UA82557C2 - Method for repair of defect section of operating pipeline - Google Patents

Method for repair of defect section of operating pipeline Download PDF

Info

Publication number
UA82557C2
UA82557C2 UAA200603894A UAA200603894A UA82557C2 UA 82557 C2 UA82557 C2 UA 82557C2 UA A200603894 A UAA200603894 A UA A200603894A UA A200603894 A UAA200603894 A UA A200603894A UA 82557 C2 UA82557 C2 UA 82557C2
Authority
UA
Ukraine
Prior art keywords
coupling
pipeline
adhesive
differs
substance
Prior art date
Application number
UAA200603894A
Other languages
Russian (ru)
Ukrainian (uk)
Inventor
Виктор Степанович Бут
Владимир Михайлович Василюк
Сергей Юрьевич Максимов
Александр Петрович Подолян
Сергей Владимирович Пудрый
Николай Дмитриевич Пукас
Александр Николаевич Тарасов
Юрий Григорьевич Федоренко
Original Assignee
Открытое Акционерное Общество «Укртранснефть»
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Открытое Акционерное Общество «Укртранснефть» filed Critical Открытое Акционерное Общество «Укртранснефть»
Priority to UAA200603894A priority Critical patent/UA82557C2/en
Publication of UA82557C2 publication Critical patent/UA82557C2/en

Abstract

Centering elements are mounted on pipeline, on those reinforcement couple is installed. Inner surface of the couple is processed with substance that excludes adhesion of glue solution to it. Ends of the couple are sealed with elastic material and under-couple space is filled with glue substance. In the couple one arranges opening in which tap is fixed, this is connected to tank filled with liquid under pressure. The technical result is in absence of stratification of glue compound at operation.

Description

Опис винаходуDescription of the invention

Винахід відноситься до техніки ремонту трубопровідного транспорту, переважно магістральних 2 нафтопроводів.The invention relates to the technique of repairing pipeline transport, mainly main 2 oil pipelines.

При тривалій експлуатації трубопроводів, на їхніх лінійних ділянках у результаті процесів корозії, механічних і хімічних впливів, з'являються численні дефекти (раковини, вм'ятини, каверни, тріщини, свищі, спучування, розшарування металу труби, гофр і т.д.). У ряді випадків дефекти є неприпустимими для безпечної експлуатації трубопроводу. 70 Широко відомий спосіб ремонту газопроводів шляхом установки на аварійній ділянці труби технологічної котушки |див., наприклад. Правила производства капитального ремонта линейной части магистральньх газопроводов. ВСН 2-112-79. - Москва: ВНИ-ИСТ, 1973, стр. 34-35). Спосіб зводиться до наступного. Аварійну ділянку трубопроводу локалізують і з неї відкачують газ. Після цього частину труби, що містить дефект, вирізають і на її місце вварюють технологічну котушку. Спосіб є радикальним, власне кажучи таким, що повторює 12 монтаж трубопроводу. Разом з тим, він має істотні недоліки, пов'язані із трудомісткістю, неминучістю великих фінансових витрат, обумовлених необхідністю стравлювання газу й вимушеним простоєм трубопроводу.During long-term operation of pipelines, numerous defects appear on their linear sections as a result of corrosion processes, mechanical and chemical influences (sinks, dents, caverns, cracks, fistulas, swelling, delamination of pipe metal, corrugations, etc.) . In some cases, defects are unacceptable for the safe operation of the pipeline. 70 A widely known method of repairing gas pipelines by installing a technological coil pipe in the emergency area | see, for example. Rules for capital repair of the linear part of main gas pipelines. VSN 2-112-79. - Moscow: VNY-IST, 1973, pp. 34-35). The method boils down to the following. The emergency section of the pipeline is localized and gas is pumped out of it. After that, the part of the pipe containing the defect is cut out and a technological coil is welded in its place. The method is radical, as it were, repeating 12 pipeline installation. At the same time, it has significant disadvantages related to labor-intensiveness, the inevitability of large financial costs due to the necessity of gas extraction and the forced downtime of the pipeline.

