CN101033391A - 钻井液用磺甲基酚醛树脂的制备方法 - Google Patents

钻井液用磺甲基酚醛树脂的制备方法 Download PDF

Info

Publication number
CN101033391A
CN101033391A CN 200610170459 CN200610170459A CN101033391A CN 101033391 A CN101033391 A CN 101033391A CN 200610170459 CN200610170459 CN 200610170459 CN 200610170459 A CN200610170459 A CN 200610170459A CN 101033391 A CN101033391 A CN 101033391A
Authority
CN
China
Prior art keywords
phenol
drilling fluid
sulfonated
hours
liquid
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 200610170459
Other languages
English (en)
Inventor
赵立勋
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 200610170459 priority Critical patent/CN101033391A/zh
Publication of CN101033391A publication Critical patent/CN101033391A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种钻井液用磺甲基酚醛树脂的制备方法。按下述步骤及重量份制成:a.依序将苯酚3.8-4.1、二元酚0.9-1.1、焦亚硫酸钠1.4-1.7、偶联剂0.1-0.2,打入循环储罐中,混合成液体循环2-3小时;b.打入反应釜中,升压1mpa,保压1小时;c.打入微波循环反应器循环2小时;d.进入下一个反应釜中,再依序加入苯酚0.3-0.6、焦亚硫氢钠2.0-2.2、分散剂0.16-0.19,循环2小时,升压2.8mpa,保压3-4小时后进入喷雾干燥机去掉水份制成粉剂,即得产品。主要适用于高矿化度抗饱和盐水基泥浆体系,抗钠盐达到36%,在井深超过7000米时,使用效果更佳。

Description

钻井液用磺甲基酚醛树脂的制备方法
技术领域
本发明涉及一种钻井液用磺甲基酚醛树脂的制备方法。
背景技术
传统的钻井液用磺甲基酚醛树脂的化学结构特征可用三点来表述:酚羟基、磺酸基、碳碳键,产品的化学结构决定产品的性能,这种传统的磺甲基酚醛树脂用于钻井液时,只对钙盐有一定的作用,达不到抗饱和盐的作用。
发明内容
为克服上述缺陷,本发明目的在于提供一种钻井液用磺甲基酚醛树脂的制备方法,使用该方法制备的磺甲基酚醛树脂在用于钻井液时,能够达到抗饱和盐的作用。
为达到上述目的,本发明是按下述步骤及重量份制成:
a、加配基料,依序将液体苯酚3.8-4.1、固体二元酚0.9-1.1、固体焦亚硫酸钠1.4-1.7、液体偶联剂0.1-0.2,打入循环储罐中,混合成液体循环2-3小时;
b、打入反应釜中,升压1mpa,保压1小时;
c、打入微波循环反应器循环2小时;
d、进入下一个反应釜中,再依序加入液体苯酚0.3-0.6、固体焦亚硫氢钠2.0-2.2、液体分散剂0.16-0.19,循环2小时,升压2.8mpa,保压3-4小时后进入喷雾干燥机去掉水份制成粉剂,即得产品。
本发明所制备的磺甲基酚醛树脂产品,在主链上引进了特殊结构的酚类分子,能够达到抗饱和盐的作用,主要适用于高矿化度抗饱和盐水基泥浆体系,抗钠盐达到36%,在超深井水基泥浆体系中,具有抗高温200℃以上、抗盐、降高温高压滤失28ml、降摩阻等特性,在井深超过7000米时,使用效果更佳;由于引入了二元酚和偶联剂,改变了传统产品的结构而使性能成倍提高,其功效是传统磺甲基酚醛树脂的两倍或以上,即一吨本发明方法所制备的磺甲基酚醛树脂相当于二吨传统磺甲基酚醛树脂的功效,换句话说,就是可以节省一半的用量,因此,本发明所制备的磺甲基酚醛树脂,从产品质量到降低成本均具有无可比拟的有益效果。
具体实施方式
本发明钻井液用磺甲基酚醛树脂的制备方法,是按下述步骤及重量份制成:
a、加配基料,依序将液体苯酚3.8-4.1、固体二元酚0.9-1.1、固体焦亚硫酸钠1.4-1.7、液体偶联剂0.1-0.2,打入循环储罐中,混合成液体循环2-3小时;
b、打入反应釜中,升压1mpa,保压1小时;
c、打入微波循环反应器循环2小时;
d、进入下一个反应釜中,再依序加入液体苯酚0.3-0.6、固体焦亚硫氢钠2.0-2.2、液体分散剂0.16-0.19,循环2小时,升压2.8mpa,保压3-4小时后进入喷雾干燥机去掉水份制成粉剂,即得产品。
上述步骤a中的最佳重量份为:苯酚4、二元酚1、焦亚硫酸钠1.5、偶联剂0.1。
上述步骤d中的最佳重量份为:苯酚0.5、焦亚硫氢钠2.1、分散剂0.17。
本发明所制备的磺甲基酚醛树脂产品,在主链上引进了特殊结构的酚类分子,能够达到抗饱和盐的作用,主要适用于高矿化度抗饱和盐水基泥浆体系,抗钠盐达到36%,在超深井水基泥浆体系中,具有抗高温200℃以上、抗盐、降高温高压滤失28ml、降摩阻等特性,在井深超过7000米时,使用效果更佳;由于引入了二元酚和偶联剂,改变了传统产品的结构而使性能成倍提高,其功效是传统磺甲基酚醛树脂的两倍或以上,即一吨本发明方法所制备的磺甲基酚醛树脂相当于二吨传统磺甲基酚醛树脂的功效,换句话说,就是可以节省一半的用量,因此,本发明所制备的磺甲基酚醛树脂,从产品质量到降低成本均具有无可比拟的有益效果。

Claims (3)

1、一种钻井液用磺甲基酚醛树脂的制备方法,其特征在于它是按下述步骤及重量份制成:
a、加配基料,依序将液体苯酚3.8-4.1、固体二元酚0.9-1.1、固体焦亚硫酸钠1.4-1.7、液体偶联剂0.1-0.2,打入循环储罐中,混合成液体循环2-3小时;
b、打入反应釜中,升压1mpa,保压1小时;
c、打入微波循环反应器循环2小时;
d、进入下一个反应釜中,再依序加入液体苯酚0.3-0.6、固体焦亚硫氢钠2.0-2.2、液体分散剂0.16-0.19,循环2小时,升压2.8mpa,保压3-4小时后进入喷雾干燥机去掉水份制成粉剂,即得产品。
2、根据权利要求1所述钻井液用磺甲基酚醛树脂的制备方法,其特征在于所述步骤a中的重量份为:苯酚4、二元酚1、焦亚硫酸钠1.5、偶联剂0.1。
3、根据权利要求1所述钻井液用磺甲基酚醛树脂的制备方法,其特征在于所述步骤d中的重量份为:苯酚0.5、焦亚硫氢钠2.1、分散剂0.17。
CN 200610170459 2006-12-29 2006-12-29 钻井液用磺甲基酚醛树脂的制备方法 Pending CN101033391A (zh)