FR2407897A1
(fr)
*
|
1977-11-03 |
1979-06-01 |
Corning Glass Works |
Procede de trempe chimique d'oculaires de lunetterie et pieces de verre analogues
|
US4273832A
(en)
*
|
1978-08-04 |
1981-06-16 |
Brockway Glass Company, Inc. |
Glass article strengthened by ion exchange substitution
|
US4218230A
(en)
*
|
1978-08-04 |
1980-08-19 |
Brockway Glass Company, Inc. |
Method of glass strengthening by ion exchange
|
FR2474020B1
(fr)
*
|
1980-01-21 |
1985-06-21 |
Brockway Glass Co Inc |
Renforcement de verres par echange d'ions
|
GB2171990B
(en)
*
|
1985-03-08 |
1988-12-07 |
Central Glass Co Ltd |
Method of strengthening glass article formed of float glass by ion exchange and strengthened glass article
|
JPH0818850B2
(ja)
*
|
1986-09-05 |
1996-02-28 |
セントラル硝子株式会社 |
化学強化ガラス
|
US4897371A
(en)
*
|
1987-02-03 |
1990-01-30 |
Nippon Sheet Glass Co., Ltd. |
Glass article protected from coloring by electron rays and method of using
|
FR2697242B1
(fr)
*
|
1992-10-22 |
1994-12-16 |
Saint Gobain Vitrage Int |
Vitrage trempé chimique.
|
US5705273A
(en)
*
|
1995-03-08 |
1998-01-06 |
The Ohio State University |
Method for strengthening dental restorative materials
|
US6516634B1
(en)
|
1999-02-12 |
2003-02-11 |
The Penn State Research Foundation |
Strengthening, crack arrest and multiple cracking in brittle materials using residual stresses
|
US8499583B2
(en)
*
|
2005-03-31 |
2013-08-06 |
Hoya Corporation |
Method of manufacturing magnetic-disk glass substrate and method of manufacturing magnetic disk
|
US8673163B2
(en)
|
2008-06-27 |
2014-03-18 |
Apple Inc. |
Method for fabricating thin sheets of glass
|
US7810355B2
(en)
|
2008-06-30 |
2010-10-12 |
Apple Inc. |
Full perimeter chemical strengthening of substrates
|
EP2321230A4
(en)
*
|
2008-07-29 |
2012-10-10 |
Corning Inc |
TWO-STAGE ION EXCHANGE FOR GLASS CHEMICAL REINFORCEMENT
|
EP2546209B1
(en)
*
|
2008-08-08 |
2015-10-07 |
Corning Incorporated |
Strengthened glass articles and methods of making
|
WO2010101961A2
(en)
*
|
2009-03-02 |
2010-09-10 |
Apple Inc. |
Techniques for strengthening glass covers for portable electronic devices
|
US20110019354A1
(en)
*
|
2009-03-02 |
2011-01-27 |
Christopher Prest |
Techniques for Strengthening Glass Covers for Portable Electronic Devices
|
US8549882B2
(en)
*
|
2009-09-30 |
2013-10-08 |
Apple Inc. |
Pre-processing techniques to produce complex edges using a glass slumping process
|
JP5736379B2
(ja)
*
|
2009-09-30 |
2015-06-17 |
アップル インコーポレイテッド |
ポータブル電子デバイスのガラスカバーを強化する技術
|
US9778685B2
(en)
|
2011-05-04 |
2017-10-03 |
Apple Inc. |
Housing for portable electronic device with reduced border region
|
DE102010009584B4
(de)
*
|
2010-02-26 |
2015-01-08 |
Schott Ag |
Chemisch vorgespanntes Glas, Verfahren zu seiner Herstellung sowie Verwendung desselben
|
US9302937B2
(en)
|
2010-05-14 |
2016-04-05 |
Corning Incorporated |
Damage-resistant glass articles and method
|
US20110293942A1
(en)
*
|
2010-05-26 |
2011-12-01 |
Ivan A Cornejo |
Variable temperature/continuous ion exchange process
|
US9213451B2
(en)
|
2010-06-04 |
2015-12-15 |
Apple Inc. |
Thin glass for touch panel sensors and methods therefor
|
US9207528B2
(en)
|
2010-06-04 |
2015-12-08 |
Apple Inc. |
Thin sheet glass processing
|
US8923693B2
(en)
|
2010-07-30 |
2014-12-30 |
Apple Inc. |
Electronic device having selectively strengthened cover glass
|
US8973401B2
(en)
*
|
2010-08-06 |
2015-03-10 |
Corning Incorporated |
Coated, antimicrobial, chemically strengthened glass and method of making
|
US10189743B2
(en)
*
|
2010-08-18 |
2019-01-29 |
Apple Inc. |
Enhanced strengthening of glass
|
US8873028B2
(en)
|
2010-08-26 |