Відомий спосіб ремонту ділянок газопроводу шляхом приварки в місцях дефектів латок дуговим методом або вибухом |див., наприклад. Нові методи ремонту лінійної частини магістральних газопроводів. - Москва: ВНИЙСТ, 1981, стор. 33-34). Спосіб має обмежене застосування. Для його реалізації необхідне скидання тиску в газопроводі з його наступною продувкою.A known method of repairing sections of a gas pipeline by welding patches in places of defects using the arc method or explosion | see, for example. New methods of repairing the linear part of main gas pipelines. - Moscow: VNYST, 1981, p. 33-34). The method has limited application. For its implementation, it is necessary to release the pressure in the gas pipeline with its subsequent purging.

Відомий спосіб ремонту лінійних ділянок трубопроводів шляхом установки ремонтної муфти, заповненою клейовою композицією |див., ЮК Раїепі Арріїсайнйоп, ОВ, 2210134А, Е16 І 55/16). Спосіб може бути використаний без зниження тиску в трубопроводі. Ремонтна конструкція складається із двох напівмуфт. У процесі роботи, напівмуфти механічно з'єднуються одна з одною, створюючи замкнену оболонку навколо ділянки трубопроводу, с що ремонтується. Далі оболонка центрується за допомогою технологічних елементів (болтів), встановлених в ге) отворах корпуса. Після цього простір між трубопроводом і муфтою герметизується з обох кінців за допомогою самозастигаючої композиції (цементу, епоксидної шпаклівки і т.д.). В ізольований проміжок через спеціальні штуцери накачується епоксидна композиція, що забезпечує високу твердість конструкції.A known method of repairing linear sections of pipelines by installing a repair coupling filled with an adhesive composition | see, Yuk Raiepi Arriisainyop, OV, 2210134A, E16 I 55/16). The method can be used without reducing the pressure in the pipeline. The repair structure consists of two half-couplings. In the process of operation, the half-couplings are mechanically connected to each other, creating a closed envelope around the section of the pipeline that is being repaired. Next, the shell is centered with the help of technological elements (bolts) installed in the holes of the housing. After that, the space between the pipeline and the coupling is sealed from both ends using a self-hardening composition (cement, epoxy putty, etc.). An epoxy composition is pumped into the isolated gap through special fittings, which ensures high structural rigidity.

Даний спосіб ремонту практично всіх типів не наскрізних дефектів, набув широкого застосування на лінійних - ділянках трубопроводів, що працюють під великим тиском |див., наприклад. Рекламу Війізп баз р/с Кіріеу Коад, (уThis method of repairing almost all types of non-through defects has become widely used on linear sections of pipelines operating under high pressure | see, for example. Advertising of Viiizp bases r/s Kirieu Koad, (u

Атрегоайе, ЮОегрузпіге, ОЕ 562 ЕЕ). Відремонтовані в такий спосіб ділянки трубопроводу мають, як правило, більш високу міцність, ніж прилягаючі неушкоджені ділянки труби. Не дивлячись на велике поширення, спосіб юю має істотні недоліки, пов'язані з неможливістю введення епоксидного наповнювача під високим тиском. Надалі, сі через зміну геометричних розмірів трубопроводу, що спричинена перепадами тиску продукту, якийAtregoaye, YuOegruzpige, OE 562 EE). Pipeline sections repaired in this way have, as a rule, higher strength than adjacent undamaged pipe sections. Despite its widespread use, the Yuyu method has significant disadvantages associated with the impossibility of introducing epoxy filler under high pressure. Further, due to the change in the geometric dimensions of the pipeline, which is caused by pressure drops of the product, which

Зо перекачується, і температурних деформацій, епоксидний шар може розшаровуватися. Це може привести до со зниження жорсткості й герметичності конструкції. Максимальний тиск заповнення простору під муфтою обмежений міцністю ізолюючих прокладок на торцях.Due to pumping and temperature deformations, the epoxy layer can delaminate. This can lead to a decrease in rigidity and tightness of the structure. The maximum pressure of filling the space under the coupling is limited by the strength of the insulating gaskets on the ends.

