CN100355456C CNB03132388XA CN03132388A CN100355456C CN 100355456 C CN100355456 C CN 100355456C CN B03132388X A CNB03132388X A CN B03132388XA CN 03132388 A CN03132388 A CN 03132388A CN 100355456 C CN100355456 C CN 100355456C
Authority
CN
China
Prior art keywords
microcapsule
alginate
calcium alginate
poly arginine
chitosan
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNB03132388XA
Other languages
English (en)
Other versions
CN1488403A (zh
Inventor
王士斌
翁连进
陈爱政
陈梅英
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Huaqiao University
Original Assignee
Huaqiao University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Huaqiao University filed Critical Huaqiao University
Priority to CNB03132388XA priority Critical patent/CN100355456C/zh
Publication of CN1488403A publication Critical patent/CN1488403A/zh
Application granted granted Critical
Publication of CN100355456C publication Critical patent/CN100355456C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Landscapes

  • Medicinal Preparation (AREA)

Abstract

本发明是关于海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊及制法。此微胶囊可为双组分单层膜复合微囊膜或为双组分双层膜复合微囊膜。本发明利用静电结合法来制备微胶囊,同时利用聚精氨酸和几丁聚糖为成膜材料用于海藻酸钙/聚精氨酸-几丁聚糖复合型微胶囊的制备,借助高压静电液滴发生装置,通过海藻酸钙外部凝胶化,用聚精氨酸和几丁聚糖成膜,再用海藻酸钠表面修饰,可制得粒径大小均匀,粒径大小范围200-1000μm可控,表面光洁的海藻酸钙/聚精氨酸-几丁聚糖复合型微胶囊。这样,不仅克服了单一物质进行成膜的缺点,并增进产品的营养作用和药理功效而使其具备介入治疗功能,可广泛用于包埋药物或者细胞用于医药和生物工程领域。