2014-10-28 |
Apple Inc. |
Non-destructive stress profile determination in chemically tempered glass
|
US8824140B2
(en)
|
2010-09-17 |
2014-09-02 |
Apple Inc. |
Glass enclosure
|
US20120111056A1
(en)
*
|
2010-11-04 |
2012-05-10 |
Christopher Prest |
Enhanced strengthening of glass
|
JP5649592B2
(ja)
*
|
2011-02-17 |
2015-01-07 |
Hoya株式会社 |
携帯電子機器用カバーガラスのガラス基板の製造方法、携帯電子機器用カバーガラスのガラス基板および携帯電子機器
|
US10781135B2
(en)
*
|
2011-03-16 |
2020-09-22 |
Apple Inc. |
Strengthening variable thickness glass
|
US9725359B2
(en)
|
2011-03-16 |
2017-08-08 |
Apple Inc. |
Electronic device having selectively strengthened glass
|
US9128666B2
(en)
|
2011-05-04 |
2015-09-08 |
Apple Inc. |
Housing for portable electronic device with reduced border region
|
JP2012236737A
(ja)
*
|
2011-05-11 |
2012-12-06 |
Asahi Glass Co Ltd |
ガラスの製造方法及びガラス
|
CN102875035B
(zh)
*
|
2011-07-15 |
2015-04-22 |
比亚迪股份有限公司 |
一种玻璃不良品返修的方法
|
TWI572480B
(zh)
|
2011-07-25 |
2017-03-01 |
康寧公司 |
經層壓及離子交換之強化玻璃疊層
|
US9944554B2
(en)
|
2011-09-15 |
2018-04-17 |
Apple Inc. |
Perforated mother sheet for partial edge chemical strengthening and method therefor
|
KR102004007B1
(ko)
*
|
2011-09-29 |
2019-07-25 |
샌트랄 글래스 컴퍼니 리미티드 |
화학 강화 유리 및 그 제조 방법
|
WO2013047676A1
(ja)
*
|
2011-09-29 |
2013-04-04 |
セントラル硝子株式会社 |
表示装置用カバーガラス及びその製造方法
|
US9516149B2
(en)
|
2011-09-29 |
2016-12-06 |
Apple Inc. |
Multi-layer transparent structures for electronic device housings
|
US10144669B2
(en)
|
2011-11-21 |
2018-12-04 |
Apple Inc. |
Self-optimizing chemical strengthening bath for glass
|
US10133156B2
(en)
|
2012-01-10 |
2018-11-20 |
Apple Inc. |
Fused opaque and clear glass for camera or display window
|
US8684613B2
(en)
|
2012-01-10 |
2014-04-01 |
Apple Inc. |
Integrated camera window
|
US8773848B2
(en)
|
2012-01-25 |
2014-07-08 |
Apple Inc. |
Fused glass device housings
|
WO2013116420A1
(en)
|
2012-02-01 |
2013-08-08 |
Corning Incorporated |
Method of producing constancy of compressive stress in glass in an ion-exchange process
|
US9359251B2
(en)
*
|
2012-02-29 |
2016-06-07 |
Corning Incorporated |
Ion exchanged glasses via non-error function compressive stress profiles
|
CN104379532B9
(zh)
|
2012-02-29 |
2021-08-24 |
康宁股份有限公司 |
可离子交换的低cte玻璃组合物以及包含该玻璃组合物的玻璃制品
|
US9946302B2
(en)
|
2012-09-19 |
2018-04-17 |
Apple Inc. |
Exposed glass article with inner recessed area for portable electronic device housing
|
US20140087193A1
(en)
*
|
2012-09-26 |
2014-03-27 |
Jeffrey Scott Cites |
Methods for producing ion exchanged glass and resulting apparatus
|
US9045364B2
(en)
|
2012-11-30 |
2015-06-02 |
Owens-Brockway Glass Container Inc |
Surface treatment process for glass containers
|
JP2014133683A
(ja)
*
|
2013-01-10 |
2014-07-24 |
Central Glass Co Ltd |
化学強化ガラス板の製造方法
|
EP2953910A1
(en)
|
2013-02-11 |
2015-12-16 |
Corning Incorporated |
Antimicrobial glass articles and methods of making and using same
|
US20140345325A1
(en)
*
|
2013-05-24 |
2014-11-27 |
Corning Incorporated |
Double ion exchange process
|
US20140356605A1
(en)
*
|
2013-05-31 |
2014-12-04 |
Corning Incorporated |
Antimicrobial Articles and Methods of Making and Using Same
|
US9512035B2
(en)
|
2013-06-17 |
2016-12-06 |
Corning Incorporated |
Antimicrobial glass articles with improved strength and methods of making and using same
|
US9459661B2
(en)
|
2013-06-19 |
2016-10-04 |
Apple Inc. |
Camouflaged openings in electronic device housings
|
US11079309B2
(en)
*
|
2013-07-26 |
2021-08-03 |
Corning Incorporated |
Strengthened glass articles having improved survivability
|
US10442730B2
(en)
*
|
2013-11-25 |
2019-10-15 |
Corning Incorporated |
Method for achieving a stress profile in a glass