Відомий спосіб ремонту локальних ушкоджень трубопроводів |див. патент Росії 2104439, Е161І 55/175). Спосіб « заснований на використанні розрізної муфти, частини якої збирають на ділянці трубопроводу, що ремонтують, й Центрують за допомогою болтів, утворюючи навколо труби замкнену оболонку. Надалі простір під муфтою о, с ізолюють за допомогою еластичної прокладки й фланців, після чого заповнюють під тиском епоксидним з» наповнювачем. Даний спосіб дозволяє здійснити якісний ремонт трубопроводу. Запресування епоксидного наповнювача в простір під муфтою здійснюється при високому тиску. У результаті цього простір гарантовано заповнюється епоксидним наповнювачем. Крім того, стінки муфти піддаються розтягуванню, а трубопроводу - стисканню. Це дозволяє компенсувати зміну геометричних розмірів трубопроводу через перепади тиску й со зменшення обсягу епоксидного прошарку в процесі усадки. Разом з тим, для реалізації способу потрібні ко трудомісткі роботи із центрування муфти, сама конструкція відрізняється складністю через наявність рознімних фланців. Потрібно склеювання ущільнювальних прокладок. о Відомий спосіб ремонту лінійної ділянки трубопроводу |див. патент України Мо 72840, Е16ЇІ 55/175). Спосіб є сл 20 розвитком попереднього, у якому центрування елементів муфти здійснюється за допомогою кільцевого шлангу.A known method of repairing local damage to pipelines | see Russian patent 2104439, E161I 55/175). The method "is based on the use of a split coupling, the parts of which are collected on the part of the pipeline being repaired and centered with the help of bolts, forming a closed shell around the pipe. Further, the space under the coupling o, c is isolated with the help of an elastic gasket and flanges, after which it is filled under pressure with an epoxy c" filler. This method makes it possible to carry out high-quality repair of the pipeline. Epoxy filler is pressed into the space under the coupling under high pressure. As a result, the space is guaranteed to be filled with epoxy filler. In addition, the walls of the coupling are subjected to stretching, and the pipeline - to compression. This makes it possible to compensate for the change in the geometric dimensions of the pipeline due to pressure drops and the decrease in the volume of the epoxy layer during the shrinkage process. However, the implementation of the method requires time-consuming work on centering the coupling, the design itself is complicated due to the presence of removable flanges. It is necessary to glue sealing gaskets. o A known method of repairing a linear section of a pipeline | see patent of Ukraine No. 72840, E16II 55/175). The method is a step 20 development of the previous one, in which the coupling elements are centered using a ring hose.