Description

海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊及制法
技术领域
本发明是关于以海藻酸钙为胶珠和以聚精氨酸-几丁聚糖为囊壁的微胶囊及制法,尤其属于应用于药物控制释放的微胶囊及制法。
背景技术
微囊化技术是把分散的固体物质颗粒、液滴或气体完全包封在一层膜中形成球状微胶囊的一种技术。利用微囊膜的保护和控制物质扩散功能,微胶囊已广泛应用于医药业、工业、农业和日常生活用品中,尤其是在药物控制释放体系中。
几丁聚糖具有良好的生物相容性,且能被生物降解,降解产物无毒性。聚精氨酸及其降解产物不仅具有良好的生物相容性、无毒性,有提高创伤物免疫功能的作用,还能改善氮平衡,提高动物存活率,促进创伤愈合作用,还可显著抑制许多实验性肿瘤的形成、生长及转移。将几丁聚糖用于药物控释体系,国内外均有大量报道。但,将聚精氨酸和几丁聚糖结合应用于微胶囊控释体系的文章和专利国内外均未见报道。
发明内容
本发明的目的在于提供一种海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊及制法,以克服了单一物质进行成膜的缺点,并增进产品的营养作用和药理功效而使其具备介入治疗功能。
本发明的海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊为海藻酸钙凝胶珠的表面形成一层的海藻酸盐/聚精氨酸-几丁聚糖的双组分单层膜复合微囊膜。
其制法为:
第一步、海藻酸钙凝胶珠的制备:通过静电液滴发生装置,将一定浓度的海藻酸钠滴入含有药用分散剂的氯化钙溶液中,发生凝胶化反应,形成具有一定粒径大小的海藻酸钙凝胶珠;
第二步、成膜反应:取一定浓度及配比的聚精氨酸、几丁聚糖混合溶液,加入海藻酸钙凝胶珠进行成膜反应,使海藻酸钙凝胶珠的表面形成一层海藻酸盐/聚精氨酸-几丁聚糖复合微囊膜,生理盐水洗涤后用较低浓度的海藻酸钠溶液修饰微胶囊表面。
本发明的海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊也可为海藻酸钙凝胶珠的表面形成一层海藻酸盐/聚精氨酸及一层海藻酸盐/几丁聚糖的双组分双层膜复合微囊膜。
其制法为:
第一步、海藻酸钙凝胶珠的制备:通过静电液滴发生装置,将一定浓度的海藻酸钠滴入含有药用分散剂的氯化钙溶液中,发生凝胶化反应,形成具有一定粒径大小的海藻酸钙凝胶珠;
第二步、成膜反应:取一定浓度的聚精氨酸溶液,加入海藻酸钙凝胶珠进行成膜反应,生理盐水洗涤后用较低浓度的海藻酸钠溶液修饰微胶囊表面,再用一定浓度的几丁聚糖进行二次成膜,使海藻酸钙凝胶珠的表面形成一层海藻酸盐/聚精氨酸及一层海藻酸盐/几丁聚糖复合微囊膜,生理盐水洗涤后用较低浓度的海藻酸钠溶液修饰微胶囊表面。
本发明的海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊还可为海藻酸钙凝胶珠的表面形成一层海藻酸盐/几丁聚糖及一层海藻酸盐/聚精氨酸的双组分双层膜复合微囊膜。
其制法为:
第一步、海藻酸钙凝胶珠的制备:通过静电液滴发生装置,将一定浓度的海藻酸钠滴入含有药用分散剂的氯化钙溶液中,发生凝胶化反应,形成具有一定粒径大小的海藻酸钙凝胶珠;
第二步、成膜反应:取一定浓度的几丁聚糖溶液,加入海藻酸钙凝胶珠进行成膜反应,生理盐水洗涤后用较低浓度的海藻酸钠溶液修饰微胶囊表面,再用一定浓度的聚精氨酸进行二次成膜,使海藻酸钙凝胶珠的表面形成一层海藻酸盐/几丁聚糖及一层海藻酸盐/聚精氨酸复合微囊膜,生理盐水洗涤后用较低浓度的海藻酸钠溶液修饰微胶囊表面。
本发明的海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊,粒径大小范围在200-1000μm内可控,表面光洁。
这样,本发明利用静电结合法借助高压静电液滴发生装置来制备微胶囊,将聚氨基酸材料优选为聚精氨酸以及几丁聚糖结合,同时用于海藻酸钙/聚精氨酸-几丁聚糖复合型微胶囊的制备。本发明制备的微胶囊,尤其属于药物控制释放的微胶囊,囊心物为蛋白、多肽类药物。海藻酸钠/聚精氨酸-几丁聚糖复合型微胶囊一方面克服了单一物质进行成膜的缺点,另一方面,由于聚精氨酸及其降解产物的营养作用和药理功效,制备出的微胶囊具有介入治疗效果。该药物载体既能保持良好的生物相容性、大分子药物亲和性、药物控制释放性能,降解产物还可吸收而且其固有的营养和药理功能使其具备介入治疗功能。本发明可用于包埋药物或者细胞用于医药和生物工程领域。
具体实施方式
下面为本发明以双组分单层膜复合微胶囊为例的具体实施步骤(以牛血红蛋白为蛋白、多肽类药物的代表为例):
第一、将1.8%的海藻酸钠溶液经0.8μm、0.45μm、0.22μm过滤后,加入牛血红蛋白使其含量为1mg/mL,混匀,超声波去除气泡后取4mL移入注射器内,经静电液滴发生装置滴入含有0.2%的Tween80分散剂的200mL1.5%(w/v)的氯化钙溶液中,发生凝胶化反应,形成具有一定粒径大小的海藻酸钙凝胶珠。
第二、将制得的海藻酸钙胶珠浸泡在20mL5mg/mL的牛血红蛋白溶液中静置吸附12小时以上。
第三、将吸附后的胶珠用生理盐水快速洗涤两次后,加入含几丁聚糖0.6%、聚精氨酸0.08%的混合液20mL进行成膜10分钟,生理盐水洗涤后,用0.15%(w/v)的海藻酸钠溶液修饰微胶囊表面,最后再用生理盐水洗涤。
第四、通过上述的方法,可制得粒径大小均匀,粒径大小范围200-1000μm可控,表面光洁的海藻酸钙/聚精氨酸-几丁聚糖复合型微胶囊。

Claims (7)

