兴彦
李鸿鸣
王定波
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHIYUAN JINFENG CHEMICAL INDUSTRIAL Co Ltd
Original Assignee
SHIYUAN JINFENG CHEMICAL INDUSTRIAL Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHIYUAN JINFENG CHEMICAL INDUSTRIAL Co Ltd filed Critical SHIYUAN JINFENG CHEMICAL INDUSTRIAL Co Ltd
Priority to CNA2008100475128A priority Critical patent/CN101270257A/zh
Publication of CN101270257A publication Critical patent/CN101270257A/zh
Pending legal-status Critical Current

Abstract

一种汽车烘干中涂漆,根据氨基树脂可作为交联剂,与醇酸树脂、聚酯树脂、环氧树脂、丙烯树脂等含羟基的树脂交联反应,经过缩和聚合固化成膜的机理,通过对醇酸树脂、环氧树脂、氨基树脂进行复配,加工生产具有硬度高、附着力好、层间结合牢、过烘烤性好、装饰性好、耐磨、保光、保色性好、成本低的中涂漆;其特征在于:把氨基树脂15-25份、聚酯树脂19-21份、环氧树脂2.7-2.9份、醇酸树脂25-35份、颜填料为16-26份、稀释剂2-7份进行复配,再加入一定比例助剂,即可制得汽车烘干中涂漆。

Description

一种汽车烘干中涂漆
技术领域
本发明涉及化工领域,尤其是一种汽车烘干中涂漆。
背景技术
涂料是一种涂覆在物体(被保护和被装饰对象)表面并能牢固附着的连续薄膜的配套性工程材料,涂料主要成膜物是否由有油脂和高分子材料(树脂)组成,不挥发的活性稀释济也属于成膜物,它是涂料牢固附着于被涂物表面上形成连续薄膜的主要物质,是构成涂料的基础,对涂膜物理化学性能起着决定作用。底漆涂料要求附着力好,防锈能力强,于面漆结合牢,面漆涂料要求装饰性好、耐酸、耐碱、耐磨、耐高温、绝缘性好;中涂涂料则要求既于底漆、面漆牢固结合、又具有附着力好、硬度高、丰满度好、光度高、耐高温性好、泛黄性小、保光保色性好、与底漆间不咬底、与面漆间不出现浮色,因此使用单一的树脂漆很难达到如此高的要求,而且成本也是高居不下。
发明内容
本发明的目的就是根据氨基树脂可作为交联剂,与醇酸树脂、聚酯树脂、环氧树脂等含羟基的树脂交联反应,经过缩和聚合固化成膜的机理,通过对醇酸树脂、环氧树脂、氨基树脂进行复配,作为成膜物,加工生产具有硬度高、附着力好、层间结合牢、过烘烤性好、装饰性好、耐磨、保光、保色性好、成本低的中涂漆,特提出一种汽车烘干中涂漆。
其技术方案为:一种汽车烘干中涂漆,其特征在于:按重量份;把氨基树脂15-25份、聚酯树脂19-21份、环氧树脂2.7-2.9份、醇酸树脂25-35份、颜填料为16-26份、稀释剂2-7份进行复配,再加入适量的助剂,即可制得汽车烘干中涂漆。
上述方案的助剂按重量份为:润湿分散剂0.2份、防沉剂0.2份、消泡剂0.2份、流平剂0.2份、浮色发花防止剂0.1份、防结皮剂0.1份。
有益效果:
按照上述发明的汽车烘干中涂漆具有成本低、硬度高、附着力好、层间结合牢、过烘烤性好、装饰性好、耐磨、保光、保色性好的汽车烘干中涂漆,既能够满足汽车涂装、涂饰市场的需求,又能够广泛应用于军用、民用、及其他工业领域。
具体实施方式
一种汽车烘干中涂漆,原材料按重量份;把氨基树脂20份、聚酯树脂20份、环氧树脂2.8份、醇酸树脂30份、颜色填料21份、稀释剂5份进行复配;助剂按重量份为:润湿分散剂0.2份、防沉剂0.2份、消泡剂0.2份、流平剂0.2份、浮色发花防止剂0.1份、防结皮剂0.1份搅拌均匀既可制得汽车烘干中涂漆。
备注:上述的一种汽车烘干中涂漆助剂在具体操作过程中可以根据实际情况调整,以达到适合应用的状态。

Claims (3)

1,一种汽车烘干中涂漆,其特征在于:由以下组分按重量份配比:氨基树脂15-25份、聚酯树脂19-21份、环氧树脂2.7-2.9份、醇酸树脂25-35份、颜填料为16-26份、稀释剂2-7份、助剂适量。
2,根据权利要求1所述的一种汽车烘干中涂漆,其特征在于:助剂由以下组分构成:润湿分散剂、防沉剂、消泡剂、流平剂、浮色发花防止剂、防结皮剂。
3,根据权利要求2所述的一种汽车烘干中涂漆,其特征在于由以下组分按重量份配比:氨基树脂20份、聚酯树脂20份、环氧树脂2.8份、醇酸树脂30份、、颜填料21份、稀释剂5份、润湿分散剂0.2份、防沉剂0.2份、消泡剂0.2份、流平剂0.2份、浮色发花防止剂0.1份、防结皮剂0.1份。
CNA2008100475128A 2008-04-25 2008-04-25 一种汽车烘干中涂漆 Pending CN101270257A (zh)