Спосіб відрізняється складністю через необхідність установки фланців. "і Відомий спосіб ремонту дефектної ділянки трубопроводу шляхом установки муфти |див. патент Росії 2222746, 161 55/175), який є прототипом винаходу, що заявляється. Спосіб може бути використаний без зниження тиску в трубопроводі. Із двох сторін ділянки, що ремонтується, встановлюють елементи, які центрують, 29 що представляють собою дріт, намотаний на трубопровід. Далі виготовляють частини розрізної муфти, довжина о якої перевищує довжину дефектної ділянки. Частини муфти притискають до елементів, що центрують, і скріпляють між собою. Після цього торці муфти герметизують, у результаті чого одержують замкнену оболонку ко навколо ділянки трубопроводу, що ремонтується. В ізольований проміжок через спеціальні штуцери закачується клейовий компаунд, що забезпечує високу твердість конструкції. Спосіб дозволяє здійснити ремонт дефектної 60 ділянки діючого трубопроводу. Для одержання максимального ефекту, потрібно скидання тиску на час роботи, що в більшості випадків практичного застосування трубопроводів є небажаним. При виконанні робіт під тиском, зміни геометричних розмірів трубопроводу виявляються некомпенсованими через неможливість створення тиску введеного в підмуфтовий простір клейового компаунда. Надалі, через зміну геометричних розмірів трубопроводу, що спричиненні перепадами тиску продукту, який перекачується, і температурних деформацій бо затверділа клейова речовина може розшаруватися. Це може привести до зниження жорсткості й герметичності конструкції.The method is complicated due to the need to install flanges. "and a known method of repairing a defective section of a pipeline by installing a coupling (see Russian patent 2222746, 161 55/175), which is a prototype of the claimed invention. The method can be used without reducing the pressure in the pipeline. From both sides of the section being repaired, centering elements 29 are installed, which are a wire wound on a pipeline. Next, parts of the split coupling are made, the length of which exceeds the length of the defective section. The parts of the coupling are pressed against the centering elements and fastened together. After that, the ends of the coupling are sealed, as a result, a closed shell is obtained around the section of the pipeline being repaired. An adhesive compound is pumped into the isolated gap through special fittings, which ensures high structure hardness. The method allows for the repair of a defective 60 section of an operating pipeline. To obtain the maximum effect, a temporary pressure release is required work, which in most cases of practical application of ash pipelines is undesirable. When performing work under pressure, changes in the geometric dimensions of the pipeline are uncompensated due to the impossibility of creating pressure of the adhesive compound introduced into the sub-coupling space. In the future, due to a change in the geometric dimensions of the pipeline, caused by pressure drops of the product being pumped, and temperature deformations, the hardened adhesive substance may delaminate. This can lead to a decrease in rigidity and tightness of the structure.

В основу винаходу покладене завдання підвищення якості ремонту дефектної ділянки діючого трубопроводу за рахунок попередньої обробки внутрішньої поверхні посилюючої муфти речовиною, що виключає адгезію до неї клейового компаунда, з наступною герметизацією торців муфти за допомогою еластичного матеріалу. Це дозволить виключити розшаровування клейової речовини при зміні геометричних розмірів трубопроводу, що ремонтується, з одночасним виключенням провисання муфти.The basis of the invention is the task of improving the quality of repair of a defective section of an operating pipeline due to the preliminary treatment of the inner surface of the reinforcing coupling with a substance that eliminates the adhesion of the adhesive compound to it, followed by sealing of the ends of the coupling with the help of an elastic material. This will make it possible to exclude the delamination of the adhesive substance when changing the geometric dimensions of the pipeline being repaired, while simultaneously excluding the sagging of the coupling.

Завдання, покладене в основу винаходу, вирішується за рахунок того, що в способі ремонту дефектних ділянок діючих трубопроводів, який складається з установки на дефектну ділянку трубопроводу частин розрізної 7/0 посилюючої муфти, скріплення її частин, центрування муфти щодо поверхні трубопроводу за допомогою елементів, що центрують, герметизації її торців, заповнення підмуфтового простору клейовою речовиною, поданою під тиском через спеціальні штуцери, відповідно до винаходу, після скріплення частин посилюючої муфти на трубопроводі, внутрішню частину муфти обробляють речовиною, що виключає адгезію до муфти клейового компаунда, а торці муфти герметизують за допомогою еластичного матеріалу.The task, which is the basis of the invention, is solved by the fact that in the method of repairing defective sections of operating pipelines, which consists of installing parts of a split 7/0 reinforcing coupling on a defective section of the pipeline, fastening its parts, centering the coupling relative to the surface of the pipeline with the help of elements, centering, sealing its ends, filling the sub-coupling space with an adhesive substance supplied under pressure through special fittings, according to the invention, after gluing the parts of the reinforcing coupling to the pipeline, the inner part of the coupling is treated with a substance that eliminates the adhesion of the adhesive compound to the coupling, and the ends of the coupling are sealed with the help of elastic material.

