WO2024048318A1 - Procédé de moulage d'élément d'extension - Google Patents

Procédé de moulage d'élément d'extension Download PDF

Info

Publication number
WO2024048318A1
WO2024048318A1 PCT/JP2023/029788 JP2023029788W WO2024048318A1 WO 2024048318 A1 WO2024048318 A1 WO 2024048318A1 JP 2023029788 W JP2023029788 W JP 2023029788W WO 2024048318 A1 WO2024048318 A1 WO 2024048318A1
Authority
WO
WIPO (PCT)
Prior art keywords
weld line
extension member
gate
pier
mold
Prior art date
Application number
PCT/JP2023/029788
Other languages
English (en)
Japanese (ja)
Inventor
賢一 松永
Original Assignee
株式会社小糸製作所
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 株式会社小糸製作所 filed Critical 株式会社小糸製作所
Publication of WO2024048318A1 publication Critical patent/WO2024048318A1/fr

Abstract

La présente invention concerne un procédé de moulage par injection d'un élément d'extension disposé dans une lampe de véhicule, en particulier un procédé de moulage par injection d'un élément d'extension comprenant une partie d'assise de pont. L'invention concerne un procédé de moulage par injection d'un élément d'extension, l'élément d'extension étant disposé dans une lampe de véhicule qui reçoit une pluralité d'unités optiques électroluminescentes, ayant une ouverture formée à l'intérieur, comprenant une partie d'assise de pont divisant l'ouverture en parties multiples, et protégeant au moins certaines des unités optiques de l'extérieur. Une matrice pour mouler l'élément d'extension est pourvue d'au moins une paire de portes dans une position faisant face à une cavité pour former la partie d'assise de pont. Un réglage est effectué pour guider la position d'une ligne de soudure formée sur la partie d'assise de pont vers une zone souhaitée par réglage de différents temps de début d'ouverture de porte pour la paire de portes. De cette manière, le développement d'une ligne de soudure est inhibé.
PCT/JP2023/029788 2022-08-31 2023-08-18 Procédé de moulage d'élément d'extension WO2024048318A1 (fr)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
JP2022137600A JP2024033782A (ja) 2022-08-31 2022-08-31 エクステンション部材の成形方法
JP2022-137600 2022-08-31

Publications (1)

Publication Number Publication Date
WO2024048318A1 true WO2024048318A1 (fr) 2024-03-07

Family

ID=90099621

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/JP2023/029788 WO2024048318A1 (fr) 2022-08-31 2023-08-18 Procédé de moulage d'élément d'extension

Country Status (2)

Country Link
JP (1) JP2024033782A (fr)
WO (1) WO2024048318A1 (fr)

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2014200980A (ja) * 2013-04-03 2014-10-27 三菱エンジニアリングプラスチックス株式会社 射出成形品
CN108943637A (zh) * 2018-08-09 2018-12-07 华域视觉科技(上海)有限公司 一种注塑工艺
JP2021146606A (ja) * 2020-03-19 2021-09-27 株式会社小糸製作所 エクステンション部材

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2014200980A (ja) * 2013-04-03 2014-10-27 三菱エンジニアリングプラスチックス株式会社 射出成形品
CN108943637A (zh) * 2018-08-09 2018-12-07 华域视觉科技(上海)有限公司 一种注塑工艺
JP2021146606A (ja) * 2020-03-19 2021-09-27 株式会社小糸製作所 エクステンション部材

Also Published As

Publication number Publication date
JP2024033782A (ja) 2024-03-13

Similar Documents

Publication Publication Date Title
JP3886672B2 (ja) 車両用前照灯
KR100211202B1 (ko) 차량램프와 그 제조장치 및 제조방법
US20100321949A1 (en) Vehicle Light
CN108571702B (zh) 机动车前照灯光模块
WO2024048318A1 (fr) Procédé de moulage d'élément d'extension
JP5238213B2 (ja) 車両用灯具の前面カバー
US10875227B2 (en) Resin molded product and molding device
WO2016208355A1 (fr) Article moulé en résine et procédé de fabrication d'un article moulé en résine
DE10231162A1 (de) Fahrzeugleuchte mit Angabezeichen
JP2013206835A (ja) 車両用灯具の製造方法
JP6776000B2 (ja) 二色成形品および二色成形品の製造方法
JP2021146606A (ja) エクステンション部材
DE102014108772B4 (de) Scheinwerfer für fahrzeuge
WO2023008563A1 (fr) Élément de couverture de feu
JPH07296609A (ja) 車両用灯具とその製造装置及び製造方法
JP2021041560A (ja) 車両用灯具カバー
JPH10247403A (ja) 車輌用灯具
KR101608640B1 (ko) 차량용 램프
JP4229085B2 (ja) 車両用前照灯
JPH06254915A (ja) スピーカグリル一体成形法
JP6602296B2 (ja) 金型
JP3859215B2 (ja) 車両灯具用樹脂部品の親子取り成形方法および成形装置
JP2018018806A (ja) 車両用灯具
JP7399715B2 (ja) 射出成形品
JP7366469B1 (ja) レンズ及びその製造方法

Legal Events

Date Code Title Description
121 Ep: the epo has been informed by wipo that ep was designated in this application

Ref document number: 23860081

Country of ref document: EP

Kind code of ref document: A1