WO2009054082A1 - 半凝固金属製品の成形金型構造および半凝固金属製品の成形方法ならびにそれらにより成形される半凝固金属製品 - Google Patents
半凝固金属製品の成形金型構造および半凝固金属製品の成形方法ならびにそれらにより成形される半凝固金属製品 Download PDFInfo
- Publication number
- WO2009054082A1 WO2009054082A1 PCT/JP2008/000481 JP2008000481W WO2009054082A1 WO 2009054082 A1 WO2009054082 A1 WO 2009054082A1 JP 2008000481 W JP2008000481 W JP 2008000481W WO 2009054082 A1 WO2009054082 A1 WO 2009054082A1
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- semi
- solidified metal
- molding
- metal product
- die
- Prior art date
Abstract
半凝固金属の成形性を良好に保持し、同時に材料、製作コストの低減、仕上げ作業の簡易化を達成させることのできる半凝固金属製品の成形金型構造および半凝固金属製品の成形方法ならびにそれらにより成形される半凝固金属製品を提供する。 下型と上型との型閉め状態で形成されるキャビティ内に半凝固金属を充填させた状態で同下型と上型の加圧相対移動により半凝固金属を圧縮させて成形させる半凝固金属製品の成形金型構造である。その上型であって成形後の製品の窓部に対応する平面位置であり型閉め途中でキャビティ部に連通する半凝固金属の逃げ用空隙を設ける。加圧時に窓部対応金属は上型の逃げ用空隙内に入ることで、加圧力の低減、成形機の小型化、仕上げ処理の簡素化を図る。
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2007279721A JP4378732B2 (ja) | 2007-10-27 | 2007-10-27 | 半凝固金属製品の成形金型構造および半凝固金属製品の成形方法 |
JP2007-279721 | 2007-10-27 |
Publications (1)
Publication Number | Publication Date |
---|---|
WO2009054082A1 true WO2009054082A1 (ja) | 2009-04-30 |
Family
ID=40579192
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
PCT/JP2008/000481 WO2009054082A1 (ja) | 2007-10-27 | 2008-03-07 | 半凝固金属製品の成形金型構造および半凝固金属製品の成形方法ならびにそれらにより成形される半凝固金属製品 |
Country Status (2)
Country | Link |
---|---|
JP (1) | JP4378732B2 (ja) |
WO (1) | WO2009054082A1 (ja) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN114472858A (zh) * | 2022-01-12 | 2022-05-13 | 松阳县链条配件有限公司 | 一种高性能链板集成自动冲压成型工艺及其加工设备 |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP6344805B2 (ja) * | 2016-07-26 | 2018-06-20 | アイダエンジニアリング株式会社 | 半凝固金属材料のプレス成形方法 |
Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH06277817A (ja) * | 1993-03-29 | 1994-10-04 | Topy Ind Ltd | 低圧鋳造装置 |
JP2656510B2 (ja) * | 1987-11-24 | 1997-09-24 | トピー工業株式会社 | 溶湯鍛造法 |
JP3418027B2 (ja) * | 1995-01-18 | 2003-06-16 | 株式会社ユーモールド | 溶湯鍛造装置 |
-
2007
- 2007-10-27 JP JP2007279721A patent/JP4378732B2/ja active Active
-
2008
- 2008-03-07 WO PCT/JP2008/000481 patent/WO2009054082A1/ja active Application Filing
Patent Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2656510B2 (ja) * | 1987-11-24 | 1997-09-24 | トピー工業株式会社 | 溶湯鍛造法 |
JPH06277817A (ja) * | 1993-03-29 | 1994-10-04 | Topy Ind Ltd | 低圧鋳造装置 |
JP3418027B2 (ja) * | 1995-01-18 | 2003-06-16 | 株式会社ユーモールド | 溶湯鍛造装置 |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN114472858A (zh) * | 2022-01-12 | 2022-05-13 | 松阳县链条配件有限公司 | 一种高性能链板集成自动冲压成型工艺及其加工设备 |
CN114472858B (zh) * | 2022-01-12 | 2023-11-24 | 松阳县链条配件有限公司 | 一种高性能链板集成自动冲压成型工艺及其加工设备 |
Also Published As
Publication number | Publication date |
---|---|
JP4378732B2 (ja) | 2009-12-09 |
JP2009106950A (ja) | 2009-05-21 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
EP1938946A4 (en) | COMPRESSION MOLDING METHOD AND DEVICE THEREOF | |
WO2006040627A3 (en) | Compression moulding apparatus and method for forming plastics objects | |
WO2006071113A3 (en) | Method and apparatus for manufacturing products | |
WO2011046311A3 (en) | Foamed resin product and foamed resin molding machine to manufacture the same | |
WO2008139868A1 (ja) | 射出成形用金型 | |
WO2010007142A3 (de) | Giessvorrichtung und giessverfahren zur herstellung hohler gegenstände mit einem beim giessvorgang gebildeten projektil | |
WO2009054082A1 (ja) | 半凝固金属製品の成形金型構造および半凝固金属製品の成形方法ならびにそれらにより成形される半凝固金属製品 | |
WO2007017418A3 (en) | Apparatuses for forming objects with undercut portions | |
CN204076698U (zh) | 一种注塑模具侧滑块抽芯结构 | |
CN207057452U (zh) | 一种零件成型模具 | |
CN106001495A (zh) | 镁合金手机壳及其铸造技术 | |
CN205326174U (zh) | 一种可实现多方向抽芯的机构 | |
WO2005068157A3 (en) | Injection compression mould with venting means | |
CN202894014U (zh) | 一种用于消音片的负角成型模具 | |
CN204220795U (zh) | 模具自动卸料结构 | |
CN204222043U (zh) | 模具自动脱料结构 | |
CN203357816U (zh) | 带有摆动旋转机构的模具 | |
CN207256767U (zh) | 汽车门板上装饰板模具先行侧抽锁模机构 | |
CN207072104U (zh) | 一种新型控制合模顺序的机构 | |
CN202143932U (zh) | 铸造模芯盒活块机构 | |
CN206122495U (zh) | 四面滑块成型式铝合金精密模具 | |
CN203567057U (zh) | 注塑模具斜顶纵向斜滑脱模机构 | |
CN205439118U (zh) | 一种便于抽芯的剃须刀外壳注塑模 | |
CN203031821U (zh) | 一种冰箱除臭器盒成型塑胶模 | |
CN201900697U (zh) | 一种用于模具的抽芯结构 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
121 | Ep: the epo has been informed by wipo that ep was designated in this application |
Ref document number: 08720367 Country of ref document: EP Kind code of ref document: A1 |
|
NENP | Non-entry into the national phase |
Ref country code: DE |
|
122 | Ep: pct application non-entry in european phase |
Ref document number: 08720367 Country of ref document: EP Kind code of ref document: A1 |