Спосіб здійснюють таким чином. На трубопроводі встановлюють елементи, що центрують. У найпростішому випадку в якості центруючих елементів можуть бути використані кільця, встановлені із двох сторін дефектної ділянки. Після цього на центруючі елементи встановлюють частини розрізної посилюючої муфти, що містять штуцери. Частини муфти стягують і скріплюють між собою.The method is carried out as follows. Centering elements are installed on the pipeline. In the simplest case, rings installed on both sides of the defective area can be used as centering elements. After that, the parts of the split reinforcing coupling containing the fittings are installed on the centering elements. The parts of the clutch are tightened and fastened together.

Внутрішню поверхню муфти обробляють речовиною, що виключає адгезію до неї клеєвої речовини. В якості 2о речовини можуть бути використані жири, полімери та ін. хімічні сполуки, які створюють додатково й антикорозійну плівку.The inner surface of the coupling is treated with a substance that prevents adhesion of the adhesive to it. Fats, polymers, etc. can be used as 2o substances. chemical compounds that additionally create an anti-corrosion film.

Після цього торці посилюючої муфти герметизують за допомогою еластичного матеріалу. Для герметизації можуть бути використані армовані герметичні камери, попередньо встановлені на трубопровід. Камери розміщують під муфтою, уздовж її торців, після чого камери під тиском заповнюють газом або рідиною. Камери сAfter that, the ends of the reinforcing coupling are sealed with an elastic material. Reinforced hermetic chambers pre-installed on the pipeline can be used for sealing. The chambers are placed under the coupling, along its ends, after which the chambers are filled with gas or liquid under pressure. Cameras of

Можуть заповнюватися еластичним герметиком.Can be filled with an elastic sealant.

Після герметизації торців муфти, підмуфтовий простір через штуцери заповнюють клеєвою речовиною. В (8) якості клеєвої речовини можуть бути використані епоксидні з'єднання, герметики на основі акрилових або алілових мономерів, епоксидно-поліуретанові герметики.After sealing the ends of the coupling, the sub-coupling space is filled with adhesive through the fittings. In (8), epoxy compounds, sealants based on acrylic or allyl monomers, epoxy-polyurethane sealants can be used as an adhesive.

Після затвердіння клеєвої речовини штуцери механічно прибирають, а отвори закривають, наприклад, ча зо Конусними різьбовими заглушками.After the adhesive solidifies, the fittings are mechanically removed, and the holes are closed, for example, with conical threaded plugs.

В окремих випадках, трубопровід може перебувати в агресивному середовищі, проникнення якого в що, підмуфтовий простір є небажаним. У цьому випадку, торцеві ущільнювачі роблять повністю герметичними, а для ю компенсації зміни внутрішнього підмуф-тового обсягу при зменшенні діаметра трубопроводу під час скидання тиску, у муфті роблять отвір, у якому закріплюють кран, з'єднаний з резервуаром, який заповнений під тиском з. рідиною, що має антикорозійні властивості. При установці муфти кран встановлюють у закрите положення, а со відкривають після закінчення процесів затвердіння клеєвої речовини.In some cases, the pipeline may be in an aggressive environment, the penetration of which into the joint space is undesirable. In this case, the end seals are made completely airtight, and in order to compensate for the change in the internal sub-coupling volume when the pipeline diameter decreases during pressure release, a hole is made in the coupling, in which a tap connected to the tank, which is filled under pressure with . liquid with anti-corrosion properties. When installing the coupling, the tap is set in the closed position, and the valve is opened after the hardening of the adhesive is finished.

Пропонований спосіб пояснюється рисунками, приведеними на фіг.1-3.The proposed method is explained by the drawings shown in Fig. 1-3.