1、海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊,其特征在于:为海藻酸钙凝胶珠的表面形成一层的海藻酸盐/聚精氨酸-几丁聚糖的双组分单层膜复合微囊膜。
2、如权利要求1所述海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊的制法为:
第一步、海藻酸钙凝胶珠的制备:通过静电液滴发生装置,将一定浓度的海藻酸钠滴入含有药用分散剂的氯化钙溶液中,发生凝胶化反应,形成具有一定粒径大小的海藻酸钙凝胶珠;
第二步、成膜反应:取一定浓度及配比的聚精氨酸、几丁聚糖混合溶液,加入海藻酸钙凝胶珠进行成膜反应,使海藻酸钙凝胶珠的表面形成一层海藻酸盐/聚精氨酸-几丁聚糖复合微囊膜,生理盐水洗涤后用较低浓度的海藻酸钠溶液修饰微胶囊表面。
3、海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊,其特征在于:为海藻酸钙凝胶珠的表面形成一层海藻酸盐/聚精氨酸及一层海藻酸盐/几丁聚糖的双组分双层膜复合微囊膜。
4、如权利要求3所述海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊的制法为:
第一步、海藻酸钙凝胶珠的制备:通过静电液滴发生装置,将一定浓度的海藻酸钠滴入含有药用分散剂的氯化钙溶液中,发生凝胶化反应,形成具有一定粒径大小的海藻酸钙凝胶珠;
第二步、成膜反应:取一定浓度的聚精氨酸溶液,加入海藻酸钙凝胶珠进行成膜反应,生理盐水洗涤后用较低浓度的海藻酸钠溶液修饰微胶囊表面,再用一定浓度的几丁聚糖进行二次成膜,使海藻酸钙凝胶珠的表面形成一层海藻酸盐/聚精氨酸及一层海藻酸盐/几丁聚糖复合微囊膜,生理盐水洗涤后用较低浓度的海藻酸钠溶液修饰微胶囊表面。
5、海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊,其特征在于:为海藻酸钙凝胶珠的表面形成一层海藻酸盐/几丁聚糖及一层海藻酸盐/聚精氨酸的双组分双层膜复合微囊膜。
6、如权利要求5所述海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊的制法为:
第一步、海藻酸钙凝胶珠的制备:通过静电液滴发生装置,将一定浓度的海藻酸钠滴入含有药用分散剂的氯化钙溶液中,发生凝胶化反应,形成具有一定粒径大小的海藻酸钙凝胶珠;
第二步、成膜反应:取一定浓度的几丁聚糖溶液,加入海藻酸钙凝胶珠进行成膜反应,生理盐水洗涤后用较低浓度的海藻酸钠溶液修饰微胶囊表面,再用一定浓度的聚精氨酸进行二次成膜,使海藻酸钙凝胶珠的表面形成一层海藻酸盐/几丁聚糖及一层海藻酸盐/聚精氨酸复合微囊膜,生理盐水洗涤后用较低浓度的海藻酸钠溶液修饰微胶囊表面。
7、如权利要求1、3或5所述的海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊,其特征在于:粒径大小范围在200-1000μm内可控,表面光洁。
CNB03132388XA 2003-08-15 2003-08-15 海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊及制法 Expired - Fee Related CN100355456C (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CNB03132388XA CN100355456C (zh) 2003-08-15 2003-08-15 海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊及制法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CNB03132388XA CN100355456C (zh) 2003-08-15 2003-08-15 海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊及制法

Publications (2)

Publication Number Publication Date
CN1488403A CN1488403A (zh) 2004-04-14
CN100355456C true CN100355456C (zh) 2007-12-19

Family

ID=34154127

Family Applications (1)

Application Number Title Priority Date Filing Date
CNB03132388XA Expired - Fee Related CN100355456C (zh) 2003-08-15 2003-08-15 海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊及制法

Country Status (1)

Country Link
CN (1) CN100355456C (zh)