|
US10118858B2
(en)
|
2014-02-24 |
2018-11-06 |
Corning Incorporated |
Strengthened glass with deep depth of compression
|
US9886062B2
(en)
|
2014-02-28 |
2018-02-06 |
Apple Inc. |
Exposed glass article with enhanced stiffness for portable electronic device housing
|
US20150274585A1
(en)
*
|
2014-03-26 |
2015-10-01 |
Apple Inc. |
Asymmetric chemical strengthening
|
TWI705889B
(zh)
|
2014-06-19 |
2020-10-01 |
美商康寧公司 |
無易碎應力分布曲線的玻璃
|
CN108609866B
(zh)
*
|
2014-07-25 |
2021-12-07 |
康宁股份有限公司 |
具有深的压缩深度的强化玻璃
|
CN107001096A
(zh)
|
2014-10-07 |
2017-08-01 |
康宁股份有限公司 |
具有确定的应力分布的玻璃制品及其生产方法
|
US10730791B2
(en)
|
2014-10-08 |
2020-08-04 |
Corning Incorporated |
Glasses and glass ceramics including a metal oxide concentration gradient
|
CN104402238A
(zh)
*
|
2014-10-27 |
2015-03-11 |
苏州安洁科技股份有限公司 |
一种超薄玻璃保护膜的加工方法
|
US10150698B2
(en)
|
2014-10-31 |
2018-12-11 |
Corning Incorporated |
Strengthened glass with ultra deep depth of compression
|
CN115536270A
(zh)
*
|
2014-11-04 |
2022-12-30 |
康宁股份有限公司 |
深层非易碎应力曲线及其制造方法
|
US20160193812A1
(en)
*
|
2015-01-06 |
2016-07-07 |
Corning Incorporated |
Method for reducing bow in laminate structure
|
EP3157880B1
(en)
*
|
2015-05-28 |
2020-11-18 |
Corning Incorporated |
Strengthened glass with deep depth of compression
|
CN106348621B
(zh)
*
|
2015-07-17 |
2019-03-01 |
蓝思科技股份有限公司 |
一种强化玻璃的强化方法
|
US9701569B2
(en)
|
2015-07-21 |
2017-07-11 |
Corning Incorporated |
Glass articles exhibiting improved fracture performance
|
US11613103B2
(en)
|
2015-07-21 |
2023-03-28 |
Corning Incorporated |
Glass articles exhibiting improved fracture performance
|
WO2017066243A1
(en)
*
|
2015-10-14 |
2017-04-20 |
Corning Incorporated |
Laminated glass article with determined stress profile and method for forming the same
|
US10611681B2
(en)
|
2015-12-08 |
2020-04-07 |
Corning Incorporated |
S-shaped stress profiles and methods of making
|
KR20240019400A
(ko)
|
2015-12-11 |
2024-02-14 |
코닝 인코포레이티드 |
금속 산화물 농도 구배를 포함하는 융합-형성가능한 유리계 제품
|
WO2017177114A1
(en)
|
2016-04-08 |
2017-10-12 |
Corning Incorporated |
Glass-based articles including a metal oxide concentration gradient
|
US10410883B2
(en)
|
2016-06-01 |
2019-09-10 |
Corning Incorporated |
Articles and methods of forming vias in substrates
|
US11059744B2
(en)
|
2016-06-14 |
2021-07-13 |
Corning Incorporated |
Glasses having improved drop performance
|
US10134657B2
(en)
|
2016-06-29 |
2018-11-20 |
Corning Incorporated |
Inorganic wafer having through-holes attached to semiconductor wafer
|
US10794679B2
(en)
|
2016-06-29 |
2020-10-06 |
Corning Incorporated |
Method and system for measuring geometric parameters of through holes
|
TW201815710A
(zh)
*
|
2016-08-31 |
2018-05-01 |
美商康寧公司 |
具有經填充之孔洞的經強化玻璃系物件及製造其之方法
|
US11078112B2
(en)
|
2017-05-25 |
2021-08-03 |
Corning Incorporated |
Silica-containing substrates with vias having an axially variable sidewall taper and methods for forming the same
|
US10580725B2
(en)
|
2017-05-25 |
2020-03-03 |
Corning Incorporated |
Articles having vias with geometry attributes and methods for fabricating the same
|
US11554984B2
(en)
|
2018-02-22 |
2023-01-17 |
Corning Incorporated |
Alkali-free borosilicate glasses with low post-HF etch roughness
|
US11152294B2
(en)
|
2018-04-09 |
2021-10-19 |
Corning Incorporated |
Hermetic metallized via with improved reliability
|
KR20210127188A
(ko)
|
2019-02-21 |
2021-10-21 |
코닝 인코포레이티드 |
구리-금속화된 쓰루 홀을 갖는 유리 또는 유리 세라믹 물품 및 이를 제조하기 위한 공정
|
GB2614518A
(en)
*
|
2021-09-22 |
2023-07-12 |
David Curtis Andrew |
Ultra thin polymer coated strengthened glass panel for accepting a thermal dye diffusion image
|