Фіг1 пояснює операцію способу установки посилюючої муфти на трубопровід. Де 1 - трубопровід, 2 - елементи, що центрують, З - ущільнювач із еластичного матеріалу, 4 -муфта, 5 - штуцери, 6 - клеєва речовина. «Fig. 1 explains the operation of the method of installing the reinforcing coupling on the pipeline. Where 1 - pipeline, 2 - centering elements, C - seal made of elastic material, 4 - coupling, 5 - fittings, 6 - adhesive. "

Фіг2 пояснює операцію способу установки камер на торцях муфти. Де 1 - трубопровід, 2 - елементи, що з с центрують, 4 - муфта, 5 - штуцери, 6 - клеюча речовина, 7 - ущільнювачі з армованих камер.Fig. 2 explains the operation of the method of installing cameras on the ends of the coupling. Where 1 - pipeline, 2 - elements that center with c, 4 - coupling, 5 - fittings, 6 - adhesive, 7 - seals from reinforced chambers.

Фіг.3 ілюструє роботу муфти при скиданні тиску в трубопроводі. Де 1 - трубопровід, 2 - елементи, що з центрують, 4 - муфта, 5 - штуцери, 6 - речовина, що клеїть, 7 - ущільнювачі з армованих камер; 8 - повітряний прошарок.Fig. 3 illustrates the operation of the coupling during pressure relief in the pipeline. Where 1 - pipeline, 2 - centering elements, 4 - coupling, 5 - fittings, 6 - adhesive substance, 7 - seals from reinforced chambers; 8 - air layer.

Фіг.А4 ілюструє роботу муфти з компенсуючим резервуаром під час скидання тиску в трубопроводі. Де 1 - со трубопровід, 2 - елементи, що центрують, 4 - муфта, 5 - штуцери, 6 - речовина, що клеїть, 7 - ущільнювачі з армованих камер; 9 - проміжок; 10 - резервуар з рідиною. ко У випадку скидання тиску у відремонтованому пропонованим способом трубопроводі, діаметри труби й сл клеєвого шару зменшується, в той час як діаметр муфти залишається незмінним. У зв'язку з низькою адгезією до 5р Внутрішньої поверхні муфти, клейовий шар залишається суцільним, а між ним і муфтою з'являється порожнина, 1 пов'язана з навколишнім середовищем через щілинні зазори в ущільнювачах торців муфти. Відсутність руйнівних «м сил запобігає розшаруванню клейового шару. При підвищенні внутрішнього тиску в трубопроводі, його діаметр і діаметр клейового шару збільшується. При тиску в трубопроводі більшому, ніж тиск, при якому проводився ремонт, окружні напруження відремонтованої труби через клейовий шар будуть передаватися на муфту. Тобто, досягається основна мета ремонту - розвантаження дефектної труби при забезпеченні герметичного ізолювання її поверхні.Fig. A4 illustrates the operation of a coupling with a compensating tank during pressure relief in the pipeline. Where 1 - pipe, 2 - centering elements, 4 - coupling, 5 - fittings, 6 - adhesive substance, 7 - seals from reinforced chambers; 9 - gap; 10 - tank with liquid. ko In the case of pressure relief in the pipeline repaired by the proposed method, the diameters of the pipe and the adhesive layer are reduced, while the diameter of the coupling remains unchanged. Due to the low adhesion to the inner surface of the coupling, the adhesive layer remains continuous, and a cavity appears between it and the coupling, 1 connected to the environment through the slit gaps in the seals of the ends of the coupling. The absence of destructive forces prevents the delamination of the adhesive layer. When the internal pressure in the pipeline increases, its diameter and the diameter of the adhesive layer increase. If the pressure in the pipeline is greater than the pressure at which the repair was carried out, the circumferential stresses of the repaired pipe will be transferred to the coupling through the adhesive layer. That is, the main goal of the repair is achieved - unloading the defective pipe while ensuring hermetic isolation of its surface.