Families Citing this family (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1329510C (zh) * 2004-11-17 2007-08-01 中国科学院沈阳应用生态研究所 一种微球菌两级复凝固定化方法
CN101537016B (zh) * 2009-04-30 2014-03-26 北京宏医耀科技发展有限公司 含骺板软骨细胞复方微胶囊制剂及其制备方法和应用
CN101947212B (zh) * 2010-09-08 2012-10-10 华侨大学 一种微包纳药物载体及其制备方法
CN101972491B (zh) * 2010-09-25 2014-01-08 上海交通大学医学院附属瑞金医院 一种葡萄串状微囊体系及其制备方法
CN102286422B (zh) * 2011-06-22 2013-03-27 南开大学 一种用于体外细胞共培养的复合微囊模型
CN104302279A (zh) * 2012-05-10 2015-01-21 聚和国际股份有限公司 用于制备微胶囊的组合物及用其所制得的药物

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1380109A (zh) * 2002-04-17 2002-11-20 苗九昌 壳聚糖、胶原和海藻酸钙复合海绵生物敷料及其制备工艺
CN1383819A (zh) * 2002-05-17 2002-12-11 天津市园艺工程研究所 一种原花青素缓释微囊

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1380109A (zh) * 2002-04-17 2002-11-20 苗九昌 壳聚糖、胶原和海藻酸钙复合海绵生物敷料及其制备工艺
CN1383819A (zh) * 2002-05-17 2002-12-11 天津市园艺工程研究所 一种原花青素缓释微囊

Also Published As

Publication number Publication date
CN1488403A (zh) 2004-04-14

Similar Documents

Publication Publication Date Title
Sun et al. Dual-layered pH-sensitive alginate/chitosan/kappa-carrageenan microbeads for colon-targeted release of 5-fluorouracil
Peniche et al. Chitosan: an attractive biocompatible polymer for microencapsulation
Javanbakht et al. Incorporating Cu-based metal-organic framework/drug nanohybrids into gelatin microsphere for ibuprofen oral delivery
Yao et al. Microcapsules/microspheres related to chitosan
Vaziri et al. Improving survivability of Lactobacillus plantarum in alginate-chitosan beads reinforced by Na-tripolyphosphate dual cross-linking
US20050226905A1 (en) Biocompatible compositions as carriers or excipients for pharmaceutical and nutraceutical formulations and for food protection
CN107970227A (zh) 一种酪蛋白/海藻酸钠复合微囊的制备方法
CN103040727A (zh) 一种药物和蛋白质缓释海藻酸盐杂化凝胶的制备方法
JPS63258406A (ja) 持続放出製剤
JPS58189031A (ja) 二重マイクロカプセル
CN114176227B (zh) 一种海藻酸钠包裹的层层自组装益生菌微胶囊及其制备方法
CN1994469A (zh) 生物降解磁性纳米颗粒及其制法和应用
CN105997936B (zh) 一种羧甲基壳聚糖纳米微粒固定化多孔多层海藻酸钠胶球的制备方法
CN100355456C (zh) 海藻酸钙/聚精氨酸-几丁聚糖复合药物控释微胶囊及制法
CN103495178B (zh) 玉米醇溶蛋白/碳酸钙复合微粒的制备及作为药物载体的应用
JP5930279B2 (ja) セルトリ細胞のマイクロカプセル化方法、得られるマイクロカプセルおよび1型糖尿病の予防および治療のためのその用途
Li et al. Preparation and property of layer-by-layer alginate hydrogel beads based on multi-phase emulsion technique
Kumar et al. Introduction to Alginate: Biocompatible, Biodegradable, Antimicrobial Nature and Various Applications
CN102304259B (zh) 一种具逐步降解性能的丝素共混材料的制备方法
Waterhouse et al. Porous three-dimensional polymer composites for tailored delivery of bioactives and drugs
CN106109400A (zh) 一种口服药物用水凝胶缓释载体和制备方法及其应用
Moon et al. Morphology and metabolism of hepatocytes microencapsulated with acrylic terpolymer-alginate using gelatin and poly (vinyl alcohol) as extracellular matrices
CN1555784A (zh) 海藻酸钙/聚组氨酸药物控释微胶囊及制法
Ouyang et al. Novel multi-layer APPPA microcapsules for oral delivery: preparation condition, stability and permeability
EP2219621B1 (en) Tri-molecular complexes and their use in drug delivery systems

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
C17 Cessation of patent right
CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20071219

Termination date: 20110815