ГФ) При необхідності, поява зовнішнього агресивного середовища в підмуфтовому просторі може бути т виключена шляхом установки повністю герметичних торцевих ущільнювачів. У цьому випадку, при скиданні тиску, зміна підмуфтового простору компенсується за рахунок рідини, що перебуває в резервуарі. Рідина бо заповнює утворену порожнину між клейовим шаром і внутрішньою поверхнею муфти. При збільшенні діаметра трубопроводу, зайва рідина витісняється в резервуар.GF) If necessary, the appearance of an external aggressive environment in the sub-coupling space can be excluded by installing fully hermetic end seals. In this case, when the pressure is released, the change in the sub-coupling space is compensated by the fluid in the tank. The liquid fills the cavity formed between the adhesive layer and the inner surface of the coupling. When the diameter of the pipeline increases, excess liquid is pushed into the tank.

Розроблений спосіб може знайти застосування практично на будь-яких трубопроводах, однак найбільший ефект може бути досягнуто при ремонті діючих магістральних газопроводів, нафтопроводів і продуктопроводів, виготовлених із труб середнього й великого діаметру (більше З0Омм). б5The developed method can be used on almost any pipelines, but the greatest effect can be achieved when repairing existing main gas pipelines, oil pipelines and product pipelines made of pipes of medium and large diameter (more than 30 mm). b5

Claims (4)

Формула винаходуThe formula of the invention 1. Спосіб ремонту дефектних ділянок діючих трубопроводів, що включає встановлення на дефектну ділянку 2 трубопроводу частин розрізної посилюючої муфти, скріплення її частин, центрування муфти відносно поверхні трубопроводу за допомогою центрувальних елементів, герметизацію її торців, заповнення підмуфтового простору клейовим розчином, що подається під тиском через штуцери, який відрізняється тим, що після скріплення частин посилюючої муфти на трубопроводі внутрішню частину муфти обробляють речовиною, яка виключає адгезію до неї клейової речовини, а торці муфти герметизують за допомогою еластичного матеріалу. 70 1. The method of repairing defective sections of operating pipelines, which includes installing parts of a split reinforcing coupling on the defective section 2 of the pipeline, fastening its parts, centering the coupling relative to the surface of the pipeline with the help of centering elements, sealing its ends, filling the space under the coupling with an adhesive solution supplied under pressure through the fittings, which differs in that after gluing the parts of the reinforcing coupling on the pipeline, the inner part of the coupling is treated with a substance that excludes the adhesion of the adhesive substance to it, and the ends of the coupling are sealed with an elastic material. 70 2. Спосіб за п. 1, який відрізняється тим, що в стінці муфти виконують отвір, у якому закріплюють закритий кран, сполучений із резервуаром, заповненим під тиском рідиною, якій притаманні антикорозійні властивості, при цьому кран відкривають після закінчення затвердіння клейового розчину.2. The method according to claim 1, which differs in that a hole is made in the wall of the coupling, in which a closed tap is fixed, connected to a tank filled under pressure with a liquid that has anti-corrosion properties, while the tap is opened after the adhesive solution has hardened. 3. Спосіб за п. 1, який відрізняється тим, що як клейову речовину використовують епоксидно-поліуретановий герметик. 12 3. The method according to claim 1, which differs in that an epoxy-polyurethane sealant is used as an adhesive. 12 4. Спосіб за п. 1, який відрізняється тим, що як еластичні герметизатори використовують армовані камери, наповнені під тиском рідиною, газом або герметиком. с 7 о че Іо) Іо) с Зо со4. The method according to claim 1, which differs in that reinforced chambers filled under pressure with liquid, gas or sealant are used as elastic sealants. s 7 o che Io) Io) s Zo so - . и? со ко 1 1 що ко 60 б5- and? so ko 1 1 what ko 60 b5
UAA200603894A 2006-04-10 2006-04-10 Method for repair of defect section of operating pipeline UA82557C2 (en)